IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1536 documents. Displaying 25 entries per page.


Preliminary evaluation of degradation patterns in wood samples from the Yenikapı shipwrecks
2013 - IRG/WP 13-10798
The uncovering of several shipwrecks during the excavation of the Marmaray Rail Tube Tunnel Project in Istanbul provides an important opportunity to evaluate waterlogged woods buried for centuries. Identification of these woods showed that a variety of species was used in the ships. One shipwreck (a galley) from the Yenikapı Marmaray was examined using electron microscopy. The micrographs rev...
C Köse, A M Taylor


Update on "Sandwich" Type Above Ground Field Test Methods
2013 - IRG/WP 13-20506
Our research group has been investigating a number of new designs for above ground field testing to try to provide rapid methods to compare the relative performance of systems in above ground, unprotected exposures. This paper provides an update on what we have found with three variations on a "sandwich" type above ground test arrangement, with comparison to the more traditional lap-joint method ...
A Zahora, L Jin, A Preston


Characterization of test fields
2013 - IRG/WP 13-20508
Test field characteristics and impact of test fields on wood degradation is important when testing wood protection. The current EN 252 standard has no requirement for knowledge of decay hazards, but most commonly a test field is known as a “brown”,- “white”,- or “soft rot” field. To understand which decay hazard wood preservatives are tested against, each test field should be character...
U Råberg, N Terziev, G Daniel


A critical view on early indicators for above ground field performance of wood
2013 - IRG/WP 13-20509
Above ground field tests are quite often a balancing act between the provision of realistic test conditions, reliable statistics, and acceptable long test durations. Within this study we therefore reviewed 543 data sets from above ground field tests performed at 36 different test sites in 8 countries in Australia and Europe. The main objective was to investigate possible correlations between early...
C Brischke, L Meyer, G Alfredsen, P-O Flæte, L Francis, M Hansson, P Larsson Brelid, J Jermer


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Statistical analysis of durability tests - Part 2: Principles of time-to-failure and application on field test data
2013 - IRG/WP 13-20512
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing is therefore essential, in combination with proper monitoring and analysis tools. A crucial concept is variability and the incorporation of variability in tests and analysis. In this paper we focus on t...
J Van den Bulcke, I De Windt, C Brischke, C R Welzbacher, A O Rapp, J Van Acker


Testing the performance of timber using 27 different field test methods
2013 - IRG/WP 13-20517
Numerous test methods to determine the durability of timber and timber products have been described in relevant literature. However, only some of these methods have been standardized and thus only very few are regularly used for resistance tests in the field. Since results from extensive comparative field studies have shown differences in moisture performance between different test methods, the ai...
L Meyer, C Brischke, J Rieken


Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2013 - IRG/WP 13-20535
A round robin involving 15 European participants was set up in 2006. The round robin consists of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. When comparing EN 84 preconditioning (two weeks water leaching) with natural preconditioning (1 year in field, above ground) according to CEN/TS 15397, no significant difference...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, B Mazela, E Melcher, R Möller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Copper leaching from copper-ethanolamine treated wood during exposure to terrestrial microorganisms
2013 - IRG/WP 13-30621
Copper-ethanolamine based wood preservatives are still the most important solutions for protection of wood in ground applications in Europe. Wood in ground is exposed to variety of organisms, which can act synergistically. In order to simulate these conditions in laboratory, Scots pine (Pinus sylvestris) specimens impregnated with copper-ethanolamine preservative of three different concentrations ...
M Humar, N Thaler, B Lesar


Field performance of wood impregnated with siloxanes using supercritical carbon dioxide
2013 - IRG/WP 13-40632
This paper presents preliminary results from a 13-month field test containing pine sapwood samples (Pinus sylvestris) impregnated with a mixture of siloxane and organic biocides using supercritical carbon dioxide as carrier. Samples were exposed above ground at a Danish field test site using matched non-treated sapwood controls for every treated sample. All samples were painted before exposure. Pi...
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Quantification of copper and chromium in field stakes after different exposure times: Remaining metal content and distribution
2013 - IRG/WP 13-50291
In order to determine the distribution of copper and chromium as well as their remaining concentration EN 252 specimens and thicker pine sapwood stakes (non standard format) were treated with a commercial CC salt in a vacuum pressure process. The stakes were installed in the test field of the Institute of Wood Research, Hamburg, in August 2010. In all cases three stakes were removed after 4, 8, 12...
T Liese, M Bahmani, E Melcher


Incidence of soft rot attack on preservative treated Douglas-fir poles: a preliminary survey
2014 - IRG/WP 14-10818
Occurrence of soft rot decay in Douglas-fir poles treated with ammoniacal copper zinc arsenate (ACZA) or pentachlorophenol in oil was studied. Soft rot was less prevalent in poles treated with penta, but some soft rot was found in approximately 20 % of poles examined. Soft rot was more common in poles treated with ACZA, and, when present, was found in almost 20% of the cells examined. The potenti...
P Torres Andrade, J J Morrell


Identification of soft-rot fungi existed in the samples from the galley excavated at Yenikapi
2014 - IRG/WP 14-10833
The shipwrecks of the Middle Byzantine period were excavated during the construction of the Marmaray railway and metro station in Yenikapı between 2004 and 2012. This has become the largest investigations because of the size and the number of the shipwrecks and its associated artifacts. In the previous report, the electron micrographs of the samples revealed that a wide range in the degree of...
T Wada, C Köse, K Igarashi


Microbial Community Analysis of Naturally Durable Wood in an Above Ground Field Test
2014 - IRG/WP 14-10826
This paper presents preliminary results of an above ground field test wherein eight naturally durable wood species were exposed concurrently at two sites in North America. Surface samples were taken at regular intervals from non-durable controls and compared to their more durable counterparts. Terminal Restriction Fragment Length Polymorphism was performed to characterize the microbial (bacteria, ...
G T Kirker, S V Diehl, P K Lebow


Variability in durability of some selected South-American wood species
2014 - IRG/WP 14-10831
Within the scope of sustainable forest management one wants to encourage the proper use of lesser known wood species. Therefore the market has to shift from a demand-driven towards a supply-driven market without loss of wood quality. It is generally known that the durability from pith to bark varies thus, affecting the overall durability of wood species. Consequently, a detailed analysis is necess...
I De Windt, P ’t Hooft, J Van den Bulcke, J Van Acker


Field trials results of preservative treated ground contact stake conducted in Korea
2014 - IRG/WP 14-30640
The field trials results from Korea preservative treated ground contact stake are reported. There was two site which was in southern area(Anmeon) and east area (Jungsun) of Korea. The CUAZ, CCA and CBHDO preservatives were use in this study. The sapwood of Japanese red pine stake was treated with these preservatives according to Korea standard method and then installed in 2003. Every year the insp...
Dong Won Son, Won Jung Hwang, Hyun-mi Lee, Dong-heub Lee, Sang-bum Park


Three-year field test of preservative-treated Canadian species in Korea
2014 - IRG/WP 14-30646
The purpose of this study was to generate field performance data in Korea on Canadian softwood species preservative-treated to Canadian standards. Two field tests of preservative-treated Canadian softwood species, one in ground contact and one above ground, were installed in Jinju, Korea in November 2010. Western hemlock and white spruce were incised and pressure-treated with alkaline copper quate...
Jieying Wang, Jong Bum Ra, P I Morris


Borate Redistribution in Glulam in an Above Ground Field Test
2014 - IRG/WP 14-30652
Researchers have refocused on the use of boratesin the wood protection industry in the last two decades due to their broad spectrum effectiveness against fungi and insects, and favourable environmental characteristics. This study was designed to determine borate distribution in a limited number of samples from a large field test of composites protected by a combination of coating and borate treatm...
P I Morris, A Temiz, J Ingram


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao


An update on durability of New Zealand grown timber
2015 - IRG/WP 15-10851
Classification and predication of in-service performances of naturally durable timber is much more difficult than preservative treated timber due to the variability of wood properties within and between trees of the same species and the variable nature of the hazard to which the timber will be exposed. A combination of field test and in-service testing has been used to classify the suitability of ...
D Page, T Singh


Building solid foundations to support market growth of preserved wood in the UK – treatment quality, product approval and the largest national field trial of preservative treated wood in 50 years
2015 - IRG/WP 15-30662
The Wood Protection Association (WPA) has just commissioned Britain’s largest ever durability trial of home grown timber, having contracted Building Research Establishment (BRE) to conduct a long term controlled field trial of sawn and pressure treated British Softwood posts at two sites with differing soil conditions. This large scale Field Trial is the last of an innovative and substantial thr...
E Suttie, G Ewbank


Durability of Fence Posts of Four Wood Species After 20 Years in Field Test
2015 - IRG/WP 15-30670
In the past years, wood consumption from native forests has drastically reduced the availability of wood. Fast-growing species such as Pinus and Eucalyptus suitably impregnated with chemicals may show a service life equal or higher than hardwood with high natural durability. The field tests have been an alternative widely used to evaluate the durability of wood and the efficiency of preservatives....
A Florian da Costa, A C Salgado de Freitas, E Meneses Oliveira


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Moisture induced risk and fungal development in various field test set-ups in and above ground
2016 - IRG/WP 16-20577
A high number of studies on the decay performance of wood in outdoor exposure have been conducted in the past. However, no testing methodology for wooden components exposed above ground reflecting the variety of different loads has been established so far. Many test protocols were modified in different ways throughout the years and results were often published in an encoded or incomplete way. This...
L Meyer-Veltrup, C Brischke


Variation in moisture content in field trials according to use class 3.2 conditions
2016 - IRG/WP 16-20580
Different test methods to determine the durability of wood in use class 3 (EN 335:2013) are available. Fungal degradation of wood requires liquid water. Different Standards (EN 335-1:2006; DIN 68 800:2011) specify the risk for decay with moisture content (mc) of above 20%. EN 335 (2013) does not specify moisture content but rather defined limited wetting conditions (use class 3.1) or prolonged wet...
S Bollmus, A Gellerich, H Militz


Previous Page | Next Page