IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1536 documents. Displaying 25 entries per page.


Evaluation of teak sawdayst Tectona grandis L Fil as a potential source to obtain a natural wood preservative in Colombia
2004 - IRG/WP 04-30356
Plantation Teak (Tectona grandis L. Fil) has been tested as a possible source of natural wood preservatives due to the known excellent durability of old-growth teak wood. Field tests (ground proximity termite and above ground simulated decking exposures) were established in Colombia in April 2003 at two different test sites with different climates (Tropical Dry and Rain forest). Teak heartwood ex...
A Castillo, Y Cabrera, A F Preston, R Morris


Micromorphology of decay in Keruing heartwood by the basidiomycetes Phellinus contiguus and Dacrymyces stillatus
2002 - IRG/WP 02-10454
This study aimed to characterise the micromorphology of fungal decay in a wooden handrailing in an above ground exposure at the Thames embankment in London. Keruing heartwood (Dipterocarpus spp.) was determined as the construction timber and the two basidiomycetes Phellinus contiguus and Dacrymyces stillatus identified as main decay organisms. Their decay patterns within Keruing heartwood were...
G Kleist, M Ray, R J Murphy


The evaluation of the effectiveness of wood preservatives by means of IUFRO's method for field tests with wooden stakes
1985 - IRG/WP 3348
Pinus elliottii and Eucalyptus saligna stakes treated with CCA-A, CCA-C, CCB, Cashew Nut Shell Oil and Benzotar solutions were exposed in seven test sites in Sao Paulo State, Brazil. After five years of exposure, between oil-borne preservatives Benzotar show better performance than CNSL (cashew nut shell liquid), and within waterborne preservatives the performance of CCB is not so good as that of ...
G A C Lopez, A M F Oliveira, E S Lepage


European standardization for wood preservation
1991 - IRG/WP 2365
Since the last IRG 21 conference in New-Zealand, there one meeting of the plenary committee and several meetings of working groups. The interprative documents prepared by CCE for expliciting the essential requirements of the CCE Directive on the construction products and specially: mechanical resistance and stability / hygiene, health and environment / safety in use are waited to valid the progra...
Anonymous


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Co-operative research project on L-joint testing. Progress report to March 1986
1986 - IRG/WP 2272
Further sets of data received from CTFT (France) after 18 months exposure, BAM (Germany) after 18 months exposure, STU (Sweden) after 9.5 months exposure and TI (Denmark) after 12 and 17.5 months exposure are presented and discussed in conjunction with data previously reported. The new data are generally in agreement with those presented previously and indicate the major difference between the co-...
J K Carey, A F Bravery


Results on field stake tests against termite – Maximum for 8 years examination at Kumamoto in Japan
2003 - IRG/WP 03-10463
Various preservative treated or modified wood and charcoal painting stakes were tested in field, maximum for eight years in Kumamoto, distributed two main termite species, Coptotermes formosanus and Reticulitermes speratus. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservative treated stakes were observed no signif...
K Suzuki


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Laboratory Evaluation and Field Trial of Chlorothalonil and Copper-based Preservatives and Leaching Performance of Copper in Copper Treated Wood
2002 - IRG/WP 02-30279
Soil block test and field trial of some Chinese plantation wood species pine and poplar treated with chlorothalonil formulations and copper-based preservatives such as ACQ-B and copper citrate (CC) were conducted. The results of soil block test indicated that chlorothalonil formulations and ACQ-B as well as CC are very effective for controlling the 2 fungi species Corious versicolor and Poria plac...
Mingliang Jiang, Ping Wang, Chungen Piao, Zhaobang Li, Quan Lu, Lei Liu


Developments in unsterile soil soft rot testing
1984 - IRG/WP 2210
Two unsterile soil test methods, the soil burial technique and a method using vermiculite burial with soil inoculation, were compared using different soils to determine their effectiveness in evaluation of wood preservatives against soft rot. Isolation of fungi and microscopy of decayed wood indicated that both methods produced accelerated soft rot attack in treated and untreated birch. Vermiculit...
P A McKaig


Collaborative soft rot tests: Tests conducted at Princes Risborough and Delft on soil samples from collaborating laboratories
1972 - IRG/WP 210
The laboratories which took part in the original collaborative soft rot test (Savory and Bravery, Holz u Org 5 (1) 58-90, 1970) sent samples of the soil used in the original test to Princes Risborough. Portions of this material were sent to Dr Hof for soil analyses at TNO and the remainder was employed at Princes Risborough for the conduct of comparative tests of soil virulence when used as a comb...
J G Savory


Performance of Borate-treated lumber in a four-year, above-ground termite field test in Hawaii
2001 - IRG/WP 01-30265
We report the fourth year of field study results from a protected above-ground field test in Hawaii simulating the sill plate (dodai) used in conventional Japanese housing construction. Field tests were established in both Hawaii and Japan to examine the efficacy of disodium octaborate tetrahydrate (DOT, 2% and 3% shell and through) wood treatments. In Hawaii, chromated copper arsenate (CCA, 4 kg/...
J K Grace, R J Oshiro, A Byrne, P I Morris, K Tsunoda


Field fencepost test of several species treated with water-borne preservatives by rural methods
1986 - IRG/WP 3385
Fencepost field results in ground-contact treated by rural methods: immersion-diffusion and sap displacement by evaporation are analyzed. Copper-chrome-arsenic and copper-fluor-chrome preservatives were used in two concentrations. The wooden species studied were: Pinus pinaster, Eucalyptus globulus and Quercus rubra. For each of the test units decay index evolution was analyzed after five years ex...
M V Baonza Merino


Effect of moisture and cellulosic substrate on decay of hardwoods by soft-rot fungi
1982 - IRG/WP 2173
The development by Forintek Canada Corp. of standard test procedures for laboratory preservative evaluations using soft-rot fungi was requested by the American Wood Preservers' Association. In Europe, through cooperative studies in the International Research Group on Wood Preservation, several attempts have been made to produce a standard procedure, but variability in results obtained bet...
A Byrne, R S Smith


Co-operative research project on L-joint testing. Progress report to March 1985
1985 - IRG/WP 2236
It was originally intended that each participant would expose L-joints in the main trial on 1 April 1983 with the first sampling at 8 months (1 December 1983) and the second sampling at 18 months (1 October 1984). In the event, some participants have had to vary this schedule. Results after the first sampling have been received from CTFT (8 months), BAM (12 months) and Sipad-IRC (8 months) and aft...
J K Carey, A F Bravery


Electricity pole treatments - Wedding Bells State Forest. Inspection September 1983
1985 - IRG/WP 3334
A survey to study the extent of soft rot in hardwood poles in N.S.W. was commenced in 1975. The results of the survey, published in 1982, indicated that a number of factors contributed towards soft rot attack on poles in service. A detailed rest on pole treatments and maintenance procedures was established in 1976, at a site in Wedding Bells State Forest near Coffs Harbour. The site selected was k...
R S Johnstone, R H Eldridge


Six-year Report on the Performance of Borate-treated Lumber in an Above-ground Termite Field Test in Hawaii
2004 - IRG/WP 04-30343
We report the fifth and sixth years of field study results from a protected above-ground field test in Hawaii simulating the sill plate (dodai) used in conventional Japanese housing construction. Field tests were established in both Hawaii and Japan to examine the efficacy of disodium octaborate tetrahydrate (DOT, 2% and 3% BAE shell and through) wood treatments. In Hawaii, chromated copper arsen...
J K Grace, A Byrne, P I Morris, K Tsunoda


Collaborative soft rot tests: Statistical treatment of results of soil analyses
1971 - IRG/WP 29
Institutes taking part in the collaborative experiments already reported forwarded samples of the soils employed in the tests to the Forest Products Research Laboratory, England. The soils were then autoclaved sterilised under uniform conditions and sent to the Department of Forest Soils, the Royal College of Forestry, Stockholm, Sweden. The results of the soil analyses are given in Table 1, toget...
A F Bravery


Soft-rot in Tabebuia sp. wood used in water cooling tower: identification and degradation capacity of the fungi
1998 - IRG/WP 98-10253
Tabebuia sp. (ipe), a native Brazilian wood, is considered of high natural resistance to decaying fungi, and has been used in harsh environments, as cooling towers. Fifty-one fungi, belonging to mitosporic fungi group (Fungi Imperfecti), were isolated from deteriorated Tabebuia sp. wood samples, collected from the mist eliminator and packing of a cooling tower in operation for about 23 years. The ...
S Brazolin, M Tomazello, I H Schoenlein-Crusius


Design of a laboratory method for evaluating the effectiveness of soft rot preservatives
1988 - IRG/WP 2312
This purpose of this work was to design a method which makes it possible to evaluate the effectiveness of products which present protect wood against soft rot, using new products·of a different nature, on wood of·Pinus sylvestris L. and Fagus sylvatica L., and which, suitably applied, avoid big economic losses deriving from lack of knowledge of the active principles suitable to present protect w...
M T De Troya, A M Navarrete


Leaching of Boron - more than 3 years of field exposure
1997 - IRG/WP 97-30143
The diffusibility of Boron in wood and thus the ability of its leaching is known since long. Nevertheless quantitative data on this process are only rarely available. To overcome this lack of information field exposure tests were started with beam-segments treated with pure boric acid and poles treated with CCB. In addition some of the beam-segments were surface-treated with a varnish to investiga...
A Peylo, H Willeitner


Soft rot fungi found in copper/chrome/arsenic treated hardwood power transmission poles in Queensland
1978 - IRG/WP 185
In Queensland the effective service life of copper/chrome/arsenic (CCA) treated hardwood telegraph and power transmission poles is being dramatically shortened due to attack by soft rot decay fungi. The Australian Wood Preservation and Pole Industries are funding research into this serious soft rot problem involving C.S.I.R.O. and the University of Queensland. The C.S.I.R.O. is actively engaged wi...
L E Leightley


Soft rot decay in CCA treated eucalypts in Queensland - A comment
1986 - IRG/WP 1301
A survey has been completed concerned with the distribution and severity of groundline soft rot decay in the CCA treated sapwood of eucalypt poles in Queensland. The survey encountered some 1000 poles of which 55% were slightly, 28% moderately and 17% severely decayed. Soft rot decay was more severe in urban than rural locations. Embedment of poles in concrete resulted in severe soft rot. No signi...
L E Leightley


Mould growth at lumber surfaces of pine after kiln and air drying
1994 - IRG/WP 94-40033
Distribution of water soluble substances in green wood and later redistribution during drying is of importance for the colonisation of wood by microorganisms. According to literature the availability of nitrogenous materials is probably a major limiting factor to the microbial colonisation of wood. King et al. (1974) and Oxley et al. (1976) have shown correlation between surface nutrient concentra...
N Terziev, J Bjurman, J B Boutelje


Previous Page | Next Page