Development of microbiological test methods for the wooden packaging of foodstuffs
2010 - IRG/WP 10-20453
Whereas different sampling methods already exist for analysing contaminated surfaces or packaging made of plastic or paper, there is no methodology that enables the sampling and quantification of microorganisms in packaging made of wood. The objective of this study was to compare the most commonly used microbiological methods and to develop a reliable quality control test adapted to wooden packagi...
I Le Bayon, H Callot, M Kutnik, C Denis, A-M Revol-Junelles, J-B Millière, M Giraud, M Gabillé, N Passédat


Synthesis of novelty borate compounds for wood preservatives: Laboratory test of leachability and decay resistance
2010 - IRG/WP 10-30520
A novel series of ammonium tetraphenylborate (ATB) and borate chemical compounds (BBC) were synthesized as wood preservatives. The leaching rates and decay resistance of boron formulations containing ATB and BBC were conducted. The laboratory leaching results showed that boron leaching rate of treated wood by ATB formulations was from 2.1% - 6.7%, while that of BBC formulations from 23.3% -59.0%. ...
Zhiqiang Li, Mingliang Jiang, Xingxia Ma


Comparison of Bifenthrin Formulations for Their Skin and Eye Irritation Potential Using the Pollen Tube Growth Test
2010 - IRG/WP 10-30521
The Pollen Tube Growth Test (PTGT) is an effective screening method for measuring the potential of a chemical formulation to affect living cells. The PTGT has been compared against other types of testing, and it shows a good correlation with, for example, the Draize rabbit eye test and the human skin patch assay. It measures the EC50, which is the effective concentration at which 50% growth is o...
S Millward, P Lobb


Mobility of Copper from MCQ in Shell-Treated Wood Exposed Above Ground
2010 - IRG/WP 10-30534
Most Canadian treated decking in service has been given just a thin shell of preservative treatment but it has still performed very well. This is because copper migrated into checks and prevented germination of basidiospores on the freshly exposed untreated wood. Unlike soluble copper systems, MCQ has its copper primarily in the form of small basic copper carbonate particles. For MCQ to be effecti...
R Stirling, P I Morris


EVIPOL® and EVIPOL®10TK - Lab and field data on the efficacy of cyproconazole and its formulations
2010 - IRG/WP 10-30539
EVIPOL® (= cyproconazole) is one of the triazoles commercially used in wood preservation. Although this active is well established in some geographical regions, little information on its efficacy against decay fungi is published yet. Therefore, threshold values derived from EN113 (after EN73 and EN84) as well as field test data (L-joint and lap-joint) are compiled. The paper focus on water diluta...
H Leithoff


Field trials of wood preservatives in UC3 retention. Part 1. Durability results after 13 years in and above ground
2010 - IRG/WP 10-30548
In 1996 an extensive field trial program was set up in order to obtain more data on wood treated with chromium and arsenic free preservatives in Use Class 3 retention. Apart from durability in and above ground, other features were also assessed, e.g. discoloration by staining fungi, depletion of active ingredients, weathering and corrosion of fasteners in con¬tact with the treated wood. Wood spec...
M Westin, J Jermer, M-L Edlund, P Larsson Brelid, I Johansson


Hydrothermal modification for upgrading the durability properties of soft deciduous wood
2010 - IRG/WP 10-40494
To extend the application potentialities of soft deciduous wood, upgrading the durability properties, hydrothermal modification (HTM) of aspen alder and birch wood was investigated. The treatment was conducted in a multifunctional laboratory device WTT. In the previous cases it has been found that the treatment at 160oC improves the durability insufficiently. The modification at 180oC ensured a hi...
B Andersons, I Andersone, V Biziks, I Irbe, J Chirkova, E Sansonetti, J Grinins, H Militz


TMT–Interlab–Test to establish suitable quality control techniques - Structure and first results
2010 - IRG/WP 10-40503
As a result of growing quality demands from manufacturers and end-consumers of thermally modified timber (TMT) recent scientific research activities are increasingly focussed on modification mechanisms and by this on the development of suitable quality control methods. To deepen the knowledge in modification mechanisms and to obtain a larger variety of scientific data for TMT depending on the trea...
C R Welzbacher


Wood protection by means of electro osmotic pulsing technology (PLEOT)
2010 - IRG/WP 10-40505
Wood protection is mainly based on chemical protection of wood. The disposal of wood preservative treated material causes restrictions in its later use or recirculation into the eco-cycle. A new protective system, electro-osmotic pulsing technology on wood, called PLEOT, is tested in a fungi test and in soil contact. Mass loss and moisture content of Scots pine sapwood samples was calculated after...
A Treu, E Larnøy


Wet and dry adhesion of coatings on modified and unmodified wood: comparison of the pull-off test and the cross-cut test
2010 - IRG/WP 10-40524
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, thermal modification) on coatings adhesion and to compare two methods of assessing the adhesion: the cross-cut test and the pull-off test both tested in dry and wet conditions. The study also investigates the effect of other parameters of the wood substrates on adhesion like the ring...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, V Georges, S Bollmus


Biological resistance of acetylated particleboards exposed to white (Trametes versicolor (and brown (Coniophora puteana) rot fungi
2010 - IRG/WP 10-40534
This research was conducted to investigate the effect of acetylation on bioresistance of particleboard produced from acetylated wood chips of Fagus orientalis exposed to white (Trametes versicolor (and brown (Coniophora puteana) rot fungi. After 12 hours soaking in acetic anhydride, in order to achieve three level of weight gains, 5, 9 and 16%, acetylated particles were heated in an oven at 120 c...
M Ghorbani kokandeh, K Doosthoseini, A N Karimi, B Mohebby, H Asghari


Towards designing eco-friendly buildings with in-built termite protection
2010 - IRG/WP 10-50273
The increase in greenhouse gases, leading to global warming, is considered by a consistent scientific worldview not due to natural variation, but due to the growing concentration of carbon dioxide (CO2), methane (CH4) and other atmospheric pollutants. Global emissions of carbon dioxide from fossil fuel combustion and cement production rose from 22.6 billion tons in 1990 to an estimated 31.2 billio...
J R J French, B M Ahmed Shiday, B Maggiolo, D Maggiolo


Termite Resistance of Different Wood Panels Treated with Bifex® under Laboratory and Field Trials
2011 - IRG/WP 11-10745
The effects of Biflex® on termite resistance of laminated chip Board, MDF (Medium Density Fiber), Ply Wood and Veen Board at 50 ppm were evaluated. Laboratory and field trials resistance tests showed that all woods treated with Biflex were resistant to termites as compared to untreated ones. It was concluded that as chemical loadings increased, termite mortalities increased, and at the same time...
F Manzoor, S A Malik, B M Ahmed Shiday, A Liaquat, N Naz


NHA Choice test: Feeding dilemma for Reticulitermes flavipes (Kollar)
2011 - IRG/WP 11-10746
An AWPA laboratory choice test was performed with Reticulitermes flavipes (Kollar) to determine the role of feeding stimulation or aggregation by N’N napthaloylhydroxylamine (NHA). Pine blocks were vacuum treated with aqueous concentrations of NHA ranging from 250-10,000ppm and exposed to one gram R. flavipes workers in the dual block choice test which included one treated and one untreated ...
F Green III, S N Kartal, P K Lebow, R A Arango


Natural durability of wood tested in different environments in Northern Europe
2011 - IRG/WP 11-10747
Moisture is often recognised as a key factor regarding the long time performance of wooden products, and one of the main challenges for timber products is to predict accurate service life in use class 3 (not covered above ground) and use class 4 (in soil or fresh water contact). A range of durability classification studies have been performed both in field and laboratory. But for several wood spec...
P O Flæte, G Alfredsen, F G Evans


Gene expression analysis of a copper-tolerant brown rot fungus on MCQ-treated wood
2011 - IRG/WP 11-10748
Most brown rot fungi are copper-tolerant, which makes them difficult to control with copper-based wood preservatives like MCQ. To better understand what biological processes are regulated, we used our model species, Antrodia radiculosa, to examine expression of genes on MCQ-treated wood. Our hypothesis was genes that decreased copper bioavailability would be up-regulated early, when wood showed ...
J D Tang, A Perkins, S V Diehl


Decay resistance attributes of teak (Tectona grandis L. f.) wood: comparison of the fungicidal activities of quinones
2011 - IRG/WP 11-10752
The implication of quinones in decay resistance of teak wood is controversial. To better understand the role of individual quinone in this property, we studied the correlations between this latter and the content of 2-(hydroxymethyl)anthraquinone, tectoquinone, anthraquinone-2-carboxylic acid, 1,4-naphthoquinone, lapachol and the new compound 4’,5’-dihydroxy-epiisocatalponol found in teak wood...
F B Niamké, N Amusant, N Lemenager, G Chaix, M-F Thévenon, C Baudassé, S Kati-Coulibaly, A Amissa Adima, I Gossan Ado, C Jay-Allemand


Methods of field data evaluation - time versus reliability
2011 - IRG/WP 11-20466
Field testing of wood and wood-based products is so far the most reliable way to get information on performance with respect to durability and expected service life. However, field trials are extremely time and cost consuming. The main objective of the present study was to investigate possible correlations between early stages of decay, preferably during the first 5 years, and the actual service l...
P Larsson Brelid, C Brischke, A O Rapp, M Hansson, M Westin, J Jermer, A Pilgård


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


The durability of acetylated radiata pine sapwood (Accoya). Results from five years testing
2011 - IRG/WP 11-30560
New Zealand grown radiata pine sapwood was modified using the Accsys PLC acetylation process (Accoya). Following treatment, various test samples were exposed in the Scion Accelerated Field Test facility (Fungus Cellar) and in exterior ground contact field tests. In the Fungus Cellar, performance was compared with that of radiata pine treated with CCA to Hazard Classes H3.2 (0.37% m/m Cu+Cr+As) and...
M Hedley, D Page, J van der Waals, K Nasheri, G Durbin


Standardized Field Trials with Micronized Copper
2011 - IRG/WP 11-30564
In 2008, an extensive review of all available data from standardized tests of micronized copper systems was published and there has been considerable work since then. This paper discusses over 20 field stake trials underway in well-known sites such as Gainesville, FL, Hilo, HI and the Dorman and Saucier sites in MS as well as tests from Australia and New Zealand. In addition, 4 ground proximity ...
C R McIntyre, M H Freeman


Study of the durability of the Maderon® against wood decay fungi and insects
2011 - IRG/WP 11-40548
Many industries produce residues that are not easily degradable. One of these is nut husks which, due to their high level of resistance to biological and environmental degradation, have become an ecological problem. Maderón® is a material invented and patented in Spain employed as an ecological substitute and a modern alternative to certain uses of wood. At present, Maderón® is commercialized ...
M T Troya, F Llinares, P Jiménez, J I Fernández-Golfín, M Conde, R Díaz


Challenges and new developments in testing electro osmotic pulsing technology (PLEOT) by means of conventional laboratory methods
2011 - IRG/WP 11-40555
A new wood protection system, electro-osmotic pulsing technology, called PLEOT, is tested in lab trials using different test setup. The technology is tested on Scots pine sapwood and beech wood samples exposed to brown- and white rot fungi. Mass loss and moisture content is calculated after testing and a chitin analysis are performed on the sample powder. Two different electrodes are used in ord...
A Treu, E Larnøy


Durability of modified wood in UC3 and UC4. Results from lab tests and 5 years testing in 3 fields
2011 - IRG/WP 11-40562
In 2005 an extensive test program including field tests was set up in order to obtain more data on the durability and long term performance of modified wood and semi-durable wood species. One of the main challenges for modified wood is to predict accurate service life time in UC3 (use class 3, above ground) and UC4 (use class 4, in soil or fresh water contact). So far, data from in-service condi...
M Westin, G Alfredsen


Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria). The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...