IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1536 documents. Displaying 25 entries per page.


Evaluation and identification of extractives from Iranian walnut (Juglans regia L.) by GC/MS technique for protection of non-decay resistant species
2008 - IRG/WP 08-10670
The use of walnut extractives is interest as environment friendly wood preservatives in the wood preservation industry. In this study, organic solvents were used to remove extractives from Iranian walnut heartwood samples. The solvent was removed by rotoevaporation, and Identification of chemical compounds in the Walnut extractives was done by using GC/MS technique. The toxicity of various extract...
S K H Hashemi, D Parsapajouh, H Khademi Eslam


Microbial Community Analysis Using Terminal Restriction Fragment Length Polymorphism (T-RFLP) Analysis: Field Study Results
2008 - IRG/WP 08-20377
The effects of chlorothalonil (CTN) and butylated hydroxytoluene (BHT) on the fungal community in southern yellow pine (SYP) were assessed using terminal restriction fragment length polymorphism (T-RFLP) analysis. Field stakes treated with 0.25% and 0.37% ammoniacal copper quat (ACQ-C), 0.1 and 0.25% CTN, and 0.1 and 0.25% CTN combined with 2% BHT were installed with untreated controls in field s...
G T Kirker, S V Diehl, M L Prewitt, W J Diehl


Mechanical strength of wood from the Vasa shipwreck
2008 - IRG/WP 08-20381
Samples from three ancient ship wrecks (Vasa, Elefanten, and Gröne Jägaren) and recent oak samples as reference were examined with regard to mechanical strength using the high-energy multiple impact (HEMI) - test method, which delivers the resistance to impact milling (RIM) of a material. Adoption and optimisation of the test method for the particular sample size of the wooden drilling cores was...
A O Rapp, C Brischke, C R Welzbacher, T Nilsson, C Björdal


Field Liners as physical barriers to prevent wooden utility pole decay in soil: An accelerated field simulation trial
2008 - IRG/WP 08-20384
Field Liners (FL’s), plastic sleeves used to protect in-ground wooden poles from fungal and termite damage, have been tested before as physical barriers to prevent contact between soil and wood and to retain wood preservative treatment. These earlier studies concentrated mostly on creosote preserved poles and early generation FL’s which were cumbersome in their application. The newer generatio...
A R Howgrave-Graham, L J Cookson, T Hale


Field Stake Tests with Copper-based Preservatives
2008 - IRG/WP 08-30459
The performance of field test stakes derived from commercially produced ground contact retention copper quat preservatives based on either soluble copper complexed with ethanolamine, or from a water-based suspension of particulate micronized copper compounds, as well as untreated southern yellow pine controls, is compared at two decay test sites. After less than one year in field test some of t...
A Preston, L Jin, D Nicholas, A Zahora, P Walcheski, K Archer, T Schultz


Above and Below-Ground Copper-Azole and Copper, Chrome Arsenate Depletion from Pinus radiata and Fagus sylvatica at Thirteen New Zealand & Australian Sites
2008 - IRG/WP 08-30460
The objective was to determine the significance of site on preservative depletion from Pinus radiata D. Don and Fagus sylvatica L. 20 x 20 x 500 mm field test stakes treated with a ground contact retention of copper amine plus tebuconazole (CuAz) and copper chrome arsenate (CCA) after approximately 5 years exposure to widely different soil and climate conditions. Site, wood species and their inter...
R Wakeling


Propolis for wood finishing
2008 - IRG/WP 08-30464
Possibilities of use of propolis for finishing of beech, maple and spruce wood were investigated. In the first part of the paper, an overview of propolis composition, properties and applications is given. 33.6 % mixture of propolis with 96 % ethanol was prepared and the ethanol solution of soluble propolis components (29.0 %) was applied to wooden substrates. Thin propolis films were formed on woo...
F Budija, M Humar, B Kricej, M Petric


Performance of wood-based composites in a protected aboveground test in southern Japan
2008 - IRG/WP 08-40391
Five kinds of untreated wood-based composites (medium density fiberboard, hardwood plywood=HP, softwood plywood, particleboard and aspen oriented strand board, hereinafter abbreviated as MDF, HP, SP, PB and OSB, respectively) were exposed to subterranean termites and microbial (decay) attack under protected aboveground conditions in a southern part of Japan (Kagoshima Prefecture) for six years. An...
K Tsunoda


The effect of gamma radiation on selected wood properties
2008 - IRG/WP 08-40394
As an easy, fast, and effective sterilisation method, gamma irradiation changes molecular structures not only in pest’s living cells, but also in wooden cell walls. Radiation-induced depolymerisation causes significant changes in some properties of wood crucial for restoration and for laboratory testing of wood-preservative effectiveness. The influence of gamma radiation concerning total amount ...
R Despot, M Hasan, A O Rapp, C Brischke, C R Welzbacher


The susceptibility of hardwood plywood to white rot
2008 - IRG/WP 08-40397
The subject of the tests was resistance of veneer hardwood plywood to activity of pure culture of white rot fungus Trametes versicolor. The tested plywood was made with the use of the following glues: urea-formaldehyde (UF), melamine-urea-formaldehyde (MUF) or phenol-formaldehyde (FF). 4, 12 and 15 mm thick plywood was tested. External veneer of the plywood was mostly alder and the inner veneer (c...
A Fojutowski, A Kropacz


Cantilever bending test of furfurylated poles
2008 - IRG/WP 08-40424
Ten, 8 m long poles of Scots pine (Pinus sylvestris) were treated with furfuryl alcohol to a WPG of approximately 40 %. A bending test was performed according to the principles in the draft European standard for wooden poles, prEN 14229 - Structural timber - Wood Poles for overhead lines. The bending strength and stiffness (MOE) for the poles tested were compared to an earlier study by the Swedish Wood Preservation Committee. In the latter study untreated, CCA-treated, ammoniacal Cu-PCP treated and creosoted poles were tested in bending. These types of poles were considered not to differ in strength and stiffness. The results of the furfurylated poles fit well with the results from the previous study. The bending strength and MOE values obtained are compared to the upper and lower 95-percentile values of the results from the previous study and all poles treated with furfuryl alcohol fit within this interval.Thus, this study indicates that a treatment with furfuryl alcohol does not result in a decrease of strength or stiffness. Further testing with a larger population of poles is necessary in order to get a statistically reliable result. In addition to further demonstration of the durability, the treatment process must be optimised to ensure full sapwood penetration and measures have to be taken to avoid the serious cracking observed in this trial before furfurylation can be considered for treatment of Pinus sylvestris poles.
R Ziethén, J Jermer, A Clang


Degradation of polychlorinated organic biocides by the wood decaying fungi
2008 - IRG/WP 08-50253
Organochlorine biocides such as lindane, pentachlorophenol sodium salt, and polychlorinated biphenyl 153 have been widely used as wood preservatives. Due to their low degradability by soil bacteria, treated waste wood products pose a serious threat to the environment. Consequently, there is an increased need for development of new strategies for their detoxification. In this work, the bioremediati...
I Vidic, L Zupancic-Kralj, K Sepcic, F Pohleven


Emission Rates of Active Substances from Preserved Wood in Use Class 3
2008 - IRG/WP 08-50256
The evaluation of an active substance or a biocidal product under the Biocidal Products Directive (BPD) requires that an environmental risk assessment is carried out. The risk assessment for wood preservatives includes scenarios for preserved wood (e.g. cladding on a house), in which the predicted environmental concentration (PEC) in soil is calculated, using an emission rate for the active subs...
E F Baines


Field Tests of naturally Durable North American Wood Species
2008 - IRG/WP 08-10675
There has been little field test performance data published on North American naturally durable species in general, and no published data on second growth material in particular. Yellow cedar (Callitropsis nootkatensis), western red cedar (Thuja plicata), eastern white cedar (Thuja occidentalis), and three wood species reputed to be moderately durable were installed in ground-contact (stakes) an...
P E Laks, P I Morris, G M Larkin, J K Ingram


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


Field testing in Colombia: Three years of evaluations and experiences
2008 - IRG/WP 08-20394
Two field test sites have been established in Colombia for the evaluation of fungal and termite resistance of treated wood. The combination of elevated temperature, high and stable humidity and high rainfall at the two test sites accelerates microbial and insect activity (Scheffer, 1971; Thornton et al, 1994; Freitag et al, 1995). Tests established include above ground termite tests, ground contac...
Y Cabrera, A Preston


Utilidad práctica de mini estacas en ensayos de campo
2009 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Performance of dip and pressure treated wood in termite ground proximity exposures in Hilo, HI, and Colombia
2008 - IRG/WP 08-30491
A number of preservative systems were evaluated for their ability to control termite attack when applied as both dip and pressure treatments. With dip treatments, better performance was observed with southern pine than spruce-pine-fir using the same solution strength treatment, probably as a result of the about 50% greater uptake with southern pine and associated deeper preservative penetration. B...
P Walcheski, A Zahora


Field Stake Performance of Parallel Strand Lumber Treated with Waterborne Copper Naphthenate
2008 - IRG/WP 08-40435
Wood and wood products have been considered a premium building material for residential and industrial structures for many centuries. More recently, structural composite lumber (SCL) products have played an increasing role in satisfying the needs of the building industry. However, both wood and wood composites are naturally biodegradable materials which require enhanced durability when used in ce...
G P Merrick, M H Freeman, J A Brient


The involvement of hydroxyl-radical-producing glycoprotein from the white-rot basidiomycete Ceriporiopsis subvermispora in wood decay
2009 - IRG/WP 09-10688
White-rot decay can be divided into two subtypes. One type involves the simultaneous degradation of all wood components through the formation of erosion troughs with a progressive thinning of wood cell walls. This type of decay is consistent with a model in which several polymer-degrading enzymes act on the exposed surfaces of the wood cell walls, producing progressive erosion from the lumen to th...
H Tanaka, Y Inoue, T Morikawa, S Itakura, A Enoki


Serpula lacrymans – calcium, iron, and foundering wooden boats
2009 - IRG/WP 09-10691
Serpula lacrymans is one of the most destructive wood-degrading brown rot fungi in temperate environments. Its virulence has often been linked to its ability to grow over non-woody materials and extract calcium (Ca) or iron (Fe) to promote wood degradation in buildings. This fungus has also been a severe problem in historic wooden warships and in modern wooden vessels, sometimes leading to founder...
J S Schilling, S M Duncan


Natural Durability Variations of Malaysian Timbers from Sarawak after 26 Years Exposure by Stake Test
2009 - IRG/WP 09-10704
An extensive graveyard stake test site was established in 1977 in Sibu, Sarawak, Malaysia, to evaluate the in-ground durability of 132 Sarawak wood species, mainly hardwoods. Test samples were planted at 100 x 50 cm spacing. Authenticated wood specimens from 3 trees of each of 132 species were processed into 20 replicated outer heartwood (or else undifferentiated heartwood) stakes of 19 x 19 x 457...
A H H Wong, Ling Wang Choon


Effects of cold treatment on wood destroying fungi important in cultural heritage
2009 - IRG/WP 09-10706
The dry rot fungus Serpula lacrymans (Wulfen:Fr.) Schroeter is notorious in building environments for its vitality, destructive potential, and the huge costs associated with remediation of damage caused to wood of cultural heritage. Due to the potentially adverse of effects of chemical treatment methods such as have been attempted in the past, more benign physical methods of treatment, e.g. heat t...
M Lüdicke, W Unger, G Binker


Degradation of wood veneers by Fenton’s reagents: effects of low molecular weight phenolic compounds on hydrogen peroxide decay and tensile strength loss
2009 - IRG/WP 09-20400
Pine wood (Pinus sylvestris) veneers strips were incubated in acetate buffer containing hydrogen peroxide and iron to mimic mechanisms of brown rot decay and assess the degradation of cellulose through analysis of the tensile properties of the decayed wood. The tensile properties of thin wood strips treated with Fenton system reagents or precursors were determined and correlated to weight loss as ...
Yanjun Xie, R Well, Zefang Xiao, B Goodell, J Jellison, H Militz, C Mai


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...