IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 760 documents. Displaying 25 entries per page.


Studies of the ray parenchyma cell ends on the radial flow of Sitka spruce (Picea sitchensis)
2000 - IRG/WP 00-40164
It is widely accepted that either ray tracheids or ray parenchyma cells offer the major flow pathways radially for the impregnation of softwood with preservative chemicals. It is now generally recognised that, if radial flow does occur through ray parenchyma cells, the cross-field pits play a dominating role for the liquid movement in the radial direction. In this case, the radial flow of fluid is...
I Usta


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


Addendum to paper for discussion in Working II
1970 - IRG/WP II 5B
In view of the limited time that will be available for discussions in Nancy, this addendum has been prepared. Arising from the previous collaborative work and Mr Bravery’s visit to most of the co-operating Institutes, a scheme of work entailing tests carried out 1) by a technique chosen by individual Institutes; 2) by an agreed standardised technique would appear to be the best approach. A compl...
J G Savory, A F Bravery


Immuno-electron microscopic localization of extracellular metabolites in spruce wood decayed by brown-rot fungus Postia placenta
1990 - IRG/WP 1441
Degradation by Postia placenta in spruce and birch wood was shown to occur not only in the wood cell wall but also in the middle lamellae region. Middle lamellae was often found to be degraded along the centerline so that cells could separate along this line. Extracellular membrane structures were found surrounding the hyphae and this matrix labelled positively with antisera produced to Postia pla...
Y S Kim, B Goodell, J Jellison


Susceptibility of CCA treated North American hardwoods to Chaetomium globosum decay
1998 - IRG/WP 98-10278
Seven species of hardwood, Beech (Fagus grandifolia), Basswood (Tilia americana), Maple (Acer rubrum), Oak (Quercus rubra), Trembling Aspen (Populus tremuloides), White birch (Betula papyrifera) and Yellow poplar (Liriodendron tulipifera) were vacuum or pressure impregnated with CCA, at four retention levels. The CCA was allowed to fix in the wood at 35°C. Red pine (Pinus resinosa) was also inclu...
U Srinivasan, Y T Ung, P A Cooper


Factors affecting decay rates in a fungus cellar II
1986 - IRG/WP 2259
Tests were initiated to investigate the influence of various factors on the decay rate in a "Fungus Cellar". Birch and pine stakes treated with chromated copper arsenate and didecyldimethyl ammronium chloride, as well as untreated control stakes, were incubated in two soils in a Fungus Cellar test and installed at two field sites for comparative purposes. The visual rating vs actual stake weight l...
P A McKaig


Effect of soil type and moisture content on soft rot testin
1986 - IRG/WP 2270
Several soils of different types were tested at a range of moisture contents for their suitability for use in a soil burial soft rot test. Their effectiveness was assessed by weight loss in CCA treated and untreated beech and birch outerwood. A horticultural loam (John Innes No. 2) was the most appropriare soil in terms of amount of weight loss caused, tolerance to changes in soil moisture content...
S M Gray


Incidence of soft rot in creosoted poles
1992 - IRG/WP 92-1554
A further population of creosote-treated poles has been assessed for the occurrence of soft rot, as a continuation of work reported in IRG Document No. IRG/WP/1368. The outer 1 cm of each core was assessed microscopically and graded for the presence of soft rot cavities in the wood cell walls; with further assessments taken at a consecutive 1cm interval for cores showing positive findings. Followi...
D J Dickinson, P W McCormack, B Calver


Extracellular substance from the white rot basidiomycete Irpex lacteus involved in wood degradation
1992 - IRG/WP 92-1571
Cellulases, phenol oxidase, and a substance that both produced and reduced H2O2 were isolated from cultures containing wood or glucose on which the white-rot fungus Irpex lacteus was growing. The rate of wood degradation by the fungus with different amounts of glucose in the medium was measured. More of the substance that produced and reduced H2O2 was found extracellularly in cultures containing w...
H Tanaka, T Hirano, G Fuse, A Enoki


The effectiveness of three tributyltin compounds in beech against soft rot fungi using a soil-bed technique: A preliminary report
1986 - IRG/WP 3390
The effectiveness, towards soft rot fungi, of bis (tributyltin) oxide, tributyltin ethanesulphonate (TBTES) and benzyltributylammonium tributyldichlorostannate in both leached and unleached beech stakes is compared to that of a CCA preservative (Tanalith CT 106), using a soilbed technique. In addition, the effect of test solvent (water or toluene) on the performance of TBTES is evaluated. Total ti...
R Hill, A H Chapman, B Patel, A Samuel, J K Carey


Relationship between degradation of wood, cellulose or lignin-related compounds and production of hydroxyl radical or accumulation of oxalic acid in cultures of brown-rot fungi
1994 - IRG/WP 94-10062
The degradation activities of brown rot fungi against wood, cellulose, and lignin-related compounds were measured in cultures containing glucose or wood as a carbon source. Also the activities of one-electron oxidation and hydroxyl radical production and the amount of oxalic acid present in the cultures were measured. The degradation activities of the fungi against wood, crystalline cellulose and ...
S Itakura, T Hirano, H Tanaka, A Enoki


Lab and field test results for wood treated with polymeric alkylphenol polysulfide
2001 - IRG/WP 01-30268
A new wood preservative based on polymeric alkyphenol polysulfide (PXTS-A) is being evaluated in a series of laboratory and field tests and the results continue to show promise. A modified formulation (PXTS-B), which contains additives to reduce the viscosity, is being evaluated along with the original formulation. Soil block decay tests comparing PXTS-B with CCA-C indicate that PXTS-B is equally ...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


An investigation of the factors influencing the rate of deterioration of timber samples due to microfungi in laboratory tests
1997 - IRG/WP 97-20116
An investigation was performed into the comparative performances of test 1 (vermiculite burial) and test 2 (soil burial) as described in ENV 807. Two test preservatives were used - copper naphthenate and propiconazole. Copper chromate was included as a reference preservative. The wood species used was beech (Fagus sylvatica). Test 1 was performed using both a mixed inoculation of the five stipulat...
I J Herring, D J Dickinson, S M Gray, J K Carey


Durability aspects of (hydro)thermal treated wood
2000 - IRG/WP 00-40160
Samples of several wood species were treated in a two steps process, subsequently hydrothermal and dry heat-treated, by the so-called PLATO-process and analysed for their resistance against fungal attack. Both PLATO-treated and dry heat-treated specimen were prepared and analysed, in order to study the influence of moisture during hydrothermal treatment of wood. The resistance against all of the s...
B F Tjeerdsma, M Stevens, H Militz


Visualising Bacteria in Wood Using Confocal Laser Scanning Microscopy (CLSM)
1998 - IRG/WP 98-10272
A fluorescent phospholipid probe was used in conjunction with confocal laser scanning microscopy (CLSM), to visualise bacteria which inhabit in radiata pine wood and degrade pit membranes. CLSM has the ability to collect fluorescent images through different emission filters at the same time, so it is possible to distinguish gram-positive and gram-negative bacteria in infected wood by counterstaini...
Ying Xiao, A P Singh, R N Wakeling


Micromorphology of decay in Keruing heartwood by the basidiomycetes Phellinus contiguus and Dacrymyces stillatus
2002 - IRG/WP 02-10454
This study aimed to characterise the micromorphology of fungal decay in a wooden handrailing in an above ground exposure at the Thames embankment in London. Keruing heartwood (Dipterocarpus spp.) was determined as the construction timber and the two basidiomycetes Phellinus contiguus and Dacrymyces stillatus identified as main decay organisms. Their decay patterns within Keruing heartwood were...
G Kleist, M Ray, R J Murphy


European standardization for wood preservation
1991 - IRG/WP 2365
Since the last IRG 21 conference in New-Zealand, there one meeting of the plenary committee and several meetings of working groups. The interprative documents prepared by CCE for expliciting the essential requirements of the CCE Directive on the construction products and specially: mechanical resistance and stability / hygiene, health and environment / safety in use are waited to valid the progra...
Anonymous


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


Bacterial degradation of Pinus radiata compression wood
1996 - IRG/WP 96-10153
An inspection of twelve year old, CCA-treated Pinus radiata wood from an industrial cooling tower showed extensive surface decay of wood. Electron microscopic examination of decaying compression wood indicated that compression wood cells were attacked exclusively by bacteria, which were of erosion and tunnelling types. As compared to the normal wood, compression wood appeared to be more resistance...
A P Singh, R N Wakeling


Suitability of cotton strip testing as a screening method for the development of wood preservative formulations
2003 - IRG/WP 03-20270
This paper outlines a simple and rapid test method for screening the efficacy of wood preservative formulations against microbiological attack using cotton strips. The method was evaluated against soft rot and was found to provide reliable information on the protection of lignocellulosic material against microbiological attack. The assessment is based on visual interpretation of decay and on a sim...
H Leithoff, I Stephan, H Härtner


Developments in unsterile soil soft rot testing
1984 - IRG/WP 2210
Two unsterile soil test methods, the soil burial technique and a method using vermiculite burial with soil inoculation, were compared using different soils to determine their effectiveness in evaluation of wood preservatives against soft rot. Isolation of fungi and microscopy of decayed wood indicated that both methods produced accelerated soft rot attack in treated and untreated birch. Vermiculit...
P A McKaig


Collaborative soft rot tests: Tests conducted at Princes Risborough and Delft on soil samples from collaborating laboratories
1972 - IRG/WP 210
The laboratories which took part in the original collaborative soft rot test (Savory and Bravery, Holz u Org 5 (1) 58-90, 1970) sent samples of the soil used in the original test to Princes Risborough. Portions of this material were sent to Dr Hof for soil analyses at TNO and the remainder was employed at Princes Risborough for the conduct of comparative tests of soil virulence when used as a comb...
J G Savory


Extracellular hydrogen peroxide-producing and one-electron oxidation system of brown-rot fungi
1990 - IRG/WP 1445
Wood-component-degrading compounds involved in the initial degradation of the cellulose and lignin in wood were isolated from wood-containing culture of brown-rot fungi, Gloeophyllum trabeum and Tyromyces palustris and partially purified by gel filtration on Sephadex G-25 and DEAE-Sepharose ion-exchange chromatography. The compounds were glycoproteins. The molecular weights of the glycoproteins as...
A Enoki, S Yoshioka, H Tanaka, G Fuse


Previous Page | Next Page