IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 3rd Interim Report
1983 - IRG/WP 4101
This paper updates the results of microbiological examination and marine borer assessment of untreated wood samples (15 x 2 x 2 cm³) and samples treated with 3, 6 and 10% CCA and CCB preservatives. Three reference species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were used at all the test sites in addition to local species chosen by participants in the test....
R A Eaton


A collaborative test to determine the efficacy of poyurethane coatings on wood samples exposed in the marine environment. 1st Interim Report
1988 - IRG/WP 4145
Wood samples coated with elastomeric polyurethane (ca. 50 mils thick) were exposed for up to 2 years in 12 tropical and temperate marine test sites with known teredinid, pholad and/or crustacean infestations. All uncoated control samples were destroyed or partially destroyed. Polyurethane-coated samples were not attacked, the surfaces of the coating were sound and the polyurethane adhered well to ...
R A Eaton


Antagonistic effect of Trichoderma spp. against Serpula lacrymans in the soil treatment test
1991 - IRG/WP 1473
Soil treatment tests for preventing growth of Serpula lacrymans were conducted using Trichoderma spp. as antagonists. Soil specimens tested were Kanuma-soil without organic matter and the horticultural soil which was collected from the test site of the stake test. Perfect efficacy of treatment with Trichoderma spp. was shown when the horticultural soil without sterilization was used as a soil spec...
S Doi, A Yamada


36 years of wood preservative tests in Tanzania
1992 - IRG/WP 92-3731
The performanee of major wood presevatives which are used widely commereially are given. These include creosote, CCA's and 5% Pentachlorophenol dissolved in heavy industrial diesel. Tests are conducted at three ecologically different using pine stakes. Results show that the striking performance of creosote and CCA's is noticeable at above 128 kg/m³ and 16 kg/m³ respectively....
K K Murira, P F Nangawe


Field trials on preserved timber out of ground contact
1978 - IRG/WP 3154
This report describes two different field trials studying the performance of preservative treatments on timber exposed to the weather, but above the ground. Results are presented on the protection afforded against decay, and on the efficiency of water-repellent preservative treatments in controlling the uptake of moisture by the timber. Proposals for a standard field test system are briefly discus...
D F Purslow, N A Williams


A method of predicting the average life of field tests on preservative-treated stakes
1977 - IRG/WP 297
The paper presents an analysis of the results of completed field stake tests on untreated and preserved timber, and develops a method of predicting the average life of incomplete stake tests on wood preservatives from the failures that have occurred so far....
D F Purslow


Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability. Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek


Methods for testing fumigant efficacies against termites
1986 - IRG/WP 1297
Methodologies for testing fumigants against termites are reviewed and factors needed to be taken under consideration for standardization listed. Toxicity should be defined by both direct exposure to the gas and under more practical "barrier" conditions which include test enclosures simulating abiotic surroundings of the termites, i.e. wood, nest material, etc. To observe latent effects, mortality ...
N-Y Su, R H Scheffrahn


Biological control of blue stain on wood with Pseudomonas cepacia 6253. Laboratory and field test
1989 - IRG/WP 1380
Pseudomonas cepacia strain 6253 was tested as a biological control agent on wood samples under laboratory conditions, as well as in the field. In the laboratory this bacterium controlled blue stain on Pinus radiata, but field test were not totally satisfactory. However, after 2 months of field test, the test samples were 1/3 to 1/2 less stained then the control samples....
R Benko


Results of field tests on the natural durability of timber (1932-1975)
1976 - IRG/WP 3105
This paper describes a continuing field stake trial to determine the natural resistance of different species of timber to decay. Data are presented for about 180 timbers, covering over 6000 stakes, and the results are discussed in terms of a natural durability classification....
D W Purslow


Isolation and identification of the fungal flora in treated wood
1976 - IRG/WP 144
J F Levy


Programme Section 2 Test methodology and assessment
1999 - IRG/WP 99-20180
IRG Secretariat


Virulence tests with fungal strains used in EN 113 CEN ring test. Results with Coniophora puteana (Schum.ex Fr.) Karst
1986 - IRG/WP 2249
D Dirol


The variability of preservative distribution in test blocks
1973 - IRG/WP 220
The techniques for the assessment of likely effectiveness of preservative systems have long been the subject of much discussion. The whole field has recently been reviewed by Hilditch and Hamblyn (1971) who described in detail many of the laboratory test procedures used, but who also indicated the deficiencies in many of these techniques. It has long been the view of many associated with the wood ...
F W Brooks, M R Gayles, R W Watson


Occurrence of manganese deposits in test stakes exposed in groung contact situations
1996 - IRG/WP 96-10182
Dark spots and flecks were frequently recognized on the surface and within non-preservative treated hard- and softwood test stakes placed in soil contact. Energy dispersive X-ray microanalysis in conjunction with electron microscopy showed the flecks to be composed primarily of manganese dioxide. Detailed transmission electron microscopy observations indicated intrusion of manganese into the wood ...
G F Daniel, T Nilsson, J Volc


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 9: Report of third inspection (2 years) in Italy
1980 - IRG/WP 461
The wood samples were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitudine 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian sea. The recorded temperature varies between 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 1 year (4/1978) and 2 years (4/1979)....
A Gambetta, E Orlandi


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 7: Second report on the samples in Papua New Guinea
1980 - IRG/WP 459
This report presents the findings to date regarding specimens installed in Papua New Guinea, as part of a world-wide marine trial of certain timbers treated with CCA or CCB preservatives. The details of the trial are set out in document number IRG/WP/414. The report discusses the findings in the context of the conditions prevailing at the trial site and of the properties of the trial timbers. The ...
S M Cragg, C R Levy


Co-operative field experiment. Performance of preservative-treated hardwoods with particular reference to soft rot: Report of condition of specimens installed in Victoria, Australia
1978 - IRG/WP 3118
J Beesley


Questionnaire concerning assessment of test data from laboratory and field tests
1992 - IRG/WP 92-2418
During the WG II session in Harrogate, UK it was announced, that possibly a working-session on the assessment of test data and correlation between laboratory and field tests might be organised during next year's meeting in Orlando. For that pupose a questionnaire was prepared. The valuable comments and input of Prof. Thomas Nilsson from Sweden is hereby greatly acknowledged....
A R Valcke


New conception for shortering the duration of fungitoxic test of wood preservatives. Part 3: Proposal for interlaboratory test on miniaturisation of wood specimens
1994 - IRG/WP 94-20053
In connection with documents IRG/WP 94-20044 and IRG/WP 94-20052 the proposal for interlaboratory test on miniaturization of wood specimens is given....
J Wazny, J J Krajewski


Ekki heartwood - is “Durable”
2002 - IRG/WP 02-10444
Severe decay damages of bridges made of ekki (Lophira alata Banks) wood which is classified as a durable species in the EN 350:2 as already reported at the 31 IRG annual meeting. This paper deals with results of long-term decay tests of ekki heartwood specimens using 3 isolates (Loweporus tephroporus 2 strains and a fungus of other sp. from damaged ekki bridges) and Trametes versicolor as a refere...
S Doi, R Itoh, S Horisawa


Test Methods – Performance Based Requirements
2004 - IRG/WP 04-20297
In this paper is briefly described the present approach to service life prediction as an essential part of the architectural engineering process. The system of testing the durability of wood is described more in detail including laboratory tests as well as field trials. It is concluded that the system has a lot of weaknesses which makes it less well suited for practical building applications. A le...
M-L Edlund, F Englund, J Jermer, T Nilsson, M Westin, K Ödeen


Test methods used for approval of wood preservatives in Indonesia
1994 - IRG/WP 94-20045
Indonesian regulation stipulates that all pesticides, including wood preservatives, must be registered and obtain legal permit from the Minister of Agriculture, c.q. the Pesticide Committee before they are eligible for public use. For that purpose they have to meet safety and efficacy requirements approved by the Pesticide Committee. To meet the efficacy requirements, wood preservatives must be te...
A Martawijaya