IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 310 documents. Displaying 25 entries per page.


Japanese standardized method for evaluating effectiveness of anti-sapstain and anti-mould chemicals
1988 - IRG/WP 2299
Japan Wood Preserving Association established a method for testing effectiveness of chemicals against sapstain and mold fungi on wood in 1979. The method is concerned with a laboratory technique using small timber specimens (20 x 50 x 3 mm³), petri dish and 5 test fungi. Effectiveness of each candidate chemical is evaluated on the basis of the relative resistance to sapstain and mold fungi which ...
K Tsunoda, K Nishimoto


Comparison of three methods of quantitative evaluation of sapstain in rubberwood
2000 - IRG/WP 00-20188
Assessing the extent of fungal stain on wood during laboratory trials is a subjective process and is subjected to considerable variation between individual evaluators and specimen. The purpose of this paper was to explore the potential of three quantitative methods of wood surface measurement of rubberwood specimens degraded by sapstain and mould fungui (Botrydiplodia theobromae, Aureobasidium pul...
A J Ashari, J W Palfreyman, A H H Wong


Accidental mold/termite testing of high density fiberboard (HDF) treated with borates and N’N-naphthaloylhydroxylamine (NHA)
2003 - IRG/WP 03-10462
High density fibreboard (HDF) was made from beech and pine furnish (50:50) and treated with boric acid (0.1-3%), borax (0.1-3%) or N'-N-(1,8-naphthalyl) hydroxylamine (NHA) (0.1-1%) prior to gluing with urea formaldehyde (UF) resin in order to determine resistance to Eastern subterranean termites (Reticulitermes flavipes Kollar), the most economically important termite species in North Am...
S N Kartal, H H Burdsall Jr, F Green III


Development and field trials of Evotek 230, a new antisapstain product
1997 - IRG/WP 97-30140
Laboratory and greenhouse studies, using freshly sawn pine boards, demonstrated that the fungicidal properties of prochloraz and carbendazim were complementary for protection from sapstain and mould under extreme conditions of close stacking and high humidity. Analysis of dip bath solutions before and after dipping 20 boards showed no evidence of any stripping of the active ingredients. Neither fu...
A Adams, J Oudenweyer, J L Lindars


Immuno-scanning electron microscopic localization of extracellular polysaccharidases within the fibrillar sheath of the brown rot fungus Postia placenta
1991 - IRG/WP 1497
Extracellular polysaccharidases of the brown-rot fungus Postia placenta were localized using colloidal gold labeled monoclonal antibodies to the B-1,4-xylanase (32-36kDa) fraction of Postia placenta. Postia placenta was grown from agar onto glass coverslips, immunolabeled with or without prior fixation, and examined by SEM. Enzymes were localized on the hyphal surface and on the clumped fibrillar ...
F Green III, C A Clausen, M J Larsen, T L Highley


Fungus cellar and antisapstain field trial studies of six triazole fungicides
1995 - IRG/WP 95-30077
The efficacy of six triazole fungicides was compared using a fungus cellar soil bed test, a rapid antisapstain laboratory trial and a 36 week antisapstain field trial. After 21 months in the fungus cellar the mean soundness of radiata pine treated with 1.5 kg/m³ of cyproconazole, azaconazole, hexaconazole, tebuconazole, propiconazole and flusilazole in combination with 1.0 kg/m³ didecydimethyl a...
R N Wakeling, J G Van der Waals, R D Narayan, J B Foster, B E Patterson, P N Maynard


Field evaluation of anti-sapstain products
1987 - IRG/WP 3402
Product A based on methylenebisthiocyanate, product B based on methylenebisthiocyanate plus 2-thiocyanomethylthio-benzothiazole, product C based on 2-thiocyanomethilthio-benzothiazole and product D based on didecyl dimethil ammonium chloride plus 3-iodo-2 propynil butyl carbarnate were evaluated on Pinus radiata sawn timber as fungicides for sapstain and mould in the Sawmill Division of the Univer...
M C Rose, A Bedoya


Evaluation of the effectiveness of Tuff Brite C in the control of sapstain in laboratory and field tests
1992 - IRG/WP 92-3718
Since 1990, the anti-sapstain product Tuff Brite C (ASC 66898) has been evaluated internationally in laboratory and field tests, and has been commercially introduced in New Zealand. The product is an aqueous flowable formulation of chlorothalonil and carbendazim. Efficacy tests which have been carried out in New Zealand, Australia, USA, South Africa and Europe are described and summarized. Tuff Br...
T L Woods, C J Klaver


Performance of proprietary formulations of anti-sapstain preservatives on Hevea brasiliensis timbers in laboratory tests
1989 - IRG/WP 3532
A total of 10 proprietary and two experimental formulations were assessed for their effectiveness against sap-stain caused by Botryodiplodia theobromae on Rubberwood (Hevea brasiliensis). Sterilized wood samples 5x20x40 mm³ were dipped in the test chemicals for 60 seconds and then inoculated with 0.5 ml of culture filtrate of Botryodiplodia theobromae for incubation in sterile, damp petri dishes....
L T Hong


Laboratory evaluation of water repellents as antisapstain treatment additives
1986 - IRG/WP 3382
Water repellent formulations consisting of five paraffin wax emulsions, three polyethylene wax emulsions, two polybutadiene resin emulsions, a polyester emulsion, and a ß-pinene polymer emulsion were subjected to water repellency tests on radiata pine sapwood. With one exception, the parafin wax emulsions were more effective water repellents than the alternative formulations and one of the paraff...
D V Plackett, C M Chittenden


Serpula lacrymans the dry rot fungus. Revue on previous papers
1989 - IRG/WP 1393
It is found that the Dry rot fungus Serpula lacrymans grows in houses only because of its need for basic materials to neutralize the oxalic acid production or heavy metals which celate the oxalic acid. The average distance from the mycelium to the basic materials is found in average to be 14.2 cm with a variation from 0-100 cm. In contrast to Serpula lacrymans the Coniophora puteana and the Rigido...
J Bech-Andersen


Screening of fungal strains for wood extractive degradation
1998 - IRG/WP 98-10254
Fungal strains were screened for their ability to degrade apolar extractives in wood from scots pine. The degradation of total wood extractives by 91 different strains was monitored in stationary batch assays incubated for 6 weeks. The results obtained show that the ability of wood-inhabiting fungi to utilize wood extractives varied greatly, even for different isolates of the same species. Fungal ...
J Dorado, M J Martinez-Inigo, T A van Beek, F W Claassen, J B P A Wijnberg, R Sierra-Alvarez


The effect of stilbenes on decay fungi of birch and aspen
2000 - IRG/WP 00-10364
Fourteen species of decay fungi, mainly species growing on birch and aspen, one leaf spot fungus of birch and the pine canker fungus Gremmeniella abietina were used to investigate how the stilbenes resveratrol and pinosylvin influence their relative growth on malt agar. With some species the ability to decay with stilbenes impregnated wood was also studied. The concentration of pinosylvin needed t...
L Syrjälä, K Von Weissenberg, A Pappinen, L Paajanen


Development of bluestain in commercially harvested logs in Britain
1996 - IRG/WP 96-10150
In Britain, mechanised harvesting of conifer forestry crops is now the preferred method of felling where terrain and access allows. However, use of mechanised harvesters can lead to excessive debarking, loosening of the bark and wood splintering with, on average, about a third of the bark removed from the more severely damaged logs. More bark has also been observed to be lost from logs harvested e...
A Uzunovic, J F Webber, D J Dickinson


Biological control of sapwood-inhabiting fungi by living bacterial cells of Streptomyces rimosus as a bioprotectant
1992 - IRG/WP 92-1564
The objective of this study is to evaluate the efficacy of antifungal activity of living bacterial cells for the protection of wood against sapwood-inhabiting fungi. The following sapwood-inhabiting fungi were selected: sapstain --Ceratocystis coerulescens, Ceratocystis minor, Ceratocystis pilifera, and Aureobasidum pullulans; mold fungi --Aspergillus niger, Penicillium spp, and Trichoderma spp. L...
S C Croan, T L Highley


Neem leaves, a potential source for protection of hardwood against wood decaying fungus
2005 - IRG/WP 05-30370
Neem leaves are widely recognized for their insecticidal, pesticidal, fungistatic and fungitoxic ability. The present study is to investigate the efficacy of neem leaves extractives against wood destroying microbes, a brown and a white rot. Neem leaves extractives prepared in various solvents such as petroleum ether, acetone, ethanol, methanol and hot water were tested at a concentration levels of...
S Dhyani, S Tripathi, V K Jain


Degradation of resin constituents in various wood species by the white rot fungus Bjerkandera sp. strain BOS55
1999 - IRG/WP 99-10301
In previous studies, the white-rot fungus Bjerkandera sp. strain BOS55 was shown to cause extensive degradation of lipophilic extractives (resin) in Scots pine wood. Further research was carried out in order to investigate the ability of Bjerkandera sp. for reducing resinous constituents in various softwood (Douglas fir, larch and spruce) and hardwood species (birch, beech and poplar). The greates...
J Dorado, T A Van Beek, F W Claassen, R Sierra-Alvarez


The microbial ecology of treated birch stakes in a soil-bed
1983 - IRG/WP 1209
The microbial ecology of small birch stakes exposed in soil beds in two Fungus Cellars was investigated. Patterns of fungal colonisation and decay initiation are described in untreated birch and copper fluosilicate-treated stakes. Results are based on fungal isolation onto selective media and direct light microscopical observations of decay features. In untreated stakes there was a rapid build-up ...
C P Clubbe


Depletion of preservatives from treated wood: Results from laboratory, fungus cellar and field test
1993 - IRG/WP 93-50001-07
This paper compares results of preservative component losses using a range of test procedures with several different water-borne preservatives. The data shows that laboratory leaching tests are in some cases comparable to, but in other cases significantly underestimate preservative component losses when compared with field or fungus cellar depletion tests. The results also suggest that preservativ...
L Jin, A F Preston


Factors affecting decay rates in a fungus cellar
1985 - IRG/WP 2242
Birch and pine stakes treated with chromated copper arsenate and didecyldimethylammonium chloride were incubated in two soils in a "Fungus Cellar" test. At three month intervals, sets of stakes were inspected and assigned visual ratings or removed from the soil beds for weight loss determination. Preliminary results after nine months exposure have shown differences in the decay rates between birch...
P A McKaig


Anti-sapstain chemicals for diffusion treatment of rubber wood
1986 - IRG/WP 3367
Performance of Sinesto B and Akzo EN 494, two formulated products of alkyl ammonium compounds, was tested as fungicidal additive in the boron solution to control mould and stain during diffusion storage of rubber wood. Sinesto B at 2.0% (a.i.) concentration has given good control over mould and its protection against sapstain was only satisfactory. Akzo EN 494 at 0.7% (a.i.) concentration has give...
R Gnanaharan


The risk assessment process. Point of view of a biocide manufacturer [Évaluation du risque. Point de vue d'un fabricant de biocide]
1990 - IRG/WP 3568
Risk assessment is an inherent part of our everyday lives. The risk assessment equation combines Hazards and Exposure. For the Wood Preservation Industry, the hazards may be characterised by the toxicity a the ecotoxicity of chemicals and the exposure by the identification of exposed people, of the exposure routes and exposure frequency. To quantify the exposure, good co-operation is required betw...
D Baur


A field trial to assess the potential of antisapstain chemicals for long-term protection of sawn radiata pine
1986 - IRG/WP 3375
Seven chemical formulations were tested as antisapstain treatments for freshly sawn radiata pine sapwood (90x50 mm²). Each formulation was used with and without a water-repellent additive and was sprayed on to 1 m long boards. The boards were then stacked into "mini" packets and stored unprotected from the weather for 6 months. Haipen 50w (at 0.2 or 0.4% active) and NaPCP (1% active) plus 1.5% bo...
J A Drysdale


Prevention of sapstain in logs using water barriers
1997 - IRG/WP 97-30147
Placing logs in ponds or under water sprinklers to keep moisture levels high enough to prevent oxygen tensions rising above inhibitory levels, is a proven method of preventing sapstain. The objective of this experiment was to determine if water barriers significantly reduce the rate of sapstain penetration into logs by maintaining moisture contents, and consequently oxygen tensions, at inhibitory ...
R N Wakeling, D R Eden, C M Chittenden, B Carpenter, I Dorset, J Wakeman, R Kuluz


Why don't more people work with Serpula lacrymans nowadays? A discussion of some of the different approaches to experimenting with this unique fungus
1989 - IRG/WP 1383
Remarkably few laboratories are currently investigating this well-known fungus. Not only has it failed to gain acceptance as a standard test organism (for wood preservative evaluation) in many countries, but is also sometimes excluded from pure research studies when it ought to be an obvious first choice as a representative basidiomycete. This paper discusses some different approaches that have be...
J D Thornton


Previous Page | Next Page