IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 310 documents. Displaying 25 entries per page.


Fungus cellar and field tests with tall oil derivatives. Final report after 11 years' testing
1993 - IRG/WP 93-30007
Two derivatives of tall oil were tested as wood preservatives in a fungus cellar and in ground contact (field test). Stakes of Pinus sylvestris sapwood were used in the tests. For the field test the size of the stakes was 20 x 50 x 500 mm³ and for the fungus cellar test 20 x 20 x 250 mm³. The stakes were vacuum-pressure treated with the two products and exposed in 1981. The field test site used ...
J Jermer, Ö Bergman, T Nilsson


SEM investigation of the production of extracellular mucilaginous material (ECM) by some wood inhabiting and wood decay fungi when grown in wood
1997 - IRG/WP 97-10193
Previous reports have illustrated the involvement of extracellular mucilage (ECM) in wood decay by Basidiomycetes. Its production is investigated in a range of stain, mould and soft rot fungi in Corsican pine, Scots pine and European beech. Fungi examined were: Chaetomium globosum, Ceratocystis coerulescens, Trichoderma harzianum, Ophiostoma piceae, Mucor sp. and Penicillium. sp. The samples were ...
A R Abu, D J Dickinson, R J Murphy


A status report on code of good practices
1991 - IRG/WP 3679
Code of Good Practices - Anti Sapstain documents, presented to IRG meetings in the past, are the basic documents for health and safety of the workers and the environment in Canada. The BC Ministry of Environnment has now issued regulations in the area of effluent discharge. While Pentachlorophenols (PCP) are not used by the industry, the documents are still used as a guideline document for the oth...
V N P Mathur, G Das


Worldwide in-ground stake test of acetylated composite boards
1997 - IRG/WP 97-40088
Acetylated wood composite stakes are being tested in ground contact (graveyard test) in seven fields around the world. Three types of acetylated wood composites were prepared: spruce fiberboard in Sweden, aspen fiberboard in Madison and rubber wood particle board in Indonesia. Two levels of acetylation were used, a high level of ~20% acetyl content and a low level of 10% acetyl content. Control bo...
R M Rowell, B S Dawson, Y S Hadi, D D Nicholas, T Nilsson, D V Plackett, R Simonson, M Westin


Fungus cellar testing as an evaluation method for performance of treated timber in ground contact
2001 - IRG/WP 01-20227
A fungus cellar method for the accelerated evaluation of performance of treated wood in ground contact is described. The test soil comprised of sandy loam, vermiculite and Japanese horticulture soil "Kanumatsuchi" in a ratio of 6:2:2 by volume. The soil was inoculated with the dominant test fungus isolated with selective medium from decayed wood samples. Pairs of treated and untreated wood specime...
Y Nagano


Changed permeability and surface properties of hornbeam wood due to its degradation by erosive strain of Phanerochaete chrysosporium
2004 - IRG/WP 04-40290
Specimens of hornbeam wood were submitted to a medium-term degradations by erosive fungus Phanerochaete chrysosporium. Biodegradations of specimens resulted in their apparent structural alterations, changes in permeability and increased intensity of interactions with polar liquids. Modified physical properties of biodegraded wood may significantly influence its penetration with polar media and che...
R Solár, S Kurjatko, L Reinprecht, M Mamon, V Vacek


An electron spin resonance study of manganese changes in wood decayed by the brown-rot fungus, Postia placenta
1988 - IRG/WP 1359
Electron spin resonance (ESR) spectrometry was used to examine wood decay by the brown-rot fungus, Postia placenta. Wood slivers of Douglas-fir, white fir, redwood, sweetgum and yellow poplar were incubated for 4 weeks in custom-made quartz ESR tubes with or without Postia placenta. In all wood species without fungus, a weak partially resolved signal (about g=2, presumably due to manganese) was de...
B Illman, D C Meinholtz, T L Highley


Assessment of the toxicity of some copper-, zinc- and boron-based wood preservatives to the cellar fungus Coniophora cerebella Schröet
1974 - IRG/WP 242
This article reports the use of a method based on the determination of the probability of the protection of timber against destruction by fungi. By converting the probability values to probit values and plotting them as a function of the amount of preservative retained in the timber, curves of the toxic effect are obtained, enabling any timber protection probability to be assessed....
V N Sozonova, D A Belenkov


Standardisation of sapstain tests - A challenge
1992 - IRG/WP 92-2403
In the last decade many new anti-sapstain products have been tested world-wide under laboratory and field conditions. Several extensive test programmes have been executed with different non-standardized test methods and procedures, with the result that the biological findings cannot be compared with each other. In this paper, gathered recommendations will be given in order to standardize test meth...
G Rustenburg, C J Klaver


Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel


The efficacy of Sentry® as a treatment for the control of sapstain in pre-infected radiata pine
2001 - IRG/WP 01-30260
Experiments were conducted to determine the efficacy of Sentry® when used to control sapstain fungi on radiata pine branch billets stored under high fungal hazard conditions. Prior to antisapstain treatment, the billets were pre-infected with a mixed inoculum of staining fungi and held from zero to 10 days at 25°C and 75% relative humidity. This was done to produce billets with different degrees...
C Chittenden, J G van der Waals, B Kreber, R N Wakeling


The use of modulus of rupture and modulus of elasticity in natural durability testing
1997 - IRG/WP 97-20117
Losses in weight, losses in bending strength and changes in elastic behaviour were assessed in a fungus cellar test with beech wood stakes (Fagus sylvatica). Results were gained after 8, 12, 16 and 20 weeks resp . The outcomes show, that the non-durable species beech is very rapidly attacked by fungi and loses up to 60% of its initial bending strength even within the first 8 weeks. Earlier researc...
L Machek, H Militz, W Gard


An evaluation of chemical treatments for the protection of radiata pine logs from fungal degrade
1986 - IRG/WP 3377
Busan 30, Busan 1009, Mitrol PQ375. and sodium pentachlorophenoxide (NaPCP) plus have been evaluated as antisapstain treatments for the long-term protection of debarked radiata pine logs. After 3 months' winter-spring storage, treated debarked logs had less surface and internal sapstain than 'control' logs. After 6 months' storage all logs had internal sapstain ...
J A Drysdale, M E Hedley, J A Butcher


Effect of mobile fungicides on fungal pre-infection in radiata pine billets.
1999 - IRG/WP 99-30191
In New Zealand, fungal infection of logs begins directly after felling and whilst severe degrade can be prevented if antisapstain-treated within 24 hours, such short turn-around times of logs are not always practicable. However, conventional antisapstain formulations in use only provide an envelope of protection on the log surface but are unable to control pre-infections below the surface. The obj...
D R Eden, T Singh, B Kreber


Experiences from a Danish large scale test by means of a new method of treatment by attack of true dry rot fungus (Serpula lacrymans) in buildings
1994 - IRG/WP 94-10064
Experiences from a new and epoch-making method of treatment in connection with the repair of attack of the true dry rot fungus, Serpula lacrymans (Fr.) S.F. Gray, are described. The paper presents the background of a large scale test comprising repair of more than 150 Danish buildings over a period of approximate 5 years. The method being both gentle to the building and presenting savings of at le...
O Munck, H Sundberg


Sentry®, a new antisapstain formulation for protecting logs and lumber. - Part 2: protection of lumber
1999 - IRG/WP 99-30189
Recent research conducted by Forest Research, Chemcolour Industries (NZ) Ltd. and Fletcher Challenge Forest Ltd. has resulted in the development of antisapstain formulations that meet the efficacy requirements of the New Zealand Forest industry for export logs. One treatment, called Sentry®, is now poised for commercial use in New Zealand for treating export logs, having undergone an extensive su...
R N Wakeling, D R Eden, C M Chittenden, J G Van der Waals, B Carpenter, I Dorset, R Kuluz, J Wakeman


The critical moisture and temperature conditions for the growth of some mould fungi and the brown rot fungus Coniophora puteana on wood
1988 - IRG/WP 1369
The growth of some mould fungi on pine and spruce sapwood was studied in 40 different constant moisture and temperature conditions. The temperature range was between +10 and +40°C and the relative humidities varied from 76 to 100% relative humidity (RH). The incubation time was 12 weeks. The mixed mould inoculation used included typical fungi growing on wood: Aspergillus versicolor, Cladosporium ...
H Viitanen, L Paajanen


Preliminary studies to assess the effects of aeration and lowered humidity on the decay capacity, growth and survival of the dry rot fungus Serpula lacrymans (Wulf ex. Fr.)
1997 - IRG/WP 97-10208
Novel microcosms were used to test separately the effects of aeration and humidity on the decay capacity, linear spread and survival of Serpula lacrymans. The application of a pumped air supply resulted in an effective cessation of fungal activity when all but the lowest of the air flow rates was used. Furthermore, the lowest air flow rate caused marked growth tropisms away from the stress. In sep...
G A Low, J W Palfreyman, N A White, H J Staines, A Bruce


Serpula lacrymans, The Dry Rot Fungus and its Tolerance towards Copper-based Wood Preservatives
2005 - IRG/WP 05-10555
Serpula lacrymans (Wulfen : Fries) Schröter, the dry rot fungus, is considered the most economically important wood decay fungus in temperate regions of the world i.e. northern Europe, Japan and Australia. Previously copper based wood preservatives were the most commonly used preservatives for pressure treatment of wood for building constructions. Because of a suspicion about tolerance toward cop...
A C Steenkjær Hastrup, F Green III, C A Clausen, B Jensen


Generation of hydroxyl radical by the brown-rot fungus, Postia placenta
1988 - IRG/WP 1360
In an electron spin resonance (ESR) survey of various liquid cultures and wood slivers innoculated with the brown-rot fungus, Postia placenta, the spin trap dimethyl-l-pyrroline N-oxide (DMPO) was used to detect the presence of the hydroxyl radical. The ESR spectra for the paramagnetic DMPO- hydroxyl radical adduct was observed in (1) nitrogen-limited, liquid cultures having 1.0% glucose or 0.1% c...
B Illman, D C Meinholtz, T L Highley


Monitoring the potential biological control agent Cartapip
2000 - IRG/WP 00-10365
Attempts to biocontrol woodstain caused by Ophiostoma species led to the development of an O. piliferum colorless mutant - Cartapip (AgraSoL). The mutant's ability to prevent sapstain of stored logs and lumber is tested in a variety of field trials in Germany, England, Canada and New Zealand. To carry out biocontrol field trials, users have to obtain a permit from a regulatory agency and ...
S Schröder, K Sterfinger, Seong Hwan Kim, C Breuil


Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox


The effect of extent and location of decay on strength loss in constructional timber
1994 - IRG/WP 94-30039
Radiata pine heartwood billets, 50 x 100 x 1000 mm³ were end-sealed and treated with copper-chrome-arsenate preservative (NZ Type I) to a range of retentions and penetration patterns. Cross-sections, 10 mm thick, were cut from the centre of each billet and used for determination of preservative distribution, for preservative analysis and for decay tests. The decay test consisted of laying samples...
M E Hedley, H Bier


Preservative effect of cellulose insulation material against some mould fungi and brown rot fungus Coniophora puteana in pine sapwood
1991 - IRG/WP 1484
The influence of mineral wool and loose-fill cellulose wool on biodeterioration of pine sapwood was studied. The test fungi were mould fungi Aspergillus versicolor, Cladosporium sphaerospermum, Penicillium sp. and Aureobasidium pullullans and brown rot fungus Coniophora puteana. Cellulose wool inhibited the growth of mould fungi on the face of wood contacted with insulation material at RH of 97 an...
H Viitanen


Screening results of fungicides for sapstain control on Pinus radiata
1983 - IRG/WP 3236
Thirty-two compounds were tested to determine their ability to contain the growth of stain, mould and rot organisms on fresh Pinus radiata D Don. A screening technique was employed using 35 to 50 mm diameter biscuits of Pinus radiata stemwood 10 mm thick. No compound was found to be cost effective when compared against the standard treatments of NaPCP (0.5% a.i.) plus borax (1.5%) and Captafol (0....
P J Hayward, J Duff, W Rae


Previous Page | Next Page