Long-term efficacy of wood dip-treated with multicomponent biocides
2005 - IRG/WP 05-30379
Biocides designed for prevention of indoor mold growth on wood-based materials need to provide long-term protection under conditions of high humidity. Specimens of kiln-dried southern pine and unseasoned southern pine, aspen, and Douglas-fir were dip-treated with borate-dimethylcocoamine (DMCA) supplemented with voriconazole, thiabendazole, or thujaplicin and evaluated at 4-week intervals for inhi...
C A Clausen, V W Yang


Creosote for wood preservation
1971 - IRG/WP 36
By creosote one usually means coal tar creosote, although there are creosotes of other origin. For example, wood tar creosote is a product of wood distillation. It is, in fact, in this connection that the word 'creosote' was first used. Early in the nineteenth century the oily product obtained by distilling wood was said to have an odour which resembled 'smoked meat&...
Anonymous


A below-ground exposure method for determining the resistance of woody and non-woody materials to attack by subterranean termites
1993 - IRG/WP 93-10012
With existing field test procedures, in which specimens are installed vertically to some of their length into the ground and spaced out from each other ("grave-yard" tests), variations in the rate of contact by termites between replicates can be common. Mechanical damage to specimens during inspection and re-installation may also be difficult to avoid. A new field test method, evaluated in Austral...
M Lenz, J W Creffield


Biochemical aspects of white-rot and brown-rot decay
1987 - IRG/WP 1319
This paper presents an overview of the decomposition of wood by white- and brown-rot fungi - the most important and potent of known wood-decay fungi. These organisms are unique among cellulose destroyers because of their strong capability to enzymatically degrade lignified material. Special emphasis is given to the following aspects of wood decomposition by white- and brown-rot fungi: (1) effects...
T L Highley


Determination of absorption, accumulation and transport of copper in mycelium of some wood decay fungi
1999 - IRG/WP 99-10323
Copper compounds are common wood preservatives. However, tolerance of some wood decay fungi to copper compounds has been observed recently. Therefore, we tried to elucidate possible causes of this phenomenon. We investigated uptake, accumulation and secretion of copper in the mycelium of potentially copper tolerant fungi (Antrodia sp.) and non tolerant fungus Trametes versicolor. We observed that ...
F Pohleven, S Breznikar, P Kalan, M Petric


The critical moisture and temperature conditions for the growth of some mould fungi and the brown rot fungus Coniophora puteana on wood
1988 - IRG/WP 1369
The growth of some mould fungi on pine and spruce sapwood was studied in 40 different constant moisture and temperature conditions. The temperature range was between +10 and +40°C and the relative humidities varied from 76 to 100% relative humidity (RH). The incubation time was 12 weeks. The mixed mould inoculation used included typical fungi growing on wood: Aspergillus versicolor, Cladosporium ...
H Viitanen, L Paajanen


L-joint trials: Part 2: The relationship between colonisation by decay fungi and long-term performance
2002 - IRG/WP 02-20251
Many of the L-joint trials conducted at BRE were assessed during the early stages to establish the rate of colonisation by fungi, principally basidiomycetes. At that time, a system of assessment incorporating colonisation studies was proposed for inclusion within the European Standard EN 330 but was rejected for the final version of the standard. The long-term trials associated with the colonisa...
J K Carey


A light and electron microscopic study of decayed CCA-treated radiata pine (Pinus radiata) wood from a cooling tower
1994 - IRG/WP 94-10056
An inspection of an industrial cooling tower in New Zealand showed surface decay of 12 year old Pinus radiata wood panels treated with CCA preservative to a retention of around 15 kg/m³ of salt. Wood decay micromorphology typical of that caused by soft rot fungi, white rot fungi, 'stripy' and 'v-shaped' erosion bacteria and cavitation bacteria were all commonly...
A P Singh, R N Wakeling, D R Page


Durability of Bamboos in India against termites and fungi and chemical treatments for its enhancement
2005 - IRG/WP 05-10553
Bamboo is a very important forest resource that benefits the life of people in a myriad ways including meeting the need for structural uses like posts, pole fencing, scaffoldings, house building, etc. Although it is one of the strongest structural material available, often succumbs to fungal decay and biodeterioration by insects (termites and powder post beetles) during storage and usage. Studies...
O K Remadevi, R Muthukrishnan, H C Nagaveni, R Sundararaj, G Vijayalakshmi


Resistance of painted wood to mould fungi. Part 3. The effect of weathering, wood substrate and fungicides on mould growth
1998 - IRG/WP 98-10284
The effect of 6 month outdoor weathering on the resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments stud...
H Viitanen, P Ahola


Which fungi should be included in the laboratory evaluation of anti-stain chemicals?
2001 - IRG/WP 01-20236
Test fungi for efficacy tests of anti-stain formulations were selected based on the assumptions that test fungi should be fungicide-tolerant antagonists and fungi resistant to both fungicides and fungicide- tolerant antagonists, and such fungi should be re-isolated from treated samples with the highest fungicidal concentration used for laboratory evaluation of fungicides. This paper discusses the ...
Hyung-Jun Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Monitoring the potential biological control agent Cartapip
2000 - IRG/WP 00-10365
Attempts to biocontrol woodstain caused by Ophiostoma species led to the development of an O. piliferum colorless mutant - Cartapip (AgraSoL). The mutant's ability to prevent sapstain of stored logs and lumber is tested in a variety of field trials in Germany, England, Canada and New Zealand. To carry out biocontrol field trials, users have to obtain a permit from a regulatory agency and ...
S Schröder, K Sterfinger, Seong Hwan Kim, C Breuil


Microscopic characteristics of microbial attacks of CCA-treated radiata pine wood
1993 - IRG/WP 93-10011
Light and electron microscopic observations were made of CCA-treated radiata timbers, which had been placed in service in a vineyard soil as supporting poles and as part of a house pile, to determine the cause of their deterioration. The house pile had failed in service after between 9 and 13 years and was of particular interest because decay was more severe in deeper regions than at the surface a...
A P Singh, R N Wakeling


Interim report on the use of borate rods for the in-situ treatment of joinery
1980 - IRG/WP 3159
In the U.K. in recent years, it has been recognised that there is a major need for in-situ treatment of joinery at risk from or showing the early signs of decay. Several techniques have been developed to provide such a treatment, one of which is based on the insertion of anhydrous borate glass rods. The tests in hand are long term and this report is confined to the mycological isolation data from ...
D J Dickinson


Use of wood-decay fungi for disposal of PCP-treated wood
1995 - IRG/WP 95-50040-33
Although PCP has been classified as a priority pollutant, PCP-treated wood products are currently allowed to be disposed of as ordinary solid (non-hazardous) wastes in the US. Non-regulated disposal of these materials is allowed because PCP concentrations in extracts from PCP-treated products such as utility poles and crossarms, determined by the Toxicity Characteristic Leaching Procedure (TCLP) h...
R T Lamar


Effect of cyclic change of temperature on fungal growth and mass loss
1994 - IRG/WP 94-10065
For estimating the effect of cycling change of temparature on fungal growth, four Japanese species, sugi (Cryptomeria japonica), hinoki (Chamaecyparis obtusa), akamatsu (Pinus densiflora) and buna (Fagus crenata), four fungal species, Tyromyces palustris, Gloeophyllum trabeum, Coriolus versicolor, Pycnoporus coccineus, and five temperature conditions, 10, 20, 27, 35°C and cyclic temperature (20°...
K Suzuki, K Okada


Preservative effect of cellulose insulation material against some mould fungi and brown rot fungus Coniophora puteana in pine sapwood
1991 - IRG/WP 1484
The influence of mineral wool and loose-fill cellulose wool on biodeterioration of pine sapwood was studied. The test fungi were mould fungi Aspergillus versicolor, Cladosporium sphaerospermum, Penicillium sp. and Aureobasidium pullullans and brown rot fungus Coniophora puteana. Cellulose wool inhibited the growth of mould fungi on the face of wood contacted with insulation material at RH of 97 an...
H Viitanen


On the effectiveness of fumigants against wood-destroying insects and fungi in wooden cultural property
1993 - IRG/WP 93-10030
Based on a survey of the history of the use of fumigants the actual agents are mentioned in relation to their biogenic effect on wood-destroying insects and fungi as well as their corrosive behavior on cultural property. Furthermore the conditions for the use of reactive fumigants in buildings are discussed. Trials to control wood-destroying insects and fungi by nitrogen and bromomethane are the m...
W Unger, A Unger


Unsuitability of the limiting dose as a criterion for assessing the toxicity of preservatives to wood-destroying fungi
1974 - IRG/WP 243
In the majority of methods for investigating preservatives for wood-destroying fungi their toxicity is assessed by determining what is called the "limiting dose". This normally denotes a range of preservative solution concentrations or retentions of dry preservative in the timber, the lower value serving to indicate the amount of preservative at which is observed the expected effect, e.g. the grow...
D A Belenkov


The probable mechanism of action of boric acid and borates as wood preservatives
1990 - IRG/WP 1450
The tetrahydroxyborate ion [B(OH)4-] acts by complexation with poly-ols and probably attacks decay fungi through extracellular substrate sequestration; intracellular substrate sequestration; enzyme inhibition; and change in membrane function. Work was carried out to investigate this further and to try to explain certain phenomena observed in the area of boron preservation. The effect of Na borate ...
J D Lloyd, D J Dickinson, R J Murphy


Poplar wood and its damages in Iran
1987 - IRG/WP 1332
In Iran poplar planting has been used for many centuries ago specially in regions without forests. It had rural uses in ancient time, but recently many fast growing poplar species have been planted and many hybrids also have been planted; the following species had been cultivated widely in Iran: Populus nigra L. var. italica, Populus alba L., Populus caspica Bornm, Populus deltoides L., Populus X....
D Parsapajouh, P Niloufari


Laboratory screening to determine the preventive effectiveness against blue stain fungi and moulds
1991 - IRG/WP 3677
This paper reports results of preservative treatment and leaching experiments, using borax, polybor and boracol 20, on small wood blocks of English oak and American pitch pine heartwood. Earlier experiments on the performance of various biocides as possible additives to bilgewater to prevent fungal decay of shipping timbers had suggested that some formulations of boron might be associated with phy...
M T De Troya, A M Navarrete


Lethal temperature for some wood-destroying fungi with respect to eradication by heat treatment
1984 - IRG/WP 1229
The lethal heat dosis as a function of temperature and time of exposure has been tested for mycelium and for wood infested by three strains of Serpula lacrymans and by Coniophora puteana, Poria monticola, Paxillus panuoides, Gloeophyllum trabeum and Gloeophyllum sepiarium. Even for Serpula lacrymans, which is well known for its sensivity to heat treatment, 30 min at 55°C were necessary to kill th...
M Miric, H Willeitner


Analysis of D-glucose metabolism of wood decay fungi using 13C-NMR and 13C-labeled substrates
2003 - IRG/WP 03-10475
D-Glucose metabolism is thought to be important during wood decay by fungi, not only for anabolic and catabolic purposes of central metabolism, but also as a potential source of peroxide required by extracellular peroxidases. There has been some confusion in the literature as to whether this peroxide-generating activity is of the glucose 1-oxidase or pyranose 2-oxidase (glucose 2-oxidase) type wi...
T H de Koker, M D Mozuch, P J Kersten


Biodegradation of wood in wet environments: A review
1997 - IRG/WP 97-10217
Wood in wet environments is attacked and degraded by soft rot fungi and erosion and tunnelling bacteria, which are more tolerant to high moisture and reduced oxygen conditions than basidiomycetes, such as white and brown rot fungi. Since basidiomycetes are normally more aggressive and can degrade wood faster than soft rot fungi and bacteria wood in wet environments can survive longer. In fact, arc...