IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 146 documents. Displaying 25 entries per page.


Characteristics of the pigments produced by sap-staining fungi
1997 - IRG/WP 97-10223
The present study was conducted to characterize the pigments produced by sap-staining fungi, Aureobasidium pullulans (de Bary) Arnaud and Ceratocystis piceae (Münch) H. and P. Sydow. The pigments isolated from tested fungi were identified as melanins by spectroscopic methods (UV and infrared spectra). The UV and the infrared spectra of the fungal pigments were similar to those of the synthetic me...
M Mori, M Takahashi


Comparison of two laboratory methods for screening potential anti-sapstain chemicals
1993 - IRG/WP 93-10036
Two methods were used to screen a number of potential anti-sapstain chemicals in the laboratory. In one method miniature boards of freshly felled Scots pine sapwood were dip treated with the candidate chemical, sprayed with a suspension of stainers or moulds and incubated for five weeks. In the other method antibiotic assay discs were treated with precise quantities of chemical, plated out on malt...
S M Gray, D J Dickinson


Commercial antisapstain chemicals in New Zealand
1980 - IRG/WP 3142
Almost all sawn timber of exotic softwoods (principally Pinus radiata) and a large proportion of indigenous sawn timber receives an antisapstain chemical treatment to prevent fungal degrade during subsequent seasoning, storage, or transportation (if exported). Antisapstain chemicals are also widely used to protect freshly peeled round produce during drying. A further, specialised, use is as the fu...
J A Butcher


The relationship between blue-stain and bark beetles
1971 - IRG/WP 19
The attack of bark beetles on standing or in newly-felled stems provides special growth conditions to wood-inhabiting fungi. In the wood attacked by bark beetles, a specific and rich fungus flora is found, and from these fungi the economically important group of blueing fungi has been more thoroughly investigated. These fungi live on nutritive substances present in the cells, especially in the med...
A Käärik


Antisapstain field trials of NeXgen in New Zealand
1997 - IRG/WP 97-30145
This document covers the results of summer and winter log trials of NeXgen, an antisapstain formulation containing methylene bis thiocyanate plus chlorothalonil. Log billets (20 - 25cm diameter) were stripped of bark using a commercial maul debarker and antisapstain treated within 8 hours of felling by dip application. Billets were stored in a pole barn and assessed for internal sapstain and decay...
R N Wakeling, T L Woods, D R Eden, C M Chittenden, B Carpenter


Development process of a new anti-sapstain formulation and its present status with the relevant problems
2001 - IRG/WP 01-30257
An anti-sapstain formulation, which contains 2-(thiocyanomethylthio)benzothiazol (TCMTB) and methylene-bis-thiocyanate (MBT) as active ingredients, was developed by a technical agreement with Buckman Laboratories (Memphis, TN, USA) as an alternative to chlorinated phenols for the Japanese market. The formulation was commercialized as BAM 12 years ago. As anti-sapstain treatment is commonly conduct...
K Nobashi, Y Nomura, K Tsunoda


Defacement of freshly sawn Corsican pine lumber by sapstain and mould fungi and the influence of arthropods
1997 - IRG/WP 97-10227
In a trial to study the arthropods associated with sapstain and mould fungi, freshly sawn Corsican pine (Pinus nigra var. maritima (Aiton) Melville) boards were block stacked at a local sawmill. Each stack was constructed in a nest arrangement with smaller boards in experimental tanks, positioned in the centre of the stacks. Boards were converted from a stock of sawlogs at monthly intervals, to pr...
N J Strong, J F Webber, R A Eaton


Log fumigation prevents enzyme-mediated sapwood discolorations in hardwoods
1993 - IRG/WP 93-10003
Non-microbial sapwood discolorations in hardwood lumber can cause economic loss by degrade of quality. Based on the hypothesis that the enzyme-mediated sapstain may develop in part from byproducts of parenchyma cells in wood, reshly felled logs of red oak (Quercus spp.) and sugar hackberry (Celtis laevigata) were fumigated under a plastic tarp with methyl bromide. Log sections were checked after f...
E L Schmidt, T L Amburgey


Database of sapstain fungi affecting lumber, logs and trees
2004 - IRG/WP 04-10534
Sapstain fungi discolour lumber, logs and tree sapwood and are often mistaken for moulds, which cause a superficial discoloration. Stained wood has a lower market value. Further, because stained wood products can potentially carry pathogenic fungi, such products may be refused by importing countries. Addressing these issues involves developing ways for accurately identifying staining fungi, docume...
S Lee, F de Giuli Vallverdu, S Alamouti, Jae-Jin Kim, A Uzunovic, C Breuil


A report of the Technical Recommendations documents for the Canadian Wood Protection and Preservation Facilities and an environmental study of storm water runoff from anti-sapstain treatment plants
1988 - IRG/WP 3478
With the completion of the Final draft of the Technical Recommendations (TR) documents for the Wood Preservation and Wood Protection Industry, there are naturally questions on what is expected from these documents and how Environment Canada and Provincial regulatory agencies may interact with the wood preservation industry. In general, it is expected that the Canadian Wood Preservation and Protect...
G Das, V N P Mathur


Migration of chlorothalonil and carbendazim in fruits stored in wood treated with the anti-sapstain formulation Tuff Brite C
1997 - IRG/WP 97-50097
Fruits and vegetables stored in treated wood boxes are in contact with the products used for the treatment. In order to obtain regulatory approval for incidental food contact it is necessary to determine the quantity of residues on these fruits or vegetables. When the active materials are used in agriculture it is required that residues found are below to the MRL fixed for these substances. In the...
J F Cooper, D Riboul, M De Vleeschauwer, T L Woods


A new type of biocide suitable for use in different fields of wood preservation
1993 - IRG/WP 93-30014
A new type of polymeric biocides was developed containing quaternary ammonium and boron ester groups as active structure elements, to overcome the disadvantages of AAC's in wood preservation use and to utilise their good performance due to a broad efficacy against fungi on the other hand. The new biocides called polymeric betains have been tested in laboratory and field tests and especial...
V Barth, H Härtner


Validation of the sapstain danger index
2000 - IRG/WP 00-10333
The Sapstain Danger Index (SDI) is a model that is used to indicate sites in the New Zealand forest where felled logs are more prone to sapstain, specifically it should indicate how soon after felling of a log should it be treated for sapstain. The validation of SDI has the goal to identify whether the SDI can be used to predict sapstain development and to eventually minimise loss of value of logs...
P A Cooper, S Downs, R l Farrell


An appraisal of anti-sapstain chemicals in Queensland, Australia
1985 - IRG/WP 3331
Eleven formulations were tested in the field for effectiveness against sapstain, mould and fungi on Pinus elliottii in Queensland. The commercially used sodium pentachlorophenoxide (0.5% a.i.) and Captafol (0.2% a.i.) performed well. Busan 1009 (0.3% a.i.), Protek T (5.0% a.i.), Woodgard E.S. and E.C. (0.8% a.i.), together with sodium tetrachlorophenoxide (0.5% a.i.) offer potential as anti-sapsta...
L E Leightley


Japanese standardized method for evaluating effectiveness of anti-sapstain and anti-mould chemicals
1988 - IRG/WP 2299
Japan Wood Preserving Association established a method for testing effectiveness of chemicals against sapstain and mold fungi on wood in 1979. The method is concerned with a laboratory technique using small timber specimens (20 x 50 x 3 mm³), petri dish and 5 test fungi. Effectiveness of each candidate chemical is evaluated on the basis of the relative resistance to sapstain and mold fungi which ...
K Tsunoda, K Nishimoto


Comparison of three methods of quantitative evaluation of sapstain in rubberwood
2000 - IRG/WP 00-20188
Assessing the extent of fungal stain on wood during laboratory trials is a subjective process and is subjected to considerable variation between individual evaluators and specimen. The purpose of this paper was to explore the potential of three quantitative methods of wood surface measurement of rubberwood specimens degraded by sapstain and mould fungui (Botrydiplodia theobromae, Aureobasidium pul...
A J Ashari, J W Palfreyman, A H H Wong


Development and field trials of Evotek 230, a new antisapstain product
1997 - IRG/WP 97-30140
Laboratory and greenhouse studies, using freshly sawn pine boards, demonstrated that the fungicidal properties of prochloraz and carbendazim were complementary for protection from sapstain and mould under extreme conditions of close stacking and high humidity. Analysis of dip bath solutions before and after dipping 20 boards showed no evidence of any stripping of the active ingredients. Neither fu...
A Adams, J Oudenweyer, J L Lindars


Field evaluation of anti-sapstain products
1987 - IRG/WP 3402
Product A based on methylenebisthiocyanate, product B based on methylenebisthiocyanate plus 2-thiocyanomethylthio-benzothiazole, product C based on 2-thiocyanomethilthio-benzothiazole and product D based on didecyl dimethil ammonium chloride plus 3-iodo-2 propynil butyl carbarnate were evaluated on Pinus radiata sawn timber as fungicides for sapstain and mould in the Sawmill Division of the Univer...
M C Rose, A Bedoya


Evaluation of the effectiveness of Tuff Brite C in the control of sapstain in laboratory and field tests
1992 - IRG/WP 92-3718
Since 1990, the anti-sapstain product Tuff Brite C (ASC 66898) has been evaluated internationally in laboratory and field tests, and has been commercially introduced in New Zealand. The product is an aqueous flowable formulation of chlorothalonil and carbendazim. Efficacy tests which have been carried out in New Zealand, Australia, USA, South Africa and Europe are described and summarized. Tuff Br...
T L Woods, C J Klaver


Performance of proprietary formulations of anti-sapstain preservatives on Hevea brasiliensis timbers in laboratory tests
1989 - IRG/WP 3532
A total of 10 proprietary and two experimental formulations were assessed for their effectiveness against sap-stain caused by Botryodiplodia theobromae on Rubberwood (Hevea brasiliensis). Sterilized wood samples 5x20x40 mm³ were dipped in the test chemicals for 60 seconds and then inoculated with 0.5 ml of culture filtrate of Botryodiplodia theobromae for incubation in sterile, damp petri dishes....
L T Hong


Laboratory evaluation of water repellents as antisapstain treatment additives
1986 - IRG/WP 3382
Water repellent formulations consisting of five paraffin wax emulsions, three polyethylene wax emulsions, two polybutadiene resin emulsions, a polyester emulsion, and a ß-pinene polymer emulsion were subjected to water repellency tests on radiata pine sapwood. With one exception, the parafin wax emulsions were more effective water repellents than the alternative formulations and one of the paraff...
D V Plackett, C M Chittenden


Screening of fungal strains for wood extractive degradation
1998 - IRG/WP 98-10254
Fungal strains were screened for their ability to degrade apolar extractives in wood from scots pine. The degradation of total wood extractives by 91 different strains was monitored in stationary batch assays incubated for 6 weeks. The results obtained show that the ability of wood-inhabiting fungi to utilize wood extractives varied greatly, even for different isolates of the same species. Fungal ...
J Dorado, M J Martinez-Inigo, T A van Beek, F W Claassen, J B P A Wijnberg, R Sierra-Alvarez


Development of bluestain in commercially harvested logs in Britain
1996 - IRG/WP 96-10150
In Britain, mechanised harvesting of conifer forestry crops is now the preferred method of felling where terrain and access allows. However, use of mechanised harvesters can lead to excessive debarking, loosening of the bark and wood splintering with, on average, about a third of the bark removed from the more severely damaged logs. More bark has also been observed to be lost from logs harvested e...
A Uzunovic, J F Webber, D J Dickinson


Biological control of sapwood-inhabiting fungi by living bacterial cells of Streptomyces rimosus as a bioprotectant
1992 - IRG/WP 92-1564
The objective of this study is to evaluate the efficacy of antifungal activity of living bacterial cells for the protection of wood against sapwood-inhabiting fungi. The following sapwood-inhabiting fungi were selected: sapstain --Ceratocystis coerulescens, Ceratocystis minor, Ceratocystis pilifera, and Aureobasidum pullulans; mold fungi --Aspergillus niger, Penicillium spp, and Trichoderma spp. L...
S C Croan, T L Highley


Anti-sapstain chemicals for diffusion treatment of rubber wood
1986 - IRG/WP 3367
Performance of Sinesto B and Akzo EN 494, two formulated products of alkyl ammonium compounds, was tested as fungicidal additive in the boron solution to control mould and stain during diffusion storage of rubber wood. Sinesto B at 2.0% (a.i.) concentration has given good control over mould and its protection against sapstain was only satisfactory. Akzo EN 494 at 0.7% (a.i.) concentration has give...
R Gnanaharan


Previous Page | Next Page