Co-operative research project on L-joint testing. Sampling after 4 years exposure
1987 - IRG/WP 2274
In September 1983, Document No: IRG/WP/2208 was distributed giving guidance on sampling after 8 months exposure and including tables on which to record the test results. Similarly in September 1984, Document No: IRG/WP/2233 was distributed concerning sampling after 18 months exposure. No major problems have been notified to Princes Risborough Laboratory concerning the sampling method. It is theref...
J K Carey, A F Bravery


Treatment groups and remedies for CCA treated hardwood and softwood poles
1999 - IRG/WP 99-40142
Different hardwood and softwood species from Bangladesh and Bhutan was investigated regarding density, green fiber stress, natural durability of heartwood and CCA treated sapwood, CCA treatability grades, sapwood thickness, and kiln-drying properties for long term use as electric poles. These properties along with the past service records for nineteen years, separated ten heardwood and five softwo...
A K Lahiry


Biological resistance of furfuryl alcohol-treated wood
1992 - IRG/WP 92-3703
Biological resistance of FFA (furfuryl alcohol)-treated wood was investigated in relation to the rise of ASE (anti-swelling efficiency) resulting from the treatment. Sapwood blocks of Japanese red pine, cedar and beech were vacuum-impregnated with various concentrations of aqueous FFA solutions to get the target levels of% (w/w) RL (resin loading). Air-dried blocks were kept in an oven at 120°C f...
J Y Ryu, Y Imamura, M Takahashi


The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


A technique for determining the efficacy of water diffusible preservative plugs for implanting in joinery in service
1987 - IRG/WP 2291
A technique is described for determining the efficacy of soluble, diffusible preservative plugs for eradicating decay in joinery. It uses blocks of Scots pine sapwood or heartwood adjusted to known moisture contents prior to the establishment of the test fungus Coniophora puteana, from a single longitudinal dowel and the subsequent introduction of the preservative plugs. Prevention of decay, eradi...
J K Carey, A F Bravery


Termite resistance of treated wood in an above-ground field test
1985 - IRG/WP 2241
A field test method has been developed for evaluating the susceptibility of wood products to termites in protected situations above ground. In this method fungal attack on the wood products is minimal, though decay has been observed in conjunction with termite attack in some specimens. Preliminary results from exposure of replicate wood samples treated with preservatives in Florida to Reticuliterm...
A F Preston, P A McKaig, P J Walcheski


Durability of Sugi (Cryptomeria japonica D.DoN ) wood treated in high temperature liquid paraffin
2002 - IRG/WP 02-40221
Sugi(Cryptomeria japonica D.DoN )wood was subject to a heat treatment in high-temperature liquid paraffin for the purpose of improving the resistance against fungi and termites without chemicals. The bath of paraffin liquid, which can provide a uniform heat transfer (±2?), was used at temperatures of 90?,120?and 150?.?ecay resistance according to JIS K 15711) was evaluated using a brown rot fungu...
Y Matsuoka, W Ohmura, S Fujiwara, Y Kanagawa


The resistance of timbers to impregnation with wood preservatives
1979 - IRG/WP 3137
It is anatomical structure which determines liquid flow rate within different timber species. This cannot be deduced from properties such as density or rate of growth, and can only be found by experiment. A standard test has been in use at the Princes Risborough Laboratory for many years, employing a pressure-impregnation treatment, and a large number of timbers have been studied. The test consist...
Anonymous


Comparative study of blue stain resistance of various types of wood stains after artificial and natural weathering
1992 - IRG/WP 92-2411
For the determination of the protective effectiveness of a preservative treatment against blue stain in service, artificial weathering has been proposed as an alternative for the natural weathering period of 6 months in the European standard EN 152. Research on a range of products and on complete finishing systems for external joinery was conducted during 1986-1990. It revealed that the decisions ...
J Van Acker, M Stevens, M Nys


Termite resistance of treated wood in an above-ground field test
1986 - IRG/WP 1300
This paper provides an update on the results from an above ground field test evaluating the effectiveness of wood preservatives against subterranean termites. Results for the one and two year inspections of treated southern pine sapwood exposed in Hawaii to Coptotermes formosanus are presented. Chromated copper arsenate is providing excellent protection as is the pyrethroid deltamethrin. Borate an...
A F Preston, P A McKaig, P J Walcheski


Application of oscillating pressure to improve treatability of refractory species
1987 - IRG/WP 3449
Under practical conditions a minimum moisture content of 80% demande by the German quality standard RAL-RG 411 can not be guaranteed throughout the year. Storage of logs with bark prolonges the drying process; a storage without bark must be avoided. A sufficient penetration according the standard can be achieved at least with a moisture content of 60%, optimal conditions may prevail between 100% a...
R-D Peek


Algal growth resistance of paints for coating of wood; a laboratory study
1997 - IRG/WP 97-10213
Twelve paints were tested for resistance against algae. In addition, one algicidal compound commercially used for remedial treatments of algal growth on paints was tested for its effectiveness for prevention of algal growth. An agar diffusion bioassay was employed in which paint films on filter paper discs were placed on mineral salt medium and sprayed with an algal suspension containing a mixture...
J Bjurman


Influence of the content of organic matter of soil on the degradation of wood by soft rot fungi
1970 - IRG/WP 27
The degradation of wood specimen burried in the soil by soft rot fungi is influenced by a number of factors. These are in particular the water holding capacity, water content, content of organic matter, pH, content of mineral nutritive substances etc. The results of the interlaboratory tests, carried out within the IRG/WP let presume that the intensity of wood degradation occurs proportionally inv...
O Wälchli


Resistance of twenty-five species of timbers to marine borer attack at Visakhapatnam, east coast of India
1994 - IRG/WP 94-30036
Observations on the natural resistance of 25 species of timbers to marine borer attack for a twelve month period at the fishing harbour, Visakhapatnam, East Coast of India, indicate that none of the species was free from borer attack. The damage was mainly by teredinids - Teredo furcifera and Lyrodus pedicellatus. Martesia striata, Teredo parski, Bankia campanellata and Lyrodus bipartitus were als...
K S Rao, M Balaji, V V Srinivasan


The study of blue stain found in coniferous timber in SR Slovenia (Yugoslavia)
1983 - IRG/WP 1177
The report concerns the problems connected with blue stain in coniferous timbers stored in warehouses at wood-processing plants in SR Slovenia (Yugoslavia). The amounts of spruce-wood (Picea abies Karst.) found to have been infected with blue stain have been measured and some of the fungi causing the stain have been identified and their biology studied. It was found that the percentage of spruce-w...
R Benko


Moisture content of logs under sprinklers
2000 - IRG/WP 00-40157
Logs are kept under sprinklers during storage for avoiding the development of sapstain fungi. According to literature, sapstain fungi do not develop if the moisture content is above 120%. It is supposed that, the water sprinklers maintain the log's moisture content above this value, but, very often, sapstain is found on sawn lumber cut from these logs. Logs are harvested and transported t...
M C Rose, A M Briones, M Fernández


Formosan Subterranean Termite Resistance to Heat Treatment of Scots Pine and Norway Spruce
2003 - IRG/WP 03-40264
New challenges to the durability of wood building materials have arisen in the U.S. The Formosan subterranean termite (Coptotermes formosanus Shiraki) now infests sizable portions of the U.S. south and their range is extending. Heat treatments offer a unique opportunity for wood-based composites because many of the process techniques already employ various thermal applications and could be easil...
W R Smith, A O Rapp, C R Welzbacher, J E Winandy


Effects of pre-harvest girdling on selected properties of red pine, red maple and Eastern larch
1999 - IRG/WP 99-40137
Trees of three species - tamarack (Larix laricina), soft maple (Acer rubrum) and red pine (Pinus resinosa) - were girdled immediately below the crown,one to two years before felling. The wood from these trees was compared with wood taken from un-girdled control trees felled at the same. Sapwood and heartwood, from the controls, and from above and below the girdle of treated trees, were examined fo...
A Taylor, P A Cooper


Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp


Natural decay resistance of some lesser known /used timber species from the forests of Tanzania
2005 - IRG/WP 05-10557
In order to manage the Tropical forest in a sustainable manner and increase the resource base for their wood industries, many Tropical African timber producing countries including Tanzania are promoting the many lesser known/used timbers in their forests as alternative sources of wood to the over-exploited primary timber species. Four lesser known/utilized timber species from the forests of Tanzan...
S A Amartey, P R Gillah, R C Ishengoma, J Gabriel, D H Kitojo


Whitewood - An external joinery timber?
1975 - IRG/WP 253
The timber used traditionally for softwood joinery in the UK is redwood (Pinus sylvestris). In the past its ready availability in the desired sizes and quality and its durability in service encouraged little competition. However, the past decade has seen some erosion of this position, particularly through the increased proportion of sapwood in redwood supplies. Since the sapwood is less durable th...
J W W Morgan


The use of lap-joints in natural durability testing: moisture content development during 36 months outside exposure trials
2000 - IRG/WP 00-20217
Lap-joint trials (following European Standard ENV 12037) were set up with 11 different softwood and hardwood species. The main aim was to evaluate the suitability of this test standard (developed for testing wood preservative effectiveness) for natural durability testing. The moisture development has been followed during a 36 months period. In this paper, the outcomes of different moisture content...
H Militz, C J Bloom


Moisture Adsorption Behaviour of Rubber Wood Decayed by Brown and White rot Fungi
2005 - IRG/WP 05-40306
Moisture adsorption behaviour of rubber wood blocks decayed by each brown rot and white rot fungi was studied. The adsorption isotherms of decayed wood were compared with the isotherm of undecayed wood. The wood decayed by brown rot adsorbed less moisture as compared to sound or undecayed wood at all humidity levels. No significant difference was observed in adsorption behaviour of white rot dec...
S S Chauhan, H C Nagaveni


Effect of humidity and temperature on fastener withdrawal resistance from CCA and ACZA treated Douglas-fir
2000 - IRG/WP 00-20209
The effects of preservative treatment on fastener withdrawal was investigated in Douglas-fir lumber conditioned to two moisture regimes. In general, conditioning samples to 19% moisture content produced more substantial changes in withdrawal resistance of galvanized fasteners than did conditioning to 12%. Treatment had little or no effect on withdrawal resistance of stainless steel fasteners. With...
Sung-Mo Kang, J J Morrell


Why don't more people work with Serpula lacrymans nowadays? A discussion of some of the different approaches to experimenting with this unique fungus
1989 - IRG/WP 1383
Remarkably few laboratories are currently investigating this well-known fungus. Not only has it failed to gain acceptance as a standard test organism (for wood preservative evaluation) in many countries, but is also sometimes excluded from pure research studies when it ought to be an obvious first choice as a representative basidiomycete. This paper discusses some different approaches that have be...
J D Thornton