Results of the resistance of acetylated wood against marine borers at three Italian sites after five years of sea immersion
2022 - IRG/WP 22-10994
The aim of this research was the determination of resistance of acetylated wood against marine decay in use class 5 (EN 335) in temperate sea waters. The resistance of acetylated Pinus radiata (radiate pine) in solid and medium density fibreboard (MDF) panels is compared with that of the untreated Scots pine, radiata pine and other untreated wood of European species such as Fagus sylvatica (Europe...
S Palanti, F Stefani, M Andrenacci, M Faimali, I Guarneri, M Sigovini, D Tagliapietra


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang


Evaluation of Decay Resistance of Copper-based Preservatives Treated-Wood exposed to different field test sites in Korea
2022 - IRG/WP 22-20679
In Korea, preservative treated wood is required to have a stamp on the surface which contains information such as wood species, use categories, and the company that treated the wood. Such stamping is necessary to safely and appropriately use the treated wood. Since majority of treated wood is being used outdoor environment, the treated wood must have efficacy against wood decay fungi or termite. I...
W-J Hwang, S-M Yoon, Y Park, Y-S Choi, H-M Lee, J-W Kim


Above-Ground Termite Resistance of Naturally Durable Species in Ontario and Mississippi
2022 - IRG/WP 22-30767
A collaborative above-ground protected termite field test was initiated by FPInnovations and the USDA Forest Service at sites in Ontario and Mississippi. The aims of the experiment were to compare the rate of attack in protected, above-ground exposures by the subterranean termite species, Reticulitermes flavipes, between northern (Ontario) and southern (Mississippi) test sites and to generate perf...
R Stirling, M Mankowski


Effects of Borax and Boric Acid as Fire Retardants on the Resistance of Pterygota macrocarpa Wood to Fire Tests
2022 - IRG/WP 22-30770
The combustible nature of wood as a building material, when exposed to hazards of fire underscores the reason for fire retardant treatments. Pterygota macrocarpa wood is commonly used by builders in Nigeria for roof and other structural applications. Therefore, this study was carried out to assess the effect of Borax and Boric acid on the fire-retardant properties of P. macrocarpa wood. Wood sampl...
J M Owoyemi, O Apogbona, T O Akinwamide


Environmentally Friendly Wood Modification based on Tannin-Furfuryl alcohol - Effect on stabilisation, mechanical properties and decay durability
2022 - IRG/WP 22-40929
Furfurylation is a well-known wood modification technology. This paper studied the effect of tannin addition on the wood furfurylation. Three kinds of dicarboxylic acids, adipic acid, succinic acid, and tartaric acid, as well as glyoxal as a comparing agent, were used to catalyse the polymerisation of furanic or tannin-furanic solutions during wood modification. Impregnation of furanic or tannin-f...
M Mubarok, E Azadeh, F O Akong, S Dumarçay, A Pizzi, C Charbonnier-Gérardin, P Gérardin


Steam Pre-conditioning Treatment Prior to Acetylation: Impact on Dimensional Stability, Moisture Response Behaviour, and White-Rot Fungal Resistance of Hevea brasiliensis and Mitragyna ciliata Wood
2022 - IRG/WP 22-40930
The effect of steam pre-conditioning treatment on the dimensional stability, moisture response behaviour, and durability against white-rot fungus P. chrysosporium of acetylated Hevea brasiliensis and Mitragyna ciliata wood species were assessed. Defect-free specimens of both species from the top, middle, and base positions were selected, prepared according to ASTM D143-09 & ASTM D-2017 standards a...
E Uchechukwu Opara, J Mayowa Owoyemi, J Adeola Fuwape


The Resistance of Some Commercially Thermally Modified American Hardwoods to Termites and Fungi
2022 - IRG/WP 22-40944
Thermally Modified Wood (TMW) is now being produced in the United States but there are few data on the durability of these materials. In this study, commercially-produced thermally modified yellow poplar (Liriodendron tulipifera), red maple (Acer rubrum), and white ash (Fraxinus americana) were evaluated for fungal and termite resistance. The resistance of the three TMW species against Gloeophyllu...
B Cortes, B Bond, A Taylor, J Lloyd


Effect of densification of Eucalyptus nitens and E. obliqua on moisture uptake, swelling, decay resistance, and fire performance
2022 - IRG/WP 22-40946
Some Australian Eucalyptus species that are abundantly available have low natural durability and poor resistance to fire. These same species are also extremely difficult to treat with preservatives or fire retardants using conventional pressure treatment methods due to a large proportion of refractory heartwood. The aim of this research was to understand whether thermo-mechanical densification had...
B Hassan, J J Morrell, F Wiesner, W Wu, B Belleville, K C Wood


Phenol formaldehyde modification and termite resistance under laboratory testing
2022 - IRG/WP 22-40952
The development of phenol formaldehyde (PF) resins as a means of impregnating solid wood is one that has been explored for several decades, both in terms of conventional impregnation processing (Impreg) or compressional impregnation (Compreg). However, it is only recently with advances in processing conditions that the method truly affords a means of achieving conventional modification for solid t...
L Nunes, A Pitman, M Duarte, B Stefanowski, D Jones


Evaluation of Decay Resistance for the Larch Wood Heat-treated with Superheated Steam
2022 - IRG/WP 22-40956
Heat-treatment of wood is a process that involves applying heat ranging 160–260°C to improve its physico-mechanical properties and resistance against wood rot fungi. The level of the changes in the wood properties by heat-treatment differs depending on the temperature and duration of heat-treatment, as well as the types of heat transfer media used for heat-treatment. The heat-treatment on wood ...
Y Park, S-M Yoon, H Kim, W-J Hwang


A novel method for assessing radial variation in termite resistance of timber
2023 - IRG/WP 23-11005
Australia has many timbers whose heartwood is highly resistant to fungal and termite attack; however, changing public policies have resulted in restricted access to many native forests where these species are found. Plantations of these same species are expected to replace these resources, but there are questions concerning whether timber from these trees will have the same resistance as the nati...
S Kleinschmidt, R McGavin


Resistance of phenol formaldehyde impregnated beech (Fagus sylvativa L.) LVL against biodegradation in soil contact
2023 - IRG/WP 23-40965
Alternatives to preservative impregnation are emphasized in Germany and other European countries. Even though these treatments significantly improve wood's resistance to decay, they often do not have a beneficial impact on the dimensional stability. One alternative product, which may be used in ground contact for items like poles and railway sleepers, could be beech (Fagus sylvatica L.) laminated ...
M Slabohm, C Brischke, S Bicke, H Militz


New wood-modification process based on grafted urethane groups: Durability of carbamamylated Scots pine (Pinus sylvestris L.) wood
2023 - IRG/WP 23-40974
Substituting commonly used toxic preservatives with wood modification treatments can make the wood material less prone to water and moisture uptake. This approach favours a more sustainable protection of wood against biodegradation. In this study, Scots pine sapwood was full-cell impregnated with an aqueous solution of urea (30%), dried at 40°C for 24h, and subsequently heat-treated at 150°C for...
C-F Lin, O Myronycheva, O Karlsson, D Jones, D Sandberg


Evaluation of the effectiveness of soaking of high-temperature plywood in low-temperature oil-based wood
2023 - IRG/WP 23-40991
We conducted a preliminary investigation to determine if soaking high-temperature plywood in a low-temperature preservative solution could achieve deeper penetration of the preservative, even in plywood made with refractory wood species such as Japanese larch. Specimens cut from commercial plywood (Japanese larch) were stored at various temperatures before being soaked in the preservative solution...
T Miyauchi, S Isaji, H Shibui, N Furuta, J Miyazaki, H Matusnaga


Do naturally sequestered biocidal metals contribute to the marine borer resistance of turpentine?
2024 - IRG/WP 24-11036
Turpentine wood is renowned for its resistance to attack by molluscan marine borers. This resistance is thought to be due to its high silica content, and possibly the presence of other, as yet unknown, compounds. Silica in turpentine wood is present as particles in rays, but in many plant species silica also occurs in cell walls. We hypothesized that Si is present in cell walls of turpentine, but ...
P D Evans, H Matsunaga, D Feng, M Turner, C Kewish


Intra-species variability of moisture dynamics in wood
2024 - IRG/WP 24-11040
Moisture dynamics of wood and wood-based materials play a major role in wood durability against different decay organisms. Their impact becomes particularly evident when wood is exposed, but not permanently wet. To date, however, this has only been taken into account indirectly and therefore inadequately when testing the durability of wood. While test methods are available, for example to determin...
C Brischke, H Purps, L Emmerich


Enhancing UV resistance and decay resistance of wood by nanoparticle dispersed linseed oil nanoemulsion
2024 - IRG/WP 24-20706
Enhancing increasing demand for eco-friendly and cost-effective wood coatings and preservatives has led to the development of water-borne formulations and use of non-toxic and natural materials such as vegetable oils and waxes. The aim of this study was to improve the UV resistance and decay resistance of wood by nanomaterial dispersed linseed oil emulsions. Highly stable nanoemulsions of linseed ...
R Bansal, R Kumar, K K Pandey


Surface treatment of cross-laminated timber to improve water repellency and UV resistance
2024 - IRG/WP 24-20716
Cross-laminated timber (CLT) has emerged as a revolutionary building material, offering a sustainable alternative to traditional construction methods. By layering and bonding multiple layers of wood at right angles, CLT creates a robust and versatile structural element capable of supporting significant loads while promoting eco-friendliness and design flexibility. However, despite its numerous adv...
M Chen, S Uphill, J Hilsenbeck, A Hughes


Influence of the substitution of phenol with lignin cleavage products in phenol-formaldehyde impregnation resins for wood modification on the fungal decay resistance and impregnation depth
2024 - IRG/WP 24-30805
The impregnation modification of wood with phenol-formaldehyde (PF) resins increases the woods dimensional stability and resistance against fungal decay. However, to decrease the usage of non-renewable resources, the substitution of phenol has been a topic of scientific interest. Lignin is a currently underutilized resource with a chemical structure that contains phenolic units. For adhesive appli...
J Karthäuser, L Tarentino, A Treu, H Militz, G Alfredsen


A novel treatment for increasing UV stabuility of wood based on citric acid and urea
2024 - IRG/WP 24-30811
Wood, a fundamental material in the Built Environment, faces challenges related to durability and weathering, notably UV degradation leading to colour changes. This study explored a novel treatment method utilising citric acid and urea to enhance the UV stability of wood. The reaction between these compounds forms fluorescent species and insoluble nanoparticles upon thermal treatment. Two treatmen...
S Jué, A Scharf, C-F Lin, R Moutou Pitti, D Sandberg, D Jones


Outdoor termite resistance performance of zinc borate (Borogard® ZB) treated parallel strand lumber (PSL) – 15 years field test results
2024 - IRG/WP 24-40999
This report discloses the outdoor termite resistance performance of PSL samples treated with zinc borate at a dosage of 0.85% BAE and 1.72% BAE in Wuxi, China. The outdoor field trial lasted for 15 years and observations were made after 6 months, 3 years, 5 years 1 month, 6 years 6 months and 15 years. The retaining rates of B2O3 and ZnO in the final samples were also tested, and the hypothesis wa...
S Shi, E Laval, K Lung, F Ascherl, R Williams, W Li, X Li


Durability of Malaysian plybamboo to mold
2024 - IRG/WP 24-41014
Durability of 3-layer plybamboo fabricated from two Malaysian bamboo species, Gigantochloa levis (beting) and Gigantochloa scortechinii (semantan) using three different adhesives - urea formaldehyde (UF), melamine urea formaldehyde (MUF) and phenol resorcinal formaldehyde (PRF) was evaluated in this study. Samples were exposed to the mold, Aspergillus brasiliensis for 4-week following the ASTM D44...
S Lipeh, A Mustapha, A S Yusoh, M K A Uyup


Analysis and performance of spruce alternative species and discarded wood for windows production
2024 - IRG/WP 24-50386
Climate change is having a significant impact on European forestry, particularly on the softwood species used for window frames. This study investigates potential replacement tree species for spruce (Picea abies), the predominant material for window frames. We evaluate Douglas fir (Pseudotsuga menziesii), Scots pine (Pinus sylvestris), thermally modified poplar (Populus nigra) and discarded silver...
B Lesar, J Levanič, M Humar, A Treu