International comparison of three field methods for assessing the in-ground resistance of preservative-treated and untreated wood to termites and fungal decay – Summary of observations after five years
2003 - IRG/WP 03-20261
Results are presented from a five-year study conducted in five locations in Australia, Thailand and the USA. Three methods of exposure were assessed (below-ground, graveyard and ground contact) for evaluating the in-ground termite and decay resistance of Pinus radiata D. Don sapwood stakes that had been vacuum pressure impregnated with CCA (Type C) and ACQ (Type D) each at two nominal retentions (...
M Lenz, J W Creffield, T A Evans, B M Kard, C Vongkaluang, Y Sornnuwat, A F Preston


A comparison of the leaching resistance of copper 2-ethanolamine and copper ethylenediamine treated Scots pine
2000 - IRG/WP 00-30233
The depletion of copper from copper 2-ethanolamine and copper ethylenediamine treated Scots pine blocks was investigated. A greater leaching resistance was found for copper 2-ethanolamine, which retained ca. 86% and ca. 50% copper after water and buffer leaching, respectively. Leached amine treated blocks also contained significant residual amine. This was consistent with other observations linked...
Xiao Jiang, J N R Ruddick


Biological resistance of electrolessly plated wood (1). Preliminary report
1994 - IRG/WP 94-40024
Surface metal coating is considered to improve biological resistance of wood as some metal ions are fungitoxic. Six wood species (three softwoods: Cryptomeria japonica, Tsuga heterophylla and Larix spp; three hardwoods: Fagus crenata, Acer mono and Betula platyphylla) were electrolessly plated with nickel or copper, and those were served for laboratory evaluation of their resistance against decay ...
M Hasegawa, K Tsunoda, T Yoshimura


Biological resistances of wood-metaborate composites using the borax solution system
2001 - IRG/WP 01-30259
Combinations of wood and metaborate composite were prepared from sapwood specimens of Japanese cedar (Cryptomeria japonica) and the borax and metallic salts system using the diffusion-penetrated process. Wood-metaborate composites were produced as follows: water-saturated specimens were first impregnated by a saturated borax solution and then diffuse-penetrated with Zn2+, Ca2+, or Pb2+ solution. B...
Liang Lin, T Furuno


Fungal decay resistance of Rubber wood treated with heartwood extract of Rosewood
2005 - IRG/WP 05-30367
Alcoholic extract of Dalbergia latifolia heartwood was studied for its toxicity towards wood decaying fungi. Rubber wood blocks were treated with this extract to three different retention levels (0.1%, 0.2% & 0.5%) and the treated wood blocks were assessed for their resistance towards two white rot and two brown rot fungi. Treated blocks showed improved resistance over the control blocks. At 0...
A K Sethy, H C Nagaveni, S Mohan, K T Chandrashekar


A real scale evaluation method and results on termite resistance of housing wall systems and floor framings
1999 - IRG/WP 99-10314
For evaluating the termite resistance of real scale houses especially housing wall systems and floor framings, a experimental building was prepared. After initial feeding of termite, this house was constructed. In this experimental building, several parts which were built by different wall systems and floor framing. The room temperature of these parts were controlled. Water can be provided in the ...
K Suzuki, K Okada, K Hagio, Y Tanaka


In situ testing the influence of melamine resins on the enzymatic activity of basidiomycetes
1999 - IRG/WP 99-30194
Waterbased methanol etherificated melamine formaldehyde resins have the potential to increase the resistance of impregnated wood against wood destroying fungi. The mechanism of the increased wood durability is not clear yet. In the present paper the possible interference of melamine resins with wood degrading enzymes of Coniophora puteana and Trametes versicolor was investigated as a possible cont...
D Lukowsky, F Büschelberger, O Schmidt


Biological degradation resistance of wood acetylated with thioacetic acid
1983 - IRG/WP 3223
Chemically, modification of wood is being considered as an alternative to conventional preservation by toxic chemicals. Acetylated wood has been reported to be quite resistant to most biodegrading organisms at weight percent gains (WPG) around 15-19. The conventional acetylation techniques with acethic anhyrdride result in generation of acetic acid. However, acetylation with thioacetic acid overco...
S Kumar, S C Agarwal


Three years of field tests with "Lignomer" stakes in ground contact
1981 - IRG/WP 3166
The "Lignomer" (Wood Polymer Composite) is a material obtained during the polymerisation of various monomers or its mixtures in wood. As laboratory tests have shown, this material is characterized by a high resistance against biological deteriorating agents. The laboratory investigations on the durability of various materials against biological deterioration are in many instances extended by field...
K Lutomski


Biological resistance of wood-based composites under protected, aboveground conditions
2005 - IRG/WP 05-20312
Five kinds of wood-based composites (density fiberboard=MDF, hardwood plywood=HP, softwood plywood =SP, particleboard=PB and aspen oriented strand board=OSB) were tested for their resistance against subterranean termites and decay under protected aboveground conditions. The exposure method was previously developed for evaluating performance of sill plates (dodai) in Japanese homes. Ten replicates ...
K Tsunoda


Biological resistance of furfuryl alcohol-treated wood
1992 - IRG/WP 92-3703
Biological resistance of FFA (furfuryl alcohol)-treated wood was investigated in relation to the rise of ASE (anti-swelling efficiency) resulting from the treatment. Sapwood blocks of Japanese red pine, cedar and beech were vacuum-impregnated with various concentrations of aqueous FFA solutions to get the target levels of% (w/w) RL (resin loading). Air-dried blocks were kept in an oven at 120°C f...
J Y Ryu, Y Imamura, M Takahashi


Termite resistance of treated wood in an above-ground field test
1985 - IRG/WP 2241
A field test method has been developed for evaluating the susceptibility of wood products to termites in protected situations above ground. In this method fungal attack on the wood products is minimal, though decay has been observed in conjunction with termite attack in some specimens. Preliminary results from exposure of replicate wood samples treated with preservatives in Florida to Reticuliterm...
A F Preston, P A McKaig, P J Walcheski


Durability of Sugi (Cryptomeria japonica D.DoN ) wood treated in high temperature liquid paraffin
2002 - IRG/WP 02-40221
Sugi(Cryptomeria japonica D.DoN )wood was subject to a heat treatment in high-temperature liquid paraffin for the purpose of improving the resistance against fungi and termites without chemicals. The bath of paraffin liquid, which can provide a uniform heat transfer (±2?), was used at temperatures of 90?,120?and 150?.?ecay resistance according to JIS K 15711) was evaluated using a brown rot fungu...
Y Matsuoka, W Ohmura, S Fujiwara, Y Kanagawa


The resistance of timbers to impregnation with wood preservatives
1979 - IRG/WP 3137
It is anatomical structure which determines liquid flow rate within different timber species. This cannot be deduced from properties such as density or rate of growth, and can only be found by experiment. A standard test has been in use at the Princes Risborough Laboratory for many years, employing a pressure-impregnation treatment, and a large number of timbers have been studied. The test consist...
Anonymous


Comparative study of blue stain resistance of various types of wood stains after artificial and natural weathering
1992 - IRG/WP 92-2411
For the determination of the protective effectiveness of a preservative treatment against blue stain in service, artificial weathering has been proposed as an alternative for the natural weathering period of 6 months in the European standard EN 152. Research on a range of products and on complete finishing systems for external joinery was conducted during 1986-1990. It revealed that the decisions ...
J Van Acker, M Stevens, M Nys


Termite resistance of treated wood in an above-ground field test
1986 - IRG/WP 1300
This paper provides an update on the results from an above ground field test evaluating the effectiveness of wood preservatives against subterranean termites. Results for the one and two year inspections of treated southern pine sapwood exposed in Hawaii to Coptotermes formosanus are presented. Chromated copper arsenate is providing excellent protection as is the pyrethroid deltamethrin. Borate an...
A F Preston, P A McKaig, P J Walcheski


Algal growth resistance of paints for coating of wood; a laboratory study
1997 - IRG/WP 97-10213
Twelve paints were tested for resistance against algae. In addition, one algicidal compound commercially used for remedial treatments of algal growth on paints was tested for its effectiveness for prevention of algal growth. An agar diffusion bioassay was employed in which paint films on filter paper discs were placed on mineral salt medium and sprayed with an algal suspension containing a mixture...
J Bjurman


The effect of moisture content on the electrical resistance of timber as detected by a pulsed current reistance meter (Shigometer)
1984 - IRG/WP 2212
The literature concerning the use of the Shigometer® for detecting decay in standing trees and wood poles is reviewed and the differences of opinion over the effect of timber moisture content on electrical resistance are highlighted. A simple experiment designed to test this effect is described and the implications of the results for testing poles in service are discussed. There was a large diffe...
P I Morris, D J Dickinson


Influence of the content of organic matter of soil on the degradation of wood by soft rot fungi
1970 - IRG/WP 27
The degradation of wood specimen burried in the soil by soft rot fungi is influenced by a number of factors. These are in particular the water holding capacity, water content, content of organic matter, pH, content of mineral nutritive substances etc. The results of the interlaboratory tests, carried out within the IRG/WP let presume that the intensity of wood degradation occurs proportionally inv...
O Wälchli


Resistance of twenty-five species of timbers to marine borer attack at Visakhapatnam, east coast of India
1994 - IRG/WP 94-30036
Observations on the natural resistance of 25 species of timbers to marine borer attack for a twelve month period at the fishing harbour, Visakhapatnam, East Coast of India, indicate that none of the species was free from borer attack. The damage was mainly by teredinids - Teredo furcifera and Lyrodus pedicellatus. Martesia striata, Teredo parski, Bankia campanellata and Lyrodus bipartitus were als...
K S Rao, M Balaji, V V Srinivasan


Formosan Subterranean Termite Resistance to Heat Treatment of Scots Pine and Norway Spruce
2003 - IRG/WP 03-40264
New challenges to the durability of wood building materials have arisen in the U.S. The Formosan subterranean termite (Coptotermes formosanus Shiraki) now infests sizable portions of the U.S. south and their range is extending. Heat treatments offer a unique opportunity for wood-based composites because many of the process techniques already employ various thermal applications and could be easil...
W R Smith, A O Rapp, C R Welzbacher, J E Winandy


Effects of pre-harvest girdling on selected properties of red pine, red maple and Eastern larch
1999 - IRG/WP 99-40137
Trees of three species - tamarack (Larix laricina), soft maple (Acer rubrum) and red pine (Pinus resinosa) - were girdled immediately below the crown,one to two years before felling. The wood from these trees was compared with wood taken from un-girdled control trees felled at the same. Sapwood and heartwood, from the controls, and from above and below the girdle of treated trees, were examined fo...
A Taylor, P A Cooper


Natural decay resistance of some lesser known /used timber species from the forests of Tanzania
2005 - IRG/WP 05-10557
In order to manage the Tropical forest in a sustainable manner and increase the resource base for their wood industries, many Tropical African timber producing countries including Tanzania are promoting the many lesser known/used timbers in their forests as alternative sources of wood to the over-exploited primary timber species. Four lesser known/utilized timber species from the forests of Tanzan...
S A Amartey, P R Gillah, R C Ishengoma, J Gabriel, D H Kitojo


Effect of humidity and temperature on fastener withdrawal resistance from CCA and ACZA treated Douglas-fir
2000 - IRG/WP 00-20209
The effects of preservative treatment on fastener withdrawal was investigated in Douglas-fir lumber conditioned to two moisture regimes. In general, conditioning samples to 19% moisture content produced more substantial changes in withdrawal resistance of galvanized fasteners than did conditioning to 12%. Treatment had little or no effect on withdrawal resistance of stainless steel fasteners. With...
Sung-Mo Kang, J J Morrell


Biocidal property of the phenolic fraction of ethanol extractives of Hopea parviflora heartwood
1993 - IRG/WP 93-30003
Natural resistance of some species of timber to fungal decay and insect damage (particularly termite) is ascribed toxic nature and quantity of certain chemical substances present in the cell wall of heartwood. These chemical substances generally known to be Phenolic and Polyphenolic compounds (Rao 1982). Earlier investigations on extractives were mainly in relation to resistance of timber to decay...
R V Krishnan, K S Theagarajan, H S Ananthapadmanabha, M Nagaraja Sharma, V V Prabhu, H C Nagaveni


Previous Page | Next Page