IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1091 documents. Displaying 25 entries per page.


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1982 - IRG/WP 3207
J Beesley


Collaborative soft rot tests: Proposals for a standardized soil burial test
1971 - IRG/WP 201
A F Bravery


Evaluation of the effectiveness of three microbiocides in the control of sapstains
1982 - IRG/WP 3212
Results of field test on the effectiveness of BUSAN 30, CAPTAN, FOLPET against mould and sapstain in Pinus elliottii are presented. The viability of use of FOLPET in Brazil as an alternative to sodium pentachlorophenate is also discussed....
S Milano, J A A Vianna Neto


An attempt to evaluate wood resistance against fungal decay in non-sterile conditions by measuring the variation of resistance to bending test
1988 - IRG/WP 2308
The main object of this work was to determine the variation of strength on large test specimens of wood (800 x 45 x 45 mm³) when exposed to accelerated fungal attacks close to natural conditions, out of test vessels. The modulus of elasticity (MOE) and the modulus of rupture (MOR) have been assessed. Thereby, the natural resistance of the wood species to fungal decay, the efficiency of preservati...
L N Trong


The resistance of painting materials and consolidants against wood-destroying insects
1997 - IRG/WP 97-10239
Natural and synthetic adhesives, varnishes, painting materials and consolidants were used in investigations of bioresistance against newly hatched larvae and beetles of Hylotrupes bajulus (L.). Animal glues, casein, drying oils and natural resins such as dammar resin and shellac, were not resistant to attack by these larvae. Similarly, semi- and all-synthetic polymers tested including hydroxypropy...
W Unger, H Fritsche, A Unger


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


Recent soft-rot research in softwoods and hardwoods
1980 - IRG/WP 1108
The purpose of this paper is to describe briefly the current status of our research on soft-rot fungi. The work to be discussed is still in progress and any results described must be regarded as provisional....
J A Butcher


Laboratory tests on natural resistance to Cryptotermes brevis (Walker) attack of native hardwoods for crossarms production
1985 - IRG/WP 1266
Eletropaulo (Eletricidade de Sao Paulo S/A) and IPT (Instituto de Pesquisas Tecnologicas do Estado de Sao Paulo S/A) are carrying on a study to evaluate wood species for crossarms in replacement of Aspidosperma polyneuron - Apocynaceae (Peroba-rosa) traditionally used for this purpose. Nineteen Amazon wood species were elected, with physical and mechanical properties equal or better than those pre...
M D Canedo, A T De Lelis


Leaching of copper, chromium and arsenic from CCA-treated Scots pine exposed in sea water
2000 - IRG/WP 00-50149
A laboratory leaching trial combining a static and a flowing seawater system was carried out to measure the leaching rates of copper, chromium and arsenic from the surface of Scots pine panels vacuum-pressure treated to 3, 6, 12, 24, and 48 kgm-3 CCA. Untreated and treated panels were exposed in flowing seawater for up to 8 weeks followed by 2 weeks submersion in static seawater which was taken fo...
C J Brown, R A Eaton


Decay resistance of wood removed from poles treated with Trichoderma
1989 - IRG/WP 1386
Wood blocks removed from a distribution pole previously treated with a biological control product (Binab FYT pellets) were exposed in soil block tests to selected basidiomycetes. The blocks were removed from regions of poles where Trichoderma colonization had been confirmed by extensive sampling and computer mapping of microbial inhabitants. The results indicate that material from pole interiors c...
A Bruce, B King, T L Highley


Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem


Basidiosporogenesis by the white-rot basidiomycetes in vitr
1994 - IRG/WP 94-10081
Basidiospores of all forest-inhabiting basidiomycetes are a primary source of infection causing wood decay. However, most studies evaluating wood preservatives have used mycelia or basidiospores obtained from wild mushrooms. The objective of this study was to demonstrate in vitro methods that promote carpogenesis and basidiosporogenesis by the white-rot basidiomycetes, Schizophyllum commune and Tr...
S C Croan


Proposals for a vermiculite burial soft rot test method
1980 - IRG/WP 283
J G Savory, J K Carey


Preliminary attempts towards the development of a small scale termite rearing chamber. Progress report
1983 - IRG/WP 1203
The results suggest that there is no evidence that the volume of the rearing chamber plays a part in the settlement of a colony. These rearing chambers present a factor of productivity (final enumeration)/(initial enumeration) of roughly 2 after one year. 90% of the colony survived. This method of breeding can be considered as feasible and cheap....
M Argoud, J C Palla, R Sternalsky


Soft rot and bacterial decay in preservative treated eucalypt power transmission poles
1982 - IRG/WP 1155
Bacterial type decay was observed in CCA and PCP treated eucalypt power transmission poles. Detailed observations made with the SEM revealed bacterial colonisation and decay, especially in fibres. Plug samples taken from poles throughout Queensland were examined for preservative retention and presence of soft-rot decay. The severity of decay was different according to location, retention and speci...
L E Leightley


Rates of emission from CCA-treated wood in the marine environment: measurement, modelling and requirements for further research
2001 - IRG/WP 01-50166-12
Accurate estimates of rates of emission of leachate from preservative treated wood are crucial for realistic predictions of the environmental impact of its use in maritime construction. Estimates are available for some commonly used preservatives, but these vary widely. Though variable, these measurements suggest that emission generally decreases exponentially with time. Part of the variation is d...
S M Cragg, C J Brown, R A Albuquerque, R A Eaton


Rational weight per weight (w/w) qualifying retention from a pole bank in Bangladesh
2000 - IRG/WP 00-40187
Weight per weight (w/w) vs weight per volume (w/v) retention study revealed that the w/w % retention is found to be appropriate and uniform for all timber species in respect of its real effectiveness. The pole species having density below 512 kg/m3 (32pcf.) showing w/v retention below 20kg/m3 (1.25pcf.) have equal w/w retention of 4%. The apparently reduced w/v retention of low density poles will ...
A K Lahiry


Questionnaire pour la préparation de fiches monographiques pour les champignons lignivores
1972 - IRG/WP 103 F
C Jacquiot


Natural Resistance of timbers to marine borer attack. COIPM/IRG CO-OPERATION. Final report concerning panels exposed in the sea at Sekondi, Ghana
1979 - IRG/WP 449
The test was carried out according to Document COIPM/72.044, Revised procedure for the testing of naturally durable timbers against marine borers. The panels of the three species remaining in the test at the end of 1978 were removed and assessed visually. An average rating was given to the panels of each species....
F F K Ampong


Biological performance of gypsum products containing borates
2000 - IRG/WP 00-30237
At suitable retentions borates have biostatic properties enabling them to be used for biodeterioration control in wood. They provide protection against decay fungi, mould, and termites, which are known to also attack gypsum products. Currently, many gypsum products contain added borates, which are used to improve physical and processing characteristics. Work examining the effect of borates at cont...
J L Fogel, J D Lloyd


The effectiveness test of chemicals against Serpula lacrymans
1984 - IRG/WP 2222
The effectiveness tests of wood preservatives against Serpula lacrymans were conducted in accordance with Japan Industrial Standard A 9302 and Japanese Wood Preserving Association Standard No. 1. Also, the soil treatment test against this fungus was carried out with two chemicals. The preservatives tested without Creosote oil (out of JIS) had sufficient preservative effect against Serpula lacryman...
S Doi


Biological control of Serpula lacrymans using Trichoderma spp
1994 - IRG/WP 94-10069
The effectiveness, or otherwise, in killing Serpula lacrymans, of a range of Trichoderma spp. in a variety of media and using two different incubation systems has been tested. In agar based systems with normal nutrients or minimal nutrients with high or low nitrogen contents and high or low iron content Trichoderma harzianum 25 proved to be the most efficient and killing Serpula lacrymans. Other s...
A J Score, J W Palfreyman


Some thoughts on the future strategy for eradicating Serpula lacrymans from a building
1989 - IRG/WP 1405
We now have a clear view of the mechanism of translocation of nutrients in the mycelium of Serpula lacrymans which is one of the physiological processes underlying the remarkable capacity of this fungus to spread through a building. Here the elements of the mechanism of translocation are dissected out to suggest avenues which might be followed in the search for new ways for eradicating the fungus ...
D H Jennings


Collaborative soft rot tests
1981 - IRG/WP 2151
There appears to be need for reconsideration of attitudes towards Standardisation of laboratory tests for determining the toxicity of preservatives to soft rot fungi. The original approach was that a limited number of test methods were available and that collaborative effort would determine the suitability of the methods for Standardisation. It has been established so far that pure culture testing...
J G Savory


Fire resistance of Alder wood treated with some chemicals. Part II. Effect of Other Chemicals on the Combustion Properties
2002 - IRG/WP 02-40235
Samples from alder wood (Alnus glutinosa (L.) Gaertn. subsp. barbata (C.A.Mey) Yalt.) were impregnated according to ASTM D 1413-88 with boron compounds (boric acid, borax, sodium perborate), vinyl monomers (styrene, methyl methacrylate), Tanalith-CBC, Phosphoric acid, Vacsol, Immersol, Polyethylene glycole (PEG-400) and their mixed solutions of chemicals in order to determine their combustion pro...
A Temiz, Ü C Yildiz


Previous Page | Next Page