Field fencepost tests of several species treated with water-borne preservatives by rural methods
1986 - IRG/WP 3385 E
Fencepost field results in ground-contact treated by rural methods: immersion-diffusion and sap displacement by evaporation are analyzed. Copper-chrome-arsenic and copper-fluor-chrome preservatives were used in two concentrations. The wooden species studied were: Pinus pinaster, Eucalyptus globulus and Quercus rubra. For each of the test units decay index evolution was analyzed after five years ex...
M V Baonza Merino


International comparison of three field methods for assessing the in-ground resistance of preservative-treated and untreated wood to termites and fungal decay – Summary of observations after five years
2003 - IRG/WP 03-20261
Results are presented from a five-year study conducted in five locations in Australia, Thailand and the USA. Three methods of exposure were assessed (below-ground, graveyard and ground contact) for evaluating the in-ground termite and decay resistance of Pinus radiata D. Don sapwood stakes that had been vacuum pressure impregnated with CCA (Type C) and ACQ (Type D) each at two nominal retentions (...
M Lenz, J W Creffield, T A Evans, B M Kard, C Vongkaluang, Y Sornnuwat, A F Preston


Effects of the specimen position on fungal colonisation and wood decay by en 113 test fungi
1998 - IRG/WP 98-20136
For testing wood preservatives according to EN 113 it is common practice to plant the test blocks on neutral supports in order to prevent (1) a diffusion of chemicals into the agar medium and (2) an excessive moistening of the specimens. The procedure was employed in EN 350-1 for testing the natural durability of solid wood. It turned out to be of problematic nature because of the individual requ...
G Kleist, M-T Lenz, R-D Peek


Tilting and vacuum treatment - two methods to obtain a non-dripping freshly treated timber
1989 - IRG/WP 3535
Modern impregnation plants are designed to prevent spread of impregnation solutions from the plant through leakage, etc. It is also important that freshly treated timber does not spread solutions through dripping on the storage area. To prevent this, the impregnation procedure is terminated with a vacuum period. In many plants in Sweden this period is minimized or even excluded to gain time. Inste...
I Johansson, M-L Edlund


Methodologies for termiticide testing and standardization
1993 - IRG/WP 93-10043
Standardization of testing methodologies for termiticides has been one of the main topics of discussion for Working Group 1b in recent IRG meetings. While it is agreed that there is a need to provide a standardized testing procedure for industry and regulatory agencies, concerns remain that such a standardized procedure may become an obstacle for developing better testing methods or innovations in...
N-Y Su


Proposal for a method aiming at the quantification of the impact of wood extraction in Life Cycle Assessment
1998 - IRG/WP 98-50113
Life Cycle Assessment has been accepted as an instrument for the assessment of the environmental impact of products. Characterisation factors for impact assessment of emissions from products have been established. To date no characterisation factor exists for the extraction of biotic resources, for example wood. Since the main disadvantage of using wood as a material lies in the extraction of reso...
P Esser, E Van der Voet


Inter-laboratory comparison of assessment methods for wood preservatives against subterranean termites: Determination of protection threshold limits for CCA
1999 - IRG/WP 99-10317
In 1996, several institutes conducted laboratory bioassays on the efficacy of unleached Pinus radiata specimens treated with copper-chromium-arsenic (CCA) and copper naphthenate (Cu Naph) at retentions of 0.5, 1.0, 2.0 and 4.0 kg/m3 (total salt for CCA; elemental copper for Cu Naph) against a range of species of subterranean termites (IRG/WP/96-10174). Each participant employed the standard test m...
J W Creffield, M Lenz


Comparison of three methods of quantitative evaluation of sapstain in rubberwood
2000 - IRG/WP 00-20188
Assessing the extent of fungal stain on wood during laboratory trials is a subjective process and is subjected to considerable variation between individual evaluators and specimen. The purpose of this paper was to explore the potential of three quantitative methods of wood surface measurement of rubberwood specimens degraded by sapstain and mould fungui (Botrydiplodia theobromae, Aureobasidium pul...
A J Ashari, J W Palfreyman, A H H Wong


Evaluation of the permeability of fast grown wood species
1995 - IRG/WP 95-40042
The low natural durability of certain species of wood, implies the need for applying a protecting treatment to increase its life in service. Because of this, a knowledge of the permeability properties of the wood is desired. In this work, a simple and reliable method to evaluate the wood permeability is presented. For that, we have been used fast grown species, with low natural durability, Poplar ...
M T De Troya, A M Navarrete, E Sanchez, J E Garcia de los Rios, E L Rodríguez Trobajo


Screening test methods with termites as first laboratory evaluation of new active substances for wood preservation
1995 - IRG/WP 95-10135
European test methods (EN) with termites have been compared with long-standing experience from screening test methods in the laboratory of Eberswalde. The results are discussed in terms on the possibility of using screening test methods as the first laboratory evaluation of new active substances in wood preservatives. The advantages and disadvantages of these methods are considered. Only a small a...
W Unger


Observations on the destruction of fishing craft in India by marine wood-borers with special reference to the West Coast
1981 - IRG/WP 472
The paper highlights the economic importance of the destruction of fishing craft in India by marine wood-destroying agencies. The annual loss involved is to the extent of over 94 million rupees. Thirty-nine spectes and one variety of woodborer have so far been recorded from India, of which Bankia campanellata, Bankia carinata, Bankia rochi, Dicyathifer manni, Lyrodus pedicellatus, Teredo clappi, T...
L N Santhakumaran, J C Jain


Methods to determine the efficacy of three water repellent additives in waterborne preservatives
1997 - IRG/WP 97-30142
The paper describes the methods used to determine the efficacy of three different water repellent additives in waterborne preservatives. The wooden samples used are pine (Pinus sylvestris) and spruce (Picea abies) that are treated with 9 different waterborne preservatives in retention for hazard class 3 (above ground commodities). There are two sample sizes exposed, cladding boards (19 x 148 mm) w...
F G Evans, B Nossen, K M Jenssen, L R Wilhelmsen, G Fuglum


Quantification of creosote migration down wooden poles and the prevention of its depletion during flood irrigation
1994 - IRG/WP 94-50032
Polyethylene field liners heat-shrunk onto soil-contact surfaces prevented decay of creosote-treated Eucalyptus grandis vineyard poles under flood-irrigation. The present work quantified losses of creosote from these poles after six and 24 months' service. After six months' service the mean creosote retention of unlined poles above the ground line was 12.62% (m/m dry wood), with ...
M Behr, A A W Baecker


Shorter-term biological control of wood decay in pre-seasoning pine roundwood as an alternative to chemical methods
1992 - IRG/WP 92-1555
Previous studies on the long-term control of decay in creosoted transmission poles, using Trichoderma and other antagonistic moulds, have met with limited success. However, it is possible biological control is more suited to control of decay on shorter time scales. An earlier study, focusing on pre-seasoning treatment of transmission poles showed that favourable porosity increases could be brought...
M W Schoeman, D J Dickinson


Test methods for modifies wood: The EU-Thematic network approach
2002 - IRG/WP 02-20255
The last decade wood modification systems have become new wood treatment methods in Europe. Alongside several industrial initiatives for heat treatments also scaling up and pilot plant projects for chemical wood modification have recently been carried out. In 2000 an initiative to create a network related to these new developments was supported by the European Commission. Within the work proposed ...
J Van Acker, D Jones


Quantification of creosote and fluoride in remedially-treated poles
1997 - IRG/WP 97-40097
Three creosoted transmission poles were put into service in 1961 and they were subsequently remedially-treated with a proprietary fluoride remedial paste formulation in 1981. The poles were removed from service in 1996 and their ground-contact regions were analysed for creosote and fluoride contents. It was found that the poles were undecayed. Creosote retentions decreased down the profiles of the...
B P Hill


Co-operative tests concerning the influence of solvent and drying method on the toxic limit of wood preservatives against Coniophora cerebella
1972 - IRG/WP 216
In the working group II of the IRG it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discussion in the mentioned working group the final program was accepted by the co-operating institutes in 1969. In the test program two fungicides, ...
T Hof


Diagnostics methods and routes proposalsto define selective sorting of demolition wood wastes
2001 - IRG/WP 01-50177
Wood wastes are more and more often used in different wood waste valorisation industries (panels, wood energy, cement factories, ...). These industries are in progress to include in their processes, wood wastes coming from demolition wood. A state of the art and an analysis have been made to propose : (1) diagnostics methods to carry out a classification of wood wastes on demolition sites and in t...
G Labat, E Bucket, C Fréret, G Deroubaix


Methods of testing anti-stain chemicals for protecting sawn timber during storage and transport
1976 - IRG/WP 273
No international standard method for testing anti-stain chemicals for protecting fresh sawn timber exists. The methods used can be divided into three types: a) Rapid screening tests for finding chemicals effective against blue-stain and mould fungi. The chemicals are tested in agar medium, in pieces of filter paper or on small pieces of wood using pure cultures. b) Laboratory tests for evaluating ...
T Vihavainen


Leaching from field test stakes. Results from two different methods of analysis
1993 - IRG/WP 93-50013
Field test stakes treated with Boliden K33 containing copper, chromium and arsenic exposed at three different fields in Sweden and rejected due to decay, have in two studies been analysed regarding leaching and remaining preservatives. The stakes have been exposed during 20 to 43 years. The density of the stakes and content of copper, chromium and arsenic have been determined in the top part of th...
F G Evans, M-L Edlund


Evaluation of rapid methods for detecting wood preservatives in waste wood
1994 - IRG/WP 94-50024
For the disposal of wood waste under ecological sound conditions information about its hazardous potential is required. Several analytical methods are available for the detection of most elements in wood preservatives. Industrial process conditions, however, demand methods with very short turn around times. In this research several methods of analysis were judged on their speed and accuracy. A num...
W J Homan, H Militz


Survey of practical methods for conditioning of forest products before preservative treatment
1971 - IRG/WP 39
The seasoning of forest products is undertaken for a wide range of end uses and is becoming increasingly required for applications and building construction and secondary manufacturing industries. A wide range of applications of new technology and specifically required seasoning schedules is being actively developed for such requirements, but less attention has been given to the means by which woo...
J Rak, T S McKnight


Quantification of methylene bis thiocyanate in wood and its effect on a sapstain fungus Ophiostoma floccosum
2006 - IRG/WP 06-10591
The mobility and concentrations of MBT at different depths of wood billets (200 mm long, 40 mm in diameter) were determined using NMR spectroscopy and ICP-ASE, and then correlated the effect of wood MBT concentrations on growth of O. floccosum in a bioassay using stereomicroscopy and confocal laser scanning microscopy (CLSM). The 13C NMR spectra showed the presence or absence of MBT in wood but w...
T Singh


Termite Response to Oil-Heat-Treated Norway spruce, Scots Pine and Eucalyptus Wood
2006 - IRG/WP 06-20325
The work here presented focused on the behaviour of subterranean termites (Reticulitermes grassei Clément) towards Oil-Heat-Treated (OHT) Norway spruce (Picea abies L.), Scots pine (Pinus sylvestris L.) and eucalyptus (Eucalyptus globulus Labill) wood, with a particular interest in the development of simple methods adequate to study the resistence of these materials to termite attack. Small test ...
L Nunes, T Nobre, C Welzbacher, A O Rapp


Re-sealing cut ends of envelope-treated softwood framing timber to protect against damage by the Australian subterranean termite Coptotermes acinaciformis: A revisitation
2006 - IRG/WP 06-20335
The claim that Australian Coptotermes acinaciformis (Froggatt) do not appear to initiate damage on timber from the end grain, thereby negating the need for treating exposed cut ends of softwood framing material (35 ? 90 mm) which has a repellent Tanalith? T envelope, was further investigated. Specimens of commercial Pinus radiata D.Don framing timber (untreated) and Pinus elliottii Englem. (untrea...
B C Peters, M Lenz, J W Creffield