IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1096 documents. Displaying 25 entries per page.


Laboratory test of some formulations against stain and mould fungi isolated from bamboo wood
2009 - IRG/WP 09-30508
To screen the effective anti-mould formulations, fungicides such as carbendazim, tebuconazole, fludioxonil, difenoconazole, prochloraz, benomyl and 8-hydroxy-quinoline copper (copper oxine) were selected to conduct the laboratory test of fungicidal activity by method of inhibition zone against Botryodiplodia theobromae Pat., Fusarium sp., Alternaria tenuis Nees., Penicillium purpurogenum Stoll, Tr...
Xingxia Ma, Airui Sun, Mingliang Jiang, Daochun Qin


The Form of Copper: Does It Really Matter?
2009 - IRG/WP 09-30513
In recent years, several micronized copper formulations for lumber treatment have supplanted the solubilized copper formulations that in turn replaced CCA after its voluntary relabeling in 2004. The micronized or dispersed copper systems use finely ground but solid copper particles and deposit those particles within the wood framework. In contrast, copper in the soluble formulations is relativel...
C R McIntyre, M H Freeman, T F Shupe, Q Wu, D P Kamdem


Synthesis of a rosin amide and its resistance to wood decay fungi
2009 - IRG/WP 09-30517
Rosin was reacted with diethyltriamine (DETA) after being modified by acryl acid with the weight ratio of 4.5:1 and a rosin amide (RA) derivative was produced at the conditions as follows: modified rosin and DETA mole ratio of 1:3.5, dimethylbenzene as water carrying agent, reaction temperature of 160-180°C, and reaction time of 8h. The chemical structure of the product as RA was identified by F...
Shuangyue Li, Shujun Li, Jing Wang


Effect of extractives on durability of Prosopis juliflora heartwood
2009 - IRG/WP 09-30518
The heartwood of Prosopis juliflora is resistant to fungal attack caused by different brown and white rot fungi. This durability due to the presence of high amounts of extractives decreases after extraction of these latter ones with different solvents. Heartwood extractives were effective in inhibiting the growth of the fungi. Depending on the concentration used, development of the fungal mycelium...
P Sirmah, K Iaych, B Poaty, S Dumarçay, P Gérardin


Biological Treatment to Improve Wood Product Quality and Durability - Fifteen Years of Effort and Experience at FPInnovations-Forintek Division
2009 - IRG/WP 09-40444
Wood plays an important role in the world economy. However, wood is subject to attack from wood-degrading fungi and insects and durability and quality of wood products are becoming increasing concerns for consumers. Development of effective and low environmental impact technologies to improve wood product quality and durability will be required to address these concerns. The application of a bio...
Dian-Qing Yang


Assessment of decay risk of airborne wood-decay fungi
2012 - IRG/WP 12-10787
The decay risk of airborne wood-decay fungi was investigated by using an air sampler. Japanese cedar disks measuring about 8 cm in diameter and 3 mm in thickness with moisture content at about 100 % were placed in a “BIOSAMP” air sampler and exposed to 1000 liters of air. Air sampling was carried out from June to September at the same sampling site in Tsukuba, Japan. The exposed disks were the...
I Momohara, Y Ota, K Sotome, T Nishimura


The resistance of thermo-oil modified wood against decay and mould fungi
2009 - IRG/WP 09-40448
Thermally modified wood in comparison to natural wood demonstrates some advantageous functional properties like decreased hygroscopicity, higher dimensional stability. It also has increased durability and improved resistance to fungal decay. However thermal modification of wood may lead to reduced strength properties what may limit the use of wood in mechanically beared constructions. The changes ...
A Fojutowski, A Kropacz, A Noskowiak


Which are the best painting methods for the beech wood products protection?
2009 - IRG/WP 09-40477
Beech wood (Fagus Sylvatica L.) is one of the most important species of the wood in Kosovo. About 33% of the trees in our country are beech wood. The wood products in Kosovo are from the beech wood. The color difference between red heart wood and white wood of the beech is significant. The main problem for the wood companies in our country is that they haven’t adequate protection against weather...
A Bajraktari


Future Directions in Wood and Engineered Wood Products Research in China
2009 - IRG/WP 09-40479
This paper has summarized the research advance of basic wood science and engineered wood products in the 20th century in China and introduced the research advance and directions of basic wood science, engineered wood products and the extensive researches based on the basic wood science such as wood chemical rheology, wood fractal analysis, wood environmental science and nano-wood material etc in t...
Guangjie Zhao


Sensitivity to Copper of Basidiospores from Copper Tolerant Fungi: Fomitopsis palustris and Oligoporus placentus
2010 - IRG/WP 10-10707
Copper continues to be an important fungicide in wood preservation. It is the primary component of the preservatives that have replaced chromated copper arsenate for treated wood in residential construction in North America. However, a co-biocide is normally needed to protect against copper tolerant organisms. Previous work has shown that the spores of at least one copper tolerant fungus, Oligopo...
C S Woo, P I Morris


The invasion channels of damage fungi in bamboo lumber
2010 - IRG/WP 10-10712
The micro-agents on bamboo lumber damage are mould, stain, and decay fungi. This research is about invasion channels of bamboo lumber damage fungi by scanning electron microscope (SEM). The results showed that the conidia of mould were only accumulated on the surface of bamboo and no hyphae detected in bamboo vascular bundle, and hyphae of stain penetrated into bamboo and grew in metaxylem vessel...
Xingxia Ma, Mingliang Jiang, Daochun Qin


Qualitative - Quantitative Analysis of Wood-Inhabiting Fungi in External Wooden Structures of the Latvian Cultural Heritage
2010 - IRG/WP 10-10728
The frequency and diversity of wood inhabiting fungi in the exterior wood were established in the Araishi lake fortress, the Lielvarde wooden castle, the Latvian Ethnographic Open-Air Museum, Riga, and twelve wooden heritage objects in the Eastern part of Latvia (Latgale). The inspected wooden structures of the external woodwork included windows, stairs, walls, floorings, roofs, fences, and benche...
I Irbe, M Karadelev, B Andersons


Early detection of colonisation by blue stain and mould on modified wood using PCR technique
2010 - IRG/WP 10-10730
The aim of this research was the early detection of fungal attack on the surfaces of modified and unmodified wood after natural weathering. The investigation was carried out by molecular techniques and the development and establishment of genus/species specific PCR for important moulds and sapstain fungi was part of this work. After adaption of the method, a monitoring of the succession of Ascomyc...
A Steitz, B Schmöllerl, N Pfabigan, S Bollmus, G Grüll


Glutathione transferases as functional biomarkers of wood degradation?
2010 - IRG/WP 10-10735
The recent release of several fungal genome sequences allows the report of an overview of fungal glutathione transferases (GSTs) focused on their function in the wood-degrading basidiomycete Phanerochaete chrysosporium. A genomic and phylogenetic analysis of GST classes in various sequenced fungi –zygomycetes, ascomycetes and basidiomycetes- revealed some specificity in GSTs distribution, in com...
E Gelhaye, M Morel


The brown rot of oak wood submerged for 6 months in the Baltic sea
2010 - IRG/WP 10-10736
The natural wood submerged or partially immersed in sea water is commonly affected by certain microorganisms. The bacteria and marine borers that decay the wood totally submerged in sea water and above sea level other microorganisms as fungi, algae, insects may attacked wood. The sea water may affect and change the properties of wood. We have tried to determine the susceptibility to decay caused b...
A Fojutowski, A Kropacz, I Pomian


Natural durability of Mulberry wood from Iran
2010 - IRG/WP 10-10737
Mulberry wood (Morus alba L.) is traditionally used in Iran to manufacture music instruments such as tar and setar. But little is know and contradictory statements are found on the natural durability of Morus alba. Moreover, in many cases, Iranian instrument makers leave freshly cut Mulberry timber into water (cold or hot) for a time period depending on the craftsman habit, without any real knowle...
A Se Golpayegani, M-F Thevenon, J Gril, K Pourtahmasi


Methods for Studying Penetration Depth of Wood Protection Products
2010 - IRG/WP 10-20432
EN 152 is an accepted standard in Europe for measuring how deep a wood protection product penetrates into the surface of treated pine wood. The method has provided consumers with a wide assortment of products that meet the specifications outlined in the standard. Because the test takes 8 or more months to carry out, artificial ageing procedures have evolved in order to standardize and speed up the...
K Hansen, L Sites, D D Nicholas


Detection of Wood Destroying Fungi Using DNA Microarray Technology
2010 - IRG/WP 10-20435
Wood decay fungi of the phylum Basidiomycota cause serious damage to wooden constructions and building elements. The elimination and the appraisement of fungal decay require an assured species identification. Conventional fungal diagnostics are mainly based on morphological characteristics by macro- and microscopy analysis. For some years, standardised and highly sensitive molecular methods focuss...
K Jacobs, N Rangno, W Scheiding, B Weiss, D Müller, C Hiller, W Brabetz


Profiling fungal community in wood decay ecosystem by Denaturing High-Performance Liquid Chromatography
2010 - IRG/WP 10-20443
A DNA-based fingerprinting technique, Denaturing High Performance Liquid Chromatography (DHPLC) was developed to profile fungal communities colonizing indoor timber. Molecular fungal diversity was assessed using amplification based on the Internal Transcribed Spacer (ITS1) rDNA of 74 wood samples collected from infected buildings in France. Due to its high sensitivity, the PCR-DHPLC technique was ...
S Maurice, G Le Floch, M Le Bras-Quéré, J P Rioult, G Barbier


DNA-based tools for rapidly detecting, quantifying and monitoring ophiostomatoid fungi on beetles, in trees and wood products
2010 - IRG/WP 10-20450
Approximately half of the trees harvested for commercial purposes are lost because of native or introduced insects or insect-vectored microorganisms. Ophiostomatoid fungi, which are well adapted to dissemination by insects, include ~140 species of saprobes and pathogens. They are present worldwide, have high economical impact and many are subject to quarantine regulation. Thus, it is necessary to ...
L Khadempour, Young Woon Lim, S Massoumi Alamouti, C Breuil


Drying Rates and Mold Growth on Various Building Materials under Different Environmental Conditions
2010 - IRG/WP 10-20454
Mold growth on building materials is a major problem for homeowners. The most suitable method to control mold growth on building materials is to utilize design features, construction tools and practices that prevent moisture accumulation, and keep the wood as dry as possible. In order to achieve this, engineers and homebuilders have to know the effects of various temperature and moisture conditi...
Dian-Qing Yang


Effects of Cunninghamia Lanceolata Heartwood Extracts on the Growth of Wood Decay Fungi
2010 - IRG/WP 10-30527
China-fir (Cunninghamia lanceolata) wood is well known for its good durability. This species is native to China and has been extensive planted there. Mainly, extractives are responsible for the wood resistance to decay fungi. In this paper, the extractives of China-fir heartwood were studied for their effects on various wood decay fungi. Sequential extraction of heartwood in hexane, ethyl acet...
Shujun Li, Jing Wang, Jian Li


Evaluation of ACQ-D treated Chinese fir and Mongolian Scots pine with different post-treatments after 20 months of exposure
2010 - IRG/WP 10-30530
The performance of alkaline copper quat-type D (ACQ-D) treated Chinese fir (Cunninghamia lanceolata Hook.) and Mongolian Scots pine (Pinus sylvestris Linn. var. mongolica Litv.) stakes after 20 months exposure in Chengdu and Guangzhou of southern China were evaluated according to AWPA standard E07-07. The ACQ-D treatments used two concentration levels (0.5 and 1.0%) and four different post-treatme...
Lili Yu, Jinzhen Cao, Wei Gao, Haitao Su


Antifungal Essential Oil Metabolites
2010 - IRG/WP 10-30531
New environmentally-friendly wood protection systems based on “green” technologies are needed to inhibit wood-inhabiting mold and decay fungi. Utilizing bioactive essential oils from select herbaceous plants is one promising approach, but the concentrations of bioactive compounds are somewhat variable even in the highest (therapeutic) grade essential oils. Purified primary metabolites from fou...
C A Clausen, B M Woodward, V W Yang


Degradation of Carbon-Based Preservatives by Black-stain Fungi
2010 - IRG/WP 10-30533
Some black-stain fungi are known to exhibit resistance to carbon-based preservatives. However, the cause of this resistance is unclear. The fungi may have mechanisms to tolerate these chemicals, or they may be able to degrade and detoxify them. Fungi capable of degrading carbon-based preservatives are of interest for possible bioremediation of carbon-based preservative-treated wood at the end of i...
R Stirling, P I Morris