Decay patterns observed in butylene oxide modified ponderosa pine attacked by Fomitopsis pinicola
1983 - IRG/WP 1183
Small blocks of ponderosa pine chemically modified by butylene oxide to three different weight percent gains (WPG) were decayed for 2 months with the brown rot fungus Fomitopsis pinicola. Wood substance loss and the type of decay pattern recognised were fairly similar both for control and blocks treated to 8 and 15 WPG. No difference in attack was observed between radial or tangential walls in lat...
T Nilsson, R M Rowell


Extracellular layers of wood decay fungi and copper tolerance
1983 - IRG/WP 1180
Extracellular layers around the hyphae of brown, white and soft rot fungi have been examined using electron microscopy. These layers were isolated for identification. Particular interest was directed towards the extracellular layers of copper-tolerant soft rot fungi....
D M Francis, L E Leightley


On the problem "House Longhorn Beetle" in hardwoods and an aid to distinguish between Hylotrypes bajulus and Hesperophanes cinereus larvae
1981 - IRG/WP 1141
S Cymorek


Report on Sub-group 5 in Raleigh, 6 May 1980
1980 - IRG/WP 1123
S Cymorek


Decay in external joinery in the United Kingdom
1978 - IRG/WP 3116
no abstract available...
J G Savory, J K Carey


United States Federal Committee on Wood Protection
1971 - IRG/WP 43
A C Jewett


Proposed test procedure to determine the effect of timber substrate on the effectiveness of a copper/chrome/arsenic preservative in seawater
1975 - IRG/WP 411
R A Eaton


Reliability-based service life prediction methodology for assessment of water protection efficiency for coatings on wood
2003 - IRG/WP 03-20268
Assessment of water protection efficiency according to EN 927-5 has been shown to give significant differences in water absorption values for different types of coatings on wood. It is shown that the combination of EN 927-5 and an artificial weathering procedure gives more information regarding expected durability and long-term performance than a single measurement of water absorption on fresh, un...
J Ekstedt


Tentative method of testing wood preservatives against blue staining
1977 - IRG/WP 259
The blue stain of sawn wood is still a real problem in Poland. Although a preservative based on sodium orthophenylphenoxide has been introduced into sawmill practice, and the technology of wood protection developed with it, new information has been obtained concerning blue stain in wood material destined for export. In order to select new chemicals or to improve the effectiveness of the ones in cu...
E Tarocinski, O Lewandowski, M H Zielinski


Natural durability and basic physical and mechanical properties of secondary commercially less accepted wood species from Brazil
2002 - IRG/WP 02-10451
The natural durability towards basidiomycete fungi and termites of several secondary timber from Brazil (Vatairea sp., Hymenolobium sp., Inga sp., Manilkara sp., Caryocar sp., Terminalia sp., Apuleia sp.) has been evaluated according to the EN 350-1. Some basic physical and mechanical properties (density, shrinkage, hardness, colour, static strength in flexion and compression) were also measured a...
M-F Thévenon, A Thibaut


Some wood-destroying Basidiomycetes. Volume 1 of a collection of monographs
1981 - IRG/WP 1121
One of the first tasks of the International Research Group on Wood Preservation, when it began its work in 1969, was to compile a series of reports on the common decay fungi which can attack wood. This volume, which contains the first of these reports, has been compiled with the help of mycologists and wood preservation specialists in France, Ghana, the Federal Republic of Germany, the Netherlands...
R Cockcroft


Marine borers as wood degraders in Bangladesh and their protection
1996 - IRG/WP 96-10186
Field study on timber piles used in Bangladeshi brackish waters revealed that untreated and pentachlorophenol treated piles drastically degraded by the attack of molluscs and pholads (marine borers). Adequately CCA-C impregnated (30 kg/m³ or 6% W/W dry oxide retention) timber piles can protect the attack of molluscs. It is very difficult to protect pholads which can invade naturally very durable ...
A K Lahiry


Recent names for some common decay fungi
1976 - IRG/WP 143
A Käärik


Marine borers and marine wood protection - Some answers and some outstanding questions - A comment
1990 - IRG/WP 4163
A brief description of the nature of hazards encountered in different parts of the marine environment is given. An attempt is then made to assess what were the essential findings of selected areas of research in the marine wood protection field and what still needs to be done. That is, if we are to more adequately understand what we are attempting to do in this field of study!...
J E Barnacle


Model questionnaire for preparation of monographic cards for wood-destroying fungi
1972 - IRG/WP 103
C Jacquiot


The role of communication in the field of environment protection: A case study "Wood Protection"
1990 - IRG/WP 3574
L Wöss


A preliminary report on lignicolous marine fungi in the Java Sea, Indonesia
1982 - IRG/WP 488
This report is part of a study on the natural durability of Indonesian timbers against marine borers conducted in Pari Island waters, Java Sea (Suhirman and Eaton, 1981), and contains preliminary information which has not yet been published....
Suhirman, R A Eaton


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


Report of an investigation of damage by wood ants in buildings in Sweden
1976 - IRG/WP 148
Wood ants in buildings occur everywhere in Sweden, particularly in maritime districts and in vicinity of larger lakes. The damage caused by Camponotus herculeanus does not differ from that caused by Camponotus ligniperda. The former occurs in all Sweden, the latter only in southern Sweden. The damage is to be found almost exclusively in dwelling houses (week-end cabins and "all-the-year round" hou...
V Butovitsch


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


Effect of sterilization method on germination of spores of wood decay fungi observed by contact agar block method
1978 - IRG/WP 2117
Previous studies of germination of spores of wood decay fungi on wood have generally concluded that method of wood sterilization has little significant effect on germination response. This study expands the numbers of test fungi as well as number of sterilization methods employed to determine the influence of sterilization method on spore germination response of decay fungi. Germination was assess...
E L Schmidt, D W French


Monographic card: Coniophora puteana (Schum. ex Fr.) Karst. (Second draft)
1978 - IRG/WP 171
A Käärik


Final draft of a monographic card for Pole Fungus A, L Harmsen, Rigidoporus vitreus (Fr.) Donk according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 178
L Harmsen


Non-enzymatic Gloeophyllum trabeum decay mechanisms: Further study
2001 - IRG/WP 01-10395
Information will be presented on the mechanisms involved in, and potential application of, non-enzymatic wood decay by brown rot decay fungi. Specifically, the hypothesized role of low molecular weight phenolate derivatives will be discussed in relation to non-enzymatic degradation of wood. The mechanism of binding of iron by cellulose, and binding and reduction of iron by fungal derivatives and m...
B Goodell, J Jellison


Characterisation of growth and stain of different groups of sapstain fungi on lodgepole pine
1999 - IRG/WP 99-10326
Canada is the world's largest exporter of softwood lumber. These softwood shipments are susceptible to a variety of wood-inhabiting fungi that can lead to sapstain discolouration, which in turn decrease the product value. Furthermore, the presence of these microorganisms may be unacceptable to the importing countries. The objective of this work is to assess the sapstaining capability and ...
C Fleet, C Breuil, A Uzunovic, A Byrne