IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3223 documents. Displaying 25 entries per page.


Organic nitrogen in wood: Growth substrates for a sapstain fungus
1993 - IRG/WP 93-10019
The nitrogen content of mature wood from lodgepole pine was 0.046% as determined by micro-Kjeldahl. Low molecular weight proteins between 14 and 21 kDa were identified in mature wood, branch wood and sap pressed from wood chips. Amino acids were quantified in acid-hydrolyzed wood samples and accounted for between 19 and 35% of the nitrogen in wood. The sapstaining ascomycete Ophiostoma piceae stra...
L D Abraham, C Breuil


Biological control of wood decay
1992 - IRG/WP 92-1531
This paper provides a general discussion of the principles underlying the concept of using biological control agents for the protection of wooden materials from decay. The rationale for the current upsurge in interest in biological control is discussed and a critical appraisal of the technology compared with the use of chemical wood preservatives is included. The advantages and limitations associa...
A Bruce


Diffusion modeling of inorganic wood preservative leaching in service
2005 - IRG/WP 05-50224-5
To evaluate the potential environmental and health implications of leaching of inorganic wood preservatives in service under different conditions, there is a need for a predictive model that provides estimates of the rate and extent of leaching over a wide range of product dimensions and exposure conditions. In this paper, we show that the leaching behavior of inorganic preservative components fr...
L Waldron, P A Cooper, Y T Ung


The use of natural and synthetical tannins to improve the dimensional stability and durability of beechwood (Fagus sylvatica)
1993 - IRG/WP 93-30016
Synthetical tannins and natural extractives of oak, spruce and chestnut have been combined with different fungicides to make the wood more dimensionally stable and more durable. The anti-shrink-efficiency and the improvement of the durability of different synthetical and natural tannins have been evaluated. The results make clear, that an application of the mentioned agents for common use cannot b...
H Militz, W J Homan


Investigation of extracellular mucilaginous material in some wood decay fungi
1996 - IRG/WP 96-10188
The external morphology of the extracellular mucilagenous material (ECM) produced by Coriolus versicolor and Coniophora puteana during colonization of Scots pine and beech was studies using SEM. Specimens were examined in the frozen hydrated, freeze-dried and critical point dried state. All technics produced artefacts but the ECM was best preserved when examined the frozen hydated state. Critical ...
A R Abu, D J Dickinson, R J Murphy


Evaluation of the insecticidal efficacy of deltamethrin and the fungicidal efficacy of its association with TCMTB + MBT in the field of wood preservation
1986 - IRG/WP 1289 E
Deltamethrin possesses many advantages for the insecticidal protection of wood: relatively low toxicity, very reduced evaporation, very prolonged retention in the wood, very slight leaching after having penetrated the wood, and absence of odour. Its association with other active agents or solvents is being studied with regard to chemical compatibility. Compatibility studies have proved positive fo...
J S Duguet


Estimates of wood-consumption rates by termites
1983 - IRG/WP 1201
Effects of 2 components; termite-biomass and experiment duration on estimates of wood-consumption rates (mg wood/g termite/day), were examined. Three models; (1) no mortality, (2) linear mortality and (3) nonlinear mortality were used to calculate mean standing-crop biomass of termites. Model (1) predicted a significantly lower wood-consumption rate than those based on models (2) and (3). No signi...
N-Y Su, J P La Fage


Silicon tetrachloride: A potential wood preservative
1980 - IRG/WP 3133
In its present form, this paper is a preliminary draft of a paper that will eventually be submitted for publication in the Forest Products Journal. We are continuing the work on the effects of silicon tetrachloride on wood and expect to have additional data for the meeting in May 1980. Specifically we are measuring the penetration rate and depth of SiCl4, and we are chemically analyzing the treate...
C W Owens, W T Shortle, A L Shigo


Serial techniques for producing fire-retardant wood products
1997 - IRG/WP 97-30127
A series of techniques including fire-retarders denoted by WFR-1, WFR-2. WFR and their applications in producing fire-retardant wood (WFR wood), fire-retardant plywood (WFR plywood), fire-retardant particleboard (WFR particleboard) and fire-retardant MDF (WFR MDF) were investigated The fire retarders were low toxic, decay resistant and less leachable. The treated wood and WFR panels were of excell...
Zhu Jia Qi, Liu Yan Ji, Gao Chao Ying


Characteristics and quantity of impregnated wood waste in Germany
1995 - IRG/WP 95-50041
The disposal of wood waste in Germany is one of the main problems not only for the wood preservation industry but also for all concerned with wood waste. Data on characteristics and quantity of wood waste are still needed. Based on criterions given in a previous paper (IRG/WP 93-50006), several assortments have been characterized with regard to their hazardous potential and their logistical aspect...
A Voss, H Willeitner


Estimation of mycelial biomass by determination of the ergosterol content of wood decayed by Coniophora puteana and Fomes fomentarius
1989 - IRG/WP 1415
The mycelial biomass of fungi decomposing wood materials may be estimated by the use of an ergosterol assay technique.ln decay tests, essentially according to EN 113, estimates made by HPLC analyses on wood decayed by Coniophora puteana and Fomes fomentarius show the increase in biomass in the wood blocks. The ergosterol contents were correlated with dry weight loss determinations. Degradation of ...
K Nilsson, J Bjurman


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Ten Year Marine Borer Exposure Trial of Chlorothalonil and Emulsified Preservatives in Australia
2003 - IRG/WP 03-30314
Results of a ten-year marine exposure trial at Townsville and Port Stephens are presented. Sawn Pinus radiata and natural round Eucalyptus obliqua specimens were treated with preservatives including creosote (HTC), pigment emulsified creosote (PEC), chlorothalonil, and the oil emulsions of CCA called PROCCA and HYCON. Basic zinc chloride treatment was also exposed at Townsville. Some of the findin...
L J Cookson, D Scown


Targeted inhibition of wood decay fungi: degradation of cotton cellulose
1999 - IRG/WP 99-10321
Brown-rot decay is responsible for 80% of the damage and replacement of wood in service. For nearly thirty years, researchers have postulated a one-electron oxidase system combining Fe+2 oxalic acid, and H2O2 in the production of hydroxy radicals which ultimately oxidize cellulose in situ. Recently, researchers have been investigating antioxicants, in combination with biocides (Schultz, et al.,199...
F Green III, T A Kuster


Microemulsion formulations for wood protection chemicals
1993 - IRG/WP 93-30030
A microemulsion is a thermodynamically stable oil-water dispersion system. As a formulation it provides many unique features such as water compatibility for water-insoluble chemicals, formulation stability, good bioavailability and environmental acceptance. This paper discusses the major criteria for the formulations of water-insoluble wood biocides and the comparison in properties between convent...
Bing Yu, L E Leightley


Field fencepost test of several species treated with water-borne preservatives by rural methods
1986 - IRG/WP 3385
Fencepost field results in ground-contact treated by rural methods: immersion-diffusion and sap displacement by evaporation are analyzed. Copper-chrome-arsenic and copper-fluor-chrome preservatives were used in two concentrations. The wooden species studied were: Pinus pinaster, Eucalyptus globulus and Quercus rubra. For each of the test units decay index evolution was analyzed after five years ex...
M V Baonza Merino


Microwave modification of wood properties - Improvements in wood permeability
2000 - IRG/WP 00-40181
A new method of microwave (MW) wood modification is described. Microwave irradiation of timber provides an improvement in wood permeability mainly in the radial and longitudinal directions. This is achieved by physically modifying ray cells and forming a large number of cavities in the radial - longitudinal planes. More extensive MW irradiation of different species transforms the wood into a new m...
G Torgovnikov, P Vinden


Site characteristics impacting historic waterlogged wood: A review
2000 - IRG/WP 00-10344
Survival of waterlogged wood from hundreds and in rare cases millions of years presents scientists with a unique opportunity to examine wood specimens which, due to select properties of the wood itself and/or the depostional environment, have not been completely degraded. Although degradation patterns of various types of microbial wood decay have been studied in detail, the site parameters of the ...
B A Jordan, E L Schmidt


Influence of variable lignin content amongst hardwoods on soft-rot susceptibility and performance of CCA preservative
1982 - IRG/WP 1151
This paper presents the outline of an argument, based on both new and established data, which relates varying lignin content to variation of soft-rot susceptibility between hardwood species and of performance of CCA preservatives in controlling soft-rot. Although more data need to be generated to prove this relationship, sufficient evidence exists for the hypothesis to be given close attention, pa...
J A Butcher, T Nilsson


Determination of the amine to copper ratio remaining in wood after leaching
2002 - IRG/WP 02-30285
The effectiveness of the protection and the environmental impact of the treated wood are two of the most important aspects that need to be understood for all preservatives. Both are particularly influenced by the loss of biocidal components from treated wood. For amine copper preservatives, copper fixation determines the leaching resistance of the copper and amine compounds formed in wood. Previou...
N Lucas, J N R Ruddick


Wood preservative potential of fractions of wood pyrolysis tar made from Japanese larch
1996 - IRG/WP 96-30102
Wood pyrolysis tar, which was discharged as a waste by-product in the production of charcoal from Japanese larch (Larix leptolepis), was separated into several fractions by solvent extraction using tetrahydrofuran, benzene and aqueous alkali. The fractions obtained were physico-chemically characterized and examined for wood preservative potential. This separation method compared favorably with fra...
T Suzuki, S Doi, M Yamakawa, K Yamamoto, T Watanabe, M Funaki


Proposal for a simple methodology for the evaluation of the preventive effectiveness of protectors applied in superficial treatments against basidiomycetes fungi
1999 - IRG/WP 99-20167
Due to the considerable effect that the relation between the lateral surface and the volume of wood blocks has on superficial treatments, this work has attempted to determine the ideal size which allows to evaluate the effectiveness of a preservative in the shortest possible time. Three wood blocks of different dimensions were tested. In addition, as it is necessary to neutralise the effect of the...
M T De Troya, A Navarrete, F Rubio, M Yuste, C Rodríguez-Borrajo, D Muñoz-Mingarro, F Llinares


The treatability of five Indonesian wood species with BFCA preservative
1987 - IRG/WP 3428
This paper deals with a preliminary study on the treatability of five Indonesian wood species, i.e. Altingia excelsa (AE), Rhodoleria teysmanii (CA), Litsea odorivera (LO), Schima wallichii (SW) and Cratoxylon arborescens (CA). Wood samples measuring 4 x 4 x 100 cm³ were dipped into BFCA preservative solution for about 30 seconds. Preservative penetration and the surface area of treated zone were...
Nana Supriana, T K Waluyo


Previous Page | Next Page