Surface color and roughness characteristics of medium density fiberboard (MDF) panels treated with fire retardants
2008 - IRG/WP 08-40420
The objective of this study was to determine surface characteristics and color change properties of Medium Density Fiberboard (MDF) treated by fire retardants (FR) with 10% concentration. Experimental panels were made using by melamine ureaformaldehyde (MUF) adhesive having 10%, 15%, 20% of melamine. The surface properties of the samples were determined using a fine stylus technique. Three roughn...
D Ustaömer, M Usta, S Hiziroglu


Leachability of Arsenic, Chromium and Copper from Weathered Treated Wood
2008 - IRG/WP 08-50255
The objective of this study was to quantify the loss of arsenic, chromium and copper from weathered treated wood under normal field conditions as most residential structures currently in service in the U.S. have been constructed at least 3 years ago. For comparison, leaching from different retention levels of weathered CCA treated wood (low, medium and high) is compared to leaching from new ACQ tr...
A R Hasan, Ligang Hu, H M Solo-Gabriele, Yong Cai, L A Fieber


Field Tests of naturally Durable North American Wood Species
2008 - IRG/WP 08-10675
There has been little field test performance data published on North American naturally durable species in general, and no published data on second growth material in particular. Yellow cedar (Callitropsis nootkatensis), western red cedar (Thuja plicata), eastern white cedar (Thuja occidentalis), and three wood species reputed to be moderately durable were installed in ground-contact (stakes) an...
P E Laks, P I Morris, G M Larkin, J K Ingram


Wood Decay Research Using Molecular Procedures, What Can It Tell Us?
2008 - IRG/WP 08-10678
There are many unanswered questions in wood decay and protection research, and no single research technique will ever answer all of these questions. The process of wood decay is a very complex series of biochemical and chemical reactions that are heavily influenced by the hundreds of bacterial and fungal species found on environmental samples of wood. There are a variety of molecular techniques b...
S V Diehl, M. L Prewitt, Young-Min Kang, L Mangum, J D Tang


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


Above Ground Field Testing – Influence of test method and location on the relative performance of various preservative systems
2008 - IRG/WP 08-20393
Standardized above ground tests such as the lap-joint or test deck methods can be very slow in producing useful information on the relative performance of wood preservative systems. It often requires many years for decay to develop in wood treated to sub-optimal concentrations of standardized preservatives, making relative comparisons of performance between new systems and established preservativ...
A Zahora


Effectiveness of MOQ® OX 50 (CCB-Oxide) wood preservative – Part 2: Field tests
2008 - IRG/WP 08-30483
MOQ® OX 50 is a chromated copper borate preservative known around the world as CCB. In Brazil, this product is the only CCB-oxide type preservative with fungicide and insecticide properties registered at the Brazilian Institute for the Environment and Renewable Resources (IBAMA) that complies with the requirements of the Brazilian and European markets for preserved wood. For over five decades, s...
A Gandolfi Jr, C Salvela, D R Macedo, J M Vidal


Polymeric Betaine as a Wood Preservative
2008 - IRG/WP 08-30487
Didecyl polyoxyethyl ammonium borate (DPAB), also known as Polymeric Betaine, was developed as a co-biocide for chromium-free copper based wood preservatives in Europe in the 1980’s. This paper summarizes the properties of DPAB as a wood preservative. Unique properties related to the betaine nature of DPAB are discussed in terms of the structure-property relationship. Physical properties of D...
H Härtner, S Schmitt, Futong Cui, H M Barnes


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Laboratory Studies on Copper Availability in Wood Treated with Soluble Amine Copper and Micronized Copper Systems
2008 - IRG/WP 08-30489
A laboratory method has been employed to investigate the level of soluble copper in wood treated with various copper-based preservative systems, such as micronized copper (particulate copper) and amine copper solutions. This report describes the methodology and preliminary results on determination of the soluble copper in the treating solutions and the treated wood by these systems, as well as th...
L Jin, P Walcheski, A Preston


Performance of dip and pressure treated wood in termite ground proximity exposures in Hilo, HI, and Colombia
2008 - IRG/WP 08-30491
A number of preservative systems were evaluated for their ability to control termite attack when applied as both dip and pressure treatments. With dip treatments, better performance was observed with southern pine than spruce-pine-fir using the same solution strength treatment, probably as a result of the about 50% greater uptake with southern pine and associated deeper preservative penetration. B...
P Walcheski, A Zahora


Alkaline copper treated wood for use in residential decking
2008 - IRG/WP 08-30490
Alkaline copper quaternary ammonium compound (ACQ) treated decking was exposed in a field experiment and the mobile copper assessed based on that collected in the leachate. The amount of copper which leached was modeled after 4 years. The results showed that boards which leached most chemical initially provided the greatest loss over four years. The reduction in the mobility of copper with time wa...
J N R Ruddick


High Temperature Treated Wood
2008 - IRG/WP 08-40429
High temperature can modify internal structure and physic-chemical properties of wood by a controlled pyrolysis process. Such treatment, among other changes in properties, modifies the wood color in a way that resembles exotic species, increasing its market value. The main objective of this work is to determine the changes in wood properties caused by the effect of temperature and time, in order t...
C C Borges, A L Barbosa, R Faber de Campos, S T Targas


Field Stake Performance of Parallel Strand Lumber Treated with Waterborne Copper Naphthenate
2008 - IRG/WP 08-40435
Wood and wood products have been considered a premium building material for residential and industrial structures for many centuries. More recently, structural composite lumber (SCL) products have played an increasing role in satisfying the needs of the building industry. However, both wood and wood composites are naturally biodegradable materials which require enhanced durability when used in ce...
G P Merrick, M H Freeman, J A Brient


Corrosion of fastener and connector in contact with alkaline copper treated wood – it is a problem
2008 - IRG/WP 08-40437
For many decades, chromated copper arsenate (CCA) was the most common wood preservative used in North America for residential and industrial applications. Since December 31, 2003, the use of CCA for residential application was voluntarily terminated. One of the most widely accepted alternative wood preservatives in Western Canada is Alkaline Copper Quaternary Compound (ACQ). This paper will compar...
J N R Ruddick


Opportunities and Needs with Treatments for the Protection of Plantation Species
2008 - IRG/WP 08-40438
The future of the wood treating industry lies increasingly on the treatment of wood derived from plantation forests. Plantation softwoods and hardwoods both provide significant opportunity for utilization coupled with protection technologies, but development programs will require much more focus and funding than is currently available. Manufacturing and treating of products from plantation fores...
A F Preston


Wood preservative obtained by recycling – preliminary selection of leaching inhibitor
2008 - IRG/WP 08-50252
Based on recycling of used household batteries, a process was developed to enable the recovery of major manufacturing components, leading to a solution of zinc (32 g.l-1) and manganese (15 g.l-1) salts, free of heavy metals. The potential use of the above solution as wood preservative was demonstrated by means of assays both of fungicidal activity -using white and brown rot fungi- and of insectici...
C Ibáñez, C Mantero, G Cecchetto, M Rabinovich, M Cerdeiras


Comparison of laboratory and natural exposure leaching of copper from wood treated with three wood preservatives
2008 - IRG/WP 08-50258
Standard and non-standard laboratory and field leaching tests were used to compare copper leaching from wood treated to above ground and ground contact specified retentions for three wood preservative systems, CCA-C, ACQ-D and a micronized copper formulation with quat DDAC as co-biocide. Copper leaching was highest for the ACQ formulation. Percent leaching was lowest for the micronized copper sy...
P A Cooper, Y T Ung


Antinomic natural self-protection mechanism in long-lasting woods: a case study with three tropical species from French Guiana
2009 - IRG/WP 09-10696
We demonstrate in this work through 3 examples that Amazonian trees may specialize long-lasting woods by means of at least to different approaches. Wallaba impregnates its wood with large amounts of weakly antifungal compounds acting in synergy, while tatajuba and louro vermelho woods are naturally impregnated with antifungal agents. Comparison of biological activities in vitro and concentrations ...
A Rodrigues, M Royer, N Amusant, J Beauchêne, G Herbette, V Eparvier, A Thibaut, L Salmen Espíndola, B Thibaut, D Stien


Accelerated weathering of nine tropical wood species from Cameroon
2009 - IRG/WP 09-10705
The natural durability of tropical species for building components has been a subject of recent concern and questioning, mainly the resistance to weathering. Weathering resistance of nine tropical species from Cameroon, namely Azobe, Bilinga, Bubinga, Teak, Dousie, Moabi, Musanga, Sipo and Padauk were evaluated using an accelerated weatherometer for 2016 hours. Measurement of moisture fluctuation,...
S Pankras, Jinzhen Cao, D P Kamdem


SEM-EDXA of CCA-treated Rubberwood (Hevea brasiliensis)
2009 - IRG/WP 09-20399
The microdistribution of chromated copper arsenate (CCA) preservative in rubberwood was studied using scanning electron microscope in conjunction with energy dispersive X-ray analyzer (SEM-EDXA). Bulk X-ray analysis showed that there was a high accumulation of chromium, copper, and arsenic in the vessels and lower concentration of the three preservative elements in fibres. Chromium appeared to rec...
I Jusoh, D P Kamdem


Degradation of wood veneers by Fenton’s reagents: effects of low molecular weight phenolic compounds on hydrogen peroxide decay and tensile strength loss
2009 - IRG/WP 09-20400
Pine wood (Pinus sylvestris) veneers strips were incubated in acetate buffer containing hydrogen peroxide and iron to mimic mechanisms of brown rot decay and assess the degradation of cellulose through analysis of the tensile properties of the decayed wood. The tensile properties of thin wood strips treated with Fenton system reagents or precursors were determined and correlated to weight loss as ...
Yanjun Xie, R Well, Zefang Xiao, B Goodell, J Jellison, H Militz, C Mai


Durability and fungal colonisation patterns in wood samples after six years in soil contact evaluated with qPCR, microscopy, TGA, chitin- and ergosterol assays
2009 - IRG/WP 09-20402
There is a need to establish new objective and sensitive methods for early detection and quantification of decay fungi in wood materials. Molecular methods have proven to be a useful tool within wood protection issues, however, this field is still poorly explored and so far relatively few have used these methods within the field of wood deterioration. Among the techniques used in the indirect quan...
A Pilgård, G Alfredsen, I Børja, C Björdal


Effect of Preservative Treatment on Fungal Colonization of Teak, Redwood, and Western Red Cedar
2009 - IRG/WP 09-20404
Fungal flora present in preservative treated samples or non-treated samples from sapwood and heartwood of teak, western red cedar, redwood, and southern yellow pine was assessed after 6 to 18 months of exposure near Hilo, Hawaii. The objectives were to compare fungal composition and diversity between treated and non-treated samples, and to examine the use of molecular techniques for assessing fung...
Y Cabrera, C Freitag, J J Morrell


Wart Morphology can Distinguish White Cypress Pine from the Less Durable Species, Black Cypress Pine
2009 - IRG/WP 09-20406
White cypress pine (Callitris glaucophylla) wood is durable enough to be used outdoors, but occasionally there are reports of its premature failure in ground contact, which may be due to its substitution by the less durable species, black cypress pine (C. endlicheri). It has been difficult to prove this, however, because the woods of both species are very similar in structure and cannot be separat...
R Heady, R Cunningham, P Evans