40 year results from the largest preservative in-ground stake trial conducted in Australia
2013 - IRG/WP 13-30624
The final results from Australia’s largest preservative in-ground stake trial are listed. There were eight test sites, six in Australia and two in Papua New Guinea. The preservatives tested include low and high temperature creosotes, PCP and various water-borne preservatives including CCA and copper chromate. The main timbers examined were sawn Pinus radiata sapwood, sawn Eucalyptus regnans hear...
L J Cookson


Performance of biocide-free preservative-protective systems modified with organosilicon compounds
2013 - IRG/WP 13-30628
The objective of the research was to determine the influence of organosilicon compounds in preservative-protective systems on the selected properties of pine wood aimed for outdoor use. The investigations were made for biocide-free systems based on alkyd resin and natural oils modified with alkylalkoxy-, amino- and glycidoxysilanes. The special attention was paid on the influence of hydrophobic pr...
B Mazela, P Hochmańska, T Krystofiak


Investigations concerning liquid absorption of six heartwood species
2013 - IRG/WP 13-40618
In order to determine the liquid absorption and the penetration different heartwood species were treated with a boric acid containing solution. Heartwood of six wood species (Fir, Spruce, Douglas fir, Scots Pine, Oak and Black locust) were used in these investigations whereby the dimension corresponds to the EN 252 format. One half of the stakes were end sealed before treatment. All stakes were im...
E Melcher, J Zwiefelhofer


Hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment
2013 - IRG/WP 13-40623
The hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment was investigated by testing the water uptake, equilibrium moisture content (EMC) at various relative humidity levels, and contact angle of the poplar wood surface. The results showed that: (1) At the first moment, the heat treatment at temperatures lower than 160 ℃ did not reduce the water uptake be...
Weiyue Xu Yuan Zhu, Jinzhen Cao


Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin


Quantification of copper and chromium in field stakes after different exposure times: Remaining metal content and distribution
2013 - IRG/WP 13-50291
In order to determine the distribution of copper and chromium as well as their remaining concentration EN 252 specimens and thicker pine sapwood stakes (non standard format) were treated with a commercial CC salt in a vacuum pressure process. The stakes were installed in the test field of the Institute of Wood Research, Hamburg, in August 2010. In all cases three stakes were removed after 4, 8, 12...
T Liese, M Bahmani, E Melcher


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Incidence of soft rot attack on preservative treated Douglas-fir poles: a preliminary survey
2014 - IRG/WP 14-10818
Occurrence of soft rot decay in Douglas-fir poles treated with ammoniacal copper zinc arsenate (ACZA) or pentachlorophenol in oil was studied. Soft rot was less prevalent in poles treated with penta, but some soft rot was found in approximately 20 % of poles examined. Soft rot was more common in poles treated with ACZA, and, when present, was found in almost 20% of the cells examined. The potenti...
P Torres Andrade, J J Morrell


Moisture performance testing of wood – Practical experiences
2014 - IRG/WP 14-20546
Different methods are used to characterize the moisture performance of wood and to quantify the effect of moisture loads on the resulting service life. These methods can be divided into direct and indirect methods. Furthermore they can be distinguished by characteristics like continuous or periodical measurements and measuring local or global moisture content (MC). Furthermore each measuring metho...
L Meyer, C Brischke, M Kasselmann, C Rösmann


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Effectiveness of Copper Indicators in Treated Wood Exposed to Copper Tolerant Fungi
2014 - IRG/WP 14-20554
Wood treated with a copper based wood preservative will typically turn a green color. While the depth of copper penetration can be readily discerned from the green color of the copper it is standard practice in research and commercial treating plants to make use of a color reagent such as Chrome Azurol S, Rubeanic acid or PAN indicator to reveal the penetration more clearly. When copper treat...
L Jin, K Brown, A Zahora, K Archer


Field trials results of preservative treated ground contact stake conducted in Korea
2014 - IRG/WP 14-30640
The field trials results from Korea preservative treated ground contact stake are reported. There was two site which was in southern area(Anmeon) and east area (Jungsun) of Korea. The CUAZ, CCA and CBHDO preservatives were use in this study. The sapwood of Japanese red pine stake was treated with these preservatives according to Korea standard method and then installed in 2003. Every year the insp...
Dong Won Son, Won Jung Hwang, Hyun-mi Lee, Dong-heub Lee, Sang-bum Park


Ammoniacal Copper Zinc Arsenate Preservative Treated Wood Ties Their Performance in Testing and Track
2014 - IRG/WP 14-30636
While not a new preservative system, Ammoniacal Copper Zinc Arsenate (ACZA), had not previously been used to protect crossties. Its performance in treating difficult or refractory species of wood has been documented through its wide range of uses approved in AWPA. The establishment of appropriate testing for railroad material use was put in place and includes laboratory, field as well as commercia...
T Carey


Three-year field test of preservative-treated Canadian species in Korea
2014 - IRG/WP 14-30646
The purpose of this study was to generate field performance data in Korea on Canadian softwood species preservative-treated to Canadian standards. Two field tests of preservative-treated Canadian softwood species, one in ground contact and one above ground, were installed in Jinju, Korea in November 2010. Western hemlock and white spruce were incised and pressure-treated with alkaline copper quate...
Jieying Wang, Jong Bum Ra, P I Morris


Chemistry of copper preservative treated wood
2014 - IRG/WP 14-30651
The reaction chemistry of micronized copper wood preservatives is fundamentally different from any previous inorganic preservative system. In order to study the chemistry, analytical procedures had to be developed which allowed the determination of the total copper as well as the copper which reacted with the wood forming copper-wood complexes. With the success of this approach it also became poss...
Wei Xue, P Kennepohl, J N R Ruddick


Visualization of gold/silver nanostars in wood by surface enhanced Raman spectroscopy
2014 - IRG/WP 14-30653
Nanotechnology is a fast growing up-to-date technology and ventures expeditiously in the wood preservative market. However, there is still a huge lack of understanding about the interaction and incorporation of nanoparticles (NSs) in wood. Surface-enhanced Raman scattering (SERS) offers unique advantages as an analytical tool with a high selectivity and sensitivity without matrix interference. Her...
C Geers, L Rodríguez-Lorenzo, M Placencia Peña, P Brodard, T Volkmer, B Rothen-Rutishauser, A Petri-Fink


Migration of copper from copper naphthenate treated Douglas-fir poles during storage
2014 - IRG/WP 14-50302
Preservative migration from treated wood products has raised concerns among regulators, especially when the biocides move into surface waters. In most cases, chemical levels are well below the acceptable minimum level, but can become a concern if large quantities of treated wood are stored in one location. One such case would be a location where utility poles are stored for use in emergency repai...
C S Love, C M Freitag, J J Morrell


VOC-free remedial treatment agent on organic solvent basis with surface cleaning by photocatalysis using titanium dioxide
2014 - IRG/WP 14-40651
Due to the EU Regulations according to the harmonisation of the European market of biocidal products and the EU Regulations regarding emissions of volatile organic compounds in residential properties a new VOC free yet organic solvent based remedial treatment agent is introduced including a potential method to clean up the wooden surface of remaining biocides after a remedial treatment using photo...
H Ahl, J Fromm, P Jüngel, E Melcher, M Pallaske


Comparison of gauge and assay retention in crossties treated with copper naphthenate
2014 - IRG/WP 14-40667
Creosote has been the most widely used preservative for wooden railroad crossties or sleepers for over 100 years. Alternative preservatives such as copper naphthenate (CuN) have been shown to provide equivalent performance against decay fungi and wood destroying insects; however, the use and specification of CuN involves an education process for treaters and railroad customers alike. One differe...
J Brient, H Tomlinson, J Hughes


Development of composite furniture using bamboo strips, bamboo mat and rubber wood veneer
2014 - IRG/WP 14-40679
Bamboo offers cost-effective component in panel form is well suited to wood substitute can be used as furniture components. In the present study, borak (Bambusa balcooa ) bamboo were used for manufacturing bamboo panel. Mitinga (B. tulda) bamboo were used for making mat and rubber wood veneers were used for manufacturing mat overlaid veneer board. Borax-boric acid (BB) treatments were given to enh...
K Akhter, M Mahabubur Rahaman, M H Chowdhury, M Zahirul Alam


Laboratory Study of Relative Leachability of Chromated Copper Arsenate Preservative from Treated Woods among Soil Types of Sarawak
2014 - IRG/WP 14-50307
Wood and soils are important natural resources from the environment and serves mankind well respectively as structural materials and natural platform erecting such materials. With shortfalls of naturally durable timber species for protected in-ground uses under Malaysian environments, Chromated Copper Arsenate (CCA) treated woods are widely used instead, incurring serious potential threats of pres...
A H H Wong, P K F Chong


Ammoniacal zinc borate as solid wood preservative
2014 - IRG/WP 14-30659
Zinc borate, well-known for its fungicidal, insecticidal and flame resistant properties, is widely used in manufacture of lignocellulose particle board. This form of borate is the least water soluble form available providing advantages as well as disadvantages for use as a wood preservative. This form does not leach from wood under conditions of high humidity, but it is also very difficult to appl...
C Ibáñez, C Mantero, A Ibarra, M Rabinovich


Influence of artificial and natural weathering on water exclusion efficacy of wood
2015 - IRG/WP 15-20559
Water exclusion efficacy (WEE) is one of the most important properties of wood that contributes to the overall performance of naturally durable wood species in outdoor above ground applications. WEE is in strong correlation with moisture dynamics of wood, its hydrophobicity and can indicates susceptibility against wood decay fungi. Despite of the importance of this parameter, WEE is not completely...
M Žlahtič, M Humar


Building solid foundations to support market growth of preserved wood in the UK – treatment quality, product approval and the largest national field trial of preservative treated wood in 50 years
2015 - IRG/WP 15-30662
The Wood Protection Association (WPA) has just commissioned Britain’s largest ever durability trial of home grown timber, having contracted Building Research Establishment (BRE) to conduct a long term controlled field trial of sawn and pressure treated British Softwood posts at two sites with differing soil conditions. This large scale Field Trial is the last of an innovative and substantial thr...
E Suttie, G Ewbank


Potential of teak heartwood extractives as a natural preservative against Nasutitermes corniger termite
2015 - IRG/WP 15-30666
Most low durability timber are treated with waterborne preservatives consisting of metallic salts, however, these substances make the process expensive and are harmful to man and the environment, requiring cares with handling, dosing and leaks. Due to these facts, several researches have shown the use of natural substances, extracted from the wood of various naturally durable species, as potential...
V Fassina Brocco, J Benigno Paes, L Gonçalves da Costa, S Brazolin