Comparative investigations on the influence of wood seasoning, wood properties and temperature on the toxic values of wood preservatives against Hylotrupes egg larvae
1970 - IRG/WP 28
Comparative tests carried out at three institutes indicated the influence of kiln temperature, position of wood specimens in the cross sectional area and test temperature on the toxic values determined in accordance with DIN 52165 with egg larvae of the house longhorn beetle (Hylotrupes bajulus L.). The preservatives applied were boric acid in distilled water and g-benzene-hexachloride dissolved i...
G Becker, T Hof, O Wälchli


Eco-tax - A new threat for wood preservation? The Belgian experience
1993 - IRG/WP 93-50001-32
At the end of January 1993, a bill was put for Belgian Parliament related to the introduction called "Eco-taxes" on a series of products, such as packaging for drinks (especially on PVC-bottles), non-returnable articles (shavers, small cameras), batteries, pesticides for non-agricultural use and paper....
G Van Steertegem, F De Jaeger


Preservative treatment of Eucalyptus saligna fence posts by the double-diffusion method
1982 - IRG/WP 3196
Eucalyptus saligna fence posts treated by the double-diffusion method with two chemical combinations showed average lives of 11.2 years (copper sulphate and potassium dichromate at 10.5 kg/m³ retention)and of 14.3 years (copper sulphate and sodium mono-H arsenate at 7.1 kg/m³ retention), as determined in five test sites in the State of Sao Paulo, Brazil. The exponential model was the best fit wh...
E S Lepage, A R De Freitas


Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem


Selective adsorption of antisapstain actives from two aqueous suspensions, and movement of actives into wood
1996 - IRG/WP 96-30103
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, NeXgenâ and Busanâ Sap Stain Preventative (Busan 1009), at three product concentration levels. Concentrations of active ingredients (NeXgen: CTL (chloro-thalonil) and MTC (methylene bisthiocyanate); Busan 1009: TCMTB (2(thiocyanomethylthio)-benzothiazole) and MTC) wer...
M J Kennedy, T L Woods


Blue stain in service on wood surface coatings. Part 2: The ability of Aureobasidium pullulans to penetrate wood surface coatings
1992 - IRG/WP 92-1557
The ability of Aureobasidium pullulans to penetrate seven different wood surface coatings was examined. Eight isolates of Aureobasidium pullulans were used. Following penetration, light microscopy was used to examine the effect of the fungus upon the coating, and growth at the wood-film interface. The fungus showed different growth capabilities with different types of surface coatings. Some isolat...
P R Sharpe, D J Dickinson


Resistance to soft rot of hardwood plywood treated with CCA salt
1983 - IRG/WP 3258
Plywood made from indigenous hardwoods was treated at an average loading of 34 kg Celcure A per m³ and was installed in a field test. After 20 years the samples were only slightly attacked by soft rot and the glue bonds were still intact....
R S Johnstone


Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal


Light organic solvent preservative treatment of glue-laminated radiata pine
1986 - IRG/WP 3380
The high permeability of radiata pine (Pinus radiata D. Don) is associated with ray-tissue and in particular the cross-field pits linking ray-tissue to tracheids. This pathway is absent in the tangential grain direction, leading to poor preservative penetration when treatment is restricted to the radial face - for example, timber fabricated into glue-laminated beams....
P Vinden


On site test for indicative determination of leaching of components of preservatives from treated timber. Part 2: New data on CCA-C, CC and CCB treated timber
1994 - IRG/WP 94-50025
The 'on site test' was published at the IRG meeting in Cannes in February 1993 (IRG/WP 93-50001/12). Since this publication many on site tests were performed parallel to so-called shower tests. The correlation between the test results of the on site tests and the shower test has been established more clearly. For chromium the correlation between both tests is indistinctive of pre...
W J Homan


Contribution to the testing of wood based board material
1982 - IRG/WP 2176
R G Lea


Dimensional stabilization of wood with dimethylol compounds
1987 - IRG/WP 3412
This study showed that a substantial degree of dimensional stability can be imparted to wood by crosslinking with low concentrations of dimethyloldihydroxyethyleneurea. It was demonstrated that by selecting the right catalyst system the cure temperature can be reduced to the point that strength loss of the treated wood is minimized....
D D Nicholas, A D Williams


Report on the treated piles and fenders in the wharves in Port Moresby harbour, and the Huon Gulf, Lae
1977 - IRG/WP 433
To investigate the resistance of Papua New Guinea timber, vacuum pressure impregnated with Copper-Chrome-Arsenic salts, to marine borer attack in the waters of Papua New Guinea....
S M Rayner, C R Levy


Wood-destroying insects found in the Eastern Black Sea sub-region of Turkey
1982 - IRG/WP 1153
The Eastern Black Sea subregion has important forest resources. The settlement areas are scattered at the countryside. That's why a good deal of wood and timber is used in the construction of buildings without sufficient protective measures in the rural areas. In the forests and rural buildings 52 wood-destroying insect species have been specified 35 of which are new in this subregion and...
O A Sekendiz


Fluorine compounds for wood preservation
1971 - IRG/WP 304
Fluoride compounds have gained a considerable importance in wood preservation, especially in Germany and some other countries of Europe. They are used as single compounde or in mixtures of different compounds. In the International Research Group on Wood Preservation which continues the activities of a former OECD-Group, it was moved to prepare a survey on fluorides in wood preservation together wi...
G Becker


Factors affecting leaching of preservatives in practice
1978 - IRG/WP 3113
At the 7th Meeting of the IRG in Poland in May 1975, the findings of collaborative laboratory leaching techniques were discussed, and the dangers inherent in using such results to predict the behaviour of preservative-treated components in service were emphasised. In order to improve our understanding of the factors governing leaching of preservatives in practice, and to identify areas where furth...
R Cockcroft, R A Laidlaw


Procedure for a collaborative study of leaching from CCA-treated timber in the sea
1988 - IRG/WP 4143
As a follow-up to the collaborative IRG/COIPM marine trial of CCA and CCB preservatives, a further trial is proposed with the objective of measuring the degree of leaching of CCA components from three timber species at marine sites in Malaysia and the U.K.. Details of the planned procedure are given....
S M Cragg, J E Barnacle, J D Bultman, R A Eaton, B R Johnson, L E Leightley, K D Singh


Contribution to study of the degradation caused in Pinus spp. poles used in field test
1989 - IRG/WP 1417
The study of the degradation produced by soil natural microflora on wood in contact with it in the field, has been going on for several years now. Our contribution to this aim in the present work has dealt with the possible relationship of the microorganisms in the soil. The microscopic visualization of wood colonization by the microorganisms, and the chemical analysis of the degraded wood compare...
M T De Troya, A Garcia, M J Pozuelo, A M Navarrete, A Cabanas


Efficacy of anhydrides as wood protection chemicals - II. Performance against soft rot fungi
1998 - IRG/WP 98-30174
Pine sapwood modified with various anhydrides and with butyl isocyanate was tested for its resistance to soft rot decay. Small stakes were exposed for 20 months in unsterile soil in a fungal cellar test. Wood modified with butyl isocyanate performed better than any of the anhydrides tested, with a threshold level of protection (less than 3% weight loss) at 12% weight percent gain (WPG). Stakes ac...
S C Forster, M D C Hale, G R Williams


Electron microscopic detection and chemical analysis of three-lamellar structures in wood-destroying fungi
1984 - IRG/WP 1240
In the course of transmission electron microscopical investigations of pine wood decay by various brown- and white-rot fungi extracellular three-lamellar structures (TLS) formed by the fungi were found in specimens stained with ruthenium red. These structures occured in the lumen of the wood cell surrounding the hypha at the outermost layer of the fungal cell wall. In the course of the investigati...
R Foisner, K Messner, H Stachelberger, M Röhr


The Thirteenth Report of the International Research Group on Wood Preservation 1983
1984 - IRG/WP 5194
R Cockcroft


Developments in wood preservation
1977 - IRG/WP 393
The purpose of this paper is to comment very briefly upon recent developments and trends in wood preservation so that members of this Working Group have a basic knowledge of activities in other countries. The last paper was prepared in April 1976 and the present paper refers to developments, since that time....
B A Richardson


Response of laboratory groups of Reticulitermes speratus (Kolbe) to different quantities of food
2003 - IRG/WP 03-10489
As part of a project aimed at improving understanding of the foraging biology of Japan’s most widespread wood-destroying termite, different sized groups of Reticulitermes speratus (0.5; 1 and 2 g) from two colonies were kept on 16 or 64 cm3 of sapwood of Cryptomeria japonica for 12 weeks in the laboratory. Patterns of wood consumption, wood consumption rates and survival are discussed....
M Lenz, T Yoshimura, K Tsunoda


Regulations of pesticides (including wood preservatives) in the United States
1977 - IRG/WP 397
G B Fahlstrom


The identification and preservative tolerance of species aggregates of Trichoderma isolated from freshly felled timber
1992 - IRG/WP 92-1553
The surface disfigurement of antisapstain treated timber by preservative-tolerant fungi remains a major problem in stored timber. Identification of a range of isolates of Trichoderma based on microscopic morphological characteristics was found to be imprecise due to the variable nature of this organism. In addition, studies to compare visual (morphological) characteristics of these isolates with t...
R J Wallace, R A Eaton, M A Carter, G R Williams