IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 669 documents. Displaying 25 entries per page.


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


Post-Manufacture Biocide Treatment of Engineered Wood I-Joists
2012 - IRG/WP 12-40596
Engineered wood I-joists, fabricated from laminated veneer lumber (LVL) flanges and oriented strand board (OSB) webs, offer many advantages over solid sawn lumber joists in residential and light commercial construction. With the expanded use of these products has come an increasing need to be able to treat them with biocides to prevent attack from decay fungi and termites during service. Historic...
A S Ross, R W Clawson


The effect of nanozycosil on the water absorption and dimensional stability of Beech wood
2012 - IRG/WP 12-40606
Zycosil is a clear penetrating water repellent. This product works by penetrating into the substrate and modifying the surface tension to inhibit water intrusion. Beech wood (Fagus orientalis) was modified by treatment with nanozycosil. Then water absorption and dimensional stability in terms of volumetric swelling percent and anti-swelling efficiency were determined and found to be improved on t...
M Ghorbani, F Bavaneghi


Scale-up of a chemical process for copper-based preservative-treated wood wastes recycling
2012 - IRG/WP 12-50286
In recent years, the development of appropriate wood waste disposal options has been encouraged by severe regulations and expensive fees associated with wastes landfilling or burning. An efficient and economically attractive leaching process was developed at laboratory scale (200 mL) for CCA-, ACQ- and CA-treated wood wastes recycling. This leaching process consisted of three leaching steps of 2 h...
L Coudert, L Gastonguay, J F Blais, G Mercier, P Cooper, P Morris, A Janin, N Reynier


Tar-oil uptake vs time in immersion treatment of short pine posts: A simple technique applicable to rural communities of Papua New Guinea
2012 - IRG/WP 12-40608
Pinus caribaea and Araucaria cunninghamii logs ca. 100 mm in diameter were shortened to lengths 25-30 cm, conditioned to at/below fibre saturation point (FSP) for immersion/dip treatment using a hot- and- cold bath open- tank process. Before oven-drying and subsequent treatment, individual test specimens were numbered, their green weights and volumes, and dry weights recorded for basic density, vo...
B K Gusamo, R Tulo


Mould growth on wood-based materials – a simulated in-service study
2012 - IRG/WP 12-20503
Ten different wood-based materials including preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce were placed in three different environments (an attic and two crawl spaces) for a period of 26 months. Mould growth was analysed at five to seven month intervals in an effort to map the growth development. The relative humidit...
G Bok, P Johansson, J Jermer


Study of the use of organosolv lignin as bio-preservative of wood
2012 - IRG/WP 12-30603
The service life of wood depends on the species, use and environmental conditions of exposure. The treatment of wood protects it against degradation by xylophagous agents, enhancing the durability of material up to 10 times, and reducing the deforestation around 12.5%. In this way, the use of treatments is necessary because increases the service life of material and protect against xylophagous age...
P S B dos Santos, A Garcia, P H G de Cademartori, D A Gatto, J Labidi


Effect of preservative treatment on mechanical performance of round and square poles made of small diameter Scots pine
2012 - IRG/WP 12-40612
A growing proportion of harvested Scots pine (Pinus sylvestris L.) timber originates from the first or second commercial thinning stands. There is a need to find economically viable and high quality wood products that can be manufactured from this raw material. Small log volume means not only demands of increased efficiency for material handling in logistics and manufacturing processes, but also c...
V Möttönen, R Stöd, K Heikkilä, H Heräjärvi


Protective nanoparticle coating reducing water absorption of wood species
2012 - IRG/WP 12-40614
Nanoparticle coatings were deposited onto different tropical wood samples for controlling the surface hydrophobicity. The styrene(maleimide) nanoparticles were synthesized in aqueous dispersions under pure conditions or in combination with 70 wt.-% palm oil. A first evaluation of the non-coated wood surfaces indicates a high dependence between the water contact angles, the average surface roughnes...
P Samyn, A Paredes, G Becker, H Van den Abbeele, L Vonck, D Stanssens


Water absorption and desorption of non treated, pressure impregnated, and pine oil treated glulam made of small diameter Scots pine and Norway spruce
2012 - IRG/WP 12-40616
A growing proportion of harvested timber originates from the first or second commercial thinning stands in Finland, which means smaller average log volumes in comparison to final felling stands. Smaller log volume means challenging wood properties such as higher proportion of juvenile wood and sapwood. Due to these facts, products made of small diameter logs are prone to twist and check, and have ...
H Heräjärvi, V Möttönen, R Stöd


Activities of moulds on wood as a function of relative humidity during desorption and absorption processes
2013 - IRG/WP 13-10794
Three different types of indoor moulds: Penicillium brevicompactum, primary colonizer; Alternaria tenuissima, secondary colonizer and Trichoderma harzianum, tertiary colonizer, grown on wood were measured for their activities under different relative humidity levels. The activities were measured by isothermal calorimetry. The activities of the moulds changed with the change of the relative humidit...
Yujing Li, L Wadsö


An assessment of soft rot in preservative-treated poles in two test sites and two network areas in New South Wales
2013 - IRG/WP 13-10801
This document presents an extended summary of recent investigations into soft rot attack of preservative treated power poles from the re-inspection of samples selected from two field sites and two in-service trials located in New South Wales, Australia. The in-ground sapwood of selected poles was assessed by probing and, after core sampling, by microscopy to determine the severity and extent of s...
W D Gardner, M A Powell, C Kirton


The assessment by visual grading, change of color and ergosterol content ratings, the resistance to mould fungi of treated with wood preservative Scots pine sapwood
2013 - IRG/WP 13-20514
The filamentous (mould) fungi belonging to Ascomycetes, Deuteromycetes group are an cosmopolitan organisms which attacks wooden elements disfiguring them, dropping their value and causing environmental and health hazard. The fungi in a short time cause mainly disfigurement of wood does not effect on strength properties of wood, but with strong prolongation of duration of conditions favourable for ...
A Fojutowski, A Koziróg, A Kropacz


Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2013 - IRG/WP 13-20535
A round robin involving 15 European participants was set up in 2006. The round robin consists of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. When comparing EN 84 preconditioning (two weeks water leaching) with natural preconditioning (1 year in field, above ground) according to CEN/TS 15397, no significant difference...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, B Mazela, E Melcher, R Möller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell


Effect of soil contact on reacted copper(II) levels in micronized copper treated wood
2013 - IRG/WP 13-30616
Small 3 to 4 mm thick and approximately 80 to 100 mm long, samples were removed from wood treated with micronized copper quat (MCQ) or micronized copper azole (MCA) and buried full length in a soil bed. Samples were removed after 2, 4 and 8 weeks. The total copper was determined by x-ray fluorescence (XRF) spectroscopy and the amount of reacted micronized copper measured by electron paramagnetic r...
Wei Xue, P Kennepohl, Xingguo Jin, J N R Ruddick


Preparation of Copper Rosinate Emulsion and Its Resistance against Wood Decay Fungi
2013 - IRG/WP 13-30619
A leaching-resistant water-borne copper preservative was prepared by means of the following three steps: (1) Gum rosin was saponified with potassium hydroxide. (2) The soap reacted with copper sulfate to form copper rosinate. (3) The copper rosinate was emulsified with a mixture of Tween 20 and Span 80. Poplar (Populus ussuriensis) wood was impregnated with 0.5%, 1.0%, 1.5%, or 2.0% of the copper ...
Mingxin Zhang, Shujun Li, Qian Wang, Bo Li, Qiong Wu


Performance of untreated wood and wood impregnated with copper-ethanolamine based preservative solutions in Northern Adriatic Sea
2013 - IRG/WP 13-30623
Sea water applications of wood are among the most challenging ones. Impregnated wood is exposed to leaching and to variety of marine borers, Limnoria sp. and Teredo sp. being the most important. In the present research, durability of pine wood impregnated with copper-amine based preservative solution (Silvanolin) of different concentrations, exposed to the sea water, was investigated according to ...
M Humar, M Petrič, J Adamek, B Lesar


40 year results from the largest preservative in-ground stake trial conducted in Australia
2013 - IRG/WP 13-30624
The final results from Australia’s largest preservative in-ground stake trial are listed. There were eight test sites, six in Australia and two in Papua New Guinea. The preservatives tested include low and high temperature creosotes, PCP and various water-borne preservatives including CCA and copper chromate. The main timbers examined were sawn Pinus radiata sapwood, sawn Eucalyptus regnans hear...
L J Cookson


Performance of biocide-free preservative-protective systems modified with organosilicon compounds
2013 - IRG/WP 13-30628
The objective of the research was to determine the influence of organosilicon compounds in preservative-protective systems on the selected properties of pine wood aimed for outdoor use. The investigations were made for biocide-free systems based on alkyd resin and natural oils modified with alkylalkoxy-, amino- and glycidoxysilanes. The special attention was paid on the influence of hydrophobic pr...
B Mazela, P Hochmańska, T Krystofiak


Investigations concerning liquid absorption of six heartwood species
2013 - IRG/WP 13-40618
In order to determine the liquid absorption and the penetration different heartwood species were treated with a boric acid containing solution. Heartwood of six wood species (Fir, Spruce, Douglas fir, Scots Pine, Oak and Black locust) were used in these investigations whereby the dimension corresponds to the EN 252 format. One half of the stakes were end sealed before treatment. All stakes were im...
E Melcher, J Zwiefelhofer


Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin


Quantification of copper and chromium in field stakes after different exposure times: Remaining metal content and distribution
2013 - IRG/WP 13-50291
In order to determine the distribution of copper and chromium as well as their remaining concentration EN 252 specimens and thicker pine sapwood stakes (non standard format) were treated with a commercial CC salt in a vacuum pressure process. The stakes were installed in the test field of the Institute of Wood Research, Hamburg, in August 2010. In all cases three stakes were removed after 4, 8, 12...
T Liese, M Bahmani, E Melcher


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Incidence of soft rot attack on preservative treated Douglas-fir poles: a preliminary survey
2014 - IRG/WP 14-10818
Occurrence of soft rot decay in Douglas-fir poles treated with ammoniacal copper zinc arsenate (ACZA) or pentachlorophenol in oil was studied. Soft rot was less prevalent in poles treated with penta, but some soft rot was found in approximately 20 % of poles examined. Soft rot was more common in poles treated with ACZA, and, when present, was found in almost 20% of the cells examined. The potenti...
P Torres Andrade, J J Morrell


Previous Page | Next Page