Residual resistance in eucalypt poles according to the degree of sanity
1984 - IRG/WP 2225
A lot of 50 eucalypt poles presenting external deterioration by fungus was taken from service and tested. These poles were classified into five degrees of sanity according to evaluation criteria adopted by the IPT Wood Division. After being classified, they were tested with respect to their bending resistance, in order to gather information about their critical degree of sanity which may define th...
F C Geraldo, S Milano, S G De Sequeira


Application of non-destructive techniques (durometric and ultrasonic) to evaluate the degradation of woods in service by Gloeophyllum trabeum
2001 - IRG/WP 01-20220
In order to establish the degree of degradation of wood used in construction, it is necessary to employ non-destructive methods (ultrasonic, durometric, densitometric). In this study, ultrasonic and Pilodyn durometric techniques have been applied to try to establish parameters of relationship between the values obtained by both, for their immediate application to wood in service. As a method of re...
M T De Troya, L Palaia, A Navarrete, V Galvañ, R Molina, A Guijarro, J Camacho


Molecular phylogeny of Ophiostoma spp. related to blue-stain in pine
2002 - IRG/WP 02-10432
Blue-stain in coniferous woods is an economically important disease in many temperate countries, caused specially by genus Ophiostoma. Classical taxonomy of genus Ophiostoma is limited for the correct identification of many species, because of the similar macroscopic and microscopic characters, as well as the existence of some species complex. Molecular identification is a good complement to eluci...
M Villarreal, F Arenal, J Sánchez-Ballesteros, M T De Troya, F Llinares, V Rubio, A Navarrete


An alternative method for the determination of lignocellulolytic enzymatic activities of white rot fungi
1998 - IRG/WP 98-10261
Some lignocellulolytic activities of wood decay fungi can be evaluated in an indirect way through the study of the decolorization that white rot fungi produces in culture media in the presence of dyes. In this assay, ten dyes were selected, which were added in concentrations of 0.00 1% - 0.003% (P/V) to four-day cultures of Trametes versicolor containing 1% of beech sawdust in a basal salt medium...
D Muñoz-Mingarro, F Llinares, F Rubio, M Yuste, C Rodríguez-Borrajo, J Jiménez, M T De Troya


Anobium punctatum De Geer (Coleoptera Anobiidae)
1980 - IRG/WP 1103
Anobium punctatum de Geer (1) est un Coléoptère qui appartient au sous-ordre des Teredilia et à la famille des Anobiidae. Cet insecte a été décrit pour la première fois par Charles de Geer, entomologiste Suédois dans ses "Mémoires pour servir à l'histoire des insectes" parues en 1774, sous le nom vulgaire de Vrillette pointillée et en latin " Ptinus (punctatus) griseo fuscus". ...
M-M Serment


Database of sapstain fungi affecting lumber, logs and trees
2004 - IRG/WP 04-10534
Sapstain fungi discolour lumber, logs and tree sapwood and are often mistaken for moulds, which cause a superficial discoloration. Stained wood has a lower market value. Further, because stained wood products can potentially carry pathogenic fungi, such products may be refused by importing countries. Addressing these issues involves developing ways for accurately identifying staining fungi, docume...
S Lee, F de Giuli Vallverdu, S Alamouti, Jae-Jin Kim, A Uzunovic, C Breuil


Quantification des émanations de substances dans l'air ambiant a partir des bois traités
1993 - IRG/WP 93-50001-27
Pesticides on wood for the purpose of its protection may evaporate. Eventual toxicity of such emanations justifies risk assessment procedures for indoor air in building. This document describes bench scale tests based on the technique of chambers developped by CTBA/BIOTEC to determine the amount of pesticides and associated substances released to the ambient air. Results obtained with various pest...
H Sageot, M Lamour


Enzymatic study of Ceratocystis sp., blue-stain fungi on Pinus nigra
1999 - IRG/WP 99-10315
One of the main problems that the forest exploitation industry has with Pinus nigra wood is the blue-stain fungi, whose causing agent is unknown. Therefore, the objective of this work has been to study, through enzymatic tests of the isolated cultures, if these fungi infect Pinus nigra in any specific way. After the incubations, isolates of Ceratocystis were obtained. These were cultured in a sali...
M T De Troya, F Rubio, D Muñoz-Mingarro, F Llinares, C Rodríguez-Borrajo, M Yuste, M J Pozuelo, J I Fernández-Golfín


Migration of chlorothalonil and carbendazim in fruits stored in wood treated with the anti-sapstain formulation Tuff Brite C
1997 - IRG/WP 97-50097
Fruits and vegetables stored in treated wood boxes are in contact with the products used for the treatment. In order to obtain regulatory approval for incidental food contact it is necessary to determine the quantity of residues on these fruits or vegetables. When the active materials are used in agriculture it is required that residues found are below to the MRL fixed for these substances. In the...
J F Cooper, D Riboul, M De Vleeschauwer, T L Woods


Variable chlordane residues in soil surrounding houses in Louisiana
1989 - IRG/WP 1404
Eight soil samples from each of 30 houses in greater New Orleans, Louisiana were collected in October, 1986 and analyzed for chlordane residues (ppm). All houses had reportedly been treated in the late 1960's or early 1970's. Chlordane occurred in all samples, and the overall mean (+ SEM) was 870.6 + 96.5 ppm. Residue levels were unaffected by construction type (slab, crawl, craw...
J P La Fage, K S Delaplane


Nondestructive assessment of biodegradation in southern pine sapwood exposed to attack by natural populations of decay fungi and subterranean termites
1994 - IRG/WP 94-20042
Field methods for evaluating decay resistance of experimentally treated materials lack a means for quantitative measurement of residual strength. Quantitative relationships between speed of impact-induced waves travelling parallel to the grain and residual compressive strength have been demonstrated in softwood attacked by brown rot-decay fungi, but the effects of termites have not been documented...
R C De Groot, R J Ross, W Nelson


Biodetioration and strength reductions in preservative treated aspen waferboard
1983 - IRG/WP 2195
Experimental aspen waferboards, bonded with liquid or powdered phenol formaldehyde resins and treated by various methods with a wide selection of preservatives, were tested for fungal resistance in accelerated laboratory trials. Mold growth on the surface as well as weight and strength losses due to the actions of decay fungi were determined. Testing of board strength after decay in high and moder...
E L Schmidt, H J Hall, R O Gertjejansen, R C De Groot


An unusual soft-rot decay pattern caused by the Ascomycete Hypoxylon mediterraneum (de Not.) J Miller
1984 - IRG/WP 1222
A distinct pattern of soft-rot decay has been observed for the fungus Hypoxylan mediterraneum (de Not.) J. Miller. This fungus also produced decay patterns typical of brown and white rot decay. The production of characteristic cavities by Hypoxylan mediterraneum was prolific in the hardwoods Eucalyptus maculata and Eucalyptus regnans, but infrequent in the softwoods, Pinus elliottii and Pinus radi...
D M Francis, L E Leightley


Evaluation of the permeability of fast grown wood species
1995 - IRG/WP 95-40042
The low natural durability of certain species of wood, implies the need for applying a protecting treatment to increase its life in service. Because of this, a knowledge of the permeability properties of the wood is desired. In this work, a simple and reliable method to evaluate the wood permeability is presented. For that, we have been used fast grown species, with low natural durability, Poplar ...
M T De Troya, A M Navarrete, E Sanchez, J E Garcia de los Rios, E L Rodríguez Trobajo


Microdistribution of water-borne preservatives in blue gum treated by full-cell process
1990 - IRG/WP 3617
The present work deals with the study of the microdistribution of copper, chrome and arsenic elements in Eucalyptus globulus Labill. sapwood, treated with a CCA water-borne preservative by full-cell process, with the help of scanning electron microscopy together with energy dispersion X-ray analysis technique. The work shows that the retention of CCA elements is high in vessels and vasicentric par...
D De Sousa Castro Reimão, J M Palacios


Creosote immersion treatments of fence-posts of different pines
1986 - IRG/WP 3386
This paper describes the preservation with creosote by immersion of fence-post of Pinus sylvestris, Pinus pinea and Pinus radiata. Taking into account the rural use of the fence-post, an easy method available in the field to the agriculturalists. A regressions analysis has been carried out, dealing with the absorption, retentions and penetrations shown after 1, 3 and 7 days of treatment. The great...
C De Arana Moncada


Information from the COIPM wood group. (With Appendix: Préserver les matériaux en milieu marin sauvegarder l'environment marin telles sont la vocation et la mission du C.O.I.P.M.)
1989 - IRG/WP 4156
During the last COIPM Meeting, up to date information on cooperative work to test the resistance of plastic wrapping for pilings were submitted and discussed. In 1986 untreated wood samples wrapped with shrinkable polyolefin sleeves were submerged in 9 stations, situated in temperate and tropical waters. After 1 or 2 years of immersion the samples showed no sign of penetration by marine borers and...
A Gambetta


Screening of the technical performance and aquatic toxicity of N-methylolacrylamide treated wood
2000 - IRG/WP 00-40166
In the course of the last decades chemical modification of wood species, with a limited natural durability, has been subjected to intensive research. As a possible alternative and supplementary treatment of non-durable wood in a range of applications it remains one of the major topics in the wood preservation world. Different modification systems have been scaled-up and are now in an industrialisi...
V Rijckaert, S De Geyter, J Van Acker, M Stevens


Studies on the fungicidal effectiveness of a petroleum derived product as a creosote alternative
1986 - IRG/WP 3384 E
This work, appears first because of the necessity to find out a profitable use for a residual product of the petrol pyrolisis, and second, because the lack of high natural durability wood used until now-a-days to build posts and sleepers in creosote lacking countries. Our main objective was pointed to the characterization of this new product and to find out the effectiveness against the wood-destr...
A M Navarrete, M T De Troya


Aquatic toxicity research of structural materials
1998 - IRG/WP 98-50114
Continuing from preliminary results reported on the aquatic toxicity of some tropical hardwoods under high hazard conditions, a more comprehensive research study is set-up in order to assess the environmental toxicology of various structural materials in water applications. Hazard class 4 preservative treated wood is tested for its toxic response on a battery of aquatic test organisms, next to con...
G M F Van Eetvelde, S De Geyter, P Marchal, M Stevens


The risk assessment process. Point of view of a biocide manufacturer [Évaluation du risque. Point de vue d'un fabricant de biocide]
1990 - IRG/WP 3568
Risk assessment is an inherent part of our everyday lives. The risk assessment equation combines Hazards and Exposure. For the Wood Preservation Industry, the hazards may be characterised by the toxicity a the ecotoxicity of chemicals and the exposure by the identification of exposed people, of the exposure routes and exposure frequency. To quantify the exposure, good co-operation is required betw...
D Baur


Suppression of termite feeding by Sudan red 7B
1988 - IRG/WP 1344
Groups of the Formosan subterranean termite, Coptotermes formosanus Shiraki, were fed for 14 days on wood shavings soaked in acetone solutions of one of three concentrations (0, 0.5, or 1%) of the dye, Sudan Red 7B. Groups of marked or unmarked termites were then placed in containers and allowed to feed on undyed wood for 21 days. Dyed termites had lower wood feeding rate, survivorship, and number...
K S Delaplane, L A Bourg, J P La Fage


Characterization of wood decay enzymes by MALDI-MS for post-translational modification and gene identification
2002 - IRG/WP 02-10442
The recent sequencing of the Phanerochaete chrysosporium genome presents many opportunities, including the possibility of rapidly correlating specific wood decay proteins of the fungus with the corresponding gene sequences. Here we compare mass fragments of trypsin digests, determined by MALDI-MS (Matrix Assisted Laser Desorption Ionization-Mass Spectrometry), with predicted mass fragments derive...
T H de Koker, P J Kersten


The efficacy of boron preparations
1987 - IRG/WP 3400
The toxicity threshold of boric acid for egg larvae of Hylotrupes bajulus Linné is approx. 0.4 kg/m³ of wood (71 g B/m³) over a 12-week test period, and approx. 0.3 kg/m³ of wood (53 g B/m³) over a 6-month test period. The corresponding values for borax are 0.5-0.6 kg/m³ of wood (56-68 g B/m³) and 0.3-0.4 kg/m³ of wood (34-45 g B/m³). The values are somewhat lower in the case of the egg l...
J T De Jonge


Analysis of the degradation of carbohydrates by blue-stain fungi
1990 - IRG/WP 1457
The topic of the degradative ability of blue-stain fungi literature is not clear. Many authors support the idea that those fungi don't have enzymatic capability to decay the wall of the ligneous cells. However, others have found some decay activity. In this study, we have attempted to analyze which wall cells soluble carbohydrates are metabolized by some blue-stain fungi, found in Spain. ...
M T De Troya, A M Navarrete, E Relano