IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 139 documents. Displaying 25 entries per page.


Physical properties variation of sound and top dying affected sundriwood (Heritiera fomes) in mangrove forest of Bangladesh
2004 - IRG/WP 04-10504
Top dying of sundri (Heritiera fomes Buch.-Ham.) in the Sundarbans is considered to be the most severe of all the diseases of tree crops in Bangladesh. The wood samples from sound, moderately affected and severely affected sundri trees from three different tree heights for every individual test were collected and their respective physical properties were examined to make a comparison. It was found...
S C Ghosh, A K M A Bosunia, M A Islam, A K Lahiry


The preventive actions of three commercial wood preservatives against Dinoderus minutus
1984 - IRG/WP 1233
Dinoderus minutus is one of the most common pest insects for the bamboos. For preventing the damages of this insect, the preventive treatment of bamboos with preservatives is necessary. But because of the environmental reasons, only limited insecticides are available in Japan. The author determined the preventive effects of three commercial products against Dinoderus minutus by the medium of the B...
K Suzuki


The effect of mortality diseases on wood quality of sissoo (Dalbergia sissoo Roxb)
2006 - IRG/WP 06-10569
Sissoo (Dalbergia sissoo Roxb.) is a lagre deciduos, fast growing, strong light demanding and leguminous tree specie. It is an important multipurpose specie widely being planted in the agro forestry and and social forestry pratices in Bangladesh, particularly in the north and south-western parts of the country. On account of its better quality, sissoo is valued as good as construction and utility ...
M M Islam, M O Hannan, G N M Ilias


Der Fall Lyctus. Skizzen über Auftreten, Bedeutung und Bekämpfung eines Holzwurms
1980 - IRG/WP 1100
Lyctus brunneus (Steph.) and allied species cause severe damage to wood throughout the world and inflict losses on producers, the trade, industries and craftsmen. Starch-containing wood is liable to attack. The history of the accidental introduction of this wood-destroyer into West-Europe and the causes for this are outlined, biological requirements for the attack as well as developments for Lyctu...
S Cymorek


Comparative study on physical properties of four fast growing timber species of Bangladesh
2006 - IRG/WP 06-10570
Ghoraneem (Melia azedarach), Rain tree (Albizia saman), Sissoo (Dalbergia sissoo Roxb.) and Akashmoni (Acacia auriculiformis) plantations are started as a fast growing timber specie from a few years back in Bangladesh. Initian objectives were to get fuel wood only from those trees, but a very positive response was found for Ghoraneem, Rain Tree, Sissoo and Akashmoni timber in the users market by c...
M M Islam, B K Dey, M O Hannan, G N M Ilias


Preventive effectiveness of petroleum derivatives against blue-stain fungi. Part 2
1993 - IRG/WP 93-30001
Solvex-Tar, a product derived from the distillation of petroleum could be suitable for the treatment against blue-stain fungi in wood used in exterior carpentry, due to its effectiveness as a fungicide. The aim of this work has been to optimize the application of this product, modifying it as necessary, so as to improve its physical characteristics without interfering with its preventive effective...
E Sanchez, M T De Troya, A M Navarrete, A Guijarro


Contradiction between uptake of preservative in practical situation and laboratory testing
1992 - IRG/WP 92-2392
By brush treatment water- and solvent-based products were applied on boards of Scots pine and Norway spruce to achieve an uptake of 100 and 200 g/ml. In addition the scope of work to achieve the required uptake of preservative was determined under practical conditions for both product groups. EN 113 (RAL-GZ 830) tests were carried out to test the biological efficacy of products. After 18 months ex...
R Gründlinger, O Janotta, M Melzer


Longterm monitoring of termite activity on multiple feeding sites: a laboratory method intended for the determination of attractant/repellent properties of wood preservatives and baits
2001 - IRG/WP 01-20225
A method is introduced allowing the continuous monitoring of the activity of a small laboratory termite- colony at 8 different feeding sites simultaneously. The test assembly consists of a small central polycarbonate-tube containing a colonie of Reticulitermes santonensis (de Feytaud) beeing connected with 8 external feeding sites by small glass-capillaries. The termites passing through the glass ...
M Pallaske, E Graf, H Takiuchi


Preventive effectiveness of petrol derivatives against blue-stain fungi
1992 - IRG/WP 92-3716
A possible application of fractions obtained on petrol pyrolysis is their use as a wood preservative against wood-decay and sap-stain fungi. From two of these fractions were prepared three different products (ST, STL and SST). The aim of this work has been the possibility of utilizing these products in the treatment of wood used for external joinery, determining their effectiveness against blue-st...
A M Navarrete, M T De Troya, E Sanchez, A Guijarro


An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Laboratory screening to determine the preventive effectiveness against blue stain fungi and moulds
1991 - IRG/WP 3677
This paper reports results of preservative treatment and leaching experiments, using borax, polybor and boracol 20, on small wood blocks of English oak and American pitch pine heartwood. Earlier experiments on the performance of various biocides as possible additives to bilgewater to prevent fungal decay of shipping timbers had suggested that some formulations of boron might be associated with phy...
M T De Troya, A M Navarrete


A technique for assessing the preventive efficacy against decay fungi of preservative treatments applied to wood
1988 - IRG/WP 2309
A method is described in which test blocks with envelope preservative treatments can be challenged by selected test fungi previously established on an untreated feeder block. The progress of the test fungus through the treated zone is monitored using novel baits or sensors inserted in holes drilled into blocks to within predetermined distances of the face being challenged. Preliminary results show...
J K Carey, A F Bravery


Suitability of cyfluthrin in wood protection
1992 - IRG/WP 92-3735
Cyfluthrin, a well-known and in agriculture and household widely used insecticide based on synthetic pyrethroides, is evaluated now concerning its suitability as insecticide in wood protection. An overview about the physical and chemical properties is given. Test results in accordance with European standards show the high efficacy and broad-spectrum activity of Cyfluthrin against wood rotting inse...
H-U Buschhaus


A novel guide for the determination of the physical properties of wood including kiln drying and full-cell preservative treatment
2004 - IRG/WP 04-20298
An ideal flow chart for the sequential experimental determination of a range of physical properties relevant to wood drying and subsequent preservation was designed as a novel guide to assist wood scientists. In this manner, data assembly and experimental processing are shown. This was designed according to experience and published literature. Aspects emphasised in this review were the physical p...
I Usta, M D C Hale


The effects of chemical modification on the physical properties of alder and spruce particleboards
2005 - IRG/WP 05-40300
In this paper, it was aimed to improve some physical properties of chemically modified particleboard, made from spruce and alder species, spreading widely at Black sea region in Turkey. Spruce and alder chips were reacted with acetic, succinic, maleic and phthalic anhydrides at constantly heat for 3 hours then, hot pressed at 150 °C by using Phenol formaldehyde (PF) resin. Target board density wa...
E Dizman, Ü C Yildiz, H Kalaycioglu, S Yildiz, A Temiz, E D Gezer


Physical and mechanical properties of wood-polymer composites prepared from alder wood (Alnus glutinosa (l.) gaertn. subsp. barbata (c.a.mey.) yalt)
2001 - IRG/WP 01-40201
In this study, the physical mechanical properties of wood-polymer composites prepared from alder (Alnus glutinosa (L.) Gaertn. subsp. barbata (C.A.Mey.) Yalt) wood were investigated. Three different monomers styrene, methyl methacrylate and styrene/methyl methacrylate (70/30) mixtures and two loading levels were used in preparation of wood-polymer composites. Of physical properties, the oven-dry s...
A Temiz, Ü C Yildiz, E D Gezer


A note on te seasoning, preservative treatment and suitability of debdaru (Polyalthia longifolia Benth & Hooker.) for poles
1995 - IRG/WP 95-40056
The main work is to determining the suitability of Debdaru (Polyalthia longifolia Benth.) as poles from Government and Village forests are investigated. The poles of Debdaru are easily treatable with CCA preservative by full-cell pressure method, but difficult to dry (air & kiln). Proper quality control must be maintain from procurement to treatment, specially during physical selection & d...
G N M Ilias, M D Rokib-ul-Hafiz


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


A non-pressure method of protection based on hurdle theory to control the spectrum of internal environmental factors which affect the decay of poles in soil contact
1993 - IRG/WP 93-20005
A field trial was conducted to establish whether superficial barrier linings on poles in soil contact could function as environmental hurdles against the growth of biological agents and thus provide preventative methodology to preclude premature failure of vineyard poles under flood-irrigation. Assessment after 52 weeks exposure to the prevailing conditions and sub-tropical environment showed that...
A A W Baecker


Study of the degradation caused by micro-organisms in Pinus sp. waterlogged wood
1989 - IRG/WP 1411
So far, the different Centers are trying the restoration and the conservation of wood structures, coming from subaquatic archeological deposits, with interest from the historic - artistic point of view. The main objective of this paper has been the determination of the decay level of Pinus sp. wood coming from a roman ship (approximately 2000 years old), where we have analyzed their physical prope...
M T De Troya, M C Escorial, J Garcia, A Cabanas


Attempts to isolate tunnelling bacteria through physical separation from other bacteria by the use of cellophane
1992 - IRG/WP 92-1535
During attempts to isolate tunnelling bacteria in pure culture, physical separation from other bacteria was successfully achieved by the use of cellophane. Cellophane was used in liquid cultures as a substrate for tunnelling bacteria that were present in a mixture with other bacteria. By tunnelling into cellophane, TB were physically removed from contaminating bacteria which could then be removed ...
T Nilsson, G F Daniel


Failure of overhead power transmission and telecommunication poles in Tanzania: Causes, preventive and remedial measures
1988 - IRG/WP 3465
Unless measures are considered urgently to combat massive pole failures occuring in service, it is likely that wooden poles may soon become unpopular. Consequently, pole users may be forced to use costlier alternatives such as underground cables and concrete or steel poles. In trying to countercheck this trend, this paper names the main agents of pole failure, discusses different models of pole fa...
K K Murira


Influences of the hydro-thermal treatment on physical properties of beech wood (Fagus orientalis)
2005 - IRG/WP 05-40303
Influences of the hydro-thermal treatment on physical properties of beech wood were studied. Wood specimens (2×2×2cm) were treated in two steps. At first step, samples were treated at 160,180 & 200ºC for 4, 5 & 6 hours. At second step, treated samples were cured based on their first step treatment temperatures (160,180 & 200ºC) for 16 hours. The treated samples were soaked in water...
B Mohebby, I Sanaei


An observation of seasoning, preservative treatment and storing of CCA treated 30 bangladeshi hardwood species for crossarms
1995 - IRG/WP 95-40058
Observed kiln seasoning, preservative pressure treatment and storing of CCA treated 30 Bangladeshi hardwood species for crossarms. It revealed that it was very difficult to kiln season and preservative pressure treatment of thirty species together in a single charge and found that when species of different specific gravity kiln season together there occur some objectionable seasoning degrades, and...
G N M Ilias, M D Rokib-ul-Hafiz


Effect of point of preservative addition on the mechanical and physical properties of strandboard treated with Tanalith 3485
2000 - IRG/WP 00-40152
Preservative has been added to a PF bonded strandboard at various different stages in the manufacturing cycle and the physical and mechanical properties of the boards have been evaluated (modulus of elasticity, modulus of rupture, thickness swelling, water absorption, internal bond strength, and shear strength). Preservative addition has been examined at five different stages namely green strand d...
G J Goroyias, M D C Hale


Previous Page | Next Page