The use of the Shigometer® and Pilodyn® as non-destructive test methods for detecting decay in CCA treated eucalypt poles
1981 - IRG/WP 2153
The groundline condition of sixty C.C.A. treated eucalypt poles comprising six different species was examined using the Pilodyn® and Shigometer®. Although sensitive to the presence of soft-rot decay, the Shigometer® would seem to offer little practical advantage in the eucalypt soft-rot decay situation, since a comparable visual examination could reveal the presence and extent of decay. Initial...
L E Leightley


Evaluation of the pulsed-current resistance meter (Shigometer®) for determination of the internal condition of utility poles
1979 - IRG/WP 2128
A number of Telecom poles, which had been removed from service to be replaced by a radio link, were inspected using an electrical resistance meter (Shigometer®). These poles were creosoted, non-durable Victorian species in service in New South Wales. Six of these poles, chosen to represent various internal conditions typical of the range of the population tested, are discussed here. Data, from tr...
J D Thornton, W G Seaman, M McKiterick


Modified Wood – Methods, testing and applications: Outcomes of the EU-Thematic Network
2003 - IRG/WP 03-40268
In the last decade, interest in the development of wood modification systems has increased in Europe. Alongside several industrial initiatives for heat treatments, there have also been scaling up and pilot plant projects for chemical wood modification. Between 2000 and 2003, the European Commission funded the "Thematic Network on Wood Modification". This paper will feature the modification process...
D Jones, W Homan, J Van Acker


Relative performance of copper/chrome/boron (CCB) and copper/chrome/arsenate (CCA) in ground contact
1992 - IRG/WP 92-3694
The performance of four retentions each of an oxide CCA formulation and a salt formulation of CCB in radiata pine and European beech was compared after 18 years' field exposure. In radiata pine CCA oxide was more effective (4 failures out of 40) than CCB (9 failures out of 40). However, in European beech CCB was substantially more effective (22 failures) than CCA oxide (all failed). Analy...
M E Hedley


The natural durability of wood in different use classes
2003 - IRG/WP 03-10457
The natural durability of important European wood species has been tested on 3970 specimen in field trials. The wood was exposed at five test fields in Germany with different climates at each site in European hazard class 4 and 3 (with and without soil contact). Within EHC 3 it was distinguished between tree different expositions (end grain sheltered, unsheltered and with water trap). The test is...
U Augusta, A O Rapp


L-joint trials: Part 2: The relationship between colonisation by decay fungi and long-term performance
2002 - IRG/WP 02-20251
Many of the L-joint trials conducted at BRE were assessed during the early stages to establish the rate of colonisation by fungi, principally basidiomycetes. At that time, a system of assessment incorporating colonisation studies was proposed for inclusion within the European Standard EN 330 but was rejected for the final version of the standard. The long-term trials associated with the colonisa...
J K Carey


Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany, where Oil-...
C R Welzbacher; A O Rapp


Japanese standardized methods for testing effectiveness of chemicals against termite attack
1986 - IRG/WP 1290
Japanese standard termiticide testing methods are reviewed. There are some standard testing methods provided by Japan Termite Control Association (JTCA) and Japan Wood Preserving Association (JWPA), though most of them are common to two organizations. Methods were standardized between JTCA and JWPA in 1981, and more recently examining system was established for authorizing efficacy of wood preserv...
K Tsunoda, K Nishimoto


Accelerated laboratory testing of preservatives on 13 North American wood species
1999 - IRG/WP 99-30201
The ability of selected water and solvent based biocides to protect wood against fungal attack was evaluated on 13 North American wood species using 7 decay fungi in a modified soil block test. Most preservatives were capable of providing protection at their recommended above ground and soil contact use levels. Many decay fungi caused substantial weight losses on blocks treated with chlorothalonil...
J J Morrell, C M Freitag


Blue Stain Testing of Alkyd and Acrylic Stains
2003 - IRG/WP 03-20273
Resistance against blue stain of semi-transparent alkyd and acrylic stains was tested by both EN 152 and the so-called reverse exposure test methods. Comparison of the results, obtained by both methods was the most important aim of this study. As expected, performance of the water-borne acrylic paint was lower compared to protective effectiveness of the alkyd stain. This difference was even more p...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


An appraisal of methods for environmental testing of leachates from salt-treated wood; part 1
1998 - IRG/WP 98-50115
The magnitude and diversity of leaching tests with salt-treated wood, performed by institutes as well as industry, strongly appeal for harmonisation towards one single method. That procedure should be well-defined, cost- and time-effective and moreover be extended with a clear detection and interpretation scheme. The paper(s) presented here tend to evaluate 2 existing leaching methods, the ENV 12...
G M F Van Eetvelde, M Stevens, F Mahieu, H-W Wegen, A Platen


Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox


Unsuitability of the limiting dose as a criterion for assessing the toxicity of preservatives to wood-destroying fungi
1974 - IRG/WP 243
In the majority of methods for investigating preservatives for wood-destroying fungi their toxicity is assessed by determining what is called the "limiting dose". This normally denotes a range of preservative solution concentrations or retentions of dry preservative in the timber, the lower value serving to indicate the amount of preservative at which is observed the expected effect, e.g. the grow...
D A Belenkov


L-joint trials: Part 3: Relative performance of a range of preservative products
2002 - IRG/WP 02-30292
Long-term trials using the L-joints described in BS EN 330 and AWPA Standard E9-97 have been in progress at BRE since 1982. This paper records the current assessments of decay of L-joints in trials started between 1982 and 1994 with treatments applied to both Scots pine sapwood (Pinus sylvestris) and spruce (Picea sp.). Data are provided on a range of active ingredients including TnBTO, PCP, a...
J K Carey


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Preservation of robinia wood (Robinia pseudoacacia L.) stakes by vintners
1982 - IRG/WP 3194
This work discusses decay resistance of robinia wood to fungi Trametes versicolor (L.ex Fr.) Pil. and Coniophora puteana (Schum. ex Fr.) Karst., and also the possibility of influencing its resistance by means of chemical protection. The results showed that natural resistance of robinia wood to these two different agents of wood decay is not the same. It is much less resistant to the fungus Conioph...
R Benko


A technique for assessing the preventive efficacy against decay fungi of preservative treatments applied to wood
1988 - IRG/WP 2309
A method is described in which test blocks with envelope preservative treatments can be challenged by selected test fungi previously established on an untreated feeder block. The progress of the test fungus through the treated zone is monitored using novel baits or sensors inserted in holes drilled into blocks to within predetermined distances of the face being challenged. Preliminary results show...
J K Carey, A F Bravery


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 1: Laboratory screening tests using a filter paper technique
1977 - IRG/WP 290
Thirty-one miscellaneous formulations have been screened using a filter paper assay technique, for their efficacy in controlling the growth of Chaetomium globosum, Cephalosporium acremonium, and a mixed inoculum of finely ground soft-rotted wood obtained from preservative treated transmission poles. The formulations consisted of various organic compounds and inorganic preparations made from differ...
H Greaves


Alternatives to CCA for ground contact protection of timber: a perspective from UK on performance and service life expectations
2002 - IRG/WP 02-30289
The proposed amendment to the European Union's Marketing and Use Directive (1976/769/EEC) in respect of arsenic in CCA wood preservatives seeks to restrict the use of CCA across the European Union. CCA is an extremely important wood preservative in the UK from the manufacturing of the product to the extent of use of CCA-treated timber. Based on our experience and judgement on the use of ...
E D Suttie, A F Bravery, T B Dearling


An Australian test of wood preservatives. Part 1: Preservatives, principles and practices
1978 - IRG/WP 2123
Between November, 1963, and July, 1964, a graveyard test of some 6000 preservative-treated stakes was installed at 8 sites equally distributed between Papua New Guinea in the tropics, through Queensland and New South Wales to Victoria. More than 40 different preservatives and preservative mixtures, mostly at several different levels of retention, were used to impregnate sawn specimens of Pinus rad...
J Beesley


Copper naphthenate-treated Southern Pine pole stubs in field exposure: - Part 1: Gradient & biodeterioration analysis 12 years after treatment
2000 - IRG/WP 00-30242
Naphthenates have been used for the preservation of timber and cellulose since their original identification in Russia in the early 1880's as part of a series of petroleum characterizations. Later work in the development of copper naphthenate as a heavy-duty preservative for poles led to the development of various treating cycles similar to other oil-borne systems. Recent work concerning ...
H M Barnes, M H Freeman


Proposals for further co-operative studies on determining toxic values against wood-destroying Basidiomycetes
1985 - IRG/WP 2247
Document IRG/WP/2194 reported the status of the programme of co-operative experiments up to and including December 1982. During discussions at IRG-13 in Turkey members endorsed the decision to complete the programme of tests and conduct repeat tests. At IRG-14 in Brisbane the report was noted but no further action agreed. At IRG-15 in Sweden a number of interested parties in the European/Scandinav...
A F Bravery


Copper linoleate: A new low toxcity wide spectrum, heavy duty wood preservative
1995 - IRG/WP 95-30082
Copper linoleate, a "fixed" copper soap has been developed and evaluated in South Africa over a 30-year period. The initial product, an organic solvent based preservative has been tested in pine poles against termites and fungi. Results indiate that the product has performed well against existing heavy duty wood preservatives such as CCA and creosote in long term field trials (30 years). The paper...
D Conradie, P Turner, W E Conradie, A J Pendlebury, T Pizzi


Report on the co-operative leaching tests
1975 - IRG/WP 246
The Work reported here was undertaken at the request of CEN to see (1) whether the standard beaker leaching method under discussion at CEN, and based on the German DIN could be made less labour intensive; and (2) whether the leaching parameters could be expressed in more general terms so that alternative procedures could be used. A co-operative experiment was set up in which the amount of leaching...
J W W Morgan


Laboratory bioassays with termites – The importance of termite biology
2005 - IRG/WP 05-10550
Subterranean termites are frequently used in bioassays to asses the effectiveness of insecticides or the resistance of materials. Termites which appear to be vigorous with high inherent levels of activity are often relied upon, yet at the end of the experiments survival may be very unsatisfactory, even in the favourable environment of controls. Consequently, results from such bioassays may be mean...
M Lenz