IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 206 documents. Displaying 25 entries per page.


Losses of pyrethroids from treated wood due to photodegradation
1998 - IRG/WP 98-30177
The fact that significant photodegradation of pyrethroids can occur in use has been established for over 20 years. It is known, mainly from experience with tsetse fly control, that such degradation leads to marked reductions in efficacy. This realisation has lead to extensive investigation into ways of stabilising this group of important insecticides. Pyrethroids are widely used as the insecticid...
J D Lloyd, M W Schoeman, F Brownsill


Observations on preservative penetration in poplar
1991 - IRG/WP 3662
In the course of studies on the CCA treatment and durability of poplar timber a zone of refractory wood at the sapwood/heartwood boundary was observed. Further studies were conducted to investigate the causes of this refractory behaviour. The initial results have suggested that the presence of lipid storage products in the ray tissue may lead to impermeability, either by directly blocking pits or ...
R J Murphy, S U Din, M J Stone


Preservative treatment of Gollah cane (Daemonorops jenkinsiana) by soaking method
2001 - IRG/WP 01-40197
The feasibility of preservative treatment of gollah cane (Daemonorops jenkinsiana (Griff.) Mart.) by soaking method was tested in the present study. Cane samples of 1m, 2m and 3m long were soaked with 10% borax and boric acid solution. The study revealed that adequate dry salt retention (DSR) in the above samples could be obtained in 3 days, 4 days and 5 days of soaking, respectively. Within these...
M Younus-uzzaman, K Akhter, M H Chowdhury


Comparison of variable, constant and fluctuating pressure methods
2001 - IRG/WP 01-40212
The objective of this work was to evaluate potential improvements in pressure treatment arising from the use of a control valve. A constant pressure of 1035 kPa was compared to the conventional variable pressure method where the pressure is allowed to drop to 860 kPa as the solution is absorbed by the wood. A fluctuating pressure method (FPM) where the pressure cycles between 1000 and 1070 kPa was...
S M McFarling, P I Morris


Alternatives to preliminary oven-drying prior to spot-testing treated timber for borate or TBTN preservative penetration
1995 - IRG/WP 95-20067
Commonly-used penetration test procedures for timber treated with borate or organotin wood preservatives demand preliminary oven-drying before application of the spot-testing reagent(s), in order to achieve reliable results. The delay of 12 hours or more during oven drying is often a nuisance. Modifications to the spot-testing procedures, involving alternative solvents and acidification conditions...
M J Kennedy, A Zosars, J Norton


Standardization of preservative treated timber species for conductor, insulator and transformer packing of REB
1996 - IRG/WP 96-40071
In order to resolve the post landing failure problem of wooden packing for conductor, insulator, transformer of REB, the names of the suitable timber species from different parts of the world, irrespective of countries of origin have been standardized along with their strength and treatability grades. The CCA treatability of some Pakistani timber species have been presented for example which was t...
A K Lahiry


Investigations of the treatability of various commercially significant Turkish timbers
1976 - IRG/WP 370 E
Timbers which naturally deteriorate quickly can only be used commercially when their life is increased by the use of chemical treatments. The treatment of the timber can only be planned on a regular basis when the treatability of the wood is known. The purpose of the experiments was therefore to determine to what extent the various types of wood could be sufficiently impregnated. The question of t...
R Ilhan


Adequate preservative treatment of kiln dried Eucalyptus camaldulensis and Acacia mangium for tropical and subtropical wood poles
1996 - IRG/WP 96-40075
The Eucalyptus camaldulensis and Acacia mangium round timbers kiln-dried at EMC and full cell pressure treated with CCA-C ensured requisite penetration and adequate dry retention (30 kg/m³ or 4% w/w). The sufficient inherent strength, seasoning property, treatability of sapwood and heartwood equivalent to 44% of radius, natural durability of heartwood, and field investigation on service performan...
A K Lahiry


Ponding of radiata pine (Pinus radiata) - 2. The effect of ponding on coating penetration into wood
1998 - IRG/WP 98-10249
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks, dried and subsequently coated with a primer and examined by light microscopy after staining sections with Sudan IV to enhance the contrast of the primer material. A correlation between the extent of ponding and the extent of coating penetration into wood was observed. The coating penetration var...
A P Singh, S S Gallagher, U Schmitt, B S Dawson, Yoon Soo Kim


Clean creosote - its development, and comparison with conventional high temperature creosote
1983 - IRG/WP 3235
Pigment emulsified creosote (PEC) is presently being tested and shows considerable stability in terms of water content, pigment level, pH, viscosity, rheological behaviour and microscopy. Timber samples from several eucalypt species have been treated with PEC and side matched samples treated with conventional high temperature creosote (HTC). The PEC treated specimens showed higher weight retention...
C W Chin, J B Watkins, H Greaves


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


Depth of foraging of subterranean termites in tropical Australia
1996 - IRG/WP 96-10141
Stakes of radiata pine (Pinus radiata D.Don) of varying lengths to 800 mm were inserted vertically in the soil with all but their lower 100 mm sheathed in a capped UPVC tube representing a physical barrier to termites. In one series of trials, termites were encouraged to aggregate at the upper ends of the tubes, in order to determine whether they would descend to the lower end of the barrier. In a...
L R Miller, M Hoschke, M Neal


Development of a disinfection treatment for oak logs to be imported from the USA
1984 - IRG/WP 3283
The European veneer industry depends greatly on oak supplies from the USA. To prevent the accidental introduction of the American Oak Wilt Disease (Ceratocystis fagacearum) into the member states of the EC, a disinfection treatment was developed for oak logs under consideration of the technical requirements of veneer production. Laboratory experiments and field trials in Germany and in the USA sho...
W Liese, M M Ruetze


Improved preservative penetration of spruce after pre-treatment with selected fungi. II. Creosote treatment, analysis and strength testing
1998 - IRG/WP 98-40106
This paper describes the creosote treatment and analysis of logs pre-treated with selected fungal agents as a method of increasing the porosity of the wood prior to preservative treatment. The paper also reports the subsequent strength testing of the timber to evaluate the effects of the fungal pre-treatment on the structural integrity of the wood. European spruce logs were pre-treated with eithe...
E J Tucker, A Bruce, H J Staines, B Rosner, K Messner


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Silicon tetrachloride: A potential wood preservative
1980 - IRG/WP 3133
In its present form, this paper is a preliminary draft of a paper that will eventually be submitted for publication in the Forest Products Journal. We are continuing the work on the effects of silicon tetrachloride on wood and expect to have additional data for the meeting in May 1980. Specifically we are measuring the penetration rate and depth of SiCl4, and we are chemically analyzing the treate...
C W Owens, W T Shortle, A L Shigo


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Microemulsion formulations for wood protection chemicals
1993 - IRG/WP 93-30030
A microemulsion is a thermodynamically stable oil-water dispersion system. As a formulation it provides many unique features such as water compatibility for water-insoluble chemicals, formulation stability, good bioavailability and environmental acceptance. This paper discusses the major criteria for the formulations of water-insoluble wood biocides and the comparison in properties between convent...
Bing Yu, L E Leightley


The treatability of five Indonesian wood species with BFCA preservative
1987 - IRG/WP 3428
This paper deals with a preliminary study on the treatability of five Indonesian wood species, i.e. Altingia excelsa (AE), Rhodoleria teysmanii (CA), Litsea odorivera (LO), Schima wallichii (SW) and Cratoxylon arborescens (CA). Wood samples measuring 4 x 4 x 100 cm³ were dipped into BFCA preservative solution for about 30 seconds. Preservative penetration and the surface area of treated zone were...
Nana Supriana, T K Waluyo


Practical experiments with Boracol 10 Rh used as a fungicide in the repair process after attack by the dry rot fungus (Serpula lacrymans)
1987 - IRG/WP 3458
The test is carried out in an old house in Nyhavn, Copenhagen. The roof and the walls close to were heavily attacked by dry rot fungus (Serpula lacrymans) because damage to the zinc covering the frontspice were letting in water to the wood and wall construction. An attack by the dry rot fungus is more complicated to repair compared with other wood destroying fungi because beside the damage on wood...
J Bech-Andersen


Penetration as Key Factor for Determining the Performance of Wood Preservatives
2004 - IRG/WP 04-20293
Stakes of Scots pine sapwood with a dimension of 4 x 4 x 75 cm³ were impregnated with preservatives containing 2 % of propiconazole which had passed the EN 113 test criteria without any problems. The penetration of the colourless preservative was determined successfully by a fungal screening test described by Sutter (1978). The test revealed the insufficient penetration behaviour within the gi...
H Leithoff, I Stephan, R-D Peek


Treatment of rubberwood (Hevea brasiliensis)
1997 - IRG/WP 97-40081
In this study treatability of rubberwood, timber from rubber trees (Hevea brasiliensis) was investigated by using both pressure and non-pressure methods. Samples with 4 cm by 4 cm cross section were sawn from the logs which were harvested from a plantation located in Batu Pahat, Johor, Malaysia. Full-cell and cold soaking methods were employed using Copper Chrome Arsenate (CCA) for the experiments...
S Hiziroglu


Influence of different treatment parameters on penetration, retention and bleeding of creosote
2003 - IRG/WP 03-40255
Creosote is an extensively used preservative for transmission poles and sleepers. The purpose of this research was to investigate the treatment parameters necessary to achieve full sapwood penetration and minimum required retention and to avoid bleeding of creosote. It was carried out as a part of the European research project WOODPOLE. Transmission poles of Scots pine (Pinus sylvestris L.) previo...
Ö Bergman


Protection of rubberwood timber. Part 1: Impregnation with boron preservatives
1989 - IRG/WP 3551
Rubberwood (Hevea brasiliensis) were treated with a 3% proprietary mixture of borax/boric acid using three different treatment schedules i.e. full-cell, full-cell to refusal and full-cell with 12 cycles of vacuum/pressure. Freshly cut samples had mean preservative retentions of 187 kg/m³, 214 kg/m³ and 178 kg/m³ respectively. Pre-air dried samples for one week had retentions of 252 kg/m³, 308 ...
L T Hong, C C K Liew


Suitability of propiconazole (R 49362) as a new-generation fungicide
1989 - IRG/WP 3529
Propiconazole (R 49362), an anti-fungal triazole-compound of Janssen Pharmaceutica, has been extensively tested to determine its potential use as a wood preserving fungicide. Various tests in both private laboratories and official institutes indicate a good activity against Basidiomycetes (brown and white rot) and Ascomycetes (blue stain-in-service). The active ingredient seems very resistant to w...