IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 267 documents. Displaying 25 entries per page.


Water absorption and desorption of non treated, pressure impregnated, and pine oil treated glulam made of small diameter Scots pine and Norway spruce
2012 - IRG/WP 12-40616
A growing proportion of harvested timber originates from the first or second commercial thinning stands in Finland, which means smaller average log volumes in comparison to final felling stands. Smaller log volume means challenging wood properties such as higher proportion of juvenile wood and sapwood. Due to these facts, products made of small diameter logs are prone to twist and check, and have ...
H Heräjärvi, V Möttönen, R Stöd


Activities of moulds on wood as a function of relative humidity during desorption and absorption processes
2013 - IRG/WP 13-10794
Three different types of indoor moulds: Penicillium brevicompactum, primary colonizer; Alternaria tenuissima, secondary colonizer and Trichoderma harzianum, tertiary colonizer, grown on wood were measured for their activities under different relative humidity levels. The activities were measured by isothermal calorimetry. The activities of the moulds changed with the change of the relative humidit...
Yujing Li, L Wadsö


CT scanning of decay in creosoted poles for overhead lines
2013 - IRG/WP 13-30634
Creosote-treated poles have been examined by means of CT scanning in order to investigate the nature of soft spots that have been found more frequently during the last five years in Sweden. CT scanning provides a very good picture of the interior of the poles and decay can easily be detected. It was concluded that the soft spots in most cases were caused by decay which in turn had to do with extre...
C-J Johansson, A Clang, I Johansson, G Berggren


Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin


Effect of electron beam irradiation on the fire retardant penetration into wood
2013 - IRG/WP 13-40642
Electron beam processing which can fast and easy change the nature of the material has received considerable attention recently. Studies using electron beam has been conducted in various fields and it has been applied in many industrial sectors. Electron beam has higher energy than other electromagnetic waves. It has excellent object permeability. It affects degradation of intermolecular cross-lin...
Dong won Son, Jong Sin Lee, Mee Ran Kang, Sang Bum Park


Effectiveness of Copper Indicators in Treated Wood Exposed to Copper Tolerant Fungi
2014 - IRG/WP 14-20554
Wood treated with a copper based wood preservative will typically turn a green color. While the depth of copper penetration can be readily discerned from the green color of the copper it is standard practice in research and commercial treating plants to make use of a color reagent such as Chrome Azurol S, Rubeanic acid or PAN indicator to reveal the penetration more clearly. When copper treat...
L Jin, K Brown, A Zahora, K Archer


Scanning Transmission X-ray Microscopy as a tool for examining chemical changes in wood cell walls due to enzymatic activity
2014 - IRG/WP 14-20556
As development of techniques for examining enzymatic activity on solid, complex biological materials, is considered to be an important factor in further development of enzyme applications and for understanding the decay of plant materials, this study explores applicability of Scanning Transmission X-ray Microscope (STXM) for determining chemical changes in enzymatically treated samples at the cell...
D Jeremic, R Goacher, R Yan, C Karunakaran, E R Master


Using Commercial Water Repellent Chemicals on Wood Protection
2014 - IRG/WP 14-30656
Lately, researchers have been looking for process and products that use environmental friendly technologies in wood protection. These sorts of innovations on wood protection should be carried out for wood evaluated at outdoor conditions. Using water repelling chemicals is one of those innovations which improve wood durability and dimensional stability by decreasing content of moisture. In this ...
G Köse, A Temiz, S Demirel, O E Özkan


Effect of Nano-Wollastonite on Water Absorption in Particleboard
2014 - IRG/WP 14-40662
Effects of wollastonite nanofibers on physical properties of particleboard were studied. Nano-wollastonite (NW) was applied at 5, 10, 15, and 20 g/kg, based on the dry weight of wood-chips, and compared with control specimens. Two application methods of NW were used: surface application (SA), and internal application (IA). Density was kept constant at 0.68 g/cm3 for all treatments. Tests were carr...
S Karimi, H Reza Taghiyari, A Karimi, P M Tahir, J Abdul Halip


A guideline for sorting easy to impregnate Scots pine sapwood based on three treatability studies from Northern Europe
2014 - IRG/WP 14-40669
Scots pine sapwood is generally considered an easy to impregnate wood species, though it reportedly faces challenges towards a homogeneous impregnation and large variations in treatability are reported for the material. This study comprises the results of three treatability tests that were performed on Scots pine (Pinus sylvestris) sapwood. The material impregnated was originated from a large ...
K Zimmer, E Larnøy, A Treu


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


New Method for Pretreatment of Railroad Crossties
2014 - IRG/WP 14-40675
Creosote has been successfully utilized for nearly 150 years for the protection of railroad crossties (sleepers) in the USA and remains today as the most widely used wood preservative for this application. One of the few shortcomings of creosote as a preservative is its inability to penetrate many of the refractory hardwood species which make up the majority of crossties in the USA. Lack of full...
A S Ross, R W Clawson Jr


Leachability and Dimensional Stability of Nanosilver-Steamed Densified Poplar
2014 - IRG/WP 14-40684
This study was aimed to investigate leachability and dimensional stability of nanosilver impregnated poplar (Popolus alba), steamed before hot compression. Wood samples were impregnated with nanosilver suspension (200 and 400 ppm) under pressure of 4 bar for 20 minutes. Steam treatment was carried out at 150°C for 2 hours. Then samples were compressed (33%) radially in a hot press at 170°C for 3...
G Rassam, A Talaei, A Ahmadi


Penetration of phenol formaldehyde (PF) resin into beech wood studied by light microscopy
2015 - IRG/WP 15-20558
In this study, we examined the distribution and penetration depth of phenol-formaldehyde (PF) resin into wood specimens by light microscopy (LM). Two PF resins from different producers, of concentrations 9, 18 and 27 wt % in water, were vacuum impregnated into European beech wood (Fagus sylvatica) blocks of 15x25x50 mm³. The presence of chemical agent in the wood was carried out by way of their i...
V Biziks, S Bicke, H Militz


Development of a new characterization method to analyse Cypermethrin penetration in wood material by immunolabelling
2015 - IRG/WP 15-30674
The preservative efficacy of organic biocides is strongly related to their capacity of penetration and retention within wood tissues. The specific detection of the pyrethroid insecticide cypermethrin is currently obtained after extraction followed by chemical analysis by chromatography techniques. However visualizing the insecticide molecule within the wood structure requires specific probes toget...
S Tapin-Lingua, K Ruel, J-P Joseleau, D Messaoudi, O Fahy, M Jequel, M Petit-Conil


Distribution and penetration of the tung oil in wood studied by high-resolution magnetic resonance imaging
2016 - IRG/WP 16-20593
Water repellents as environment-friendly treatments are gaining their popularity as non-biocidal solutions for wood protection. One of the most important water repellents for wood besides waxes and organosilicon compounds are drying oils. Tung oil is one of the best performing oil. However, tung oil, similarly as other oils, does not penetrate deeply into wood, due to its high viscosity. In order...
M Žlahtič, U Mikac, I Serša, M Merela, M Humar


A Comparison on Penetration of Silica Sol in Scots pine and Southern pine wood
2016 - IRG/WP 16-40722
Penetration is one of the most important issues to be considered in wood impregnation with various kinds of chemicals in liquid form. Scots pine (Pinus sylvestris) and Southern pine (Pinus spp.) are two frequently used wood species for treatment, such as preservative treatment. With the development of treating systems, some micro- or nano-sized aqueous modifiers are emerging in the market, which p...
Mingyang Sun, Jinzhen Cao


Impregnation of railway sleepers - Pressure gradient and transversal penetration
2016 - IRG/WP 16-40731
Based on the possible ban of creosote in the future, the need for oil based alternative products has gained in importance. Due to possible differences in impregnation properties compared to creosote the need for re-implementing former technology is given, to determine if momentarily used impregnation processes have to be modified. The here reported tests measure the pressure gradient during the im...
M Starck, A Gellerich, H Militz


The effect of acetylation on physical properties of beech (Fagus orientalis) and Alder (Alnus subcordata) wood
2016 - IRG/WP 16-40759
In this study the effect of acetylation on physical properties such as water absorption, volumetric swelling and anti-shrink efficiency (ASE) of beech and alder were investigated. After 24 hours soaking in acetic anhydride, in order to achieving two surface of weight gains, acetylated samples were heated in oven at 120 0C for 90 and 360 minutes. Then water absorption and dimensional stability in...
M Akhtari, M Arefkhani


Evaluation of Particulate Materials as a Physical Barrier against Termites under Floor of Experiment House
2017 - IRG/WP 17-10900
In Japan, the damages by the subterranean termites (Coptotermes formosanus and Reticulitermes speratus) are more common. Recently the more attention is paid to the less- or non-chemical methods for termite control. As a non-chemical treatment, physical barriers using particles such as gravels were investigated in terms of environmental safety, cost effectiveness, and duration of performance, and t...
Y Yanase, Y Fujiwara, Y Fujii, T Mori, T Yoshimura, S Doi


Quality of the impregnated wood in the Slovenian hardware stores
2017 - IRG/WP 17-20606
Ten different samples from Slovenian hardware stores were analysed. Samples were treated with copper based wood preservatives and designed and advertised to be used in heavy duty applications in use classes 3.2 or 4. In order to determine the quality of the treatment penetration, retention and fungicidal properties were determined. Retention was determined with XRF analysis, while modified EN 113 ...
M Humar, B Lesar, N Thaler, D Kržišnik, N Kregar, S Drnovšek


Overview of the treated wood quality control program in the United States with the recent challenges and advances
2017 - IRG/WP 17-20616
In the past two decades, there have been significant and rapid changes in wood protection technologies for residential applications which have moved away from long established heavy duty metal oxide based products such as chromated copper arsenate (CCA). The successor generation of wood protection systems usually contain copper as the primary biocide, in combination with carbon-based co-biocides s...
L Jin


Effects of heat treatment on sound absorption coefficients in nanosilver-impregnated and normal solid woods
2017 - IRG/WP 17-40770
Effects of impregnation with silver nano-suspension as well as heat-treatment on sound absorption coefficients (AC) were studied in tangential direction of five different solid woods based on their importance. AC was measured at two frequencies of 250 and 500 Hz. A 400 ppm nanosuspension was used for the impregnation; silver nanoparticles had a size range of 30-80 nm. Based on the obtained results...
A Esmailpour, J Norton, H R Taghiyari, H Zolfaghari, S Asadi


Effect of Particle Size on Wax Distribution in Paraffin Wax Emulsion Impregnated Wood
2017 - IRG/WP 17-40779
Paraffin wax emulsion impregnation has been a common eco-friendly approach for improving water repellency of wood. In this study, southern pine (Pinus spp.) and Scots pine (Pinus sylvesteris L.) samples were impregnated with paraffin wax emulsions of different solid contents and particle sizes, and then the time domain nuclear magnetic resonance (TD-NMR) was used to elucidate the influence of part...
Wang Wang, Jinzhen Cao, Yiheng Huang


In-service performance of treated plywood bridge decks in Australia
2017 - IRG/WP 17-40794
Engineered wood products have a long history of use in bridge construction in Australia. The first bridges incorporating chemically protected engineered wood components were installed in the 1850’s and some survive to this day. Preservative treated plywood bridge deck panels have been employed since the 1980’s as a replacement for the more traditional hardwood plank decks. This paper report...
M A Powell


Previous Page | Next Page