IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3025 documents. Displaying 25 entries per page.


The preventive actions of three commercial wood preservatives against Dinoderus minutus
1984 - IRG/WP 1233
Dinoderus minutus is one of the most common pest insects for the bamboos. For preventing the damages of this insect, the preventive treatment of bamboos with preservatives is necessary. But because of the environmental reasons, only limited insecticides are available in Japan. The author determined the preventive effects of three commercial products against Dinoderus minutus by the medium of the B...
K Suzuki


The influence of gaseous oxygen concentration on fungal growth rates, biomass production and wood decay
1998 - IRG/WP 98-10283
The effects of air and several levels of oxygen balanced with nitrogen (% oxygen (v/v) nitrogen to 100%) on growth rates, biomass production and wood decay were investigated. The best technique for measuring daily growth rates in anaerobic jars was found to be by using 40 mm petri dishes which were attached to the walls of the jars. At the end of the test period the same petri dishes were also use...
S M Kazemi, D J Dickinson, R J Murphy


Biocontrol and bioprotection of wood decay and sapstain fungi
2003 - IRG/WP 03-10474
The most serious damages caused in the wood industries by decay and sapstain fungi, and the growing international pressures on the use of biocides products with toxic active ingredients harmful to human health and the environment, have made it necessary to search for alternative chemical products to protect the wood, and for the possibility to use micro-organisms as biological controllers. This la...
M T De Troya, F Rubio, M Villarreal, F Arenal, F Llinares, V Rubio, D Muñoz-Mingarro, N Acero


Preliminary study on relation of wood structure to copper/chrome/arsenic (CCA) distribution in kempas (Koompassia malaccensis)
1995 - IRG/WP 95-40054
Kempas had been treated with copper/chrome/arsenic (CCA) preservative using full cell process. Analysis of preservative distribution at the micro level in relation to wood structure was carried out using scanning electron microscope (SEM) and energy dispersive X-ray (EDXA) analysis. The results showed that CCA elements were detected in all wood tissues at different ratios. Distribution of chemical...
S Ani, S Salamah


Natural durability of Iranian saxual wood (Haloxylon persicum) against the fungal decay
1991 - IRG/WP 1515
Haloxylon persicum is vidly planted in the deserfic region of Iran. At the present time, in the age of 30, these small trees are ready for cutting for the different uses, specially for rural buildings. But there's any knowledge about its durability. In this study the laboratory tests were carried out in accordance to European Standard. 5 fungi were used as: Trametes versicolor, Coniophora...
D Parsapajouh, F H Schweingruber, K Richter


Acceleration of the fixation of chromated wood preservatives by UV-radiation
1989 - IRG/WP 3544
Preliminary laboratory tests demonstrated that the fixation of chromated water-borne wood preservatives may be accelerated by UV-radiation. The degree of fixation depends on the intensity of radiation and the prevailing temperature. Three hours radiation at 20°C in a device for artificial weathering diminished the leaching of chromium to 43% and of copper to 23% compared to not-radiated samples. ...
H M Illner, H Willeitner, K Brandt


A Preliminary Report on the Properties of Engineered Wood Composite Panels Treated with Copper Naphthenate
2005 - IRG/WP 05-40294
This paper reports on our preliminary investigation of the properties of randomly oriented strandboard which had waterborne or powdered copper naphthenate (CuN) incorporated into the board during manufacture. When compared to zinc borate-treated controls (ZnB), the mechanical properties of strandboard (MOR, MOE, work-to-maximum load, internal bond strength) were not adversely affected by treatmen...
J W Kirkpatrick, H M Barnes


Leachability And Decay Resistance of Copper-Treated Wood
2004 - IRG/WP 04-30337
Samples of scots pine sapwood (Pinus sylvestris L.) were treated with solutions of (Copper II sulfat-5 hydro + fluoroboric acid) and (Copper II sulfat-5 hydro + fluoroboric acid + boric acid) in order to determining to leachability and decay resistance against brown rot fungus (Postia placenta) and white rot fungus (Coriolus versicolor). Results indicated that the copper in treated wood is less s...
A Temiz, T Nilsson, I Deemirtas, Ü C Yildiz


Degradation of the gelatinous-layer in aspen and rubber wood by the blue stain fungus Lasiodiplodia theobromae
1996 - IRG/WP 96-10168
Studies on the degradative ability of the blue stain fungus Lasiodiplodia theobromae Pat. have shown several strains to cause significant weight losses (i.e. ca 20%) in the temperate and tropical wood species, aspen (Populus tremula) and rubber wood (Hevea brasiliensis). In addition to the consumption of soluble carbohydrates and extractives, major changes in the ultrastructure of fibre cell walls...
O Encinas, G F Daniel


Decrease of the antidecay resistance of beech wood treated with organotin fungicides after its natural ageing
1998 - IRG/WP 98-30185
The antidecay resistance of beech-wood samples (120 x 8.5 x 8.5 (MM)) treated with tributyltin fungicides gradually decreased due to prolongation of their natural ageing: tributyltin fungicides (TBTO, TBTS, TBTCA, TBT-DEDTK were applied by pressure impregnation technique in ethanole solutions (c = 0. 1%, 0.33% or 1%); treated beech-wood samples were naturally aged without their contact with grou...
L Reinprecht


Characterization of tropical wood-decaying fungi by RFLP analysis of PCR amplified rDNA
1998 - IRG/WP 98-10251
Five brown-rot fungi (Tyromyces palustris, Gloeophyllum trabeum, Antrodia sp., Poria placenta, Coniophora puteana) and three white-rot fungi (Coriolus versicolor, Pycnoporus sanguineus, Lentinus squarrosulus) registred as representative wood-decaying fungi for international standards of wood durability tests have been characterized using molecular tools (PCR/RFLP). The Internal Transcribed Spacer ...
A Zaremski, M Ducousso, Y Prin, D Fouquet


Study of the degradation of retified wood through ultrasonic and gravimetric techniques
1994 - IRG/WP 94-40030
One of the non-polluting processes that increase the natural durability of wood is a thermal treatment in an atmosphere poor in oxygen, producing what is normally denominated "retified wood". In this study the validity of a non-destructive technique (ultrasound) in order to determine the biodegradation suffered by wood across time has been studied. For this reason, the behavior of a wood species (...
D T De Troya, A M Navarrete


Health and safety aspects of the use of wood preservatives in Sweden
1977 - IRG/WP 396
The Act on products Hazardous to Health and to the Environment (Swedish Code of Statutes SFS 1973:329) came into force on 1st July 1973. The Act cancelled and superseded the Poison Act, the Pesticides Act and the PCB Act from 1962, 1962 and 1971 respectively. Regulations for the implementation of the Act are contained in the Ordinance on Products Hazardous to Health and to the Environment (SFS 197...
B Henningsson


Bioefficacy of boric acid grafted onto wood
1999 - IRG/WP 99-30202
The use of borate treated wood in outdoor is limited because of the migration of borate. The objective of this study is to investigate the fixation of boric acid in wood using polyethylene glycol (PEG-400) to form polyester borate and isocyanato group as coupling agent. FT-IR was used to monitor the reaction between boric acid and PEG. Elemental analysis was conducted to evaluate the C, H, and N v...
Weining Cui, D P Kamdem


Resistance of Teak, Balau, keruing and Chengal Wood species against marine borers attack
2004 - IRG/WP 04-10513
Wood samples of Teak (Tectona grandis) , Keruing (Dipterocarpus alatus),Yellow Balau (Shorea laevis) and Chengal (Balanocarpus heimii) were treated by Creosote, using Ruping method. The dimension of samples were 200 x 75 x 20 mm and the retention were 188, 186, 331, 40 kg /m3 respectively. Both treated and untreated samples were installed in sea water (Mahshar in Persian gulf and Bandar Torkman an...
A Rezanejad


Chelura terebrans (Crustacea: Amphipoda) is capable of degrading wood independently of its associate, Limnoria
1992 - IRG/WP 92-4180
Chelura terebans has been reported to be dependent on the tunnelling activities of Limmmoria. However, this study has shown that Chelura is capable of excavating its own grooves in the surface of blocks of the low density hardwood, balsa (Ochroma lagopus). When reared on blocks of balsa, Chelura ingests small wood particles. These particles often show evidence of degradation due to tunnelling bact...
S M Cragg, G F Daniel


Albumin borate: A new non-toxic, wide-spectrum, long-term wood preservative
1998 - IRG/WP 98-30167
Boron, widely recognized for its broad range of activity towards both fungi and insects and for its low mammalian toxicity, can not provide long term protection to treated timber due to its high leachability. Boron, in the form of boric acid, can be partially fixed to timber by the formation of an association with egg albumin, which is insolubilized by heat-induced coagulation. Chemical investiga...
M-F Thévenon, A Pizzi, J-P Haluk


Treatment of wood-based panel products with volatile borate
1990 - IRG/WP 3616
The paper presents recent developments in the use of volatile borate esters for the preservative treatment of wood based board materials. Several advances on previous reports are discussed. In laboratory studies, treatment times of approximately ten minutes at 20°C on boards at equilibrium moisture content provided full penetration and retentions of 1% wt/wt boric acid. Biological tests have been...
P Turner, R J Murphy, D J Dickinson


Effect of vegetable compost on leaching of CCA components from treated wood - An Update
1995 - IRG/WP 95-50048
In an earlier study, the effect of compost on CCA-C leaching was compared with leaching losses under different exposure conditions. Small treated cubes (25 mm³) were destructively sampled over a 12 month period and the residual CCA determined for exposure to compost in a compost bin, exposed to natural rain and buried in soil. This study provides a comparison after 3 years of samples exposed to c...
P A Cooper, Y T Ung


Wood decay of Pinus sylvestris L. by marine fungi
1990 - IRG/WP 1463
Waterlogged wood decay by marine microorganisms represents a major problem for the conservation of wood structures of historic value. It is important to know which kind of decay affects the wood from a conservation point of view. Enzyme activities of 14 marine fungi belonging to several localities were studied. Also, the weight loss and the rot type suffered by the wood at a microscopic level were...
M C Escorial, M T De Troya, J E Garcia de los Rios


Soil-bed studies. Part 2: The efficacy of wood preservative
1983 - IRG/WP 2205
Various methods of decay assessment were investigated. Three stages or phases of decay were identified which could be used to describe the efficacy of a preservative system or virulence of a soil-bed testing medium. These included the lag, decay, and senescent phase. Premature senescence could arise if wood samples became waterlogged. It was concluded that time to failure was unsuitable as a metho...
P Vinden, J F Levy, D J Dickinson


The effect of mortality diseases on wood quality of sissoo (Dalbergia sissoo Roxb)
2006 - IRG/WP 06-10569
Sissoo (Dalbergia sissoo Roxb.) is a lagre deciduos, fast growing, strong light demanding and leguminous tree specie. It is an important multipurpose specie widely being planted in the agro forestry and and social forestry pratices in Bangladesh, particularly in the north and south-western parts of the country. On account of its better quality, sissoo is valued as good as construction and utility ...
M M Islam, M O Hannan, G N M Ilias


A comparison between the effects of ACC & CFK on the durability of beech, hornbeam and cottonwood by using Dipping & Bethel methods in the North of Iran
1997 - IRG/WP 97-40089
From the economical point of view, increasing the lumber durability by the application of preservative treatments is very important. In this study, samples were randomly selected from Fagus orientalis Lipsky., Carpinus betulus L. and Populus deltoides Bartr. in two forms (Board & Squared cross-section) and have been treated with ACC & CFK by using Dipping & Bethel methods. The matched ...
D Parsapajouh, V Etemad, K Pourtahmasebi


Microwave conditioning of Pinus radiata D. Don for preservative treatment
2000 - IRG/WP 00-40182
This paper reviews the effect of pressure steam conditioning on the permeability and treatability of green radiata pine heartwood and the potential for substituting microwave conditioning for steaming. The penetration of liquids into radiata pine occurs mainly in the radial tissue. The permeability of green radiata pine improves following steam conditioning by blowing out the soft radial tissue. T...
P Vinden, G Torgovnikov, J Romero


Occurrence of marine wood borers at three ports in Andhra Pradesh, India
2004 - IRG/WP 04-10509
Marine wood borers are a specialised group of organisms which destroy the wooden structures and cause huge monetary losses. They are site specific and their distribution depends on the water quality of a particular area. Seven species of wood borers such as Martesia striata, Teredo furcifera, T. parksi, Lyrodus pedicellatus, L. bipartita, Bankia campanellata and B. carinata have been identifi...
B Tarakanadha, M.Balaji, R Ramamurthi, K S Rao


Previous Page | Next Page