Diagnosis of failures in wood beams from historical house in Banská Štiavnica – Relations between ultrasonic measurements and bending properties
2010 - IRG/WP 10-20437
Various degrees of rot and other damages in ceiling beams with dimensions of 6500-8800 x 160-200 x 240-310 mm (length x height x width) situated in one historical bourgeois house in the UNESCO town Banská Štiavnica, Slovakia were determined visually and by the PUNDIT-plus ultrasonic device. Subsequently, for seventeen of the most bio-damaged fir (Abies alba Mill.) beams chosen for exchange were ...
L Reinprecht, M Pánek


Service life prediction of wooden components – Part 1: Determination of dose-response functions for above ground decay
2010 - IRG/WP 10-20439
Scots pine sapwood (Pinus sylvestris L.) and Douglas fir heartwood (Pseudotsuga menziesii Franco) specimens were exposed in double layer field trials at 24 different European test sites under different exposure conditions (in total 28 test sets). The material climate in terms of wood moisture content (MC) and wood temperature was automatically recorded over a period of up to eight years and compar...
C Brischke, A O Rapp


Service life prediction of wooden components – Part 2: Impact of material, exposure and design details
2010 - IRG/WP 10-20440
Dose-response functions permit to estimate the moisture and temperature induced decay potential for any wooden building component and exposure, and thus the service life to be expected. In part 1 of this series dose-response functions were established as a result of double layer field trials carried out at 24 European test sites over up to eight years. Using them makes it no longer necessary to co...
C Brischke, B Lauenstein, M Bilstein, T Bornemann, A O Rapp


Development of microbiological test methods for the wooden packaging of foodstuffs
2010 - IRG/WP 10-20453
Whereas different sampling methods already exist for analysing contaminated surfaces or packaging made of plastic or paper, there is no methodology that enables the sampling and quantification of microorganisms in packaging made of wood. The objective of this study was to compare the most commonly used microbiological methods and to develop a reliable quality control test adapted to wooden packagi...
I Le Bayon, H Callot, M Kutnik, C Denis, A-M Revol-Junelles, J-B Millière, M Giraud, M Gabillé, N Passédat


Chemical protection of historic timber structures: Results and future needs
2010 - IRG/WP 10-40487
The paper concentrates on the analysis of the effectiveness of chemical protection for timber structures in the Russian State Museums “Kizhi” (Karelia) and “Vitoslavlitsy” (Novgorod). The condition of historic timber was tested at the monuments treated with PCP, borax, potassium carbonate, boric acid, Pinotex chemicals in the 1970-80. Long-term analysis revealed that in many cases the...
M Kisternaya, V Kozlov


Repairing of wooden elements by beta-method using carbon, steel or beech rods
2010 - IRG/WP 10-40488
Presented paper is focused on repairing of wooden elements by Beta joints reinforced with carbon, steel or beech rods, and on comparing the efficiency of these joints with traditional carpentry joints. In model laboratory experiments have been determined the bending strength (fm) and the modulus of elasticity (E) of control or original elements (fm-Control; Eo) from Norway spruce (Picea abies Kars...
L Reinprecht


Study on the thickness swelling of mould-resistant chemical treated bamboo strand woven outdoor flooring
2010 - IRG/WP 10-40489
To prevent bamboo strand woven flooring from mould, several preservatives were chosen to treat bamboo strand before dipping into adhesives and pressing. The thickness swelling and mould resistant effect of the finished board were studied. Results showed that different preservatives had different influences on the thickness swelling of BSWF, and in order to reduce the thickness swelling of the fini...
Fangli Sun, Binfu Bao, Shenyuan Fu, Anliang Chen


Reconstruction and Restoration of some Zagreb’s Wooden Heritage buildings
2010 - IRG/WP 10-40498
In the last ten years, the huge amount of wooden buildings houses and objects of Zagreb’s cultural heritage were restored with fine workmanship. As the wood was one of the most used construction materials, the scientists and specialists from the Faculty of Forestry also took part in those restoration and reconstruction processes. The aim of this article is to inform and advice the restorers on t...
R Despot, M Hasan


Degradations and conservation strategies for an XVIII-th century wooden church from Oltenia County, Romania
2010 - IRG/WP 10-40521
The wooden churches construction has a rich tradition in Romania, the technique spreading from North – Maramures, to South, especially in hill and mountain areas. The church from Ursi village, Oltenia County, represents a particular case, the church being abandoned since 1913. The lack of a roof for a long time resulted in severe deterioration of the whole structure. Yet the inner and outer wall...
G Niculescu, O Chachula, A Nicolaescu


Growth conditions for fungal decay in wooden constructions – practical experience versus literature
2011 - IRG/WP 11-10758
Data regarding moisture and temperature requirements of decay fungi found in literature have been compared to experience from observations in a large number of Norwegian buildings. A number of selected situations are discussed, among those exposure to high relative humidity, exposure to free water and decay in the supposedly adverse conditions on Svalbard. The moisture content in wood has to be at...
M Sand Sivertsen, J Mattsson


Cobblestone Church in Gross Gievietz: Historic Wooden Construction and Potential for Conservation and Use
2011 - IRG/WP 11-10760
A majority of cobblestone churches situated in the German Federal State Mecklenburg-Vorpommern demonstrates immense construction deficiencies and are threatened by decay. The historic cobblestone church located in Groß Gievitz, built in the 13th century, is one such church in which the roof beam constructions have degraded considerably due to deficiencies in reconstruction measures. This paper d...
A Schulze, W Unger


Service life prediction of wooden components - Part 3: Approaching a comprehensive test methodology
2011 - IRG/WP 11-20464
This paper is the third in a series on 'service life prediction' of wooden components and should be considered as a discussion paper. The authors tried to analyze the topic with a look from a distance and comment sometimes with a smile on the current controversial discussion about SLP issues. Nevertheless, the viewpoints of different groups, such as natural scientists, engineers, approva...
C Brischke, C R Welzbacher, L Meyer, T Bornemann, P Larsson Brelid, A Pilgård, E Frühwald-Hansson, M Westin, A O Rapp, S Thelandersson, J Jermer


Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


Performances of Douglas fir in real outdoor use conditions
2011 - IRG/WP 11-20472
The European standard EN 350-2 classifies Douglas fir as moderately resistant to fungal decay on the basis of standardized laboratory and field tests. However, the lifespan expectancy of outdoor structures such as cladding, decking and elements of wood construction carpentry may also vary according to environmental conditions (climate, exposure to weathering), maintenance and design. An investigat...
M Kutnik, S Lepetit, S Le Nevé


Fixed Borates Anyone?
2011 - IRG/WP 11-30563
The quest for a borate based preservative system that resists leaching or is “fixed” has long been a research goal. Boron fixation has been attempted with numerous strategies but there have been problems associated with past methods. This paper discusses new fixation systems based on bio-materials and presents up to five year outdoor exposure testing on full-size decks. Generally, the new f...
C R McIntyre, M A Lake


Standardized Field Trials with Micronized Copper
2011 - IRG/WP 11-30564
In 2008, an extensive review of all available data from standardized tests of micronized copper systems was published and there has been considerable work since then. This paper discusses over 20 field stake trials underway in well-known sites such as Gainesville, FL, Hilo, HI and the Dorman and Saucier sites in MS as well as tests from Australia and New Zealand. In addition, 4 ground proximity ...
C R McIntyre, M H Freeman


Tannin resin-boron for outdoor wood protection and fire retardancy
2011 - IRG/WP 11-30567
Boron in the form of boric acid is well known for its efficacy against wood destroying organisms, as well as for its high leachability from treated wood when in outside exposure. Moreover, due to the European directive 2008/58/EC, boric acid is only authorized at low levels. In order to keep considering boric acid as an interesting active ingredient for wood protection, the issue is now to fix it ...
M-F Thévenon, G Tondi, N Leménager, S Wieland, A Pizzi


Effectiveness of Water Based Bentonite-Borate Slurry for In-situ Remedial Protection of Historic Wooden Piles: The Eurobor Protocol, Part 2
2011 - IRG/WP 11-30574
The study of the biocide product Eurobor®, water mixture of boric acid, borax and sodium bentonite, aimed to verify previous findings regarding borates penetration from a clay-water mixture of foundation timber. The product was applied on samples from 100 year old timber foundation from the city of Göteborg. Although in ground for this long the timber was in acceptable god condition due to groun...
M. Theorin, K. Fimmerstad, K-M. Bandh


The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon


The Effectiveness of Machined Profiles at Reducing the Checking of Wooden Decking
2011 - IRG/WP 11-40541
This study tests the hypothesis that ‘the ability of surface profiling to reduce checking of deck boards exposed to weathering will vary with wood species and profile type’. Southern pine (Pinus sp.) and Pacific silver fir (Abies amabilis) deck boards were machined to produce three different types of surface profiles: flat (control), ribbed (V-shaped grooves), and rippled (U-shaped grooves). B...
P Evans, I Cullis, P Morris


A Critical Review and Survey of the US Wooden Pallet Industry: Focusing on Market Segmentation & N. American Trends
2011 - IRG/WP 11-40545
This paper reviews the history and current and predicted future use values in N. America. Included in this work is historical data on rationality and wood species used to manufacture wooden pallets in the USA and an ongoing current market survey sent to the 1000 largest manufacturers and re-manufacturers in the USA based on SIC Code 2448(Standard Industrial Code Classification). Although CHEP, the...
M H Freeman


Evaluation of an optimized industrial process aiming to improve the natural durability and mechanical behavior of bamboo for outdoor use
2011 - IRG/WP 11-40554
Mao Bamboo (Phyllostachys pubescens) is characterized by high contents of sugar and starch and by high hygroscopicity, which makes it susceptible to biodegradation, and specifically to fungal decay. Still, many bamboo based products regularly enter the European wood construction market, competing with traditional solid wood products used for outdoor decking and cladding. The performance of a heat ...
F Simon, M Kutnik, I Le Bayon, G Moisset, V Gatimel


The overview of ISPM 15 implementation in Croatian wood-working companies
2011 - IRG/WP 11-30576
Croatia is a small European county, but in the same time a great country according to it’s tradition in the forestry and wood working industry. However, around 48% of it’s territory is afforested. As the export is one of the main directions in the Croatian development conception, the production and distribution of wood package intended for the international trade, is one of the most important ...
R Despot, V Jambrekovic, M Hasan


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Comparative studies on the moisture performance and durability of wooden facades
2012 - IRG/WP 12-20492
Wooden claddings are traditionally used in many parts of the world. Also modern structures are frequently made from timber and timber engineering panel products. However, wood has to compete with other cladding materials and its durability needs to assure sufficient functional and aesthetic service life. Besides many other factors the durability of a wooden facade is dominated by its moisture perf...
T Bornemann, C Brischke, J-M Lück