Decrease of the antidecay resistance of beech wood treated with organotin fungicides after its natural ageing
1998 - IRG/WP 98-30185
The antidecay resistance of beech-wood samples (120 x 8.5 x 8.5 (MM)) treated with tributyltin fungicides gradually decreased due to prolongation of their natural ageing: tributyltin fungicides (TBTO, TBTS, TBTCA, TBT-DEDTK were applied by pressure impregnation technique in ethanole solutions (c = 0. 1%, 0.33% or 1%); treated beech-wood samples were naturally aged without their contact with grou...
L Reinprecht


A comparison between the effects of ACC & CFK on the durability of beech, hornbeam and cottonwood by using Dipping & Bethel methods in the North of Iran
1997 - IRG/WP 97-40089
From the economical point of view, increasing the lumber durability by the application of preservative treatments is very important. In this study, samples were randomly selected from Fagus orientalis Lipsky., Carpinus betulus L. and Populus deltoides Bartr. in two forms (Board & Squared cross-section) and have been treated with ACC & CFK by using Dipping & Bethel methods. The matched ...
D Parsapajouh, V Etemad, K Pourtahmasebi


A study of decay type variability in variously treated Fagus sylvatica and Pinus radiata field test stakes exposed at a vineyard for 30 - 45 months
1998 - IRG/WP 98-10271
Pinus radiata test stakes were treated with 10 kg/m3 of CCA plus 4 lower retentions in a geometric series of 1.5. Fagus sylvatica was treated with 15 kg/m3 and 2 lower retentions. Both timber species were also treated with equivalent retentions of various new generation preservatives (P. radiata was also treated with creosote). Whilst these stakes were exposed at 11 sites in New Zealand (NZ) and 2...
R N Wakeling, A P Singh


Comparative life cycle assessment of Swiss railroad sleepers
1998 - IRG/WP 98-50117
The results of an environmental LCA carried out on railway sleepers made of prestressed concrete, sectional steel and creosote impregnated beech as used on main lines of Switzerland's railways are presented. All extractions from and insertions into the environment which were connected with the manufacture, use and disposal of the different types of sleeper were inventoried and assessed, i...
T Künniger, K Richter


Investigation on different variation factors in the results of mycological test and means to reduce and avoid them
1986 - IRG/WP 2264
In order to clarify the causes of the dispersion observed in the results obtained with mycological tests made in accordance with standard EN-113, different factors assumed to be sources of the variations were studied. These included the moisture content of the test samples during the test, the influence of certain technological properties of the wood, the virulence of the fungus strains, the metho...
D Dirol


Acetylated solid wood. Laboratory durability test (part 2) and field trials
1995 - IRG/WP 95-40048
Degradation of acetylated beech, pine and poplar by soft rot fungi was related to strength loss in a laboratory test. No strength loss was noticed for poplar acetylated to a weight percent gain (WPG) of more than 11.2% and beech with a WPG of 12.8%. Several field trials were set up to determine the durability of acetylated products in practice. They included a field test to determine the durabilit...
E P J Beckers, H Militz, M Stevens


Biological resistance of aldehyde-treated wood
1994 - IRG/WP 94-40018
Biological resistance of wood treated with aldehyde cross-linking agents such as glyoxal, glutaraldehyde and dimethylol dihydroxy ethyleneurea (DMDHEU) were investigated. Sapwood blocks of Japanese cedar and Japanese beech, measuring 20 x 20 x 10 mm³ (T x R x L), were vacuum-impregnated at room temperature with 5-25% of aldehyde solutions. Blocks were kept in the solution for 1 week to gain the o...
S Yusuf, Y Imamura, M Takahashi, K Minato


An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Improvements of stability and durability of beechwood (Fagus sylvatica) by means of treatment with acetic anhydride
1991 - IRG/WP 3645
In the present investigations, beechwood (Fagus sylvatica) was treated with non-catalysed acetic anhydrid at 120°C and some physical- and biological parameters of the treated wood were compared with those of non-treated wood. The radial and tangential shrinkage and swelling, respectively, and the absorption capacity of the acetylated wood against moisture is considerably lower. The durability aga...
H Militz


Soft rot - Soil burial - Tests. Influence of the water content of the soil on wood decay
1972 - IRG/WP 212
The decay of wood samples buried in the soil is influenced by various factors. Decisive are the water content, the content of organic substances, pH-value content of mineral nutritive substances etc. of the soil. For the tests, carried out by the EMPA until now, it was always started with a water content of 35%, refered to the dry weight of the EMPA-soil = 75% of its water capacity. In order to in...
O Wälchli


Relative performance of copper/chrome/boron (CCB) and copper/chrome/arsenate (CCA) in ground contact
1992 - IRG/WP 92-3694
The performance of four retentions each of an oxide CCA formulation and a salt formulation of CCB in radiata pine and European beech was compared after 18 years' field exposure. In radiata pine CCA oxide was more effective (4 failures out of 40) than CCB (9 failures out of 40). However, in European beech CCB was substantially more effective (22 failures) than CCA oxide (all failed). Analy...
M E Hedley


Effect of cyclic change of temperature on fungal growth and mass loss
1994 - IRG/WP 94-10065
For estimating the effect of cycling change of temparature on fungal growth, four Japanese species, sugi (Cryptomeria japonica), hinoki (Chamaecyparis obtusa), akamatsu (Pinus densiflora) and buna (Fagus crenata), four fungal species, Tyromyces palustris, Gloeophyllum trabeum, Coriolus versicolor, Pycnoporus coccineus, and five temperature conditions, 10, 20, 27, 35°C and cyclic temperature (20°...
K Suzuki, K Okada


Effect of wood species on decomposition efficiency of metham sodium
1992 - IRG/WP 92-3699
The effect of wood species and temperature on efficiency of metham sodium (32.1% sodium N-methyldithiocarbamate) decomposition to methylisothiocyanate (MITC) was investigated on 10 hardwoods and 9 conifers over a 144 hour period. Gas chromatographic analyses of headspace samples and ethyl acetate extracts of the wood revealed that decomposition never approached the theoretical decomposition effici...
J J Morrell


Hardwood field experiment - 10 year report
1989 - IRG/WP 3560
The international hardwood field experiment was planned in 1976 and set up in some 34 different sites around the world. The test stakes include 4 reference species common to each site and in most cases at least 2 species of local importance (supplementary species). It was hoped that a picture of performance of a range of economically important timber species would be built up and at the same time ...
D J Dickinson, S M Gray


A marine borer test with water-borne preservatives
1980 - IRG/WP 452
The use of preservative treated timber in sea-water where marine borers are active is of great economic importance, since untreated wood immediately will be damaged. Vacuum/pressure treated timber has been tested in several marine exposure trials on the Swedish west coast since the 1930s (Hager 1941, Hultman 1949, Sandstrom 1951, Nylinder-Norman et al. 1974). Since new interesting materials or pre...
B Henningsson, E Norman


Preservative-efficacy of boric acid-triethanol amine solution against wood-decay fungi
1994 - IRG/WP 94-30050
Laboratory preservative-efficacy tests were conducted using boric acid-triethanol amine (BTEA) solution in accordance with the JIS A 9201 (1991) test method excluding the standard weathering process. Sapwood specimens of Picea jezoensis or Fagus crenata to achieve nominal retentions of 0.40-41.2 kg/m³ of boric acid were exposed to Tyromyces palustris, Coriolus versicolor, Serpula lacrymans or Cha...
S Doi, M Mori, Y Mineki


The influence of the location of a wood defect on the modulus of elasticity determination in wood durability testing
2004 - IRG/WP 04-20287
This study investigates the influence of the location of a wood failure in stakes upon elastic changes observed in beech specimens with the resonance vibration technique. Natural failures were simulated by artificially created defects at different locations of the test stake. The results indicate that the location of an attack in a stake is important for the measurement outcome. When the attack is...
L Machek, H Militz


Tests with ammoniacal copper and alkyl ammonium compounds as wood preservatives
1984 - IRG/WP 3299
Formulations based on copper and alkyl ammonium compounds in ammonia solution have been tested in a fungus cellar on Pinus radiata and Fagus sylvatica. This type of products gives promising results as wood preservatives, especially on hardwood and are safe to destroy by e.g. combustion. The best results were achieved with a dialkyl ammonium compound, Cu/octyldecyl dimethyl ammonium chloride (NH3)....
C-E Sundman


Soluble nutrient influences on toxicity and permanence of CCA preservatives in wood
1980 - IRG/WP 3144
The influence of soluble carbohydrate and nitrogenous components concentrated at evaporative surfaces of wood on the toxicity and permanence of CCA preservatives has been examined using soil-burial techniques. Nutrient concentrations in lime (Tilia vulgaris Hayne) have been shown to be associated with reduction of toxic limits of preservatives to an extent in which a 100% increase in preservative ...
B King, G M Smith, A Bruce


On the occurrence of Phialophora species in preservative treated wood in ground contact
1977 - IRG/WP 163
Phialophora is a fairly large genus comprising about thirty described species. They are widespread in very diverse environments, such as soil, sea water, wood and wood pulps. Some species are known as parasites on plants and animals, including man. Phialophora species were early known for their ability to produce blue stain in timber. Later it was discovered that several species were able to produ...
T Nilsson, B Henningsson


Evaluation of a new anti-sapstain formulation
1994 - IRG/WP 94-30035
A new anti-sapstain mixture, which consists of 2% IPBC (3-iodo-2-propynylbutyl carbamate) and 1.5% DCOI (4,5-dichloro-2-n-octylisothiazolin-3-one), was evaluated by three methods in the laboratory. A standardized test (JWPA standard 2) demonstrated that the new anti-sapstain formulation was highly effective in controlling growth of monocultures of five test fungi on wood substrate. When exposed to...
K Tsunoda, H Kumagai, M Sakurai


Effect of test site, preservative and wood species on decay type Glenbervie pastoral and radiata pine forest sites
2000 - IRG/WP 00-30248
Pinus radiata stakes were treated with 0.8, 1.2, 1.8, 2.7 and 4.1 kg/m3 of CCA and Fagus sylvatica with 2.7, 4.1 and 6.1 kg/m3 of CCA. Both wood species were also treated with equivalent retentions of a copper plus triazole preservative (CT) (0.89, 1.3, 2 and 3 kg/m3 of copper for pine & 2.5 and 4 for beech) and chlorothalonil plus chlorpyriphos in oil (CC) (1.4, 2.1, 3.2 and 4.8 kg/m3 of chlo...
R N Wakeling


Laboratory tests on the natural durability of timber methods and problems
1984 - IRG/WP 2217
In literature a large variety of test methods is mentioned to examine the natural resistance of timber against fungal attack. This concerns the kind of sampling as well as the test procedure, the test fungi, the duration of test, and the classification of the resistance according to the test results. These variations, however, are of great influence on the test result. Long term exposure will lead...
H Willeitner


Influence of different resin treatments on the dimension stability of wood
1997 - IRG/WP 97-40090
The dimension stability of wood is considered to be an important contribution to its durability and its performance in practice. A number of different treatments have been developed to improve the dimension stability of wood. One applied method is the treatment of wood with monomers or resins. The application of appropriate impregnation conditions seemed to be essential to enhance the efficiency o...
M Sailer, A O Rapp


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud