IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 351 documents. Displaying 25 entries per page.


A technique for determining the efficacy of water diffusible preservative plugs for implanting in joinery in service
1987 - IRG/WP 2291
A technique is described for determining the efficacy of soluble, diffusible preservative plugs for eradicating decay in joinery. It uses blocks of Scots pine sapwood or heartwood adjusted to known moisture contents prior to the establishment of the test fungus Coniophora puteana, from a single longitudinal dowel and the subsequent introduction of the preservative plugs. Prevention of decay, eradi...
J K Carey, A F Bravery


Studies on the fungicidal effectiveness of a petroleum derived product as a creosote alternative
1986 - IRG/WP 3384 E
This work, appears first because of the necessity to find out a profitable use for a residual product of the petrol pyrolisis, and second, because the lack of high natural durability wood used until now-a-days to build posts and sleepers in creosote lacking countries. Our main objective was pointed to the characterization of this new product and to find out the effectiveness against the wood-destr...
A M Navarrete, M T De Troya


Wood protecting chemicals for the 21st century
1993 - IRG/WP 93-30018
After assessing the past research with protection chemicals, this paper proposes future avenues for research and development in wood protection. Three scenarios are put forward for consideration. First, more is not better and future systems will emphasize combination formulations which enhance properties while providing biological efficacy. Second, current systems, especially those based on copper...
H M Barnes


Durability of some alternatives to preservative treated wood
2004 - IRG/WP 04-30353
The environmental discussion in Sweden has lead to an increasing use of naturally durable domestic wood species and wood treated according to alternative methods for use above ground. A number of these alternatives have been tested according to field- and laboratory tests and compared to wood treated with preservatives for above ground use. Seven untreated wood species, four alternative wood treat...
M-L Edlund


Application of oscillating pressure to improve treatability of refractory species
1987 - IRG/WP 3449
Under practical conditions a minimum moisture content of 80% demande by the German quality standard RAL-RG 411 can not be guaranteed throughout the year. Storage of logs with bark prolonges the drying process; a storage without bark must be avoided. A sufficient penetration according the standard can be achieved at least with a moisture content of 60%, optimal conditions may prevail between 100% a...
R-D Peek


The effect of moisture content on the electrical resistance of timber as detected by a pulsed current reistance meter (Shigometer)
1984 - IRG/WP 2212
The literature concerning the use of the Shigometer® for detecting decay in standing trees and wood poles is reviewed and the differences of opinion over the effect of timber moisture content on electrical resistance are highlighted. A simple experiment designed to test this effect is described and the implications of the results for testing poles in service are discussed. There was a large diffe...
P I Morris, D J Dickinson


Influence of the content of organic matter of soil on the degradation of wood by soft rot fungi
1970 - IRG/WP 27
The degradation of wood specimen burried in the soil by soft rot fungi is influenced by a number of factors. These are in particular the water holding capacity, water content, content of organic matter, pH, content of mineral nutritive substances etc. The results of the interlaboratory tests, carried out within the IRG/WP let presume that the intensity of wood degradation occurs proportionally inv...
O Wälchli


Moisture content of logs under sprinklers
2000 - IRG/WP 00-40157
Logs are kept under sprinklers during storage for avoiding the development of sapstain fungi. According to literature, sapstain fungi do not develop if the moisture content is above 120%. It is supposed that, the water sprinklers maintain the log's moisture content above this value, but, very often, sapstain is found on sawn lumber cut from these logs. Logs are harvested and transported t...
M C Rose, A M Briones, M Fernández


Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp


The effect of oil-borne preservative treatments on the shear strength of FRP/wood composite adhesive bonds
2003 - IRG/WP 03-40265
Reinforcement of structural wood components with Fiber Reinforced Polymer (FRP) will enhance the beam’s strength, but actual data on long-term durability is sparse, not well documented or not readily accessible. In this study, bond properties of FRP-wood composite materials were investigated following treatment with creosote or copper naphthenate preservatives. The properties investigated inclu...
B Herzog, B Goodell, R Lopez-Anido


Application of paint primers after light organic solvent preservative treatment
1986 - IRG/WP 3381
The application of three alternative paint primers is investigated, including a slow-drying oil-based primer, a fast-drying oil-based primer, and a fast-drying water-based primer. The treatment schedules employed, in particular the evacuation period after treatment, have a marked effect on subsequent paintability. Priming can potentially be carried out immediately after treatment with approved Tim...
P Vinden


Whitewood - An external joinery timber?
1975 - IRG/WP 253
The timber used traditionally for softwood joinery in the UK is redwood (Pinus sylvestris). In the past its ready availability in the desired sizes and quality and its durability in service encouraged little competition. However, the past decade has seen some erosion of this position, particularly through the increased proportion of sapwood in redwood supplies. Since the sapwood is less durable th...
J W W Morgan


The use of lap-joints in natural durability testing: moisture content development during 36 months outside exposure trials
2000 - IRG/WP 00-20217
Lap-joint trials (following European Standard ENV 12037) were set up with 11 different softwood and hardwood species. The main aim was to evaluate the suitability of this test standard (developed for testing wood preservative effectiveness) for natural durability testing. The moisture development has been followed during a 36 months period. In this paper, the outcomes of different moisture content...
H Militz, C J Bloom


Potential use of an emulsified tar oil fraction as a wood preservative: Preliminary technological and environmental assessment
1994 - IRG/WP 94-50028
In order to meet the recent environmental concern specifications of creosote are altered, the B[a]P content is limited and restrictions on the emission of volatile organic compounds (VOC) and higher polyaromatic hydrocarbons (PAH) are expected in some countries. Research has been conducted on an emulsion of a selected tar oil fraction. Using a waterborne formulation opens new perspectives for targ...
G M F Van Eetvelde, R Leegwater, M Stevens


Why don't more people work with Serpula lacrymans nowadays? A discussion of some of the different approaches to experimenting with this unique fungus
1989 - IRG/WP 1383
Remarkably few laboratories are currently investigating this well-known fungus. Not only has it failed to gain acceptance as a standard test organism (for wood preservative evaluation) in many countries, but is also sometimes excluded from pure research studies when it ought to be an obvious first choice as a representative basidiomycete. This paper discusses some different approaches that have be...
J D Thornton


Changes of copper and chromium content after leaching in wood impregnated with the CCB and CB preservatives
2000 - IRG/WP 00-50147
The objective of the study was impregnated with CCB and CB preservatives pine wood of moisture content varying from 12% to 55% subjected to leaching. Losses of copper and chromium were determined for individual layers of wood up to 3 cm from the girth. The results were compared to the total amount of metals determined in water extracts. The degree of leaching of metal ions from wood of 55% moistur...
B Mazela


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


Analysis of the boron content of preservative treated oak and pitch pine heartwood before and after leaching
1992 - IRG/WP 92-3697
Studies to determine the effects, if any, of a variety of boron formulations on heartwood of English oak and American Pitch pine have been previously reported (King et al (1991)). Small wood blocks were treated, at 10°C or 45°C, with borax, polybor or Boracol 20 for periods of 1 month or 4 months then analysed or continuously leached with tap water for a period of 1 month. Reported results showe...
S McCutcheon, G M Smith, J W Palfreyman, B King


Soft rot in heartwood of preservative-treated pole stubs of Eucalyptus cypellocarpa L. Johnson
1983 - IRG/WP 1204
Pole stubs of Eucalyptus cypellocarpa L. Johnson, treated in the sapwood with certain waterborne preservatives and exposed for 21 to 23 years in a dry tropical region were severely soft-rotted in the heartwood, as well as the sapwood. They broke with a brash fracture when stress tested (loaded as a cantilever) in the field. The severe soft rot in the heartwood was not detected by the knife test or...
J E Barnacle, G C Johnson, M A Tighe


Protection of pine sawtimber and sawn timber against blue stain in Poland
1983 - IRG/WP 3193
The purpose of this paper is the synthesis of more important results of basic and applied research that have been grouped in the following problems: 1.: Fungi causing blue stain in the pine wood, occurring in Poland. 2.: Moisture content changes of pine sawtimber and sawn timber as the factor of blue stain producing fungi development. 3.: Effect of sapwood moisture content on the degree of wood st...
E Tarocinski, M H Zielinski


Factors affecting the resistance of fibre building boards to fungal attack
1975 - IRG/WP 252
Fungal decay is initiated at lower moisture contents in standard and tempered hardboards (18%) than in pine sapwood (26%). In contrast, in a saturated atmosphere, the equilibrium moisture contents of standard hardboard (14%) and of tempered hardboard (12.5%) are much lower than the moisture content permitting decay initiation whilst the equilibrium moisture content of pine sapwood (25.1%) approach...
C Grant, J G Savory


Effects of the delay in the beginning of treatment on absorption and distribution of water-soluble salts in posts treated by sap-replacement method
1992 - IRG/WP 92-3719
One of the most important matters in green wood treatments, such as sap-replacement method, is knowing the longest time available for beginning treatment without losing efficacy. In this paper, the influence of this factor on absorptions and distribution of the preservative into the wood is analized. Tree start-up times were first chosen: 3-6 hours, 48 h and 120 h after being cut down. The treatme...
M V Baonza Merino


Blue Staining of Coated Modified and Unmodified Wood
2006 - IRG/WP 06-10589
We investigated resistance of unmodified, DMDHEU modified and oil heat treated uncoated and coated Scots pine wood against blue stain fungi. Both EN 152-1 and the reverse exposure tests showed excellent resistance of DMDHEU and especially of oil heat treated wood against blue staining. It is not needed to add any additional protective coating layers to prevent modified wood from staining. However,...
M Petric, M Pavlic, M Humar, M Tomažic


Resistance of pine and spruce heartwood against decay - The effect of wood chemical composition and coating with water-borne wood oil product
2006 - IRG/WP 06-10597
Natural durability of wood has been widely studied, but the combination of the natural durability and different treatments has not been the focus of many studies. The durability of wooden products is mainly based on the water permeability and the resistance against organisms. In this study, the water absorption and decay resistance of sapwood and heartwood of Scots pine and Norway spruce were exam...
H Viitanen, S Metsä-Kortelainen, T Laakso


Termite Response to Oil-Heat-Treated Norway spruce, Scots Pine and Eucalyptus Wood
2006 - IRG/WP 06-20325
The work here presented focused on the behaviour of subterranean termites (Reticulitermes grassei Clément) towards Oil-Heat-Treated (OHT) Norway spruce (Picea abies L.), Scots pine (Pinus sylvestris L.) and eucalyptus (Eucalyptus globulus Labill) wood, with a particular interest in the development of simple methods adequate to study the resistence of these materials to termite attack. Small test ...
L Nunes, T Nobre, C Welzbacher, A O Rapp


Previous Page | Next Page