Biodetioration and strength reductions in preservative treated aspen waferboard
1983 - IRG/WP 2195
Experimental aspen waferboards, bonded with liquid or powdered phenol formaldehyde resins and treated by various methods with a wide selection of preservatives, were tested for fungal resistance in accelerated laboratory trials. Mold growth on the surface as well as weight and strength losses due to the actions of decay fungi were determined. Testing of board strength after decay in high and moder...
E L Schmidt, H J Hall, R O Gertjejansen, R C De Groot


Fungal decay resistance of Rubber wood treated with heartwood extract of Rosewood
2005 - IRG/WP 05-30367
Alcoholic extract of Dalbergia latifolia heartwood was studied for its toxicity towards wood decaying fungi. Rubber wood blocks were treated with this extract to three different retention levels (0.1%, 0.2% & 0.5%) and the treated wood blocks were assessed for their resistance towards two white rot and two brown rot fungi. Treated blocks showed improved resistance over the control blocks. At 0...
A K Sethy, H C Nagaveni, S Mohan, K T Chandrashekar


Monitoring a Timber Bridge in Norway
2004 - IRG/WP 04-40282
We have instrumented three different timber bridges in Norway for the Norwegian Public Roads Administration. The goal was to learn more about the properties of timber bridges. We have instrumented Evenstad Bridge, Daleråsen Bridge and the last year Flisa Bridge. All bridges are have creosoted glulam trusses and creosoted stress laminated deck. Evenstad and Flisa have an asphalt deck on top, while...
F G Evans


Tilting and vacuum treatment - two methods to obtain a non-dripping freshly treated timber
1989 - IRG/WP 3535
Modern impregnation plants are designed to prevent spread of impregnation solutions from the plant through leakage, etc. It is also important that freshly treated timber does not spread solutions through dripping on the storage area. To prevent this, the impregnation procedure is terminated with a vacuum period. In many plants in Sweden this period is minimized or even excluded to gain time. Inste...
I Johansson, M-L Edlund


Investigations on testing with soft rot fungi by the vermiculite-burial method
1972 - IRG/WP 215
With the object of developing a test method to determine the effectiveness of wood preservatives against soft rot attack, tests have been carried out with pure fungal cultures using vermiculite as the substrate for untreated and preservative impregnated wood blocks. In these tests the suitability of common commercial, simple disposable beakers was proved successful as a substitute for the glass bo...
W Kerner-Gang, M Gersonde


Recycling and disposal of timber treated with waterborne copper based preservatives
1993 - IRG/WP 93-50008
Recycling and disposal technologies are briefly reviewed. Details are given of chemical extraction techniques suitable for recovery of copper from timber treated with a new copper based preservative, and traditional chromium based products. Details of thermal decomposition tests according to the DIN 53436 protocol under flaming and non-flaming conditions are given. The decomposition products were ...
J A Cornfield, S Vollam, P Fardell


A comparison of the diffusion of boron from two types of solid preservative rods into the heartwood of 3 Eucalypt pole species
2000 - IRG/WP 00-30227
The ability of boron to diffuse from polyborate and boron/fluoride rods through the heartwood of three eucalypt pole species (blackbutt, red ironbark and spotted gum) was examined. The aim was simply to determine the effects of rod type, wood species and time on the longitudinal diffusion of boron in eucalypt heartwood. Rapid diffusion of boron from polyborate or boron/fluoride preservative rods o...
P J Beutel, P D Evans


Anti-fungal properties of pyrolytic oils derived from softwood bark
2000 - IRG/WP 00-30218
Thermal decomposition of balsam fir and white spruce mixed bark residues at 450°C and under vacuum (< 20 kPa abs.) results in high yields of pyroligneous liquors rich in phenolic content. This vacuum pyrolysis process has been scaled-up to a pyrolysis plant with a feed capacity of 3.5 t/h of softwood bark, which is the largest plant of this type in the world. The pyrolytic aqueous condensates ...
D Mourant, Dian-Qing Yang, Xiao Lu, C Roy


Evaluation of white-rot fungal growth on Southern Yellow pine wood chips pretreated with blue-stain fungi
2000 - IRG/WP 00-10349
White-rotting basidiomycetes do not colonize on southern yellow pine. This study seeks to reduce the resinous extractive content of southern yellow pine by treating it with blue stain fungi. The mycelial growth of wood-inhabiting ligninolytic white-rot fungi can be achieved on pretreated southern yellow pine wood. Aureobasidium, Ceratocystis, and Ophiostoma spp. removed 70% to 100% of the extracti...
S C Croan


Blue stain in timber in service. Preliminary results of the IRG collaborative tests to compare natural and artificial weathering
1978 - IRG/WP 286
The collaborative programme was initiated at IRG Meetings in Wildhaus, 1976. The six collaborators were BAM (Berlin), Cuprinol Ltd (UK), EMPA (Switzerland), GORI (Denmark), PRL (UK) and Imperial College (UK). Experimental plans were finalised in December 1976 and panels treated by Cuprinol Ltd early in 1977. Natural weathering was carried out by BAM, Cuprinol, EMPA, GORI and PRL during April-Septe...
A F Bravery, D J Dickinson


Fungal decay of acrylate treated wood
2004 - IRG/WP 04-30357
Natural durability of wood species is variable. Chemical wood preservatives, such as biocides are necessary for extension of their service life. Many methods have been developed to increase the resistance of wood and wood products against wood-destroying organisms during the last years. The most frequently used methods are chemical and thermal modification of wood. In wood modification the basic c...
Z Tiralova, L Reinprecht


Biological degradation resistance of wood acetylated with thioacetic acid
1983 - IRG/WP 3223
Chemically, modification of wood is being considered as an alternative to conventional preservation by toxic chemicals. Acetylated wood has been reported to be quite resistant to most biodegrading organisms at weight percent gains (WPG) around 15-19. The conventional acetylation techniques with acethic anhyrdride result in generation of acetic acid. However, acetylation with thioacetic acid overco...
S Kumar, S C Agarwal


Three years of field tests with "Lignomer" stakes in ground contact
1981 - IRG/WP 3166
The "Lignomer" (Wood Polymer Composite) is a material obtained during the polymerisation of various monomers or its mixtures in wood. As laboratory tests have shown, this material is characterized by a high resistance against biological deteriorating agents. The laboratory investigations on the durability of various materials against biological deterioration are in many instances extended by field...
K Lutomski


After 18 years, preservative dipping and brush treating continue to provide protection to shingles of western wood species
1997 - IRG/WP 97-30156
The presence of residual preservation in dip-treated and brush-treated shingles of various species from the western United States was assessed 18 years after installation using Aspergillus bioassays. The performance of western redcedar (Thuja plicata) was compared to western hemlock (Tsuga heterophylla), sugar pine (Pinus lambertiana) and western larch (Larix occidentalis). Untreated shingles of a...
T C Scheffer, D J Miller, J J Morrell


Northern oak wood and its damages in Iran
1988 - IRG/WP 1377
The Northern oak species of Iran designated Quercus castaneaefolia C.A.M. is distributed widely in caspian littoral. In natural conditions (healthy) has favourable quality and it is used mostly in rural construtions, sleepers, parquets, cross arms for electric and communication poles, it is used also indoor and window construction, benches and finally veneer. This wood in the case of sleepers and ...
D Parsapajouh, P Niloufari


Protection of freshly felled timber against attack by bark boring insects
1981 - IRG/WP 1143
This report describes two experiments with the insecticide formulation Perigen, which contains the synthetic pyrethroid permethrin. At 0.2% w/v active ingredient individual logs were protected against bark boring beetles for 18 weeks. At 0.3% w/v active ingredients Perigen gave similar protection against insect attack to stacks of recently felled unbarked pine logs. This protection was at least eq...
J Dominik, P R Skidmore


A comparative analysis of Coniophora olivacea (Fr. ex Pers.) Karst. and Coniophora puteana (Schum. ex Fr.) Karst. test strains
1993 - IRG/WP 93-20004
Investigations were carried out to compare pure cultures of Coniophora olivacea (Fr. ex Pers.) Karst. used as a test fungus in Australia and other Pacific countries, and Coniophora puteana (Shum. ex Fr.) Karst. which is used in Europe. Comparisons included morphology, growth rate and dry mass of mycelium, decay capacity, influence of temperature, toxic value of CCA and quaternary ammonium compound...
J Wazny, L J Cookson


Variation in biological performance of CCA caised by preservative application method
1996 - IRG/WP 96-40072
A series of laboratory studies to investigate the influence of treatment application method on CCA performance in Cosican pine has been completed. Biological decay tests, such as serial exposures, were used to induce decay in wood at preservative retentions of up to 10 kg/m³ CCA salts. Significant differences in performance of the preservative against either brown, white or soft rot decay fungi w...
P R Newman, R J Murphy


Pollution in wood preservation - Aspects and problems
1973 - IRG/WP 55
In the field of wood preservation too, pollution problems have to be considered. They originate with the wood preservatives used. The extent of pollution differs widely with the type of preservative and the treatment process used. Per unit of impregnated timber, pollution will be lower if treatment is performed in treating plants than in distributed places. It will be highest for the old type Bouc...
H Willeitner


A review of the implementation of results-based standards for preservative treated timber
1999 - IRG/WP 99-20156
European standards for the specification of preservative treated timber are written in terms of the results achieved in the commodity by the treatment process. This is described in terms of penetration and retention of preservative. Results from a study on the commercial application of this approach in the UK show the difficulties associated with applying the new European standards; particularly w...
E D Suttie, A S Hughes, R J Orsler


Specifying preservative-treated resistant timber: Conforming to European Standards
2001 - IRG/WP 01-20235
The most common construction timbers used in the UK are of low natural durability and, generally, resistant to preservative treatment. These include species of spruce, hemlock and fir. However, their characteristically limited and non-uniform uptake of preservatives may still confer sufficient protection to give satisfactory durability performance in terms of biological resistance. This paper desc...
E D Suttie, A F Bravery, T B Dearling


The role of mechanised harvesters in the dissemination of fungal inoculum into radiata pine logs in New Zealand
2002 - IRG/WP 02-10426
A joint research programme has been initiated between Forest Research, New Zealand and Forintek Canada Corp., Canada, to determine the role of mechanical tree harvesters on disseminating fungal inoculum into logs. Mechanical harvesters cause loosening and removal of bark and also damage the surface of the wood with their feed rollers leaving indentations up to several centimetres deep. Results ...
D O’Callahan, B Kreber, A Uzunovic


Influence of the decay of spruce chips by the selected fungi on their chemical structure and the pulp properties
2004 - IRG/WP 04-10510
The paper focuses on changes in the weight and in the molecular structure of spruce chips submitted to long-term storing as well as to medium- and long-term model rotting degradation caused by some chosen fungi identified at storing processes on the pile. For the model decay of chips under laboratory conditions during 3 or 6 weeks the white-rot fungi: Phanerochaete chrysosporium, Heterobasidion an...
R Solár, L Reinprecht, A Geffert, F Kacík


Decay potential of various New Zealand Phlebiopsis gigantea strains using a soil block method
1999 - IRG/WP 99-10309
The objective of the current study was to determine the decay potential of different strains of Phlebiopsis gigantea using Pinus radiata and European Fagus sylvatica, respectively. A soil block method was used to determine mass weight loss of P. radiata and F. sylvatica following 10 weeks incubation with different strains of P. gigantea. For comparison, Trametes versicolor, Postia placenta, Gloeop...
B Kreber, J G Van der Waals


Cavitation bacteria
1984 - IRG/WP 1235
A form of bacterial wood degradation is described. The term "cavitation bacteria" has been coined in order to describe the discrete cavities that are formed within the wood cell walls. The bacteria observed within the cavities appeared to be polymorphic with rounded as well as filamentous forms recognised. TEM studies suggest that the bacteria produce diffusable wood-degrading enzymes. Cavitation ...
T Nilsson, A P Singh