Resistance of acetylated wood to biological degradation. Evaluation of field test
1997 - IRG/WP 97-30139
Acetylated wood samples were tested in ground contact (stake test) at two test fields, one in Simlångsdalen, Sweden, and one in Viikki, Finland, according to European standard EN 252. The test samples were inspected annually and their condition was compared with that of untreated controls and of samples treated with two reference CCA preservatives. The use of untreated controls and preservative t...
P Larsson Brelid, R Simonson, Ö Bergman


Growth of sapstain fungi in scots pine and the effect of timber ageing
1998 - IRG/WP 98-10269
A trial was initiated to study the growth of known isolates of sapstain fungi in scots pine (Pinus sylvestris) which had been naturally aged or sterilised by autoclaving or irradiation. Sawlogs cut from commercial thinnings were reduced to billet size and the exposed ends were painted with a bituminous sealant to reduce moisture loss. Some billets were inoculated after autoclaving or gamma-irradia...
N J Strong, J F Webber, R A Eaton


Persistance of active ingredients in treated wood
1993 - IRG/WP 93-50001-20
Disposing of chemically protected waste wood implies the distinction between surface and pressure treatment. Considering that barked round-wood merely contains, after 7 months open storage, less than 30 g per ton of bark or 25 mg per ton of sapwood, depending on the type of insecticide, the bark or sapwood shavings may be incinerated normally, according to less severe legal prescriptions than for ...
E Graf, P Manser, S Rezzonico, B Zgraggen


Movement of borates in a range of timber species at various moisture contents
1998 - IRG/WP 98-30181
Borate-based wood preservatives are used in industrial pre-treatment as well as remedial treatment of timbers in situ. In both of these areas, understanding the mobile nature of these compounds is important in optimizing the main benefits of borates. Considerable work has been conducted on movement of borates in dip-diffusion treatment of freshly felled wood, as well as focusing on subsequent diff...
M W Schoeman, J D Lloyd, M J Manning


Timber preservatives and corrosion
1983 - IRG/WP 3228
A survey of preservative treated timber commodities has illustrated problems that may be caused by corrosion. After treatment, timber should be compatible with commonly used fasteners. Whilst many corrosion methods have been used in the past, no standardized method is used by workers in timber preservation. The Queensland Department of Forestry is developing laboratory test methods for assessing c...
R I Davis


Multicomponent biocide systems protect wood from decay fungi, mold fungi, and termites for interior applications
2004 - IRG/WP 04-30333
Concerns about indoor air quality due to mold growth have increased dramatically in the United States. In the absence of proper moisture management, fungicides need to be developed for indoor use to control mold establishment. An ideal fungicide for prevention of indoor mold growth on wood-based materials needs to specifically prevent spore germination and provide long-term protection under condit...
C A Clausen,V W Yang


Resistance of six timber species, treated with CCA and CCB, against marine borer attack in Goa waters (India)
1991 - IRG/WP 4166
Panels of Lagerstroemia speciosa, Toona ciliata, Olea dioica, Pinus insignis, Acrocarpus fraxinifolius and Borassus flabellifer, pressure-treated with a 6.6% solution of Copper-Chrome-Arsenic (CCA) and 6% solution of Copper-Chrome-Boric (CCB), were exposed along with untreated controls, in triplicate, in Goa waters to, assess their resistance to damage by marine borers. The control panels were all...
L N Santhakumaran, R V Krishnan


Sampling and analysis of NeXgen-treated timber
1998 - IRG/WP 98-20134
Green sawn timber surfaces of the softwood Caribbean pine and the hardwood white cheesewood were treated by dipping, spraying, and precise spiking with the antisapstain product NeXgen. After storing for either two hours or two weeks, the treated surfaces were sampled by one of four alternative protocols, which included two involving a square wad sampling punch (one hit or six hits), one involving ...
M J Kennedy, D E Ferlazzo, T L Woods, M H Freeman


Field tests with Antiblue and Biocide TT for the prevention of sapstain and mould fungi on Pinus elliottii timber
1992 - IRG/WP 92-3682
Freshly cut and sawn Pinus elliottii timber was dipped in four concentrations of Antiblue (active ingredient sodium pentachlorophenate) and Biucide TT (local substitute), at four immersion times and stacked in the open at Chisengu sawmill. Five weeks later, the timber was assessed for the incidence and intensity of stain and mould. The results showed that Antiblue was the better chemical providing...
A J Masuka


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Detoxification of methylene bisthiocyanate by bacteria isolated from freshly felled, anti-sapstain treated timber
1993 - IRG/WP 93-10017
The microbial defacement of freshly-felled timber treated with organic biocides continues to be a major problem in stored lumber. As part of a study to investigate the depletion in chemical activity of methylene-bis-thiocyanate (MBT) in green timber, bacteria were isolated from freshly-felled boards of Corsican pine (Pinus nigra var. maritima Arnold) previously treated with different biocides. The...
R J Wallace, R A Eaton, G R Williams


Detection of methanogenic bacteria in mining timber
1988 - IRG/WP 1352
Methane explosions in gold mines have been attributed to spontaneous ignition of methane/air mixtures. Biogenesis of methane in the heartwood of diseased trees has been shown, but never in timber in service. Studies were therefore undertaken to establish whether methanogens were present in wooden pit props. Core samples were removed by Pressler increment borer from props in disused areas 2,600 m d...
L D Abraham, K Westlake, R I Mackie, J F Putterill, A A W Baecker.


Cytoplasmic and extracellular localization of manganese II dependent peroxidase(s) in white rot fungi during degradation of woody materials
1989 - IRG/WP 1416
The manner by which lignin is degraded in-situ in natural substrates by white rot fungi still remains a controversial issue particularly the distribution and role(s) played by lignin degrading enzymes (i.e. manganese II peroxidase and lignin peroxidase). In the present study, use was made of anti-manganese II peroxidase and immunolabelling techniques in conjunction with transmission electron micro...
G F Daniel, B Pettersson, T Nilsson, J Volc


Tunnelling bacteria
1983 - IRG/WP 1186
The micromorphology of decay in wood caused by a certain group of single-cell bacteria, called tunnelling bacteria (TB), is described. TB are characterised by their tunnelling ability within the secondary cell walls of wood fibres. Pure cultures of TB have not yet been obtained although the typical decay patterns can be reproduced using mixed bacterial cultures. Some indications of lignin degradin...
T Nilsson, G F Daniel


Chitosan for wood protection - state of the art
2005 - IRG/WP 05-30378
The aim of this paper was to give a state of the art description of chitosan as a wood protecting agent. Chitosan is a metal free natural compound derived from crustacean shells and is under evaluation as an environmentally benign wood protecting agent. Information from journals states that chitosan may act both fungistatically and at higher concentrations, as fungitoxic, but the mode of action is...
M Eikenes, G Alfredsen, E Larnøy, H Militz, B Kreber, C Chittenden


Fungal siderophores and their rôle in wood biodegradation
1990 - IRG/WP 1442
Iron and other metals such as manganese, play an important role in the metabolic functions of fungi that cause wood deterioration. These transition metals are also found in, or associated with, the extracellular fungal enzymes shown to be directly involved in the decay process. Recently our research group was able to show that siderophores (low molecular weight biological chelators) are produced b...
J Jellison, B Goodell, F Fekete, V Chandhoke


Micromorphology of decay in Keruing heartwood by the basidiomycetes Phellinus contiguus and Dacrymyces stillatus
2002 - IRG/WP 02-10454
This study aimed to characterise the micromorphology of fungal decay in a wooden handrailing in an above ground exposure at the Thames embankment in London. Keruing heartwood (Dipterocarpus spp.) was determined as the construction timber and the two basidiomycetes Phellinus contiguus and Dacrymyces stillatus identified as main decay organisms. Their decay patterns within Keruing heartwood were...
G Kleist, M Ray, R J Murphy


Microbial decay in an extremely durable Malaysian hardwood Belian (Eusideroxylon zwageri) - an overview
1997 - IRG/WP 97-10216
The heartwood of Belian (Eusideroxylon zwageri) is highly regarded among the naturally durable Malaysian hardwoods, and is therefore a choice timber for soilcontact use in the humid tropics such as untreated telecommunication poles, fence posts and railway sleepers. The high microbial resistance of the wood is evidenced by the mere superficial degradation observed in some pole samples after 20 yea...
A H H Wong, A P Singh


Leaching of active components from preservative-treated timber. Stages 2 & 3: Laboratory testing and comparison with semi-field testing
2004 - IRG/WP 04-20303
This part of the project is focussed on leaching from preservative-treated wood obtained by the laboratory test method CEN/OECD draft guideline, February 2003 ”OECD guideline for the testing of chemicals proposal for new guideline XXX. Estimation of Emissions from Preservative-treated Wood to the Environment: Laboratory Method for wood held in the storage yard after treatment and for wooden comm...
N Morsing, B Lindegaard


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Efficacy of fumigants in the eradication of decay fungi implanted in southern pine timbers
1986 - IRG/WP 3365
Southern pine timbers (15.2 cm x 15.2 cm x 4.26 m) were fumigated at midlength to evaluate the effectiveness of the fumigants chloropicrin, Vapam, Diazomet, Busan 40, Vanicide 51, Vanicide TH, sodium bisulfite, and ethanolamine in eradication of decay fungi. The fumigants were introduced into 2.54 cm holes which were closed immediately with rubber stoppers. Movement and persistence of lethal conce...
T L Highley, W E Eslyn


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 14: Report of sixth inspection (60 months) in Australia
1983 - IRG/WP 499
The IRG/COIPM International Marine Test was installed at Goat Island, Sydney Harbour, in December, 1977. The results of inspections made at 6, 12, 24, 36 and 48 months have previously been reported. This document records the data obtained on the 16.12.82, i.e. after 60 months exposure, at which time only 4 of the test frames remained in test. The surface water temperature at the time of inspection...
L J Cookson, J E Barnacle


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong