Laboratory investigations about the mobility of some inorganic wood preservatives in soils
1998 - IRG/WP 98-50101-22
Wood preservatives and components of wood preservatives leached from impregnated wood can enter the soil and thus contribute to the pollution of the groundwater. However, there is lack of understanding concerning the interacting parameters of wood preservative, leachate, soil and soil solution. To characterise of the behaviour of active ingredients and for the assessment of their environmental imp...
E Melcher, R-D Peek


Proposed test procedure to determine the effect of timber substrate on the effectiveness of a copper/chrome/arsenic preservative in seawater
1975 - IRG/WP 411
R A Eaton


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1983 - IRG/WP 3269
G C Johnson, J D Thornton


An approach to testing the preventive effectiveness of preservative treatments for wooden joinery
1981 - IRG/WP 2156
The ecological sequence established in field trial samples exposed out of ground contact has shown the need for outdoor exposure in testing potential joinery preservative pretreatments. A system of exposure of L-joint units is proposed. Data obtained by examining samples destructively show promise as the basis for predicting service life after relatively short exposure periods (within 2 years)....
J K Carey, A F Bravery, J G Savory


A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 322
H Alliot


Leaching of Active Components from Preservative Treated Timber. Stage 1: Semi-Field Testing
2004 - IRG/WP 04-20302
The project is aiming at finding realistic leaching rates from preservative-treated wood in use class 3 (above ground). The project focuses on developing a field trial method for investigating leaching. Panels are subjected to outdoor exposure under natural weather conditions at a test field at the Danish Technological Institute. The leachate is collected and monitored by chemical analysis of the...
N Morsing, B Lindegaard


Preservative-treated wood as a component in the recovered wood stream in Europe – A quantitative and qualitative review
2004 - IRG/WP 04-50218
Wood preservatives have been used for the protection of timber products in the European market in appreciable quantities for about 100 years. Between the 1960s up to the present day this usage has been particularly noticeable. The aim of this paper is to present quantitative and qualitative data on the volumes of preservative treated wood placed on the market in the UK and Sweden and to evaluate t...
R J Murphy, P Mc Quillan, J Jermer, R-D Peek


Current and future options for managing used preservative-treated wood
1995 - IRG/WP 95-50042
The amount of preservative-treated wood available for disposal will continue to increase exponentially in the next several decades as landfill availability declines. At the same time, recent legal ruling on competitiveness among utilities and disposal of ash has clouded the economic outlook for combustion of treated wood for energy recovery. This report identifies current and future options for ma...
R C De Groot, C Felton


Use of biossay to determine CCF and CCB preservative retentions in treated Pinus sylvestris
1984 - IRG/WP 2216
The retention of each a copper/chromium/boron and copper/chromium/fluoride preservative in pressure treated pinepoles was tested by bioassay using Aspergillus niger as test fungus. Small samples of 5 mm³ were taken from various depth of the poles and placed on potato-dextrose agar plates. The inhibition of fungal growth depends on the preservative retention in the cubes and corresponds closely to...
J C Moreschi, H Willeitner


Laboratory fumigations to determine the minimum temperature for methyl bromide eradication of the oak wilt fungus in red oak
1983 - IRG/WP 3243
Laboratory chamber fumigations of naturally-infected ret oak log sections exterminatet the oak wilt fungus in sapwood at temperatures down to 0°C. Only low, sporadic fungus survival was observed when log sections were gassed with methyl bromide at -5°C and aired for 4 da. at 0°C. Lower temperature treatments were not effective even if gas levels or exposure times were increased by 50%....
E L Schmidt


Wood preservation in East European countries
1989 - IRG/WP 3527
The paper discusses the main problems of wood preservation in Bulgaria, Czechoslovakia, German DR, Hungary, Poland, Rumania and the USSR. The main types of wood preservatives produced have been presented, as well as the state of standarization to test their properties. There have been considered methods of wood treatment in use and application range of treated wood....
J Wazny


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests
1980 - IRG/WP 2135
With the exception of acid-copper-chromate, zinc-chrome-arsenate, and sodium pentachlorophenoxide, the relative performance of preservatives in the fungus cellar was similar to that in the field....
M E Hedley


Treatment of dried sawn spruce and redwood building timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands
1978 - IRG/WP 3123
Treatment of dried sawn spruce and redwood Building Timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands. The aim of this article is to give the reader a modest description of the evaluation of fundamental research in wood preservation into a practical application....
H F M Nijman, N Burgers


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


The collaborative developement of soil acceptance criteria for timber treatment chemicals in New Zealand
1995 - IRG/WP 95-50040-34
In New Zealand, the issue of potential contamination on timber treatment sites arose in the late 80's due to the long history of use of PCP by the industry. One of the recommendations from the task group set up to investigate the issue was the development of a set of acceptance criteria to define trigger levels for remediation. A technical group from the government, industry and regional ...
H C Boyd


Improved resistance of Scots pine and Spruce by application of an oil-heat treatment
2000 - IRG/WP 00-40162
Spruce (Picea abies L. Karst.) and Scots pine (Pinus sylvestris L.) were subject to a heat treatment which was carried out in an oil-bath. The aim was to improve the dimensional stability of the treated wood and its resistance against fungi. The bath of vegetable oil provides a uniform heat transfer at temperatures of 180°C, 200°C and 220°C and protects the submersed wood from oxygen. Heat trea...
M Sailer, A O Rapp, H Leithoff


A new approach to the maintenance of wooden railway sleepers. (Second report)
1988 - IRG/WP 3492
The microenvironment and micro-ecology of wooden railway sleepers was investigated to assess their condition to determine the necessary treatment, repair and replacement criteria. In this report the efficacy of the secondary preservative treatment with solid boron rods is discussed and the development of an in-situ, nondestructive test method based on the creation and assessment of structural dyna...
W Beauford, P I Morris, A M Brown, D J Dickinson


A wood preservative for the future: Copper dimethyldithiocarbamate
1994 - IRG/WP 94-30045
The development of a new wood preservative, copper dimethyl-dithiocarbamate (CDDC) is reviewed in this paper. CDDC is formed in situ by dual pressure treatments. Laboratory and field efficacy trials, physical and chemical properties of the preservative solutions and treated wood, and plant handling characteristics of the system are examined....
D K Stokes, M H Freeman, T L Woods, R D Arsenault


The benefits to New Zealand of boron salt treatment of Pinus radiata
1992 - IRG/WP 92-3692
The historical reasons for New Zealand adopting boric salt diffusion of Pinus radiata are summarised, and present day processes and their associated costs are given. The biological hazards of using Pinus radiata untreated are then argued, using endemic fungal and insect species as examples, as well as a discussion of the risks from species that may yet be accidentally introduced into the country....
D J Cross


How best to specify retentions of preservative treatments: kg/m3 or % (m/m)
1998 - IRG/WP 98-20151
When specifying treatments according to the European Standard EN 351-1, retentions in the analytical zone are based on the amount of product found to be effective in biological tests; this is expressed in terms of the retention of the product per unit volume (kg/m3) for penetrating treatments and per unit area (g/m2) for superficial treatments. However, to check whether the retentions have been ac...
J K Carey


Fumigation as a remedial treatment: A review of North American literature
1983 - IRG/WP 3253
The development of the use of fumigants for eliminating decay in timber and roundwood in North America is reviewed. Initial experiments on oak wilt identified volatile chemicals which eradicated decay in roundwood. Subsequently, extensive experimentation on Douglas-fir poles in service showed that treatment with chloropicrin eliminated internal decay for more than ten years. Vorlex was also quite ...
J N R Ruddick


The effect of temperature on the rate of fixation of an alkyl ammonium compound (AAC) wood preservative
1984 - IRG/WP 3293
The rate of fixation of an alkyl ammonium compound wood preservative was measured by soaking samples of wood wool in various preparations of the preservative for arbitrary times followed by immediate leaching in water. The wood wool was then analysed for residual preservative. The results indicated that fixation was very rapid and increased at higher temperatures....
P Vinden


Co-operative Field Experiment: Performance of preservative-treated timber: Report on condition of specimens after seven years installed in New South Wales - Australia
1986 - IRG/WP 3362
R S Johnstone


Phytotoxic effects of preservative treated props for agricultural use
1989 - IRG/WP 3550
The phytotoxic effect due to the use of wood treated with organic preservatives for agricultural purposes was studied. The assays were carried out on plants tutored with props of Pinus sylvestris treated with three different organic wood preservatives. Pre-assays were carried out to observe the reaction on the plants, spreading directly the preservative on different parts of the plant and to the s...
D Franco, M V Baonza Merino


Protecting wooden structures
1980 - IRG/WP 392
Chromium-containing chemicals that effectively retard weathering of wood improve performance of subsequently applied finishes. Current work is focusing on the performance of wood-derived products (plywood, hardboard, fiberboard, particle board) after surface treatment with inorganic chemicals. The overall objective of the continuing research is to investigate new environmentally safe procedures to...
W C Feist