Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 2: Laboratory fungal bioassays
2000 - IRG/WP 00-20204
Extracts from sawmill residues of the naturally durable white cypress, Callitris glaucophylla were tested for fungicidal activity in a series of laboratory bioassays. The effects of different extraction solvents, techniques and sources of material on the biocidal efficacy of the resultant extracts were evaluated. Soil jar decay tests were used initially however, contractual time constraints necess...
M A Powell, L M Stephens, L Francis, M J Kennedy


Corrosion of zinc-coated nails used with preservative-treated western red cedar shakes in service
1982 - IRG/WP 3197
The corrosion of metal fasteners used with certain wood species and with preservative-treated woods can be a serious problem. The chemical reactivity of western red cedar (Thuja plicata Donn) extractives to iron and copper is well documented and wood preservative treatments containing copper, chromium, and/or ammonium hydroxide can be expected to similarly attack some metals. This problem is compo...
R S Smith, E L Johnson, A J Cserjesi


The natural durability assessment of secondary hardwood species - laboratory tests
1998 - IRG/WP 98-10295
Laboratory tests have been undertaken to assess the natural durability of 16 species of lesser known hardwoods, or hardwoods from non-traditional sources, including teak from three different plantations. Resistance to decay by both basidiomycetes and soil-inhabiting micro-fungi has been established. ´The data indicated that published information on the durability of these timbers should be treat...
J K Carey, S J Hendry


An electron spin resonance study of manganese changes in wood decayed by the brown-rot fungus, Postia placenta
1988 - IRG/WP 1359
Electron spin resonance (ESR) spectrometry was used to examine wood decay by the brown-rot fungus, Postia placenta. Wood slivers of Douglas-fir, white fir, redwood, sweetgum and yellow poplar were incubated for 4 weeks in custom-made quartz ESR tubes with or without Postia placenta. In all wood species without fungus, a weak partially resolved signal (about g=2, presumably due to manganese) was de...
B Illman, D C Meinholtz, T L Highley


Assessment of the toxicity of some copper-, zinc- and boron-based wood preservatives to the cellar fungus Coniophora cerebella Schröet
1974 - IRG/WP 242
This article reports the use of a method based on the determination of the probability of the protection of timber against destruction by fungi. By converting the probability values to probit values and plotting them as a function of the amount of preservative retained in the timber, curves of the toxic effect are obtained, enabling any timber protection probability to be assessed....
V N Sozonova, D A Belenkov


Some experiences with attack of microorganisms on wooden constructions supporting foundations of houses and bridges
1997 - IRG/WP 97-10232
Reconstructions of bridges and public buildings or damage of houses during the construction of subway lines in Berlin have led to a number of inspections of wooden foundations, mostly pine or spruce piles, representing service lives of between ca. 70 and 140 years. In all cases bacterial attack was found both in wood submerged in ground water and in surface water. The extent of deterioration diffe...
M Grinda


Preservative treatments of window components with a water-based borate formulation
2000 - IRG/WP 00-40171
Factory finished window joinery components were treated with an aqueous borate preservative in order to investigate penetration and retention levels, associated drying times; and the potential impact of using a water-based treatment on finished items. It was found that by using borates applied by light double vacuum schedules, it was possible to meet standards for penetration and retention, to air...
J Jermer, J D Lloyd


Fungi used in standard tests on the toxicity value of wood preservatives in various European countries
1975 - IRG/WP 255
The aim of the present paper is to make the comparative analysis of test fungi used in various European countries in order to define the toxicity value of wood preservatives against fungi of the Basidiomycetes class. Only the methods with national standard rank, present on the currently binding standards list are taken for consideration. The analysis of similarities and differences in the choice o...
J Wazny


Prediction of Weight Percent Gain (WPG) of furfurylated wood by FT-NIR spectroscopy
2004 - IRG/WP 04-20295
Wood modification based on furfuryl alcohol improves several important wood properties, such as the resistance to fungal decay and insect attack, hardness, dimensional stability, bending strength and stiffness. The improvements of wood properties depend on the weight percent gain (WPG) due to furfurylation. Fourier transform near infrared (FT-NIR) spectroscopy was used to calibrate PLS-regression ...
M Eikenes, P O Flæte, E Ystrøm Haartveit, S Lande


Effectiveness of a newly registered antisapstain preservative in preventing stain of Eucalypt timber in Australia
2000 - IRG/WP 00-30229
An antisapstain trial was conducted on two sites (Alexandra and Trentham) in order to establish the concentration of a newly registered antisapstain preservative (consisting of benzalkonium chloride (BAC) & 3-iodo-2-propynyl butyl carbamate (IPBC) & disodium octoborate (boron)) needed to prevent stain of Eucalypt timber. After 20 weeks of exposure at the Trentham site, the water treated bo...
J Snow, P R S Cobham, N Ryan


Fungal Stain Development in Canadian Hardwood Logs
2004 - IRG/WP 04-10505
In most sawmills around the world, trees are harvested into logs and stored in the forest or in a log yard for a period of time before being sawn into lumber. These logs may be attacked by various pigmented fungi, which results in staining of the wood. Since hardwood species are used to a great extent in furniture manufacturing and in the making of other valuable wood products, the reduction of wo...
Dian-Qing Yang, M-C Bisson


Standardisation of sapstain tests - A challenge
1992 - IRG/WP 92-2403
In the last decade many new anti-sapstain products have been tested world-wide under laboratory and field conditions. Several extensive test programmes have been executed with different non-standardized test methods and procedures, with the result that the biological findings cannot be compared with each other. In this paper, gathered recommendations will be given in order to standardize test meth...
G Rustenburg, C J Klaver


Life-cycle assessement of treated wood: A view from the roa
1996 - IRG/WP 96-50078
Life Cycle Assessement (LCA) is being used increasingly as a tool to structure information on the environmental characteristics of material and processes. This paper is based on the experience gained from our LCA studies on treated wood products over the last 4 years. The comprehensive and logical examination af the information available on treated timber provided by LCA has allowed identification...
W Hillier, R J Murphy, D J Dickinson, J N B Bell


Removal of CCA from Spent CCA-Treated Wood
2002 - IRG/WP 02-50192
A novel method for the removal of CCA components from spent CCA-treated wood has been developed. The CCA-treated wood was first converted into liquid in the presence of polyethylene glycol and glycerin at mild temperatures (120 – 150 0C) by using sulfuric acid as catalyst. The resulting viscous liquefied wood was then resolved in acetone/water solvent. The hazardous components (i.e., Cr, As, and...
Lianzhen Lin, Chung-Yun Hse


Moisture uptake and volumetric swelling as probable factors also affecting leaching in CCA-treated wood. A preliminary study of treated Eucalyptus saligna sapwood
2003 - IRG/WP 03-30318 IRG/WP 03-30318
A number of factors affecting leaching of CCA from treated wood have been variously investigated and discussed. However, the possible effects of moisture movement in treated timbers on leaching have not received attention yet. The present study examines and compares moisture uptake and volumetric swelling in CCA-treated and untreated sapwood of Eucalyptus saligna, and tries to establish a correl...
R Venkatasamy


The influence of wood moisture content on the fungitoxicity of methylisothiocyanate in Douglas fir heartwood
1987 - IRG/WP 3430
The fumigant methylisothiocyanate (MIT) effectively controls decay fungi in large wood structures, but the influence of environmental factors on its performance are not well understood. Experiments found wood moisture content to greatly influence the fungitoxicity and sorption of MIT in Douglas fir heartwood. At constant, low MIT vapor concentrations (less than 1 µg/cc air), wood at 10% MC bound ...
A R Zahora, J J Morrell


Effectiveness of copper/chromium salts as wood preservatives against Limnoria tripunctata Menzies in laboratory tests
1977 - IRG/WP 431
During the last joint meeting of IRG and COIPM a co-operative programme of tests with copper/chromium salts as wood preservatives against marine borers was discussed and agreed. In this connection the results of a laboratory test in the BAM with Limnoria tripunctata Menzies will be of interest. But as the respective paper is written in German (H. Kühne; G. Becker: Laboratoriumsversuche über die ...
H Kühne


Termite and decay resistance of particleboard composed of white cypress pine and radiata pine
1997 - IRG/WP 97-10200
Phenol-formaldehyde bonded particleboard was manufactured from blends of non-durable radiate pine (P. radiate) and heartwood of the naturally durable species, white cypress pine (C. glaucophylla). Board specimens were subjected to bioassays using two termite species, M. darwiniensis and C. acinaciformis, and the basidiomycete fungi, C. puteana and P. ostreatus, and the durability of specimens was ...
P D Evans, J W Creffield, J S G Conroy, S C Barry


Attempt for developing a new method for above ground field testing of wood durability
2000 - IRG/WP 00-20199
Field testing remains the most appropriate way for evaluation of wood preservatives or natural durability of wood species. Above ground tests are designed to answer specific questions concerning the outdoor utilisation of wood. Such methods supply additional information and confirm or reject preliminary laboratory results. The European standard (ENV 12037, "lap-joint") for assessment of the durabi...
N Terziev, M-L Edlund


A modified method to determine the toxic values of chemicals against Lyctus africanus (Lesne) by larval transfer method (laboratory method)
2005 - IRG/WP 05-20309
Lyctus africanus (Lesne) is the commonest species widely distributed by trade throughout India. It is one of the most important insect pest attacking logs, branchwood and and practically every kind of manufactured wooden article that contains sapwood. Presently, in India many short rotation and alternate timbers are being used for making many finished products .The inclusion of sapwood containin...
R Muthukrishnan, O K Remadevi


Experiences with penetration of copper-based wood preservatives
2001 - IRG/WP 01-20233
In the Nordic countries there is a long tradition of result type based specifications for preservative-treated wood. A common Nordic standard for treated pine (Pinus sylvestris) wood was published in 1976. After a revision in 1989 this standard, then named INSTA 140, defined four classes of treated wood: M, A, AB and B. Treaters producing according to this standard had to be affiliated to a qualit...
J Jermer, F G Evans, I Johansson


International comparison of three field methods for assessing the in-ground termite resistance of materials - highlights after two years
1999 - IRG/WP 99-20157
First-year results of a comparative study, evaluating the in-ground termite resistance of a range of materials, including CCA and ACQ-treated timbers, using the below-ground exposure, ground contact and graveyard methods against diverse termite faunas were provided in IRG/WP/98-20132. Further annual inspections have confirmed early trends and identified notable differences between sites and method...
M Lenz, J W Creffield, A F Preston, B M Kard, C Vongkaluang, Y Sornnuwat


Wood protection by surface treatment of two borate preservatives, TIM-BOR® and BORA-CARE®, for the formosan subterranean termite and eastern subterrean termite
1993 - IRG/WP 93-10044
TIM-BOR® (disodium octaborate tetrahydrate: DOT, Na2B8O134H2O) and BORA-CARE® (40% DOT in ethylene glycol) are two borate products marketed for treating wood in use by brushing or spraying onto the wood surface. The active ingredients presumably diffuse into wood by the 10-15% existing wood moisture. Few data, however, are available to demonstrate the diffusion rate. Su & Scheffrahn (1991) s...
M Toroko, N-Y Su


Natural decay resistance of some lesser-used tropical hardwoods from Ghana
2002 - IRG/WP 02-10438
Ghana is a tropical African country that is rich in diverse timber species. In order to reduce over-exploitation of the popular timber species and increase the resource base for the wood industry, lesser-used or lesser-known timber species are being promoted locally and for export. To do this successfully, it is essential to determine the physical, mechanical and biological properties of these tim...
S A Amartey, F R Hanson


The effect of hemicellulose degradation on the mechanical properties of wood during brown rot decay
2001 - IRG/WP 01-20219
Incipient decay of wood by brown rot fungi causes measurable strength losses in wood before measurable weight loss occurs. Previous studies have shown that the high levels of strength loss that occur during incipient brown rot decay may be related to loss in hemicellulose. This paper investigates the effect of decay on hemicellulose composition and the relationship to the mechanical properties of ...
S F Curling, C A Clausen, J E Winandy