Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Virulence of two Laboratory Test Strains and one Natural Isolate of Rhodonia (Oligoporus) placenta against Thermally Modified Pine and Beech Wood
2013 - IRG/WP 13-20524
Rhodonia (Oligoporus) placenta is known as a relative aggressive basidiomycete fungus against thermally modified timber. In durability lab tests, this often results in a lower durability class, compared to other test fungi. In the reported work, the virulence of three different strains of Rhodonia placenta for untreated and thermally modified timber was determined and compared. Therefore, two lab ...
K Plaschkies, W Scheiding, K Jacobs, N Rangno


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell


State of progress of utilisation of supramolecular gels for formulations of water-soluble wood preservation salts
2013 - IRG/WP 13-30630
This article is a compilation of the work done so far concerning the utilization of supramolecular hydrogels, built on low-molecular-weight amphiphilic molecules and containing boron salts conferring fungicidal properties. Mixing boron with thermoreversible hydrogels allows the formation of a supra molecular network incorporating boron and important amount of water upon gelification of the solutio...
F Obounou Akong, P Gérardin, M-F Thévenon, C Gérardin-Charbonnier


Hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment
2013 - IRG/WP 13-40623
The hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment was investigated by testing the water uptake, equilibrium moisture content (EMC) at various relative humidity levels, and contact angle of the poplar wood surface. The results showed that: (1) At the first moment, the heat treatment at temperatures lower than 160 ℃ did not reduce the water uptake be...
Weiyue Xu Yuan Zhu, Jinzhen Cao


Study of UV resistance and natural weathering of coatings on chemically modified wood
2013 - IRG/WP 13-40629
In this study, UV resistance and weathering performance of rubberwood (Hevea brasiliensis) and radiata pine (Pinus radiata) modified with benzoyl chloride and acetic anhydride was studied. Performance of polyurethane based wood coatings on modified wood was also evaluated. Unmodified and chemically modified specimens were exposed to accelerated and natural weathering. Modified and unmodified woo...
K K Pandey, K Srinivas


Field performance of wood impregnated with siloxanes using supercritical carbon dioxide
2013 - IRG/WP 13-40632
This paper presents preliminary results from a 13-month field test containing pine sapwood samples (Pinus sylvestris) impregnated with a mixture of siloxane and organic biocides using supercritical carbon dioxide as carrier. Samples were exposed above ground at a Danish field test site using matched non-treated sapwood controls for every treated sample. All samples were painted before exposure. Pi...
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Durability of alternatives to CCA-treated wood - Results from field tests after 11 years exposure
2013 - IRG/WP 13-30633
The present study was initiated as a consequence of restrictions against the use of CCA-type wood preservatives in Sweden in the 1990s. New copper-based formulations were introduced on the market and to some extent, also alternatives to preservative-treated wood, such as thermally and chemically modified and linseed oil treated wood as well as heartwood of non-tropical naturally durable wood s...
P Larsson Brelid, M-L Edlund


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Investigating the potential role of creosote oil for the water repellent purposes in fiberboards
2013 - IRG/WP 13-40635
Effect of wood steaming during fiber generation processes and creosote oil on the properties of fiberboard, manufactured from creosote treated solid wood were investigated. Pulp fiber was generated by alkaline pretreatment of waste creosote impregnated wood which being fiberized by laboratory defibrator, atmospherically. These fibers blended with 0, 15, 30, 45 and 100 percent by weight of wood...
M Sheikholeslami


Natural durability of plantation-grown coast redwood (Sequoia sempervirens) in New Zealand
2014 - IRG/WP 14-10817
There is wide variation in the wood properties of plantation-grown coast redwood in New Zealand. Contributing factors are the seed source, silviculture, growth and age of the trees in the plantation forests. Little is known about how these factors affect the variation of wood properties among and within the trees of New Zealand’s coast redwood forests. Heartwood of plantation-grown coast redwood...
D O’Callahan, T Jones, C Low, C Chittenden


Variability in durability of some selected South-American wood species
2014 - IRG/WP 14-10831
Within the scope of sustainable forest management one wants to encourage the proper use of lesser known wood species. Therefore the market has to shift from a demand-driven towards a supply-driven market without loss of wood quality. It is generally known that the durability from pith to bark varies thus, affecting the overall durability of wood species. Consequently, a detailed analysis is necess...
I De Windt, P ’t Hooft, J Van den Bulcke, J Van Acker


Unexpected natural decay resistance strategies of durable tropical woods Bocoa prouacencis, Vouacapoua americana, Inga alba and relationship with specific gravity and wood extractives
2014 - IRG/WP 14-10832
The study of decay resistance in wood is of interest for wood end-users but also for the global carbon balance since wood biodegradation is a key driver of forest ecosystem functioning through its impacts on carbon and nutrient cycling. We studied the specific gravity and wood extractive contents in order to understand decay resistance against soil microflora after 90 days exposure of sapwood and ...
N Amusant, M Migg, B Thibaut, J Beauchene


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


Using Commercial Water Repellent Chemicals on Wood Protection
2014 - IRG/WP 14-30656
Lately, researchers have been looking for process and products that use environmental friendly technologies in wood protection. These sorts of innovations on wood protection should be carried out for wood evaluated at outdoor conditions. Using water repelling chemicals is one of those innovations which improve wood durability and dimensional stability by decreasing content of moisture. In this ...
G Köse, A Temiz, S Demirel, O E Özkan


Field performance of wax treated wood
2014 - IRG/WP 14-30649
The durability and outdoor performance of wax treated Scots pine sapwood was investigated in above ground field tests. Therefore wood impregnated with three different waxes was exposed in horizontal lap-joint test which is running since eight years. Durability, wetting resistance and the susceptibility to checking has been investigated. In summary, all wax treated wood performed better compared to...
C Brischke, E Melcher


Resistance to Decay Fungi of Scots Pine Impregnated with Natural and Chemical Preservatives
2014 - IRG/WP 14-30650
In this study, heart-wood and sap-wood specimens of the Scots pine which is naturally grown in Turkey were treated with natural (valex) and some chemical preservatives such as CCA - C (Copper / Chrome / Arsenic), CBA - A (Copper / Boron / Azole). The wood protective efficacies of these preservatives were investigated by means of fungi decay test (EN 113). As a result of the study it was found t...
S Yildiz, U B Şimşek


Hydroponic Phytoremediation of Chromated Copper Arsenate (CCA) and Copper Contaminated Water
2014 - IRG/WP 14-50304
The removal of selected metals by duckweed (Lemna minor) and parrotfeather (Myriophyllum aquaticum) from a simulated aqueous environment contaminated with Chromated Copper Arsenate (CCA) and copper sulfate was studied in a controlled laboratory experiment. The duckweed and parrotfeather’s tissues were analyzed to evaluate the removal of copper (Cu), chromium (Cr), and arsenic (As) from CCA cont...
C Keith, H Borazjani, S Diehl, Y Su, Fengxian Han, B Baldwin


Nano-Zycosil in MDF. Part I: Gas and Liquid Permeability
2014 - IRG/WP 14-40652
Effects were studied of zycosil nanoparticles, with size range from 20 to 80 nm, on liquid and gas permeability of medium density fiberboard. Nanozycosil was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. The obtained results indicated that the addition of zycosil to the mat resulted in a significant increase...
H Reza Taghiyari, A Karimi, P M D Tahir, O Schmidt, E Bari, P Nouri , A Jahangiri


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao


Effect of Nano-Wollastonite on Water Absorption in Particleboard
2014 - IRG/WP 14-40662
Effects of wollastonite nanofibers on physical properties of particleboard were studied. Nano-wollastonite (NW) was applied at 5, 10, 15, and 20 g/kg, based on the dry weight of wood-chips, and compared with control specimens. Two application methods of NW were used: surface application (SA), and internal application (IA). Density was kept constant at 0.68 g/cm3 for all treatments. Tests were carr...
S Karimi, H Reza Taghiyari, A Karimi, P M Tahir, J Abdul Halip


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


The Physical Properties of Heat Treated Fir Wood and Outdoor Durability
2014 - IRG/WP 14-40677
Wood might be easily susceptible to degrade by biotic and abiotic factors. Therefore, wood should be protected from fungi, insects and other degradation factors by applying treatment methods. Especially, for the wood have used in the external environment. Chemical treatment methods have some disadvantages such as use of toxic chemicals (Arsenic and chromium) and treatability of refractory wood spe...
O E Özkan, H Vurdu, A Temiz, G Köse


Experiences with an industrial system for controlled thermal wood modification in pressurized unsaturated steam
2014 - IRG/WP 14-40678
Thermal wood modification in pressurized reactors has a long history, but these processes are to date industrially scarcely used, because of the relatively complicated process equipment, compared to the more common high-temperature processes in kilns at atmospheric pressure. However, based on our practical experience with the FirmoLin® process, supported by recent scientific findings, it is foun...