Preliminary evaluation of the answers to the 2nd IRG/WP-questionnaire on the state of pollution control in the field of wood preservation
1982 - IRG/WP 3209
This preliminary evaluation of the answers to the 2nd IRG/WP-Questionnaire only gives a general survey on those questionnaires which the author received until April 30th, 1982. Details, such as correlations between importance of wood preservation and pollution control, as well as a comparison of the answers with those to the first questionnaire (Doc. IRG/WP/369), could not be considered due to lac...
H Willeitner


Improvement in dimensional stability against water of the main Spanish timbers impregnated with water repellent organic protectors
1988 - IRG/WP 3468
The study reported the increase of dimensional stability against water of the main Spanish timbers, both broadleaved and coniferous, after impregnation in the autoclave with organic protector, with contains 33.3% water repellent waxes and resins. The proposed Spanish standard, U.N.E. n° 56541 is used, where dimensional stability of the impregnated wood is expressed as a% of that of the non-impreg...
J A Rodríguez Barreal


New principles for the protection of wood: Impregnation with waterborne resins
1995 - IRG/WP 95-40047
The environmental impact of classical wood preservatives as well as the use of tropical wood species with high natural durability is regarded increasingly critically in the public. Therefore other partially new principles for the protection of wood, like chemical modification, or treatment with resins were examined especially in USA, Japan and in Europe with promising results predominantly in the ...
A O Rapp, R-D Peek


Dura-Treet II, a water dispersible pentachlorophenol
1980 - IRG/WP 3165
During the past several decades, penta petroleum wood treating has become increasingly popular. Penta is an effective chemical compound against wood organisms causing decay and rot, is safe to handle, also clean and easy to use. In terms of preservative cost, it has been and remains by far the least expensive of the three major preservatives. However, when the cost of petroleum carrier is added, t...
D B Hatcher


The effect of a chelator mediated fenton system on activation of TMP fibres and decolorization of synthesized dyes
2004 - IRG/WP 04-50223
The purpose of this work is to improve our current knowledge of the non-enzymatic mechanisms involved in the brown rot degradation of wood, but also to study the potential applications of a chelator-mediated Fenton system in activation of wood fibers and decolorization of synthesized dyes. In this work, Electron Spin Resonance (ESR) spin-trapping techniques were used to study the generation of hyd...
Yuhui Qian, B Goodell, J Jellison


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


Effect of a water repellent additive on the performance of ACQ treated decks
2000 - IRG/WP 00-40168
The performance of a water repellent (WR) additive formulated for use with ACQ has been evaluated. The water repellency of wood treated with this formulation was studied in laboratory and field tests. The change in moisture content of ACQ/WR treated boards under field exposure conditions is compared with that of CCA/WR treated boards. Although the water repellency of the ACQ/WR system is lower tha...
F Cui, A R Zahora


Evaluation of the natural durability and ultrasonic method for decay detection of some european hardwood and softwood species
2004 - IRG/WP 04-10537
This paper presents the first part of an investigation on the natural durability of mixed plywood made of durable and non durable plies from the following selected timbers : Cedrus atlantica, Cupressus sempervirens, Castanea sativa, Populus sp. I 214 and Fagus sylvatica. In order to carry out this study, the natural durability of the massive wood used to manufacture the plywood panels was asses...
F Faraji, M-F Thévenon, B Thibaut


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 19: Report on the condition of specimens at Sekondi, Ghana after 42 months
1984 - IRG/WP 4109
The results of the first formal inspeation of CCA- and CCB- treated test panels exposed at Sekondi, Ghana, in June 1980, are presented. All untreated control panels of both reference and local species have been destroyed. Of the% CCA- treated specimens, only those of Pinus sylvestris (reference species) and Mitragyna stipulosa (local species) have not been attacked. 3% CCB-treated local species ha...
F F K Ampong


Mobility and bioavailability of wood preservation chemicals in soil - actual field measurements
1998 - IRG/WP 98-50101-11
Wood material intended for outdoor use is often impregnated with chemicals to withstand attack from fungi and bacteria. Both inorganic and organic substances are used to protect the wood, and they are used in a toxic and bioavailable form. At wood preservation facilities severe soil contamination can be encountered due to spills and deposition of sludge, especially at old sites. Two sites, one whe...
S Andersen, G Rasmussen


Health and safety regulations on the use of wood preservatives in Switzerland
1980 - IRG/WP 3148
There is not any doubt that the chemical protection of wood (besides the architectional-constructional wood protection) is of utmost importance for the increase of the durability of technically used timber. The toxic properties of wood preservatives make certain legal regulations necessary for the protection of human beings, animals and the environment. Thereby wood preservatives fall under the po...
O Wälchli


Diffusion and interaction of components of water-borne preservatives in the wood cell wall
1988 - IRG/WP 3474
This study investigates the rates of diffusion and ultimate distributions of copper and arsenate components of wood preservatives in wood cell walls following vacuum treatment. Adsorption studies of copper on red pine (Pinus resinosa) and trembling aspen (Populus tremuloides) wood confirm the importance of cation exchange reactions on the ultimate distribution of copper in the wood substance and i...
P A Cooper


Variation in natural durability of British grown Douglas fir ((Pseudotsuga menziesii (Mirb.) Franco). Part II. Effect of extractive contents and taxifolin
2002 - IRG/WP 02-10446
The previous paper (Part I: Effect of density and growth rate) described the variation in natural durability of 4 Douglas fir (DF) seed origins (Darrington, J. Landing, Naselle and Hawkinsville) in a pure culture decay test and fungal cellar test. The pure culture tests were performed against two brown rot fungi (Coniophora puteana and Postia placenta). In the fungal cellar test soft rot was the p...
S Akhter, M D C Hale


Natural resistance of twenty-five timber species to marine borer attack in Goa waters (India)
1992 - IRG/WP 92-4178
Natural durability of 25 species of Indian timbers has been discussed, based on data collected from test panels exposed in Goa waters (west coast of India. for a period of 7 months. All the timber species, except Cleistanthus collinus, were heavily destroyed within 7 months on account of the combined attack by Martesia striata (Linnaeus) and Lyrodus pedicellatus (Quatrefages). Cleistanthus collinu...
L N Santhakumaran, G Srimannarayana, K Nagaiah


Natural Durability studies and Changes in wood chemistry of some Ghanaian hardwoods during decay by white- and brown-rot fungi
2004 - IRG/WP 04-10542
The natural decay resistance of Esa (Celtis mildbraedii), Wawabima (Sterculia rhinopetela) and Dahoma (Piptadeniastrum africanum) obtained from Ghana was determined according to BS EN 113 (1997). Esa was found not durable to the white-rot, but very durable to the brown-rot; Wawabima was very durable to both white- and brown-rots; and Dahoma was durable to the white-rot, and very durable to the bro...
Zeen Huang, K Maher, S A Amartey


Optimisation of an analytical method for the determination of total fluoride in preservative-contaminated soils using water steam distillation and an ion-selective electrode
1999 - IRG/WP 99-20153
This paper describes a simple modified procedure for the quantitative fluoride determination of different origin in a soil matrix using a water steam distillation and an ion-selective electrode. Distillation methods generally require a preliminary preparation step like fusing. The modified method presented here is based on the direct distillation of fluoride so that no further sample preparation i...
E Melcher


Differentiation of Scots pine heartwood and sapwood by near infrared spectroscopy
2003 - IRG/WP 03-10459
In Scandinavia Scots pine heartwood has, in recent years, gained popularity as material for external structures exposed to moderate risk of decay. As non-durable sapwood surrounds the heartwood in pine trunks it is of crucial importance to separate this wood from the heartwood during log processing into heartwood products. Heartwood and sapwood can be differentiated by visual evaluation of colour ...
P O Flæte, E Ystrøm Haartveit


The susceptibility of acetylated Pinus radiata to mould and stain fungi
1992 - IRG/WP 92-1548
The aim of this investigation was to determine the effect of 5, 10, 15 and 20 percent acetylation weight gains on the susceptibility of Pinus radiata sapwood to mould and stain fungi, and to establish if an acrylic paint, an oil-based stain and a water repellant gave superior protection from fungal growth on wood treated to 20% acetylation weight gain, compared to untreated wood. One treatment set...
R N Wakeling, D V Plackett, D R Cronshaw


The accelerated L-joint test method for determination of the out of ground natural durability
1998 - IRG/WP 98-20146
The accelerated L-joint test incorporates a moistening device and uses a close end water trap in an open joint connection with a laminated tenon member consisting of the perishable reference wood species scots pine sapwood and beech. After one year of exposure it is possible to show a distinct identification of natural durability classes 4 and 5 against the more durable wood species. Both weight ...
J Van Acker, C Brauwers, M Stevens


Biosorption of metals for wood waste effluent clean up
1997 - IRG/WP 97-50090
The common filamentous fungi can sorb metal ions from aqueous solutions. The biosorption of metal ions like copper Cu2+, chromium Cr6+ and arsenic As5+ by dead fungal mycelia was investigated. Two industrial fermentation byproducts are tested: Mucor miehei and Aspergillus oryzae. The adsorption of metal ions depends on parameters such as chemical treatment of fungi before biosorption (acid or basi...
S Legay, G Labat


Standardization of CCA treated 45 hardwood species grown in Bangladesh for REB crossarms
1995 - IRG/WP 95-20059
Researches on 45 hardwood species grown in Bangladesh regarding density, moduli of rupture (MOR), colour and treatability of sapwood and heartwood, seasoning property and natural durability of heartwood revealed that both sapwood and heartwood of 17 species could be full cell pressure treated with CCA at impregnation pressure of 14-18 kg/cm² and only sapwood of rest 28 species could be pressure t...
A K Lahiry


Recovery of copper, chromium, and arsenic compounds from the waste preservative-treated wood
1991 - IRG/WP 3651
In Japan, about 40 percents of waste wood is incinerated and the residue is dumped into the landfill site. The waste preservative-treated wood, which is mixed in nontreated wood, is incinerated in the same way, too. However, it will cause the serious problems that the gases contained with high concentration arsenic compounds are discharged from the smokestacks of the incineration facilities and th...
A Honda, Y Kanjo, A Kimoto, K Koshii, S Kashiwazaki


Electrochemical deterioration of wood in sea-water
1981 - IRG/WP 464
In the specialistic literature only few items can be found dealing with the specific kind of wood deterioration called electrochemical corrosion of wood. This deterioration occurs predominantly on marine vessels, yachts, and other marine craft where wood is jointed by means of various metal connectors. Up to date information demonstrates that in wood surrounding copper connectors, when in proximit...
J Raczkowski


An aquaria test of the natural resistance against marine borers of some commercial timbers available in Australia
1996 - IRG/WP 96-10145
The natural resistance of the heartwood of 22 different timbers grown or commercially available in Australia was examined. Radiata pine sapwood both untreated, and treated with 5.4 kg/m³ CCA salt, was included for comparison. Small timber blocks were exposed for one year in tanks containing either Limnoria tripunctata or Lyrodus pedicellatus. Four softwood species tested were heavily attacked and...
L J Cookson


Comparison of various types of bait containers designed to aggregate large numbers of foraging subterranean termites from natural populations in below-ground mound colonies
1995 - IRG/WP 95-10116
At Walpeup in the semi-arid mallee country of north-west Victoria (350 km from Melbourne), there are several indigenous subterranean termite species, none of which build above-ground mound colonies but build their colonies below-ground and/or in trees. This paper describes a baiting experiment in which three types of bait containers were compared in their ability to aggregate large numbers of fora...
J R J French, B M Ahmed