Treatment of particleboard with isocyanate resin to impart improved dimensional stability and water repellency
2000 - IRG/WP 00-40178
Standard particleboard panels (for interior use) of 16 mm nominal thickness were cut into samples measuring 6.4 mm x 78 mm2. The samples were divided into 4 end matched batches. Two batches were treated with isocyanate resin and cured. The other 2 batches were left untreated. One of the treated batched and 1 of the untreated batches were edge sealed with epoxy resin prior to isocyanate resin appli...
K M Filcock, P Vinden


The biological natural durability of timber in ground contact
1994 - IRG/WP 94-20051
The BRE ground contact field trials for the determination of the biological natural durability of different timber species have recently been reviewed. The data obtained from these trials have been used to appraise the different ways in which natural durability may be expressed. It is concluded that the use of the mean as a method of assigning the timber to one of five durability classes may be ac...
G A Smith, R J Orsler


A preliminary report on lignicolous marine fungi in the Java Sea, Indonesia
1982 - IRG/WP 488
This report is part of a study on the natural durability of Indonesian timbers against marine borers conducted in Pari Island waters, Java Sea (Suhirman and Eaton, 1981), and contains preliminary information which has not yet been published....
Suhirman, R A Eaton


Water-repellent additive for CCA
1991 - IRG/WP 3655
Hickson have developed a water repellent additive for incorporation into copper-chromium-arsenate timber treatment solutions. The water repellent emulsion shows good stability in the treatment solution, is easily incorporated and applied in a single stage treatment. No modifications to the additive is safe to treatment schedule are usually needed and use. Weathering of the treated wood is substant...
P Warburton, R F Fox, J A Cornfield


The isolation of actinomycetes from wood in ground contact and the sea
1980 - IRG/WP 1110
M S Cavalcante, R A Eaton


Creosote movement from treated wood immersed in fresh water: Initial PAH migration
2003 - IRG/WP 03-50201
Creosote has a long history of successful use as a wood preservative, but polycyclic aromatic hydrocarbons (PAHs) in this preservative have raised environmental concerns, particularly when creosote-treated wood is used in aquatic environments. A number of models have been developed to predict the risk of creosote use in aquatic environments, but one limitation of these models is a lack of data o...
Sung-Mo Kang, J J Morrell, J Simonsen, S T Lebow


Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson


Examination of timbers from the Mary Rose in storage
1988 - IRG/WP 4149
Timbers from the Tudor ship, Mary Rose, have been examined for the presence of fungal fruiting structures. Wood specimens were also examined for the presence of microbial decay patterns using light and scanning electron microscopy. Structural timbers were surveyed using the Pilodyn for an overall picture of the extent of decay. Mary Rose timbers were predominantly inhabited by marine fungi. Fourte...
R Mouzouras


A comparison between methods for evaluating the water repellency of wood
1989 - IRG/WP 2328
Wood specimens treated with a number of water repellent formulations have been tested for their water repellency according to four laboratory test methods, based on weight increase, swelling and contact angle measurements, in order to assess the degree of agreement between the different methods. Treatments representing formulations with a wide range of water repellent efficiency were tested both i...
R Nussbaum


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


Biodegradation of creosote/naphthalene-treated wood in the marine environment
1977 - IRG/WP 428
The present study was undertaken to determine the biodegradability of marine grade creosote and selected components, including naphtalene, and to determine the effectiveness of (up to 40%) creosote in protecting wood from microbial attack. Also, the impact(s) of creosote and naphtalene-enriched creosote on the microbial ecology os estuarine environments was examined....
P A Seesman, R R Colwell, A Zachary, A J Emery


Computerised data acquisitioning, handling and processing in wood preservation studies
1984 - IRG/WP 2218
The computerisation of data acquisitioning, handling and processing in weathering studies on wood treated with protective coatings is discussed. An integrated system comprising a data base, statistical package and a custom written graphical processor is explained. Two treatments are compared and the correctness of a mathematical weathering model is evaluated....
T Rypstra, K Vos


Assessment of the natural durability of four Ghanaian hardwoods against the white-rot fungus Coriolus versicolor and soft-rot using laboratory tests
2003 - IRG/WP 03-10498
The natural durability of two lesser-utilized species (LUS) (Corynanthe pachyceras Welw. (pamprana) and Glyphaea brevis (Sprengel) Monachino) (foto) from three forest districts, and two related primary species (Nauclea diderrichii (de Wild.) Merr. (opepe) and Nesogodornia papaverifera (A. Chev.) R. Capuron.) (danta) from one district in Ghana is assessed against Coriolus versicolor Linnaeus Quelet...
C Antwi-Boasiako, A J Pitman, J R Barnett


Adequate preservative treatment of tropical and subtropical hardwoods for electric anchor logs
1997 - IRG/WP 97-40101
Most available 27 different hardwood species grown in Bangladesh was investigated regarding suitability as CCA-C (chromated copper arsenate type-C) impregnated anchor logs for rural electrification programme. The kiln-drying properties, sapwood thicknesses, CCA treatability grades of sapwood and heartwood, natural durability of heartwood and CCA retainability at specific assay zone separated 27 ha...
A K Lahiry


Assessment of contamination of soil and water at a CCA treatment plant: A demonstration project
1996 - IRG/WP 96-50067
Soil, sludge, dust and water samples were collected at a copper/chromium/arsenic wood preservation plant. Contamination of soil, sludge, dust and surface water with copper, chromium and arsenic was detected. Levels of contamination were sufficiently high to require remediation. Contamination originated from preservative solution dripping from recently treated wood. Migration of contaminants was vi...
P N Durrant, D C R Sinclair, G M Smith


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Surface coatings for impregnated wood
1992 - IRG/WP 92-3684
The use of proper surface coatings enhances the aesthetic and protective properties of impregnated wood. Good results with especially water-borne coatings have been obtained for class-A impregnated L-joints and claddings in field tests started in 1982....
L Kotama


The window joinery test hut
1975 - IRG/WP 257
D F Purslow


Natural durability studies in an accelerated field simulator - A novel approach
1983 - IRG/WP 2197
A study of the natural durability of untreated timbers to both decay and termite attack is described. The work illustrates the versatility of the Accelerated Field Simulator as a novel approach to biodeterioration research....
G C Johnson, J D Thornton, J W Creffield, C D Howick


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


A natural exposure weathering test for the evaluation of preservative performance
1992 - IRG/WP 92-2400
Natural exposure weathering tests were carried out by externally exposing treated wood samples for varying periodes of time up to 36 months. In the laboratory these samples were assayed for residual preservative effeciveness using Coniophora puteana FPRL 11E. The results indicated a loss in efficacy over and above that determined using artificial ageing procedures such as EN73 (evaporative ageing)...
J Brown, G R Williams


Some observations on miniaturised soil/block tests
1988 - IRG/WP 2317
Results are presented for miniaturised soil/block tests carried out in 120 ml capacity glass jars. The four test fungi (Coniophora puteana, Coriolus versicolor, Gloeophyllum trabeum and Poria placenta) reacted differently to different moisture regimes established by varying the soil moisture content. Acceptable levels of decay were achieved by the three brown rot fungi with soil at 110% whc; howev...
J K Carey


Effect of double-vacuum and vacuum-pressure impregnation with water-borne preservatives on the dimensional characteristics of spruce
1990 - IRG/WP 3613
Air-dried planed spruce (Picea abies) samples were treated with a water-borne preservative (micro-emulsion) and one oil-borne type both containing azaconazole and deltamethrin. Each set of samples contained equal number of specimens with different growth ring orientation, heartwood content and density. In addition to the preservative retention and the penetration of a.i., the swelling of the sampl...
J Van Acker, M Stevens, G Rustenburg


Collaborative soft rot tests: Proposed amendments to Document No: IRG/WP/208
1973 - IRG/WP 224
J K Carey, J G Savory


300 years water-logged wood: Treatability with CCA-C
1998 - IRG/WP 98-40103
The treatability of 300 years water-logged and recent wood (Abies bornmülleriana M.) was assessed by dip treatment and vacuum and pressure cycling with CCA-C. Treatment runs were evaluated on the basis of weight gain retention and radial and tangential penetration measurements. The preservative penetration and retention levels in the 300 years water-logged wood were higher than in the recent wood...