The resistance of thermo and thermo-oil modified black poplar wood (Populus nigra L.) to Basidiomycetes fungi
2012 - IRG/WP 12-40585
The share of area taken by poplar tree species in Poland account for 2.0% of the area of state forests, 4.8% of national parks and for 2.3% in the privately-owned forests. It is shown and expected an increase in the share of poplar stands connected with plantation of fast growing trees. The poplar wood is not resistant to Basidiomycetes fungi, easy attacked by insects and in consequence is regarde...
A Fojutowski, A Kropacz, A Noskowiak


A survey of factors affecting decay resistance of wood modified with acetic anhydride
2012 - IRG/WP 12-40594
From the range of information published, acetylation appears well suited to provide adequate protection against biological attack for materials derived from typically non-durable wood species. Acetylated wood is now commercially available both in Europe and in the USA. But still there are a lot of unanswered questions related to fungal decay mechanisms in acetylated wood. The paper summarize exist...
G Alfredsen, P O Flæte, H Militz


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


Tar-oil uptake vs time in immersion treatment of short pine posts: A simple technique applicable to rural communities of Papua New Guinea
2012 - IRG/WP 12-40608
Pinus caribaea and Araucaria cunninghamii logs ca. 100 mm in diameter were shortened to lengths 25-30 cm, conditioned to at/below fibre saturation point (FSP) for immersion/dip treatment using a hot- and- cold bath open- tank process. Before oven-drying and subsequent treatment, individual test specimens were numbered, their green weights and volumes, and dry weights recorded for basic density, vo...
B K Gusamo, R Tulo


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and imported Russian spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Effect of growth rate and radial position on the natural durability of Douglas-fir
2012 - IRG/WP 12-10791
In terms of natural durability, Douglas-fir (Pseudotsuga menziesii (Mirb.) Franco) fame owns to the favourable characteristics of centuries-old trees harvested in old-growth North American forests. The properties of wood coming from plantations harvested between 50 and 100 years-old are likely to be different. In such stands, plantation density and thinning intensity may have a large impact on the...
C Pollet, J-M Henin, B Jourez, J Hébert


Sustainable Mycological Alternatives in Natural forest and Conifer plantations in México
2012 - IRG/WP 12-10792
Concepts of mycoforests, mycosylviculture and their relationship to education, production and sustainable management of fungi in forests in México are analyzed. These concepts may be applied in Mexican protected areas, parks and forestry rural communities and improve socio-economic conditions. Two decades ago commerce of wild edible mushroom in the world was relatively small; mushroom industries ...
F Garza Ocañas, A Carrillo Parra


Termite resistance of wood impregnated with phenol-formaldehyde (PF) modified boron compounds
2012 - IRG/WP 12-30604
In order to investigate the effect of phenol-formaldehyde (PF) modified boron compounds on termite resistance of two main plantation-grown wood species, namely, Masson pine (Pinus massoniana Lamb.) and Chinese fir (Cunninghamia lanceolata (Lamb.) Hook.), laboratory termite tests and field tests were carried out according to AWPA standard E1-97 and AWPC protocols/2007. Different concentrations of b...
Jinzhen CAO, Liping YU, Xuexiang HE


The chemistry of wood degradation by Basidiomycetes studied in a van Krevelen diagram
2013 - IRG/WP 13-10805
The atomic composition ratios of decayed wood by Basidiomycetes are mapped in a van Krevelen diagram. It is shown that the wood residue after decay is chemically reduced, rather than oxidized. A previously developed and verified theoretical model for thermal wood modification, relating atomic composition ratios to moisture sorption and fungal resistance properties has tentatively been applied to w...
W Willems, H Militz


Grading UK Grown Larch for Durability
2013 - IRG/WP 13-10809
This paper reports on a joint study by BRE, the Forest Products Research Institute and TRADA Technology into the feasibility of grading UK grown larch to maximise its natural durability. The research was undertaken to assist sawmills and timber specifiers in the selection of larch timber suitable for external cladding. The findings indicate that the heartwood of larch has variable durability due t...
D Jones, I Davies, P Sharphouse, E Suttie


Resistance of Consolidated Deteriorated Wood to Wood Decay Fungi
2013 - IRG 13-10812
The main purpose of the experiment was to establish which consolidating products in impregnated wood are the most effective against wood decay fungi. Five different consolidators were tested: Paraloid B-72, Consolidating restaurateur, SG 715 BLANC (epoxy resin), R.712 polyester and the wood consolidant agent containing nano particles, which is still in development. From the already damaged wood ...
F Pohleven, A Valantič, M Petrič


Statistical analysis of durability tests - Part 1: Principles of distribution fitting and application on laboratory tests
2013 - IRG/WP 13-20504
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing are therefore essential in combination with proper monitoring and analysis tools. A crucial concept is variability in testing and analysis, especially for a biological material such as wood. The larger ...
I De Windt, J Van den Bulcke, C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar,


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


The assessment by visual grading, change of color and ergosterol content ratings, the resistance to mould fungi of treated with wood preservative Scots pine sapwood
2013 - IRG/WP 13-20514
The filamentous (mould) fungi belonging to Ascomycetes, Deuteromycetes group are an cosmopolitan organisms which attacks wooden elements disfiguring them, dropping their value and causing environmental and health hazard. The fungi in a short time cause mainly disfigurement of wood does not effect on strength properties of wood, but with strong prolongation of duration of conditions favourable for ...
A Fojutowski, A Koziróg, A Kropacz


Virulence of two Laboratory Test Strains and one Natural Isolate of Rhodonia (Oligoporus) placenta against Thermally Modified Pine and Beech Wood
2013 - IRG/WP 13-20524
Rhodonia (Oligoporus) placenta is known as a relative aggressive basidiomycete fungus against thermally modified timber. In durability lab tests, this often results in a lower durability class, compared to other test fungi. In the reported work, the virulence of three different strains of Rhodonia placenta for untreated and thermally modified timber was determined and compared. Therefore, two lab ...
K Plaschkies, W Scheiding, K Jacobs, N Rangno


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


Preparation of Copper Rosinate Emulsion and Its Resistance against Wood Decay Fungi
2013 - IRG/WP 13-30619
A leaching-resistant water-borne copper preservative was prepared by means of the following three steps: (1) Gum rosin was saponified with potassium hydroxide. (2) The soap reacted with copper sulfate to form copper rosinate. (3) The copper rosinate was emulsified with a mixture of Tween 20 and Span 80. Poplar (Populus ussuriensis) wood was impregnated with 0.5%, 1.0%, 1.5%, or 2.0% of the copper ...
Mingxin Zhang, Shujun Li, Qian Wang, Bo Li, Qiong Wu


Influence of selected additives on organic fungicides for control of bamboo mold fungi
2013 - IRG/WP 13-30626
In order to assess the long-term efficacy of supplemented organic fungicides in outdoor applications, additives - including the antioxidant butylated hydroxytoluene (BHT) and a UV absorber and free radical scavenger benzotriazole (BTA), were selected to mix with the fungicides propiconazole or tebuconazole. Freshly cut samples from four-year old bamboo stems were treated with combinations of the c...
Sun Fangli, B Goodell, Chen Anliang, Bao Binfu, Zhang Shaoyong


Performance of biocide-free preservative-protective systems modified with organosilicon compounds
2013 - IRG/WP 13-30628
The objective of the research was to determine the influence of organosilicon compounds in preservative-protective systems on the selected properties of pine wood aimed for outdoor use. The investigations were made for biocide-free systems based on alkyd resin and natural oils modified with alkylalkoxy-, amino- and glycidoxysilanes. The special attention was paid on the influence of hydrophobic pr...
B Mazela, P Hochmańska, T Krystofiak


The resistance of high performance acetylated wood to attack by wood-destroying fungi and termites
2013 - IRG/WP 13-40621
The resistance of high acetyl solid timber (Accoya) and medium density fibreboard (Tricoya) to attack by wood-destroying fungi and termites was investigated under both laboratory and field conditions. Laboratory studies were conducted in Japan, New Zealand and USA. Field studies were conducted in Australia, Japan, New Zealand, Thailand and UK. The results of the laboratory and field studies agains...
J Alexander, J Hague, M Roberts, Y Imamura, F Bongers, E Suttie


Decay resistance of thermally modified Scots pine after 6 years’ exposure above ground
2013 - IRG/WP 13-40624
In the present study the performance of boards treated by ThermoWood process were studied above ground and the results given are based on a “modified” horizontal double- layer test. The base layer of boards was in direct contact with ground and the conditions were much harder than in the standard method. After six years’ exposure clear differences were found between untreated Scots pine and ...
H Viitanen, S Metsä-Kortelainen, A Nurmi, S Jämsä


Resistance of WPC against wood destroying fungi
2013 - IRG/WP 13-40627
The investigation of biological durability is a fundamental topic to assess the performance of Wood Plastic Composites (WPC) particularly for outdoor applications. In the last years, different test setups based on existing standards on the field of wood as well as the field of plastics were used for WPC. But the test methodologies give different information about the durability of the tested mater...
A Gellerich, S Bollmus, A Krause


Combined effects of thermal modification and ACQ-D impregnation on properties of southern yellow pine wood
2013 - IRG/WP 13-40637
In this study, samples of southern yellow pine sapwood were first thermally modified and then treated by the alkaline copper quat-type D (ACQ-D) wood preservative. Two heating temperature (180℃ and 220℃) and two concentrations of ACQ-D solution (0.9% and 1.35%) were used in the experiments. The combined effects of thermal modification and ACQ-D on leaching performance, mechanical prope...
Wang Wang, Yuan Zhu, Jinzhen Cao


Comparison of moisture loss and its increment during the rehearsal process based on natural drying and water soaking application with or without sealing the trial discs of Common black poplar (Populus nigra L.)
2013 - IRG/WP 13-40639
This study was subjected to be set up to prove the pattern of moisture loss and moisture increment within the same wood samples prepared as the discs (30x23±3 cm diameter) with or without the bark intact during drying and in the duration of the water soaking application. In this concept, wood was exemplified by Common black poplar (Populus nigra L.) of the five 12 year old trees that are grown in...
I Usta


Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...