Non-structural carbohydrates mobilization throughout the stem of Tectona grandis: A strategy for enhancing the wood natural durability
2010 - IRG/WP 10-10729
Non-structural carbohydrates (NSC) storage is an important feature of heartwood substances formation. Radial distributions of NSC before and after chemical (acid and basic) hydrolysis, were quantified using a spectrophotometric method after enzymatic reaction and the corresponding macromolecules of conjugated NSC analyzed by HPLC, were studied in teak stem with reference to wood in environmental c...
B F Niamké, N Amusant, D Stien, A Amissa Adima, C Jay-Allemand


Early detection of colonisation by blue stain and mould on modified wood using PCR technique
2010 - IRG/WP 10-10730
The aim of this research was the early detection of fungal attack on the surfaces of modified and unmodified wood after natural weathering. The investigation was carried out by molecular techniques and the development and establishment of genus/species specific PCR for important moulds and sapstain fungi was part of this work. After adaption of the method, a monitoring of the succession of Ascomyc...
A Steitz, B Schmöllerl, N Pfabigan, S Bollmus, G Grüll


Structural changes, basidiomycete richness, enzyme activity and proteomic profiling of decay resistant and non-resistant woods over 18 months in soil contact
2010 - IRG/WP 10-10733
Wood decay fungi damage wood by production of enzymes that attack the structural components. The objective of this study was to better understand which suite of decay genes and proteins are expressed during biodeterioration of three different wood types in forest soil over time. Variation in decay genes and proteins were determined for pine (non-resistant), cedar (naturally durable), and ACQ-treat...
Youngmin Kang, S Diehl, L Prewitt, D Nicholas


Natural durability of Mulberry wood from Iran
2010 - IRG/WP 10-10737
Mulberry wood (Morus alba L.) is traditionally used in Iran to manufacture music instruments such as tar and setar. But little is know and contradictory statements are found on the natural durability of Morus alba. Moreover, in many cases, Iranian instrument makers leave freshly cut Mulberry timber into water (cold or hot) for a time period depending on the craftsman habit, without any real knowle...
A Se Golpayegani, M-F Thevenon, J Gril, K Pourtahmasi


Decay Resistance of Maple (Acer Insigne) Wood Against White Rot
2010 - IRG/WP 10-10740
In this study, the decay resistance of maple (Acer insigne) in natural state and treated with ACC (Acid copper chromate) was investigated against the white rot fungus (Coriolus versicolor). ACC is a kind of water borne preservatives that was used in this study for treating specimens under vacuum and pressure (Bethell procedure) with 3 percent concentration. In conducting mentioned evaluation, koll...
V Tazakor Rezaei


Natural durability of African Padauk and Niove. Comparison of new trials and former data from the CIRAD database
2010 - IRG/WP 10-10743
African Padauk (Pterocarpus soyauxii) and Niove (Staudia kamerunensis) were tested in laboratory against Basidiomycetes. The results were calculated according to the requirements of EN 350-1 (1994) and XP CEN/TS 15083-1 (2006). Padauk samples showed a high durability and very small variations between trees and within tree. Niove presented a high durability, but with notable differences according ...
Y N N’Kolo Meze’e, N Leménager, C Baudassé, M-F Thévenon


Methods for Studying Penetration Depth of Wood Protection Products
2010 - IRG/WP 10-20432
EN 152 is an accepted standard in Europe for measuring how deep a wood protection product penetrates into the surface of treated pine wood. The method has provided consumers with a wide assortment of products that meet the specifications outlined in the standard. Because the test takes 8 or more months to carry out, artificial ageing procedures have evolved in order to standardize and speed up the...
K Hansen, L Sites, D D Nicholas


Stained wood: The identification of natural dyes and mordants in wooden works of art
2010 - IRG/WP 10-20434
On the basis of current knowledge only natural-colored wood species crafted to veneers were used for the decorative design of furniture and wooden interior in classical antiquity.First applications of artificially stained wood can be dated to the late Middle Ages. In the Renaissance wooden works of art were manufactured by using intarsia of natural-colored, fungus-stained and artificially stained ...
A Unger, W Unger


Service life prediction of wooden components – Part 2: Impact of material, exposure and design details
2010 - IRG/WP 10-20440
Dose-response functions permit to estimate the moisture and temperature induced decay potential for any wooden building component and exposure, and thus the service life to be expected. In part 1 of this series dose-response functions were established as a result of double layer field trials carried out at 24 European test sites over up to eight years. Using them makes it no longer necessary to co...
C Brischke, B Lauenstein, M Bilstein, T Bornemann, A O Rapp


DNA-based tools for rapidly detecting, quantifying and monitoring ophiostomatoid fungi on beetles, in trees and wood products
2010 - IRG/WP 10-20450
Approximately half of the trees harvested for commercial purposes are lost because of native or introduced insects or insect-vectored microorganisms. Ophiostomatoid fungi, which are well adapted to dissemination by insects, include ~140 species of saprobes and pathogens. They are present worldwide, have high economical impact and many are subject to quarantine regulation. Thus, it is necessary to ...
L Khadempour, Young Woon Lim, S Massoumi Alamouti, C Breuil


Improved analysis of field test data related to service life prediction of tropical wood species
2010 - IRG/WP 10-20458
Long field trials of wood in ground contact give valuable data on the natural durability of the material. The European Standard EN 350 gives guidance on how to perform these durability classification, but is limited to the use of averages of in-service life of a set of specimens compared to a reference set. Starting from a database of visual assessment of field stake testing, it is possible to obt...
J Van den Bulcke, A Wong, Ling Wang Choon, Yoon Soo Kim, J Van Acker


Effects of Cunninghamia Lanceolata Heartwood Extracts on the Growth of Wood Decay Fungi
2010 - IRG/WP 10-30527
China-fir (Cunninghamia lanceolata) wood is well known for its good durability. This species is native to China and has been extensive planted there. Mainly, extractives are responsible for the wood resistance to decay fungi. In this paper, the extractives of China-fir heartwood were studied for their effects on various wood decay fungi. Sequential extraction of heartwood in hexane, ethyl acet...
Shujun Li, Jing Wang, Jian Li


Natural compounds: A review of their use for wood protection
2010 - IRG/WP 10-30545
A lot of research in the field of wood protection has focused on natural compounds but very few of these have been implemented by industry. This review is an attempt to bring together information from selected area of work: - A brief review of the work done on natural products as organic biocides for wood protection. - Table containing information on natural products, their use as organic biocid...
T Singh, A P Singh


The Effects of Natural Weathering on the Properties of Heat Treated Alder Wood
2010 - IRG/WP 10-40484
Heat treatment is an effective method to improve the dimensional stability and biological durability of wood. The heat treatment technology and the heat treated wood products were recently introduced to Turkey. However, only a few studies have been reported on the effect of natural weathering on the properties of heat treated wood in both Turkey and the world. In this study, heat treated alder (Al...
S Yildiz, Ü C Yildiz, E D Tomak


Evaluation of formulation type on the efficacy of bifenthrin as a glueline termiticide for veneer based wood products
2010 - IRG/WP 10-40486
Field trials were carried out in Australia on Coptotermes acinaciformis to evaluate the efficacy of various bifenthrin formulations. One trial tested plywood made by Zelam at their research facility in New Zealand and compared three emulsifiable concentrate formulations (EC), a suspension concentrate (SC) and an encapsulated formulation (CS). A second trial compared laminated veneer lumber (LVL)...
P Lobb, A Siraa


The situation of wood preservation in Italy
2010 - IRG/WP 10-40502
This document summarizes the situation of wood preservation in Italy at the present time. Information on the Italian climate and biological hazard of wood commodities are extracted and updated from a document of Gambetta et al., 1985. Data about wood production and industry are obtained by INFC, National Inventory of Forest and Forest Carbon Sink, by ISTAT, the National Institute of Statistics and...
E Conti, S Palanti


Performance of selected types of coated and uncoated modified wood in artificial and natural weathering
2010 - IRG/WP 10-40510
The objective of the present work was to investigate the influence of commercial wood modification methods on weathering behaviour and coating performance. It was aimed to compare modification methods and to set up maps of weathering behaviour for these methods with and without a semi-transparent wood stain. Artificial and natural weathering trials were carried out with a selection of different ty...
G Grüll, L Podgorski, M Truskaller, I Spitaler, V Georges, S Bollmus, A Steitz


Testing of decay resistance of sapwood and heartwood of thermally modified Scots pine and Norway spruce
2010 - IRG/WP 10-40523
Thermal modification at elevated temperatures changes the chemical, biological and physical properties of wood. One of the main targets of thermal modification is to increase the biological durability and decay resistance of wood. Although the effects of thermal modification on wood have been widely studied, the significance of sapwood and heartwood on the resistance of thermally modified wood has...
H Viitanen, S Metsä-Kortelainen


Climate change and wood protection, increasing demand of long life wood products and decreasing production of treated wood
2010 - IRG/WP 10-50269
Several new topics related to wood protection sector has appeared in Japan, as the awareness of climate change becomes bigger and bigger. The “Basic act for housing (2006)” and the “Long-life housing promotion act (2009)” were enforced to form a safe and high quality housing stock and to form a long-service-life housing respectively. Despite of the favorable background for wood protection ...
K Yamamoto, H Kato


Riverbed Construction Technology using Thinned Timbers for Carbon Dioxide Sink in Korea
2010 - IRG/WP 10-50271
The Climatic Change Convention is a big burden in limiting the energy usage like the blood of economy. The certification standard about the carbon storage of timbers after harvesting them is expected to be an important role in setting the goal for future reduction of the green house gas(CO2). The extension of a timber's life span through its preservation is one of technologies for carbon sink...
Dong-heub Lee, Won-Joung Hwang


Determination of Equilibrium Moisture Content (EMC) of wood in the neighboring Countries of Iran
2011 - IRG/WP 10-40540
The mean value of annual temperature and relative humidity of 33 cities in Azerbaijan, Armenia, Turkmenistan, Afghanistan, Pakistan, Oman, United Arab Emirates, Bahrain, Qatar, Kuwait, Iraq and Turkey were determined using climatic data of the past 11 years. The EMC values were calculated using the Hailwood-Horrobin sorption model and its annual fluctuation, together with Temperature and relati...
A A Enayati, H Z Hosseinabadi


Natural durability of wood tested in different environments in Northern Europe
2011 - IRG/WP 11-10747
Moisture is often recognised as a key factor regarding the long time performance of wooden products, and one of the main challenges for timber products is to predict accurate service life in use class 3 (not covered above ground) and use class 4 (in soil or fresh water contact). A range of durability classification studies have been performed both in field and laboratory. But for several wood spec...
P O Flæte, G Alfredsen, F G Evans


Service life prediction of wooden components - Part 3: Approaching a comprehensive test methodology
2011 - IRG/WP 11-20464
This paper is the third in a series on 'service life prediction' of wooden components and should be considered as a discussion paper. The authors tried to analyze the topic with a look from a distance and comment sometimes with a smile on the current controversial discussion about SLP issues. Nevertheless, the viewpoints of different groups, such as natural scientists, engineers, approva...
C Brischke, C R Welzbacher, L Meyer, T Bornemann, P Larsson Brelid, A Pilgård, E Frühwald-Hansson, M Westin, A O Rapp, S Thelandersson, J Jermer


Investigating extraction of bifenthrin from composite wood products
2011 - IRG/WP 11-20467
Bifenthrin is added to resin prior to lay-up of plywood and laminated veneer lumber to provide termite protection. Analysis of this chemical in resins can be challenging. The potential for using ground wood in place of sawn material to recover bifenthrin was investigated using laminated veneer lumber composed of Douglas-fir veneers analyzed by three laboratories. Although the results differed amo...
J J Morrell, L Bell, J Norton, C Shaw


Performances of Douglas fir in real outdoor use conditions
2011 - IRG/WP 11-20472
The European standard EN 350-2 classifies Douglas fir as moderately resistant to fungal decay on the basis of standardized laboratory and field tests. However, the lifespan expectancy of outdoor structures such as cladding, decking and elements of wood construction carpentry may also vary according to environmental conditions (climate, exposure to weathering), maintenance and design. An investigat...