The natural durability assessments of secondary timber species - field trials
1998 - IRG/WP 98-10297
Secondary or 'alternative' hardwood timber species can replace traditional hardwoods and contribute significantly to satisfying the overall demand for hardwoods in the UK timber market. A selection of these 'alternative' hardwoods is currently being tested at BRE-WTC for natural durability both in ground contact (to EN252) at two field sites, and out of ground c...
E D Suttie, R J Orsler


Eucalyptus globulus. Impregnability in relation with plantation and crop
1992 - IRG/WP 92-2402
Eucalyptus globulus Lasill is currently classified in Pr EN 350 on the basis of the characteristics of the first log. In practice, there are usually several following crops of branches developped on each stump in plantations. Up to a diameter of 8 cm, round wood of 2nd crop and further crops present a maximum of sapwood and characteristics which differ significantly from the basic classification a...
D Dirol


Treatability and natural durability of some lesser used or unused wood species of Bangladesh
2000 - IRG/WP 00-40170
A research study was conducted to determine the natural durability and treatability of heartwood of some lesser used or unused wood species. The treatability of species has been studied along with certain anatomical concepts association with preservative penetrability of the wood. It was observed that grain structure and presence of tyloses appeared to be correlated with penetrability of the wood....
K Akhter, M Younusuzzaman, M H Chowdhury


Variation in natural durability of British grown Douglas fir ((Pseudotsuga menziesii (Mirb.) Franco). Part I. Effect of density and growth rate
2002 - IRG/WP 02-10445
Seed origin trials of Douglas fir (Pseudotsuga menziesii) in Britain have provided important information on growth differences between origins (Lines, 1987), but the variation in wood properties between origins has not been reported. The present paper describes a study of the variation in natural durability against two brown rot fungi (Coniophora puteana and Postia (Poria) placenta) and in a fung...
S Akhter, M D C Hale


Durability of exterior natural wood finishes in Brazil
1985 - IRG/WP 3343
Wood finishes systems were evaluated in natural weathering conditions during 5 (five) years, over "Parana-pine" (Araucaria angustifolia). Test samples results show that: - Semitransparent wood preservative stains, based on polimerized linseed oil, provided very good protection to the wood, compared with the one based on alkyd varnish; - Solid color wood preservative stains provided good durability...
D R Macedo


Influence of felling time on the natural durability of norway spruce (Picea abies (L.) Karst.)
1998 - IRG/WP 98-10250
Natural durability was tested in a laboratory test according to EN 113. The test fungi were Coniophora puteana and Poria placenta. Additionally, the test method was modified by using water agar instead of malt agar, so that wood was the only nutrient source for the fungi. In a third attempt the samples were inoculated with Trichoderma harzianum before testing. The trees were felled on the 22.7.97...
M Hirmke, K Messner, J Fellner, A Teischinger, R Wimmer


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


Soft Rot Decay of Cengal (Neobalanocarpus heimii) Heartwood in Ground Contact in Relation to Extractive Microdistribution
2003 - IRG/WP 03-10501
The heartwood of cengal (Neobalanocarpus heimii, fam. Dipterocarpaceae) is naturally durable. A square-sawn utility pole specimen of cengal heartwood, after 30 years in ground contact, showed 10-15 mm surface decay all around the ground line position, accompanied with isolated surface termite attack at the decayed region. Light and transmission electron microscopy (TEM) of the decayed regions prov...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi, Kwang Ho Lee


Laboratory evaluation of termite resistance of five lesser-known Malaysian hardwoods used for roof and ceiling construction
2001 - IRG/WP 01-10398
The general laboratory procedure of AWPA E1-97 was used to evaluate the termite resistance of 5 lesser- known species (LKT) of Malaysian hardwoods: Kekatong (Cynometra sp.), Kelat (Eugenia spp.), Mempening (Lithocarpus spp.), Perah (Elateriospermum tapos) and Pauh Kijang (Irvingia malayana) against the subterranean termite Coptotermes curvignathus over 28 days. Kempas (Koompassia malaccensis) and ...
A A H Wong, Kee Suan Cheok, J K Grace


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Occurrence of termite species on decaying heartwood specimens exposed 18 to 23 years at an Australian site
1998 - IRG/WP 98-10270
The occurrence of species of subterranean termites on hardwood and softwood specimens (including preservative-treated), exposed in-ground at a semi-arid site at Walpeup (north-western Victoria), 18 to 23 years after installation, is reported. This paper presents maps of the cumulative occurrence on specimens, after six annual inspections, of the following species: Coptotermes acinaciformis, Hetero...
J W Creffield, J-D Thornton, G C Johnson


Above-Ground Durability Estimation in Australia. Results after 16 years exposure
2005 - IRG/WP 05-20314
A program of research was established in 1987 to examine the above-ground durability of a selection of timbers that are commercially significant in Australia. Test samples were assembled in an L-Joint design and placed on exposure racks in a format to replicate joinery that is exposed to the weather above ground. Both painted and unpainted material has been exposed. Test samples have been evaluat...
L P Francis, J Norton


Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


Moisture content development in lap-joints of different wood species in outside exposure trials
1998 - IRG/WP 98-20143
Lap-joint trails (following European Standard EN 12037) were set up with 11 different softwood and hardwood species. Half of the number of the lap-joint specimens were coated with an alkyd coating. The moisture development has been followed during a 19 months period. In this paper, the out comes of different moisture contents evaluations are presented. The results show, that the moisture content o...
H Militz, M Broertjes, C J Bloom


Chemical treatment of ten Amazonian timber species of low natural durability
1991 - IRG/WP 3640
The objective of this work was to evaluate the performance of 10 amazonian wood species of low natural durability, to treatment with CCA preservative (2% concentration): it was concluded that all species studied are easily treated with this preservative. The sapwood showed high absorption and total penetration. The heartwood is relatively easy to preserve, exception to Parkia nitidae (Fava), Quale...
C S Neta, B F Vianez


Assessment of untreated Papua New Guinea timbers against subterranean termites. Final report
1993 - IRG/WP 93-10041
Four years after the exposure of eight timber species of varying density against subterranean termites in a field trial, Kwila was still generally sound while Taun, Malas and PNG Walnut were beginning to be attacked slightly to moderately. Calophyllum, Kamarere, PNG Beech and White Cheesewood were severely attacked and failed. Results after the period of exposure shows that Kwila rates highly as t...
H C Konabe, M Rokova


Laboratory tests on the natural durability of timber methods and problems
1984 - IRG/WP 2217
In literature a large variety of test methods is mentioned to examine the natural resistance of timber against fungal attack. This concerns the kind of sampling as well as the test procedure, the test fungi, the duration of test, and the classification of the resistance according to the test results. These variations, however, are of great influence on the test result. Long term exposure will lead...
H Willeitner


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Natural durability of Norwegian wood species for above ground applications – Project presentation and preliminary results
2006 - IRG/WP 06-10594
In Norway exterior wood structures have traditionally nearly exclusively been made of treated and untreated Norway spruce (Picea abies (L.) Karst) and Scots pine (Pinus sylvestris L.). In recent years there has been a tendency that other tree species, like various domestic hardwoods and imported species have been used in exterior above ground applications, often unfinished. For several wood speci...
P O Flæte, G Alfredsen, F G Evans


A dynamic approach to assess the modulus of elasticity in wood decay testing
1998 - IRG/WP 98-20139
In this study, the changes in elastic behaviour and mass losses of different hardwood and softwood species exposed to decay in a laboratory soil tests were assessed. Wood decay was monitored using different assessment methods, namely: mass loss and changes in elastic behaviours (MOE) determination. Elastic changes were determined by static and dynamic methods, for the latter, acoustic technique wa...
L Machek, H Militz, R Sierra-Alvarez


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 1: Optimisation of the extraction conditions
2000 - IRG/WP 00-30238
As the first phase of a large project aimed at recovering 'waste' durability components from sawmill residues of Callitris glaucophylla, several solvents and extraction methods were evaluated, initially in the laboratory and then at pilot industrial scale. Extracts were compared by crude total dissolved solids content, by chemical analysis using GC-MS and LC-MS, and by laboratory...
M J Kennedy, Hui Jiang, L M Stephens


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 4: Analysis of extracts and treated wood for active components
2000 - IRG/WP 00-20215
In order to facilitate the commercial implementation of a large project aimed at recovering 'waste' durability components from sawmill residues of Callitris glaucophylla, it has been essential to develop analytical methodology for the important bioactive components of the heartwood extract. This methodology will be used 1) to standardise the activity of successive production batc...
Hui Jiang, M J Kennedy, L M Stephens


Termite resistance of Malaysian and exotic woods with plantation potential: Field evaluation
1998 - IRG/WP 98-10289
An in-ground resistance of selected Malaysian and exotic timbers to attack by a representative aggressive subterranean Coptotermes termite was evaluated as part of an on-going collaborative research between the Forest Research Institute of Malaysia and the University of Hawaii on termite control of building timbers under humid tropical conditions. A test site at FRIM, highly susceptible to the sub...
A H H Wong, J K Grace, L H Kirton


Preservative treatment of common timbers and bamboos of Bangladesh for rural electrification infrastructure
1998 - IRG/WP 98-40104
Researches revealed new treatment grades, treatment groups, grading groups, natural durability grades, strength groups and a new preservative combination for remedial treatment and sterilization of most common timbers and bamboos of Bangladesh. The obtained findings are applicable for equivalent timber species having equivalent climatic condition. Sapwoods are always perishable and timbers with wh...