The use of natural and synthetical tannins to improve the dimensional stability and durability of beechwood (Fagus sylvatica)
1993 - IRG/WP 93-30016
Synthetical tannins and natural extractives of oak, spruce and chestnut have been combined with different fungicides to make the wood more dimensionally stable and more durable. The anti-shrink-efficiency and the improvement of the durability of different synthetical and natural tannins have been evaluated. The results make clear, that an application of the mentioned agents for common use cannot b...
H Militz, W J Homan


Variable tolerance of Ophiostoma spp. and Diplodia pinea to commercial antisapstain products
1998 - IRG/WP 98-10266
A recent survey of the occurrence of sapstain fungi in New Zealand, conducted at The University of Waikato, provided the opportunity to examine fungicidal tolerance amongst new isolates. It also enabled a comparison of tolerance amongst new isolates with those used in routine antisapstain screening trials at Forest Research. A rapid antisapstain laboratory disc trial was used to determine the ext...
D R Eden, C M Chittenden, B Kreber, J G Van der Waals, R N Wakeling, R L Farrell, T Harrington


Serial techniques for producing fire-retardant wood products
1997 - IRG/WP 97-30127
A series of techniques including fire-retarders denoted by WFR-1, WFR-2. WFR and their applications in producing fire-retardant wood (WFR wood), fire-retardant plywood (WFR plywood), fire-retardant particleboard (WFR particleboard) and fire-retardant MDF (WFR MDF) were investigated The fire retarders were low toxic, decay resistant and less leachable. The treated wood and WFR panels were of excell...
Zhu Jia Qi, Liu Yan Ji, Gao Chao Ying


Assessment of untreated Papua New Guinea timbers against subterranean termites. Progress report 2
1993 - IRG/WP 93-10040
Eight species of Papua New Guinea wood including Kwila (Intsia palembanica), Taun (Pometia pinnata), Malas (Homalium foetidum), PNG Walnut (Dracontomelon dao), Calophyllum (Calophyllum sp.), Kamarere (Eucalyptus deglupta), PNG Beech (Nothofagus spp.) and White Cheesewood (Alstonia scholaris) were exposed groun contact for their natural durability against subterranean termites. Inspection after 42 ...
M Rokova, H C Konabe


Evaluation of tropical wood by-products as a potential source for termite control products
2001 - IRG/WP 01-10408
Termites damaging in houses represent an ever growing threat in Europe, where the phenomenon has accelerated during the last ten years, as well as in the tropics, where infestations are permanent. To fight against this plague, the current methods used, through injection of organochloric or organophosphorized products into the timber structures and walls, are belonging to the past due to the toxici...
A Zaremski, S Robert, J-L Clement, D Fouquet


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


Evaluation of the natural durability and ultrasonic method for decay detection of some european hardwood and softwood species
2004 - IRG/WP 04-10537
This paper presents the first part of an investigation on the natural durability of mixed plywood made of durable and non durable plies from the following selected timbers : Cedrus atlantica, Cupressus sempervirens, Castanea sativa, Populus sp. I 214 and Fagus sylvatica. In order to carry out this study, the natural durability of the massive wood used to manufacture the plywood panels was asses...
F Faraji, M-F Thévenon, B Thibaut


Variation in natural durability of British grown Douglas fir ((Pseudotsuga menziesii (Mirb.) Franco). Part II. Effect of extractive contents and taxifolin
2002 - IRG/WP 02-10446
The previous paper (Part I: Effect of density and growth rate) described the variation in natural durability of 4 Douglas fir (DF) seed origins (Darrington, J. Landing, Naselle and Hawkinsville) in a pure culture decay test and fungal cellar test. The pure culture tests were performed against two brown rot fungi (Coniophora puteana and Postia placenta). In the fungal cellar test soft rot was the p...
S Akhter, M D C Hale


Natural resistance of twenty-five timber species to marine borer attack in Goa waters (India)
1992 - IRG/WP 92-4178
Natural durability of 25 species of Indian timbers has been discussed, based on data collected from test panels exposed in Goa waters (west coast of India. for a period of 7 months. All the timber species, except Cleistanthus collinus, were heavily destroyed within 7 months on account of the combined attack by Martesia striata (Linnaeus) and Lyrodus pedicellatus (Quatrefages). Cleistanthus collinu...
L N Santhakumaran, G Srimannarayana, K Nagaiah


Natural Durability studies and Changes in wood chemistry of some Ghanaian hardwoods during decay by white- and brown-rot fungi
2004 - IRG/WP 04-10542
The natural decay resistance of Esa (Celtis mildbraedii), Wawabima (Sterculia rhinopetela) and Dahoma (Piptadeniastrum africanum) obtained from Ghana was determined according to BS EN 113 (1997). Esa was found not durable to the white-rot, but very durable to the brown-rot; Wawabima was very durable to both white- and brown-rots; and Dahoma was durable to the white-rot, and very durable to the bro...
Zeen Huang, K Maher, S A Amartey


Gaseous boron treatments of wood and wood products
1992 - IRG/WP 92-3691
Treatment of wood and wood products by gaseous organoborates has now been under study for about 5 years. This technique has potential for boron treatment of a wide range of substrates from solid wood through to wood composite materials such as particleboard or wet and dry formed fibreboards. The vapour treatment technique is proving to be very flexible in that it can be adapted to integrate into a...
A J Bergervoet, R Burton, K Nasheri, D R Page, P Vinden


Differentiation of Scots pine heartwood and sapwood by near infrared spectroscopy
2003 - IRG/WP 03-10459
In Scandinavia Scots pine heartwood has, in recent years, gained popularity as material for external structures exposed to moderate risk of decay. As non-durable sapwood surrounds the heartwood in pine trunks it is of crucial importance to separate this wood from the heartwood during log processing into heartwood products. Heartwood and sapwood can be differentiated by visual evaluation of colour ...
P O Flæte, E Ystrøm Haartveit


The accelerated L-joint test method for determination of the out of ground natural durability
1998 - IRG/WP 98-20146
The accelerated L-joint test incorporates a moistening device and uses a close end water trap in an open joint connection with a laminated tenon member consisting of the perishable reference wood species scots pine sapwood and beech. After one year of exposure it is possible to show a distinct identification of natural durability classes 4 and 5 against the more durable wood species. Both weight ...
J Van Acker, C Brauwers, M Stevens


Standardization of CCA treated 45 hardwood species grown in Bangladesh for REB crossarms
1995 - IRG/WP 95-20059
Researches on 45 hardwood species grown in Bangladesh regarding density, moduli of rupture (MOR), colour and treatability of sapwood and heartwood, seasoning property and natural durability of heartwood revealed that both sapwood and heartwood of 17 species could be full cell pressure treated with CCA at impregnation pressure of 14-18 kg/cm² and only sapwood of rest 28 species could be pressure t...
A K Lahiry


Comparison of Temporal Changes in Metal Leaching and Aquatic Toxicity from Wood Treated with CCA and Alternative Preservatives
2005 - IRG/WP 05-50236
This study compares the temporal variation of chemical leaching and aquatic toxicity of wood treated with chromated copper arsenate (CCA) and other copper-based wood preservatives (alkaline copper quaternary (ACQ), copper boron azole (CBA), copper citrate (CC) and copper dimethyldithiocarbamate (CDDC)). Treated wood blocks were leached for 21 days and the leachate collected was analyzed for prese...
B Dubey, T G Townsend, G Bitton, H M Solo-Gabriele


An aquaria test of the natural resistance against marine borers of some commercial timbers available in Australia
1996 - IRG/WP 96-10145
The natural resistance of the heartwood of 22 different timbers grown or commercially available in Australia was examined. Radiata pine sapwood both untreated, and treated with 5.4 kg/m³ CCA salt, was included for comparison. Small timber blocks were exposed for one year in tanks containing either Limnoria tripunctata or Lyrodus pedicellatus. Four softwood species tested were heavily attacked and...
L J Cookson


Comparison of various types of bait containers designed to aggregate large numbers of foraging subterranean termites from natural populations in below-ground mound colonies
1995 - IRG/WP 95-10116
At Walpeup in the semi-arid mallee country of north-west Victoria (350 km from Melbourne), there are several indigenous subterranean termite species, none of which build above-ground mound colonies but build their colonies below-ground and/or in trees. This paper describes a baiting experiment in which three types of bait containers were compared in their ability to aggregate large numbers of fora...
J R J French, B M Ahmed


Weathering trials on natural wood finishes in New Zealand
1986 - IRG/WP 3383
The weathering properties of various transparent and semi-transparent exterior finishes for New Zealand-grown radiata pine are currently being examined. After 12 to 16 months' weathering, unpigmented water repellents have failed to provide satisfactory protection from weathering under field test conditions. With the exception of two formulations, penetrating oil-based stains are already s...
D V Plackett, C M Chittenden


Biological and physical properties of phenolic-resin treated wood before and after natural weathering
1999 - IRG/WP 99-40132
Biological and physical properties of phenolic resin-treated particleboards, which were made from fast growing tress and agrowaste as raw materials, were evaluated before and after natural weathering in tropical climate. The particles were sprayed with a mixture of a low molecular weight phenol-formaldehyde resin (5.0, 7.5 and 10% loading) and the adhesive phenol resin (8% loading). Results with l...
S Yusuf, Y Sudiyani, H Kajita, Y Imamura, M Takahashi


Subterranean termite foraging behaviour and the development of baiting methods used for termite control by the Division of Forest Products
1994 - IRG/WP 94-10058
Given the premise that alternatives to current subterranean termite control measures using organochlorine insecticides and arsenic trioxide have been actively researched by our Division for over ten years, emphasis on baiting methods in controlling these termites has been a major facet of our research. Recently, the new Australian Standard (AS 3660 -1993) was released which outlined the use of phy...
J R J French, J W Creffield, B M Ahmed


Environmental evaluation of products by life cycle analysis [La problématique de lévaluation environnementale des produits à partir de l'analyse de leur cycle de vie et de leur "écobilan"]
1993 - IRG/WP 93-50002
In the last years a significant evolution in terms of industrial environment emerged. It has been realized that regulations on specific pollutants, controls on industrial sites, although indispensable actions, had to be completed with extended approaches based on the assessment of products and integrated substance chain management. To take into account such an approach, methodological researches h...
G C Landrieu


Possible durability transfer from durable to non durable wood species. The study case of teak wood
2001 - IRG/WP 01-10392
Teakwood is well known for its excellent natural durability, mostly due to its high proportion of extracts. Amongst these extracts, quinones, and more precisely some naphtoquinones (such as lapachol) and anthraquinones (such as tectoquinone) appear to play a crucial role in the resistance to wood decay organisms. At a laboratory scale, sawdust from malaysian teak heartwood has been extracted under...
M-F Thévenon, C Roussel, J-P Haluk


The natural durability of five Indonesian timber species against marine borers - A field test in Indonesia
1981 - IRG/WP 474
This paper presents results of a natural durability field test using five species of Indonesian timbers against marine borers. An attempt is also made to assess any difference in durability between the lower and upper part of the trunks. Results of marine fungal identification, soft-rot assessment, and marine-borer assessment of CCA-treated test blocks will be reported in separate papers...
Suhirman, R A Eaton


The natural history of teredinid molluscs and other marine wood borers in Papua New Guinea
1975 - IRG/WP 410
The teredinids, commonly known as teredos or shipworms, are bivalve molluscs adapted to boring into wood. They are most closely related to the Family Pholadidae, or piddocks, which bore into mud, stone and coral. The teredinids have a relatively small, hemi-spherically shaped shell, the elongated body extending beyond the posterior end of the shell valves. The soft body, protected by the wood and ...
S M Rayner


Nondestructive assessment of biodegradation in southern pine sapwood exposed to attack by natural populations of decay fungi and subterranean termites
1994 - IRG/WP 94-20042
Field methods for evaluating decay resistance of experimentally treated materials lack a means for quantitative measurement of residual strength. Quantitative relationships between speed of impact-induced waves travelling parallel to the grain and residual compressive strength have been demonstrated in softwood attacked by brown rot-decay fungi, but the effects of termites have not been documented...
R C De Groot, R J Ross, W Nelson