Your search resulted in 412 documents. Displaying 25 entries per page.


Performance of preservative-treated timber against biodeterioration in Indian waters
1984 - IRG/WP 4106
Results on the investigation on the durability of panels of 32 timber species, pressure-treated with various preservatives and exposed along the Indian coast for varying periods upto a maximum of 15 years, are summarised. Panels of even non-durable timber gave excellent results against biodeterioration after treatment. Their life was comparable to that of treated durable timber. The preservative t...
L N Santhakumaran, J C Jain, M C Tewari


Laboratory evaluation of termite resistance of five lesser-known Malaysian hardwoods used for roof and ceiling construction
2001 - IRG/WP 01-10398
The general laboratory procedure of AWPA E1-97 was used to evaluate the termite resistance of 5 lesser- known species (LKT) of Malaysian hardwoods: Kekatong (Cynometra sp.), Kelat (Eugenia spp.), Mempening (Lithocarpus spp.), Perah (Elateriospermum tapos) and Pauh Kijang (Irvingia malayana) against the subterranean termite Coptotermes curvignathus over 28 days. Kempas (Koompassia malaccensis) and ...
A A H Wong, Kee Suan Cheok, J K Grace


Soft Rot Decay of Cengal (Neobalanocarpus heimii) Heartwood in Ground Contact in Relation to Extractive Microdistribution
2003 - IRG/WP 03-10501
The heartwood of cengal (Neobalanocarpus heimii, fam. Dipterocarpaceae) is naturally durable. A square-sawn utility pole specimen of cengal heartwood, after 30 years in ground contact, showed 10-15 mm surface decay all around the ground line position, accompanied with isolated surface termite attack at the decayed region. Light and transmission electron microscopy (TEM) of the decayed regions prov...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi, Kwang Ho Lee


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Occurrence of termite species on decaying heartwood specimens exposed 18 to 23 years at an Australian site
1998 - IRG/WP 98-10270
The occurrence of species of subterranean termites on hardwood and softwood specimens (including preservative-treated), exposed in-ground at a semi-arid site at Walpeup (north-western Victoria), 18 to 23 years after installation, is reported. This paper presents maps of the cumulative occurrence on specimens, after six annual inspections, of the following species: Coptotermes acinaciformis, Hetero...
J W Creffield, J-D Thornton, G C Johnson


Above-Ground Durability Estimation in Australia. Results after 16 years exposure
2005 - IRG/WP 05-20314
A program of research was established in 1987 to examine the above-ground durability of a selection of timbers that are commercially significant in Australia. Test samples were assembled in an L-Joint design and placed on exposure racks in a format to replicate joinery that is exposed to the weather above ground. Both painted and unpainted material has been exposed. Test samples have been evaluat...
L P Francis, J Norton


Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


Rapid loss of lignin at wood surfaces during natural weathering
1992 - IRG/WP 92-2390
Thin veneers of radiata pine (Pinus radiata D. Don) were exposed to natural weathering over a period of 30 days. Incident UV radiation was monitored at the test site. FTIR internal reflectance spectroscopy was used to study the chemical changes taking place at the veneer surface during weathering. Spectra obtained show that after only 3 days exposure there was substantial delignification at veneer...
P D Evans, K J Schmalzl, A J Michell


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


Moisture content development in lap-joints of different wood species in outside exposure trials
1998 - IRG/WP 98-20143
Lap-joint trails (following European Standard EN 12037) were set up with 11 different softwood and hardwood species. Half of the number of the lap-joint specimens were coated with an alkyd coating. The moisture development has been followed during a 19 months period. In this paper, the out comes of different moisture contents evaluations are presented. The results show, that the moisture content o...
H Militz, M Broertjes, C J Bloom


Chemical treatment of ten Amazonian timber species of low natural durability
1991 - IRG/WP 3640
The objective of this work was to evaluate the performance of 10 amazonian wood species of low natural durability, to treatment with CCA preservative (2% concentration): it was concluded that all species studied are easily treated with this preservative. The sapwood showed high absorption and total penetration. The heartwood is relatively easy to preserve, exception to Parkia nitidae (Fava), Quale...
C S Neta, B F Vianez


Assessment of untreated Papua New Guinea timbers against subterranean termites. Final report
1993 - IRG/WP 93-10041
Four years after the exposure of eight timber species of varying density against subterranean termites in a field trial, Kwila was still generally sound while Taun, Malas and PNG Walnut were beginning to be attacked slightly to moderately. Calophyllum, Kamarere, PNG Beech and White Cheesewood were severely attacked and failed. Results after the period of exposure shows that Kwila rates highly as t...
H C Konabe, M Rokova


Laboratory tests on the natural durability of timber methods and problems
1984 - IRG/WP 2217
In literature a large variety of test methods is mentioned to examine the natural resistance of timber against fungal attack. This concerns the kind of sampling as well as the test procedure, the test fungi, the duration of test, and the classification of the resistance according to the test results. These variations, however, are of great influence on the test result. Long term exposure will lead...
H Willeitner


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Studies on the permeability of Norway spruce (Picea abies)
1987 - IRG/WP 2295
It is well known that the bordered pits play a dominating role for liquid transport in softwoods. The mechanism behind pit aspiration during drying or heartwood formation seems to be well understood. The reason why the fixation of the membrane (torus) to the pit opening remains almost irreversible is, however, still unclear. A technique has been developed combining so-called "solvent exchange dryi...
I Johansson, K Nordman-Edberg


Natural durability of Norwegian wood species for above ground applications – Project presentation and preliminary results
2006 - IRG/WP 06-10594
In Norway exterior wood structures have traditionally nearly exclusively been made of treated and untreated Norway spruce (Picea abies (L.) Karst) and Scots pine (Pinus sylvestris L.). In recent years there has been a tendency that other tree species, like various domestic hardwoods and imported species have been used in exterior above ground applications, often unfinished. For several wood speci...
P O Flæte, G Alfredsen, F G Evans


A dynamic approach to assess the modulus of elasticity in wood decay testing
1998 - IRG/WP 98-20139
In this study, the changes in elastic behaviour and mass losses of different hardwood and softwood species exposed to decay in a laboratory soil tests were assessed. Wood decay was monitored using different assessment methods, namely: mass loss and changes in elastic behaviours (MOE) determination. Elastic changes were determined by static and dynamic methods, for the latter, acoustic technique wa...
L Machek, H Militz, R Sierra-Alvarez


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 1: Optimisation of the extraction conditions
2000 - IRG/WP 00-30238
As the first phase of a large project aimed at recovering 'waste' durability components from sawmill residues of Callitris glaucophylla, several solvents and extraction methods were evaluated, initially in the laboratory and then at pilot industrial scale. Extracts were compared by crude total dissolved solids content, by chemical analysis using GC-MS and LC-MS, and by laboratory...
M J Kennedy, Hui Jiang, L M Stephens


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 4: Analysis of extracts and treated wood for active components
2000 - IRG/WP 00-20215
In order to facilitate the commercial implementation of a large project aimed at recovering 'waste' durability components from sawmill residues of Callitris glaucophylla, it has been essential to develop analytical methodology for the important bioactive components of the heartwood extract. This methodology will be used 1) to standardise the activity of successive production batc...
Hui Jiang, M J Kennedy, L M Stephens


Leaching amount of wood preservatives from treated wood in different size during outdoor exposure for 6 months
2000 - IRG/WP 00-50160
Eighteen impregnated specimens with CCA, ACQ, and BAAC preservatives were subjected to a outdoor leaching test. Test specimens, 10 x 10 x 25 cm3, 5 x 10 x 25 cm3, 2 x 10 x 25 cm3 in size, were cut from Japanese cedar (Cryptomeria japonica). Both of end surfaces were sealed with a silicone sealer in the half number of specimens. Total leaching amounts of copper from the open-end ACQ specimens of 10...
K Yamamoto, S Motegi, A Inai


Comparative natural resistance of eighty-two timber species to damage by marine borers at Goa (India)
1996 - IRG/WP 96-10139
Natural bioresistance of eighty-two species of Indian timbers to attack by marine wood-borers has been presented based on data collected from test panels exposed in Goa waters (west coast of India) for periods ranging from five to thirteen months. All the timber species, except Artocarpus gomeziana and Pterocarpus santalinus, were completely destroyed within a short period of three to six months. ...
L N Santhakumaran


Preservative treatment of Gollah cane (Daemonorops jenkinsiana) by soaking method
2001 - IRG/WP 01-40197
The feasibility of preservative treatment of gollah cane (Daemonorops jenkinsiana (Griff.) Mart.) by soaking method was tested in the present study. Cane samples of 1m, 2m and 3m long were soaked with 10% borax and boric acid solution. The study revealed that adequate dry salt retention (DSR) in the above samples could be obtained in 3 days, 4 days and 5 days of soaking, respectively. Within these...
M Younus-uzzaman, K Akhter, M H Chowdhury


Termite resistance of Malaysian and exotic woods with plantation potential: Field evaluation
1998 - IRG/WP 98-10289
An in-ground resistance of selected Malaysian and exotic timbers to attack by a representative aggressive subterranean Coptotermes termite was evaluated as part of an on-going collaborative research between the Forest Research Institute of Malaysia and the University of Hawaii on termite control of building timbers under humid tropical conditions. A test site at FRIM, highly susceptible to the sub...
A H H Wong, J K Grace, L H Kirton


An appraisal of the vertical distribution of attack of untreated and treated wood by warm water sphaeromatids at some tropical sites - A discussion paper
1986 - IRG/WP 4124
Examples of the vertical distribution of burrows of warm water sphaeromatids relative to tide levels and mud line from sites in India, Papua New Guinea and tropical Australia are discussed in detail. These data show clearly that these animals concentrate their attack of resistant natural wood or resistant treated wood in the tidal zone, particularly around Mean Sea Level. Supportive evidence from ...
J E Barnacle, L J Cookson, C N McEvoy


Preservative treatment of common timbers and bamboos of Bangladesh for rural electrification infrastructure
1998 - IRG/WP 98-40104
Researches revealed new treatment grades, treatment groups, grading groups, natural durability grades, strength groups and a new preservative combination for remedial treatment and sterilization of most common timbers and bamboos of Bangladesh. The obtained findings are applicable for equivalent timber species having equivalent climatic condition. Sapwoods are always perishable and timbers with wh...
A K Lahiry