Your search resulted in 919 documents. Displaying 25 entries per page.


Comparison of laboratory and natural exposure leaching of copper from wood treated with three wood preservatives
2008 - IRG/WP 08-50258
Standard and non-standard laboratory and field leaching tests were used to compare copper leaching from wood treated to above ground and ground contact specified retentions for three wood preservative systems, CCA-C, ACQ-D and a micronized copper formulation with quat DDAC as co-biocide. Copper leaching was highest for the ACQ formulation. Percent leaching was lowest for the micronized copper sy...
P A Cooper, Y T Ung


Categorization of 300 timber, bamboo and cane grown in Bangladesh based on their families, origins, growths, physical and mechanical properties
2009 - IRG/WP 09-10684
In this study the 300 timber, bamboo and cane plants grown in Bangladesh have been classified into various categories based on their taxonomic families, origin of species, rate of growth, color of wood, texture of wood, shrinkage of wood, equilibrium moisture content (EMC) of wood, flammability of wood, cutting and sawing properties of timber, finishing and polishing qualities of wood, machining p...
A K Lahiry


Durability and fungal colonisation patterns in wood samples after six years in soil contact evaluated with qPCR, microscopy, TGA, chitin- and ergosterol assays
2009 - IRG/WP 09-20402
There is a need to establish new objective and sensitive methods for early detection and quantification of decay fungi in wood materials. Molecular methods have proven to be a useful tool within wood protection issues, however, this field is still poorly explored and so far relatively few have used these methods within the field of wood deterioration. Among the techniques used in the indirect quan...
A Pilgård, G Alfredsen, I Børja, C Björdal


Wart Morphology can Distinguish White Cypress Pine from the Less Durable Species, Black Cypress Pine
2009 - IRG/WP 09-20406
White cypress pine (Callitris glaucophylla) wood is durable enough to be used outdoors, but occasionally there are reports of its premature failure in ground contact, which may be due to its substitution by the less durable species, black cypress pine (C. endlicheri). It has been difficult to prove this, however, because the woods of both species are very similar in structure and cannot be separat...
R Heady, R Cunningham, P Evans


Ensure Durable Wood-Frame Construction under the Climate and Biological Hazards in Shanghai
2009 - IRG/WP 09-20413
This paper provides technical background for developing durability-related provisions for the Shanghai wood-frame construction code. It summarizes the related climate, decay and termite hazards in this area as well as traditional durability solutions used for wood and wood hybrid constructions in China. The overall durability principles or philosophy used throughout this durability chapter are to ...
Jieying Wang, Chun Ni, Jiahua Zhang


Potential synergy between natural product extracts for limiting fungal decay
2009 - IRG/WP 09-30495
Natural products often exhibit tremendous potential for inhibiting various microorganisms when they are tested in petri dish tests, but perform poorly when tested in vivo. The failures can often be attributed to a lack of broad spectrum activity against the range of organisms present in a natural environment. One method for overcoming this challenge is to use extracts from a number of sources with...
M Maoz, C Freitag, J J Morrell


Effect of extractives on durability of Prosopis juliflora heartwood
2009 - IRG/WP 09-30518
The heartwood of Prosopis juliflora is resistant to fungal attack caused by different brown and white rot fungi. This durability due to the presence of high amounts of extractives decreases after extraction of these latter ones with different solvents. Heartwood extractives were effective in inhibiting the growth of the fungi. Depending on the concentration used, development of the fungal mycelium...
P Sirmah, K Iaych, B Poaty, S Dumarçay, P Gérardin


Biological Treatment to Improve Wood Product Quality and Durability - Fifteen Years of Effort and Experience at FPInnovations-Forintek Division
2009 - IRG/WP 09-40444
Wood plays an important role in the world economy. However, wood is subject to attack from wood-degrading fungi and insects and durability and quality of wood products are becoming increasing concerns for consumers. Development of effective and low environmental impact technologies to improve wood product quality and durability will be required to address these concerns. The application of a bio...
Dian-Qing Yang


Component leaching from CCA, ACQ and a micronized copper quat (MCQ) system as affected by leaching protocol
2009 - IRG/WP 09-50261
Leaching results for Cu, Cr and As (CCA) and Cu (ACQ and MCQ) from southern pine are compared for laboratory tests (AWPA E11, and draft OECD methods I and II) and natural weathering of horizontally and vertically oriented lumber samples over two seasons. This paper expands on results and comparison of results presented at the IRG regional meeting in Costa Rica in Dec 2008 (Cooper and Ung 2008) a...
P A Cooper, Y T Ung


Termite resistance of some modified wood species
2009 - IRG/WP 09-40449
During the last few decades, researchers worldwide have investigated and developed new treatment techniques to improve intrinsic wood properties. Some of these techniques were introduced to the market recently and are gaining in importance.. Various wood properties of these new materials have been studied intensively. These include physical-mechanical properties (dimensional stability, moisture ...
H Militz, B C Peters, C J Fitzgerald


Termite Resistant Properties of Wood and Natural Fiber Plastic Composites - AWPA E1 Test Data
2009 - IRG/WP 09-40466
This paper deals with resistance properties of wood plastic composites against Formosan Subterranean Termites (FSTs) based on the AWPA E1 test standard. Sixteen laboratory WPC formulations, four WPC commercial materials, and southern pine (Pinus sp.) wood control were tested for termite mortality, sample weight loss, and sample damage rating. The results show that FSTs did attack WPC products in ...
Q Wu, T Shupe, J Curole, K Ragon, M Voitier, M Freeman, D Ring


Properties of thermally modified wood of Eucalyptus globulus from Spanish plantations
2009 - IRG/WP 09-40469
This article provides the results of a study about the properties of thermally modified wood of the Southern blue gum (Eucalyptus globulus L.) from Spanish plantations. Although this specie is mainly used for chipping to obtain boards and paper pulp, its high mechanical and strength properties provide great potential for structural use or different solid wood products. A comparison of the properti...
Ó González Prieto, M C Touza


Microscopy evaluation of microbial decay patterns in wood stakes after 6 years in soil contact
2010 - IRG/WP 10-10715
Most studies on wood modification have so far been concerned with service life predictions rather than investigating the decay protection mechanism. Very little is known about the mode of action of these new treatments and about the strategies used by wood degraders in order to utilize the wood material despite a treatment. Access to such knowledge would allow further modification and improvement ...
A Pilgård, C G Björdal


Influence of extractives on durability of Cupressus lusitanica heartwood
2010 - IRG/WP 10-10716
Identification of extractives present in Cupressus lusitanica heartwood has been conducted using GC-MS analyses. The chromatogram of toluene/ethanol extracts indicated the presence of high amounts of benzaldehyde and numerous of terpenic compounds such as cedrol, agathadiol, epimanool, bornyl acetate, -cedrene and -cedrene. Effect of extractives on cypress natural durability has be...
A Mohareb, P Sirmah, L Desharnais, S Dumarçay, M Pétrissans, P Gérardin


Early detection of colonisation by blue stain and mould on modified wood using PCR technique
2010 - IRG/WP 10-10730
The aim of this research was the early detection of fungal attack on the surfaces of modified and unmodified wood after natural weathering. The investigation was carried out by molecular techniques and the development and establishment of genus/species specific PCR for important moulds and sapstain fungi was part of this work. After adaption of the method, a monitoring of the succession of Ascomyc...
A Steitz, B Schmöllerl, N Pfabigan, S Bollmus, G Grüll


Stained wood: The identification of natural dyes and mordants in wooden works of art
2010 - IRG/WP 10-20434
On the basis of current knowledge only natural-colored wood species crafted to veneers were used for the decorative design of furniture and wooden interior in classical antiquity.First applications of artificially stained wood can be dated to the late Middle Ages. In the Renaissance wooden works of art were manufactured by using intarsia of natural-colored, fungus-stained and artificially stained ...
A Unger, W Unger


The biological durability approach for wood product performance and service life prediction
2010 - IRG/WP 10-20457
The performance of wood-based products under conditions that enable biodegradation are of concern to all who envisage sustainable use of forest based products. This concern is also the basis of classification of wood species on the basis of their biological durability. Engineers are looking for options to transfer such classification into practical service life values for constructions and related...
J Van Acker, J Van den Bulcke, L De Boever


Effects of Cunninghamia Lanceolata Heartwood Extracts on the Growth of Wood Decay Fungi
2010 - IRG/WP 10-30527
China-fir (Cunninghamia lanceolata) wood is well known for its good durability. This species is native to China and has been extensive planted there. Mainly, extractives are responsible for the wood resistance to decay fungi. In this paper, the extractives of China-fir heartwood were studied for their effects on various wood decay fungi. Sequential extraction of heartwood in hexane, ethyl acet...
Shujun Li, Jing Wang, Jian Li


Natural compounds: A review of their use for wood protection
2010 - IRG/WP 10-30545
A lot of research in the field of wood protection has focused on natural compounds but very few of these have been implemented by industry. This review is an attempt to bring together information from selected area of work: - A brief review of the work done on natural products as organic biocides for wood protection. - Table containing information on natural products, their use as organic biocid...
T Singh, A P Singh


Field trials of wood preservatives in UC3 retention. Part 1. Durability results after 13 years in and above ground
2010 - IRG/WP 10-30548
In 1996 an extensive field trial program was set up in order to obtain more data on wood treated with chromium and arsenic free preservatives in Use Class 3 retention. Apart from durability in and above ground, other features were also assessed, e.g. discoloration by staining fungi, depletion of active ingredients, weathering and corrosion of fasteners in con¬tact with the treated wood. Wood spec...
M Westin, J Jermer, M-L Edlund, P Larsson Brelid, I Johansson


Analysis of phenolic extractives from various Tunisian species trees -Study of its potential valorisation
2010 - IRG/WP 10-30552
Phenol extractives are naturally synthesized compounds taken from several trees. It is well demonstrated that the presence of phenol compounds is positively correlated with the durability of wood. This property is very interesting for outdoor uses of wood with a limited treatment. Phenol compounds may also be used in the formulation of glue. In the aim to improve the knowledge on Mediterranean tr...
I Oueslati, F Charrier, K Seffah, A Moubarik, N Ayed, A Zerizer, B Charrier


The Effects of Natural Weathering on the Properties of Heat Treated Alder Wood
2010 - IRG/WP 10-40484
Heat treatment is an effective method to improve the dimensional stability and biological durability of wood. The heat treatment technology and the heat treated wood products were recently introduced to Turkey. However, only a few studies have been reported on the effect of natural weathering on the properties of heat treated wood in both Turkey and the world. In this study, heat treated alder (Al...
S Yildiz, Ü C Yildiz, E D Tomak


Fungal decay resistance and mechanical properties of plywood panels made from maritime pine (Pinus pinaster) and bonded with cornstarch-quebracho tannin-phenol formaldehyde adhesive
2010 - IRG/WP 10-40490
The aim of this work is to demonstrate the performances of cornstarch-quebracho tannin-based resins designed as adhesive in the plywood production. In this way, the cornstarch and quebracho tannin was introduced in the classic adhesive formulation in order to supply a part of phenol-formaldehyde (PF). In order to evaluate the mechanical performances of optimal cornstarch-quebracho tannin-PF, plywo...
F Charrier, A Moubarik, A Allal, A Pizzi, B Charrier


Hydrothermal modification for upgrading the durability properties of soft deciduous wood
2010 - IRG/WP 10-40494
To extend the application potentialities of soft deciduous wood, upgrading the durability properties, hydrothermal modification (HTM) of aspen alder and birch wood was investigated. The treatment was conducted in a multifunctional laboratory device WTT. In the previous cases it has been found that the treatment at 160oC improves the durability insufficiently. The modification at 180oC ensured a hi...
B Andersons, I Andersone, V Biziks, I Irbe, J Chirkova, E Sansonetti, J Grinins, H Militz


Development of markers to predict decay durability of heat treated wood
2010 - IRG/WP 10-40496
Effect of heat treatment temperature on elemental composition of Scots pine sapwood (Pinus sylvestris) has been investigated in the range of temperatures between 220 and 250°C. Results revealed an important increase of carbon content, while oxygen content significantly decreases. Independently of the heat treatment temperature, elemental composition is strongly correlated with the mass losses due...
Ž Šušteršic, A Mohareb, M Chaouch, M Pétrissans, M Petric, P Gérardin


Previous Page | Next Page