Development of decay in untreated, second-growth Douglas-Fir using two exposure techniques in North Queensland
1997 - IRG/WP 97-20110
The results of two exposure techniques for evaluating the development of wood decay in untreated, mill-run lumber from second-growth Douglas-fir containing both sapwood and heartwood are presented. Nominal 50 mm by 100 mm by 2.5 m (2 in. by 4 in. by 8 ft) lumber, No 2 and better, was obtained from a production run in a mill that was processing second growth, Coastal Douglas-fir in western Oregon, ...
J Norton, S Kleinschmidt, R C De Groot, D Crawford


Antifungal properties of new quaternary ammonium and imidazolium salts against wood decay, staining and mould fungi
2004 - IRG/WP 04-30347
The biological activity of twenty-four potential wood preservatives – imidazolium and quaternary ammonium salts with a modified anion structure was determined employing screening agar-plate and agar-block methods. Experiments were carried out on Scots pine (Pinus sylvestris L.) wood. The aim of the performed studies was to investigate the effect of structure modification of IC and QAC with organ...
J Zabielska-Matejuk, W Wieczorek


Leaching of inorganic wood preservatives – Investigating the relationship between leachability, dissociation characteristics and long-term leaching potential
2003 - IRG/WP 03-50199
Estimation of the leaching properties of preservative components is greatly affected by the leaching test method applied since not all methods equally consider the physical components responsible for leaching. These include: wetting of the wood and penetration of water (affected by dimensions, amount of end grain, permeability, duration and nature of water exposure); solution of preservative comp...
L Waldron, Y T Ung, P A Cooper


A new laboratory technique devised with the intention of determining whether, related to practical conditions, there should be a relationship between growth rate and decay capacity (of different strains) of Serpula lacrymans
1989 - IRG/WP 1384
Most laboratory techniques for the determination of growth rate not only use a medium (agar) unrelated to practice, but also yield values that are often far less than those found in practice. Also, most laboratory techniques for the determination of decay capacity ensure that the whole of a small test block becomes fully surface-colonised within the first few days; whereas in Australian practice S...
J D Thornton


Less environmental impact of wood preservatives by considering the risk of attack in addition to the hazard class system
1995 - IRG/WP 95-50040-10
Hazard classes, which are standardized in Europe in EN 335, are most useful to direct chemical wood preservation towards the organisms which may attack wood in the various fields of utilisation. However, hazard only signifies the fact that an attack may occur without considering the actual risk to attack. To minimize the application of chemicals with respect of less environmental impact it is nece...
H Willeitner


Effects of methoprene on Coptotermes formosanus (Isoptera: Rhinotermitidae)
1987 - IRG/WP 1322
Methoprene affected differentiation and survival of Coptotermes formosanus Shiraki in laboratory studies. At 5, 9, 13, and 17 weeks, superfluous intercastes and presoldiers were produced when termites were allowed to feed on concentrations of 1,000 and 2,000 ppm methoprene in wood blocks. Colony numbers were significantly reduced after 13 and 17 weeks of exposure to the insect growth regulator. Te...
S C Jones


Effect of mineral wools on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi
1991 - IRG/WP 1481
The influence of stone wool and glass wool on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi was studied. Mass losses of pine wood caused by Serpula lacrymans and Gloeophyllum trabeum were increased when stone wool was present. Glass wool had no influence on mass losses. Coniophora puteana, Serpula lacrymans and Gloeophyllum trabeum grew into stone wool and destroy...
L Paajanen, A-C Ritschkoff


Three dimensional computer representations of growth of microbial populations in wood
1984 - IRG/WP 1243
Creosoted distribution poles inoculated with either Lentinus lepideus, biological control organisms including Triochoderma or combinations of both were extensively sampled to monitor the spread of organisms. A computer program which enabled the results to be portrayed in a three dimensional graphic form was developed and is illustrated. Results showed that computer mapping of this type usefully en...
A Bruce, B King, C Bruce, G M Smith


The yeast Pichia sp. As a short-term biological control agent to fungal spoilage of sawn softwood timber
2000 - IRG/WP 00-10362
Previous work has found isolates of the yeast Pichia to be a successful biological control agent toward moulding of fruits. An isolate was tested for the ability to protect sapwood of Pinus sylvestris timber against visual degrade by surface growth of moulds and staining fungi. Successful protection of autoclaved wood sprayed with a mixture of common wood moulding fungi was achieved when the yeast...
C Payne, H J Staines, A Bruce


Effects of terpene compounds on the growth and peroxidase activity of Phellinus pini
1979 - IRG/WP 2130
The volatile compounds myrcene, limonene, a-pinene, a-terpineol, D-fenchol and 1,8-cineole, present in the oleoresin fraction of coniferous wood, were tested individually and as mixtures for their effect on the growth and peroxidase activity of cultures of six strains of Phellinus pini (Fr.) A.Ames and one strain of Phellinus chrysoloma (Fr.) Donk (Phellinus pini var. abietis (Karst.) Pilát). Phe...
L Väisälä


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Second international symposium on wood preservation "The challenge safety-environment" 8-9 February 1993, Cannes-Mandelieu, France
1993 - IRG/WP 93-50001
Contains the following 34 Documents (IRG/WP 93-50001/1 - IRG/WP 93-50001/34) and 4 abstracts: A methodology for the life-cycle assessment of treated timber products (IRG/WP 93-50001/1) Initial results and observations of a model system to assess the efficacy and environmetal impact of preservative treated wood (IRG/WP 93-50001/2) Borates as wood preservatives - an environmental, health and safe...
Anonymous


Development on Damage Functions of Wood Decay for Building Envelope Design
2005 - IRG/WP 05-10556
For the hygrothermal analyses of building envelope systems for insulation design, we tried a natural decay test of wetted wood specimens without any inoculation of fungi. Three principal experimental types: under steady-state conditions (Experiment A), at a cyclic water dripping under Non-steady conditions (Experiment B) and at a cyclic water dipping under-steady conditions (Experiment C), were ca...
H Suzuki, Y Kitadani, K Suzuki, A Iwamae, H Nagai


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


The use of a physical field model to study the effects of remedially treated timber on the growth of perennial ryegrass (Lolium perenne) and rye (Secale cereale), and the accumulation of toxic preservative constituents in Lolium perenne
1995 - IRG/WP 95-50040-02
Low cost laboratory model systems can be used to give relatively rapid indications of the environmental effects of preservative treated timber in soil contact. This paper details the effects of remedially treated timber on the growth of crops of Lolium perenne and Secale cereale seeded on soilbeds of different texture in close proximity to remedially treated creosoted pole sections. Lolium perenne...
D C R Sinclair, G M Smith, A Bruce, H J Staines


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


Data requirements for wood preservatives in the EU Biocides Directive
2001 - IRG/WP 01-50166-08
Directive 98/8/EC of the European Parliament and of the Council concerning the placing of biocidal products (the Biocidal Products Directive, BPD) lays down the requirements on data needed for authorisation of a biocidal product and approval of its active substance(s). The dossier must contain data needed for the proper risk assessment of the biocidal product. A detailed technical guidance documen...
H Braunschweiler


The influence of gaseous oxygen concentration on fungal growth rates, biomass production and wood decay
1998 - IRG/WP 98-10283
The effects of air and several levels of oxygen balanced with nitrogen (% oxygen (v/v) nitrogen to 100%) on growth rates, biomass production and wood decay were investigated. The best technique for measuring daily growth rates in anaerobic jars was found to be by using 40 mm petri dishes which were attached to the walls of the jars. At the end of the test period the same petri dishes were also use...
S M Kazemi, D J Dickinson, R J Murphy


The effect of malt and agar trademarks on growth, decay and stilbene resistance of fungi
2000 - IRG/WP 00-20202
Effects of malt and agar trademarks used in growth media on growth of fungi in cultures, amount of decay they cause in birch samples and their resistance to stilbenes were tested. It was tested also had the conditions where fungus cultures were stored before inoculation of test plates some effect on the results. Fungi used in these tests were white rot fungus Trametes versicolor and brown rot fung...
L Syrjälä, L Paajanen, A Pappinen


Risk reduction from curative treatments, restoration and maintenance of building and individual housing - simple precautions that make the difference
2005 - IRG/WP 05-50224-15
This document explores the potentialities of risk reduction, from activities of remediation in construction, developped at small scale by professionals or individuals on targets like moulds, rots, termites and other wood destroying insects, with products distributed for professional or do-it-yourself purposes. At the first stage, an inventory of the type / interest of products / processes is carri...
G Ozanne


Optimum growth conditions for the metal-tolerant wood decay fungus, Meruliporia incrassata TFFH 294
1999 - IRG/WP 99-50142
There is a worldwide need for alternative methods for the treatment and disposal of CCA-treated waste wood. Illman and Highley (IRG/WP 96-10163) reported the isolation of a unique strain of Meruliporia incrassata (TFFH 294) with tolerance to CCA. The strain is capable of degrading CCA treated waste wood, giving a 40% weight loss in the ASTM soil block test. The strain is an ideal candidate for deg...
V W Yang, B Illman


SEM investigation of the production of extracellular mucilaginous material (ECM) by some wood inhabiting and wood decay fungi when grown in wood
1997 - IRG/WP 97-10193
Previous reports have illustrated the involvement of extracellular mucilage (ECM) in wood decay by Basidiomycetes. Its production is investigated in a range of stain, mould and soft rot fungi in Corsican pine, Scots pine and European beech. Fungi examined were: Chaetomium globosum, Ceratocystis coerulescens, Trichoderma harzianum, Ophiostoma piceae, Mucor sp. and Penicillium. sp. The samples were ...
A R Abu, D J Dickinson, R J Murphy


Standardisation of sapstain tests - A challenge
1992 - IRG/WP 92-2403
In the last decade many new anti-sapstain products have been tested world-wide under laboratory and field conditions. Several extensive test programmes have been executed with different non-standardized test methods and procedures, with the result that the biological findings cannot be compared with each other. In this paper, gathered recommendations will be given in order to standardize test meth...
G Rustenburg, C J Klaver


Environmental risk assessment of treated timber in service: The Environment Focus Group approach
2000 - IRG/WP 00-50162
In the context of the Biocidal Products Directive (98/8/EC), and of the OECD work on wood preservatives, the Environment Focus Group (EFG), comprising 8 institutes and the European Wood Preservative Manufacturers Group, has been working on the environmental risk assessment of treated timber in service. A literature review of emissions from treated timber has revealed that very little existing data...
G Deroubaix, G Labat, I Le Bayon, S Legay, P Marchal, C Yrieix, E Melcher, R-D Peek, S De Geyter, J Van Acker, W J Homan, D J Dickinson, R J Murphy, E D Suttie, A J Nurmi, A-C Ritschkoff, D Rudolph, I Stephan, D Aston, E F Baines, J B Simonin


Attempt for developing a new method for above ground field testing of wood durability
2000 - IRG/WP 00-20199
Field testing remains the most appropriate way for evaluation of wood preservatives or natural durability of wood species. Above ground tests are designed to answer specific questions concerning the outdoor utilisation of wood. Such methods supply additional information and confirm or reject preliminary laboratory results. The European standard (ENV 12037, "lap-joint") for assessment of the durabi...
N Terziev, M-L Edlund