Dimensional stabilization and decay resistance of wood treated with brown-rotted lignin and copper sulfate
1990 - IRG/WP 3608
The objective of this study was to evaluate the potential usefulness of brown-rotted lignin (BRL) as a dimensional stabilization and copper complexing agent for wood treatment. For dimensional stabilization, aqueous solutions of the lignin extract were combined with either copper sulfate, glyoxal or other additives. Anti-shrink efficiency (ASE) values as high as 42% were obtained with wood treated...
L Jin, D D Nicholas, T Schultz


Organic nitrogen in wood: Growth substrates for a sapstain fungus
1993 - IRG/WP 93-10019
The nitrogen content of mature wood from lodgepole pine was 0.046% as determined by micro-Kjeldahl. Low molecular weight proteins between 14 and 21 kDa were identified in mature wood, branch wood and sap pressed from wood chips. Amino acids were quantified in acid-hydrolyzed wood samples and accounted for between 19 and 35% of the nitrogen in wood. The sapstaining ascomycete Ophiostoma piceae stra...
L D Abraham, C Breuil


Biological control of wood decay
1992 - IRG/WP 92-1531
This paper provides a general discussion of the principles underlying the concept of using biological control agents for the protection of wooden materials from decay. The rationale for the current upsurge in interest in biological control is discussed and a critical appraisal of the technology compared with the use of chemical wood preservatives is included. The advantages and limitations associa...
A Bruce


Mechanistic aspects of the reactions of copper complexes with lignin in the presence of hydrogen peroxide and lipid hydroperoxide model compounds as proposed for white rot fungi
2001 - IRG/WP 01-10399
The structural principles and the oxidative reactions of the catalytic system consisting of copper, hydroperoxides, and copper coordination compounds that contain aromatic nitrogen atoms are similar to those of catalytic centers of oxidative enzymes involved in delignification reactions of white rot fungi. The system is capable of selectively degrading lignin and its low molecular weight would all...
K Fackler, P Lamaipis, E Srebotnik, M Humar, C Tavzes, F Pohleven, M Sentjurc, T Watanabe, K Messner


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Evaluation of the insecticidal efficacy of deltamethrin and the fungicidal efficacy of its association with TCMTB + MBT in the field of wood preservation
1986 - IRG/WP 1289 E
Deltamethrin possesses many advantages for the insecticidal protection of wood: relatively low toxicity, very reduced evaporation, very prolonged retention in the wood, very slight leaching after having penetrated the wood, and absence of odour. Its association with other active agents or solvents is being studied with regard to chemical compatibility. Compatibility studies have proved positive fo...
J S Duguet


Biocontrol of Reticulitermes santonensis by entomopathogenic fungi
1999 - IRG/WP 99-10324
Biocontrol of subterranean termites by entomopathogenic fungi has already been studied but little work has been done on Reticulitermes santonensis. This paper deals with the screening of 8 fungi strains for their pathogenicity towards R. santonensis. Spores from Metarhizium anisopliae, Beauveria bassiana and Absidia coerulea were used to contaminate 25 termite workers in petri dishes. Bioassays we...
I Le Bayon, D Ansard, C Brunet, I Paulmier, A-M Pruvost


Silicon tetrachloride: A potential wood preservative
1980 - IRG/WP 3133
In its present form, this paper is a preliminary draft of a paper that will eventually be submitted for publication in the Forest Products Journal. We are continuing the work on the effects of silicon tetrachloride on wood and expect to have additional data for the meeting in May 1980. Specifically we are measuring the penetration rate and depth of SiCl4, and we are chemically analyzing the treate...
C W Owens, W T Shortle, A L Shigo


Extracellular hydrogen peroxide-producing and one-electron oxidation system of brown-rot fungi
1990 - IRG/WP 1445
Wood-component-degrading compounds involved in the initial degradation of the cellulose and lignin in wood were isolated from wood-containing culture of brown-rot fungi, Gloeophyllum trabeum and Tyromyces palustris and partially purified by gel filtration on Sephadex G-25 and DEAE-Sepharose ion-exchange chromatography. The compounds were glycoproteins. The molecular weights of the glycoproteins as...
A Enoki, S Yoshioka, H Tanaka, G Fuse


Which substrate to use in a laboratory test with soft rot micro-fungi: vermiculite or unsterile soil?
1991 - IRG/WP 2372
A draft European Standard is being proposed by CEN TC 38 in which a vermiculite-burial and a soil-burial test to be carried out in succession are required. Various experiments with both procedures were set up with CCA, CC and propiconazole-formulations. The results show that vermiculite and unsterile soil yield comparable threshold values against soft rot. This poses the question of whether a two-...
A R Valcke


Influence of variable lignin content amongst hardwoods on soft-rot susceptibility and performance of CCA preservative
1982 - IRG/WP 1151
This paper presents the outline of an argument, based on both new and established data, which relates varying lignin content to variation of soft-rot susceptibility between hardwood species and of performance of CCA preservatives in controlling soft-rot. Although more data need to be generated to prove this relationship, sufficient evidence exists for the hypothesis to be given close attention, pa...
J A Butcher, T Nilsson


Decay and termite resistance of wood treated with boron-containing quaternary ammonia compound, didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin
2004 - IRG/WP 04-30334
This study evaluates the decay and termite resistance of surface-treated wood with didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin emulsion. DBF is a quaternary ammonia compound and contains boric tetrafluoride (BF4-) as a counter ion in its chemical structure. In the study, DBF was incorporated with an acryl-silicon type resin to increase water-resista...
S N Kartal, W J Hwang, K Shinoda, Y Imamura


Electricity pole treatments - Wedding Bells State Forest. Inspection September 1983
1985 - IRG/WP 3334
A survey to study the extent of soft rot in hardwood poles in N.S.W. was commenced in 1975. The results of the survey, published in 1982, indicated that a number of factors contributed towards soft rot attack on poles in service. A detailed rest on pole treatments and maintenance procedures was established in 1976, at a site in Wedding Bells State Forest near Coffs Harbour. The site selected was k...
R S Johnstone, R H Eldridge


Dimensional stability and decay resistance of wood upon modification with some new type chemical reactants
1994 - IRG/WP 94-40028
Solid wood of home grown species can be upgraded by chemical modification with environmentally acceptable chemicals. The best kwown example of modification reaction is acetylation with acetic anhydride. A continued search for reactive chemicals other than acetic anhydride is ongoing, aiming at the improvement of technical properties of wood. This contribution deals with the results of a screening ...
P Goethals, M Stevens


Effect of thickened boron in preventing conidial germination of sapwood-inhabiting fungi
1994 - IRG/WP 94-30059
We evaluated the efficacy of thickened boron preservative "Diffusolä" in preventing conidia germination of sapwood-inhabiting fungi using plate bioassay, Southern Yellow Pine and sweetgum block tests, and green pine log sections. The test fungi were sapstain fungi Ceratocystis coerulescens, Ceratocystis minor, and Aureobasidum pullulans and mold fungi, Aspergillus niger, Penicillium spp, and Tric...
S C Croan


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 5: Interim report
1980 - IRG/WP 454
Wood samples (15 x 2 x 2 cm³) were treated with one copper/chrome/arsenic (CCA) and one copper/chrome/boron (CCB) preservative using the following concentrations - O, 3, 6, 10%. Treated samples of three reference wood species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were supplied to all participants. Additional local species were chosen by participants and included in the test at t...
R A Eaton


Soft-rot in Tabebuia sp. wood used in water cooling tower: identification and degradation capacity of the fungi
1998 - IRG/WP 98-10253
Tabebuia sp. (ipe), a native Brazilian wood, is considered of high natural resistance to decaying fungi, and has been used in harsh environments, as cooling towers. Fifty-one fungi, belonging to mitosporic fungi group (Fungi Imperfecti), were isolated from deteriorated Tabebuia sp. wood samples, collected from the mist eliminator and packing of a cooling tower in operation for about 23 years. The ...
S Brazolin, M Tomazello, I H Schoenlein-Crusius


Pretreatment decay in air-seasoning Scots and Corsican pine poles in England
1989 - IRG/WP 1390
British grown Scots and Corsican pine poles were sampled for colonization by basidiomycetes after air-seasoning for 6 to 9, or 16 to 20 months. The amount of infection present in these poles was compared with that in poles which were imported from Finland. After 6 to 9 months seasoning, the British grown pine poles were heavily infected with Peniophora gigantea, Cylindrobasidium evolvens, Stereum ...
A R Zahora, D J Dickinson


The effect of of sorbitol on the decay of boric acid treated Scots pine
1991 - IRG/WP 1509
The tetra-hydroxy borate ion is known to undergo complexation with polyols of biological importance and probably protects treated timber by this action. The inhibitory effect of boric acid upon fungal growth and dehydrogenases has been shown to be prevented by the addition of certain polyols. This work was extended, with a study of the effects of a polyol on the performance of boric acid in treate...
J D Lloyd, D J Dickinson, R J Murphy


Soft rot fungi found in copper/chrome/arsenic treated hardwood power transmission poles in Queensland
1978 - IRG/WP 185
In Queensland the effective service life of copper/chrome/arsenic (CCA) treated hardwood telegraph and power transmission poles is being dramatically shortened due to attack by soft rot decay fungi. The Australian Wood Preservation and Pole Industries are funding research into this serious soft rot problem involving C.S.I.R.O. and the University of Queensland. The C.S.I.R.O. is actively engaged wi...
L E Leightley


The evaluation of a survey of dry rot damages in Japan
1983 - IRG/WP 1179
The damage of wooden houses from Serpula lacrymans has increased in Japan, particularly in the northern area, Hokkaido Prefecture (See Figure 1). The weather conditions in Asahikawa have been recorded. The data obtained from the survey carried out over the five years from 1975 to 1980 were previously reported to the 5th International Biodeterioration Symposium which was held in Aberdeen, Scotland ...
S Doi


Soft rot decay in CCA treated eucalypts in Queensland - A comment
1986 - IRG/WP 1301
A survey has been completed concerned with the distribution and severity of groundline soft rot decay in the CCA treated sapwood of eucalypt poles in Queensland. The survey encountered some 1000 poles of which 55% were slightly, 28% moderately and 17% severely decayed. Soft rot decay was more severe in urban than rural locations. Embedment of poles in concrete resulted in severe soft rot. No signi...
L E Leightley


Decay resistance of Siberian larch wood against brown rot fungus. - Part 3. The variation between plus trees and their grafted clones
2000 - IRG/WP 00-10350
The aim of the study was to estimate the variation in the decay resistance of Siberian larch (Larix sibirica Ledeb.) wood using mature plus trees and their grafted clones. Samples were collected with an increment core borer from 11 original plus trees and their 25-year-old grafted seed orchard clones. A typical brown rot fungus, Coniophora puteana (Schum. ex Fr.) Karst. (BAM Ebw. 15), was used as ...
H Viitanen, L Paajanen, M Venäläinen, A Harju, P Velling


Inhibitory effects of leachates from Scots pine wood on germination of some wood rotting fungi
1986 - IRG/WP 1282
Leachates from sapwood of Pinus sylvestris inhibited or reduced the germination of basidiospores of the wood decay fungi tested. The fungi were selected among those preferentially colonizing hardwood or softwood, representatives for brown rot and white rot fungi, early basidiomycete colonizers and late basidiomycete colonizers in above-ground parts of pine as well as fungi found in high frequencie...
J Bjurman


Mould growth at lumber surfaces of pine after kiln and air drying
1994 - IRG/WP 94-40033
Distribution of water soluble substances in green wood and later redistribution during drying is of importance for the colonisation of wood by microorganisms. According to literature the availability of nitrogenous materials is probably a major limiting factor to the microbial colonisation of wood. King et al. (1974) and Oxley et al. (1976) have shown correlation between surface nutrient concentra...
N Terziev, J Bjurman, J B Boutelje