Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


The wood-attacking insects in wooden houses of an old open air museum in southern Finland
1989 - IRG/WP 1409
Harmful insects of wood in a open-air museum were investigated in 1985-1988 by order of the National Board of Antiquities and Historical Monuments of Finland in nine old log houses. Many thousands of insects and altogether 1073 anobiids (Coleoptera, Anobidae) were obtained by window and light traps. The most common Anobiidae-species were Hadrobregmus confusus (Kraatz) 60.3%, Hadrobregmus pertinax ...
H Viitanen, M Pulkkinen


On the occurrence of Phialophora species in preservative treated wood in ground contact
1977 - IRG/WP 163
Phialophora is a fairly large genus comprising about thirty described species. They are widespread in very diverse environments, such as soil, sea water, wood and wood pulps. Some species are known as parasites on plants and animals, including man. Phialophora species were early known for their ability to produce blue stain in timber. Later it was discovered that several species were able to produ...
T Nilsson, B Henningsson


The long road to understanding brown-rot decay. A view from the ditch
1995 - IRG/WP 95-10101
Interest in understanding how brown-rot fungi decay wood has received increasing interest in recent years because of a need to identify novel targets that can be inhibited for the next generation of antifungal wood preservatives. Brown-rot fungi are unique in that they can degrade holocellulose (cellulose and hemicellulose) in wood without first removing the lignin. Furthermore, they degrade holoc...
F Green III, T L Highley


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


Mold and stain fungi associated with Radiata pine logs imported from New Zealand
2000 - IRG/WP 00-10346
The Korean sawmills have recently realized the importance of prevention of fungal discoloration due to increased losses in revenue. Before establishing integrated control strategies of fungal discoloration, more complete knowledge about causal organisms is needed. As a first step, we initiated a through survey of mold and stain fungi colonized commercially important softwood species (Pinus densifl...
Jae-Jin Kim, Gyu-Hyeok Kim


Preservative treatment of green timber by diffusion
1984 - IRG/WP 3291
The preservative treatment of green timber by diffusion is reviewed together with criteria which influence the economics of the process. New process options are described which should overcome some of the technical and economic disadvantages of double diffusion. These include the use of coagulating agents which increase the viscosity of the preservative solution and facilitate treatment by momenta...
P Vinden


Evaluation of a utility pole inspection procedure
1996 - IRG/WP 96-20084
Methods were developed and are currently being utilized to appraise residual strength of utility poles based on visual assessment of increment cores. Strength tests, mycological descriptions and anatomical analyses were performed on eight utility poles taken out of service and one new (never in service) pole. Samples were obtained from increment cores removed from 6 levels in the pole: 2 feet, gro...
S E Anagnost, C J K Wang


Effect of test site, preservative and wood species on decay type Glenbervie pastoral and radiata pine forest sites
2000 - IRG/WP 00-30248
Pinus radiata stakes were treated with 0.8, 1.2, 1.8, 2.7 and 4.1 kg/m3 of CCA and Fagus sylvatica with 2.7, 4.1 and 6.1 kg/m3 of CCA. Both wood species were also treated with equivalent retentions of a copper plus triazole preservative (CT) (0.89, 1.3, 2 and 3 kg/m3 of copper for pine & 2.5 and 4 for beech) and chlorothalonil plus chlorpyriphos in oil (CC) (1.4, 2.1, 3.2 and 4.8 kg/m3 of chlo...
R N Wakeling


Laboratory tests on the natural durability of timber methods and problems
1984 - IRG/WP 2217
In literature a large variety of test methods is mentioned to examine the natural resistance of timber against fungal attack. This concerns the kind of sampling as well as the test procedure, the test fungi, the duration of test, and the classification of the resistance according to the test results. These variations, however, are of great influence on the test result. Long term exposure will lead...
H Willeitner


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Micromorphology of Schizophyllum commune attack in pine (Pinus sylvestris) wood
1983 - IRG/WP 1184
The decay pattern caused by Schizophyllum commune in pine latewood tracheids was studied using both light and transmission electron microscopy. The attack began as isolated concentric slits within the S2 layer with extensive lamellation and separation of individual wall layers observed in subsequent stages of decay. The slits resulting from attack appeared to be formed in thin, regular concentric ...
T Nilsson, G F Daniel


Effect of bioextracts on colonisation of radiata pine sapwood by three sapstain fungi
2003 - IRG/WP 03-10485
The objective of this study was to investigate the effect of aqueous bioextracts prepared following two-week incubation of forest soil, garden compost and chicken manure respectively, on the ability of Ophiostoma flocossum, Leptographium procerum and Sphaeropsis sapinea to colonise unseasoned radiata pine sapwood. The research showed that all bioextracts tested retarded the rate of fungal colonis...
J van der Waals, C Chittenden, B Kreber


Water-Borne Copper Naphthenate: An Emerging Wood Preservative
2002 - IRG/WP 02-30280
Waterborne copper naphthenate (WB Cu-N) was used to treat southern yellow pine (Pinus spp) and red maple (Acer rubrum) stakes. The treated stakes were exposed in test sites located in Florida, Michigan and Mississippi for 3 to 6 years. Copper Chromium Arsenate (CCA), Ammoniacal Copper Quat (ACQ) and Oil-borne Copper Naphthenate (OB Cu-N) were also used to treat some stakes for comparison. Results...
P Nzokou, D P Kamdem, M H Freeman


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


The Protection of Wood with Oxy-aluminium Compounds
2002 - IRG/WP 02-30286
Wood inorganic composites (WICs) containing aluminium compounds were developed and tested in relation to some essential requirements of preservative treated wood. Four different oxy-aluminium treatments were developed and identified according to the final insoluble compounds formed (sodium aluminate, aluminium hydroxide, magnesium aluminate and aluminium borate) in wood. Vacuum impregnation or dou...
F A Ximenes, P D Evans


A dynamic approach to assess the modulus of elasticity in wood decay testing
1998 - IRG/WP 98-20139
In this study, the changes in elastic behaviour and mass losses of different hardwood and softwood species exposed to decay in a laboratory soil tests were assessed. Wood decay was monitored using different assessment methods, namely: mass loss and changes in elastic behaviours (MOE) determination. Elastic changes were determined by static and dynamic methods, for the latter, acoustic technique wa...
L Machek, H Militz, R Sierra-Alvarez


Susceptibility of CCA treated North American hardwoods to Chaetomium globosum decay
1998 - IRG/WP 98-10278
Seven species of hardwood, Beech (Fagus grandifolia), Basswood (Tilia americana), Maple (Acer rubrum), Oak (Quercus rubra), Trembling Aspen (Populus tremuloides), White birch (Betula papyrifera) and Yellow poplar (Liriodendron tulipifera) were vacuum or pressure impregnated with CCA, at four retention levels. The CCA was allowed to fix in the wood at 35°C. Red pine (Pinus resinosa) was also inclu...
U Srinivasan, Y T Ung, P A Cooper


Susceptibility of painted wood to discolouring fungi - influence of binder, solvent and surfactant
1992 - IRG/WP 92-3714
Previous studies have shown that the basic composition of paints, without fungicide addition, can significantly contribute to the varying microbial susceptibility of painted wood. Previously, non-weathered water-borne acrylic paints applied to wood without a primer were shown to be more susceptible to mould attack than solvent-borne alkyd paints. The present study was initiated to reveal if this d...
J Bjurman, C Herder


A non-pressure method of protection based on hurdle theory to control the spectrum of internal environmental factors which affect the decay of poles in soil contact
1993 - IRG/WP 93-20005
A field trial was conducted to establish whether superficial barrier linings on poles in soil contact could function as environmental hurdles against the growth of biological agents and thus provide preventative methodology to preclude premature failure of vineyard poles under flood-irrigation. Assessment after 52 weeks exposure to the prevailing conditions and sub-tropical environment showed that...
A A W Baecker


Factors affecting decay rates in a fungus cellar II
1986 - IRG/WP 2259
Tests were initiated to investigate the influence of various factors on the decay rate in a "Fungus Cellar". Birch and pine stakes treated with chromated copper arsenate and didecyldimethyl ammronium chloride, as well as untreated control stakes, were incubated in two soils in a Fungus Cellar test and installed at two field sites for comparative purposes. The visual rating vs actual stake weight l...
P A McKaig


Soil-bed decay resistance evaluation of strandboards treated with preservative at different points of the manufacture process after 18 months exposure
2002 - IRG/WP 02-40230
Strandboards were treated with a copper-boron water-based preservative at different points of manufacture process namely, green strand diffusion, vacuum, spray application in the resin blender and post manufacture heat and cold quench. Preservative was applied to achieve five different retentions (0, 1.5, 3, 6, 12 kg m-3). The modulus of rupture and modulus of elasticity were assessed before expo...
G J Goroyias, M D C Hale


Targeted inhibition of wood decay (Using everything but the kitchen sink)
1997 - IRG/WP 97-10203
Low molecular weight oxidative decay agents have been implicated in the degradation of wood by brown-rot decay as evidenced by chemical analysis of brown-rotted wood and detection of oxalic acid and hydroxy radicals. Fenton chemistry (H2O2 / Fe++) is often proposed as the mechanism for generating hydroxy radicals. Previous authors have shown iron to enhance the brown-rot hydrolysis of wood, while ...
F Green III, T A Kuster, T L Highley


Fungal colonisation of the keelson and associated structures of a nineteenth century wooden frigate: Concepts of community structure and development
1994 - IRG/WP 94-10072
The early stages of microbial colonization and succession of wooden surfaces exposed to the sea have been extensively studied as have the community structures of archaeological timbers subjected to submergence and then retrieval from the sea. The frigate UNICORN, a largely intact 19th century wooden ship based in Dundee, Scotland, provides the microbial ecologist with a unique opportunity to study...
N A White, J W Palfreyman, G M Smith


Evaluation of chlorothalonil for stain and mould control on lumber
1992 - IRG/WP 92-3713
Chlorothalonil is a commercially important fungicide with many industrial and agricultural applications. It has a very low mammalian toxicity and is considered to be an environmentally benign material. This paper describes the laboratory evaluation of chlorothalonil as a wood antisapstain treatment. Chlorothalonil was tested as three formulation types - an emulsifiable concentrate (EC), a water-ba...
P E Laks, T L Woods, D L Richter


Previous Page | Next Page