IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 449 documents. Displaying 25 entries per page.


CCB Preservative treatment of split muli (Melocanna baccifera ) bamboo by soaking process
2006 - IRG/WP 06-40336
This study was carried out in order to investigate the retention of chemicals inside the split muli ( Melocanna baccifera ) bamboo after preservative treatment by soaking process. Treatment with 10% aqueous solution of CCB (copper-chrome-boron) was applied in split bamboo of two sizes (1/4 part and 1/8 part) at three different moisture contents and five time periods (24, 48, 72, 96, 120 hours). It...
K Akhter, M H Chowdhury


Wood plastic composites from modified wood; Part 1 - Conceptual idea, mechanical and physical properties
2006 - IRG/WP 06-40338
Wood plastic composites, WPCs, are rapidly taking shares from preservative treated wood on the decking market. However, the long term performance of the WPC products in this application is uncertain. Therefore, in an attempt to increase the long term performance and durability, the substitution of the unmodified wood component with modified wood has been studied in the work presented in this paper...
P Larsson Brelid, B K Segerholm, M Westin, M E P Wålinder


The Influence of Extractives on Western Redcedar’s Equilibrium Moisture Content
2006 - IRG/WP 06-40331
The high natural durability of western redcedar (Thuja plicata Donn) heartwood is often attributed to the presence of the thujaplicins, which are toxic to fungi. However, sound, twenty-five year old western redcedar shakes and shingles were found to contain only traces of the thujaplicins, but significant quantities of plicatic acid (which is only weakly toxic to fungi). This suggests that factors...
R Stirling, P I Morris


Service life prediction of plywood
2007 - IRG/WP 07-20367
Plywood is the wood based panel showing the best physical and mechanical properties for application under moist construction conditions. Appropriate physico-mechanical durability for exterior applications in transportation or construction systems can be guaranteed by assessment of the glue bond quality and mechanical characteristics. However, due to the fact that mainly non-durable wood species ar...
J Van Acker, J De Smet


Use of Moisture Meters with Treated Wood
2007 - IRG/WP 07-40382
Drying wood treated with waterborne preservatives after treatment to near outdoor EMC conditions improves its physical performance characteristics. This is primarily due to the reduced checking, splitting and warping which can occur when wet wood, particularly if restrained from shrinking by being nailed or otherwise fastened, shrinks in use. Monitoring of the drying process, rate, and end point...
W B Smith, Hwan Myeong Yeo, C Stark, B Morey, C Tascioglu, P Schneider, D Herdman, M Freeman


The effect of wood moisture content and rod dosage on movement of boron through Douglas-fir heartwood
2007 - IRG/WP 07-30431
The potential for moisture sorption by boron rods following application to wood to affect subsequent boron diffusion was investigated in small Douglas-fir blocks conditioned to 30, 60 or 90% moisture content (MC). MCs tended to decline over the 180 day test period, but there was no evidence that the rods acted to draw moisture away from the wood. As expected, boron movement tended to increase with...
Y Cabrera, J J Morrell


Micro-Distribution of Metals in Wood Treated with a Nano-Copper Wood Preservative
2007 - IRG/WP 07-40360
The microdistribution of copper in southern pine treated with a newly-developed nano-copper wood preservative was examined to determine if it differed from that reported for wood treated with conventional copper-based wood preservatives. Field Emission Scanning Electron Microscopy (FE-SEM) in combination with x-ray microanalysis (EDX) revealed the presence of nano-sized copper and iron particles i...
H Matsunaga, M Kiguchi, P Evans


Effect of barriers on moisture content of treated and non-treated utility poles
2007 - IRG/WP 07-40369
The potential for non-biocidal barriers to slow moisture sorption was investigated using butt treated western redcedar poles immersed in either water or moist soil over a 2 year period. Moisture sorption was initially slowed by the barriers, but openings at the bottoms of the barriers eventually allowed moisture to migrate upward. Moisture levels in wrapped poles eventually reached those found in...
C S Love, J J Morrell


The Role of Moisture Content in Above-ground Leaching
2007 - IRG/WP 07-50245
This paper reviews previous reports on the moisture content of wood exposed above ground and compares those values to moisture contents obtained using simulated rainfall and immersion methods. Laboratory leaching trials with CCA-treated specimens were also conducted and the results compared to published values for leaching of CCA-treated specimens exposed above ground outdoors. Previous researcher...
S Lebow, P Lebow


Control of Moisture Content in Wood Materials for Mold Growth
2007 - IRG/WP 07-10630
Mold growth on wood materials is a major concern for house owners, as it can cause health and aesthetic problems. Mold fungi, present everywhere, usually appear as black or gray patches on wood surfaces in humid environments, and are common in houses. Like any living organism, molds need food, water, oxygen, and a specific temperature range in order to grow. To avoid mold growth on wood materia...
Dian-Qing Yang


Kd values of Cu, Cr, As in different soil matrix
2007 - IRG/WP 07-50247
Chromated copper arsenate (CCA), a long history of successful preservative, have raised environmental concerns. Adsorption characteristics of domestic soils for chromium, copper, and arsenic were assessed by measuring distribution coefficient (Kd) values of these metal components. The results revealed that Kd values were higher in chromium, followed by arsenic and copper in soil matrix. Different...
Sung-Mo Kang, Seung-Hun Shin, Ja-Oon Koo


Water Absorption of Various Building Materials and Mold Growth
2008 - IRG/WP 08-10657
Mold growth is a major problem for house owners, as it often occurs on the surface of building materials in damp houses. The principal method to control mold growth on building materials is to prevent water penetration into the materials. A study was recently conducted to determine water absorption rates of different wood species and panel materials used as building materials, when water intrusi...
Dian-Qing Yang


An Important Wood Destroying Beetle: Anobium punctatum (De Geer) (Coleoptera: Anobiidae) and Distribution of Western Black Sea region
2008 - IRG/WP 08-10666
Anobium punctatum (De Geer) is an economically important insect species regarding damage to wooden structures. The damage mostly occurs in historic wooden buildings, wooden chairs, tables and seats. It has been determined in the Istanbul, Ankara, Ayancik, Bartin, Rize, Trabzon, Gumushane and Gole regions of Turkey. There is no detailed study in terms of the distribution of this insect and the d...
A Toper Kaygin, Y Yildiz, Ü C Yildiz, S Yildiz, S M Onat, N K Özkazanç, B Kaygin, S Çelíkyay


In-service performance of wood depends upon the critical in-situ conditions. Case studies.
2008 - IRG/WP 08-20382
Wood is a unique building material, but is by nature designed to deteriorate. A detailed understanding of the factors and interactions involved are important when working with service life prediction of wooden components in buildings. Wood may experience exponential fungal degradation caused by variation in the climatic factors within a small limited area and by minor imperfection in the wooden ...
L Ross Gobakken, J Mattsson, G Alfredsen


A preliminary note on the role of moisture absorption rate in durability assessment
2008 - IRG/WP 08-20383
The rate of moisture uptake was studied in 15 wood species using vermiculite at varying moisture levels as the exposure medium. As might be expected, moisture uptake varied widely among the species studied. While some of the more durable wood species were also resistant to moisture uptake, this was not always true. The results are discussed in relation to performance in under varying environmenta...
J J Morrell, L P Francis


Service life prediction of wood: scale-dependent tools within a bio-engineering framework
2008 - IRG/WP 08-20387
Service life prediction (SLP) is a complex yet essential method for the building industry. Accurate and precise assessment of the components is crucial for a strong position of wood on the market. As it is a biological material, wood has an inherent variability and is susceptible to fungal attack. Therefore a profound knowledge of these characteristics is the corner stone of SLP for wood products....
J Van den Bulcke, J Van Acker, M Stevens


Amine Oxides for Use in Wood Protection: III. Penetration Aids for Wood
2008 - IRG/WP 08-30461
This paper highlights the advantages of using amine oxides as penetration aids for quaternary ammonium compounds (quats) and azoles in the area of wood protection. It was found that the use of amine oxide effectively enhanced the penetration and distribution of quats and azoles. For both southern yellow pine (SYP) and Douglas fir wood samples, the addition of cocodimethylamine oxide (Barlox® 12) ...
Xiao Jiang


Micro-Distribution of Micronized Copper in Southern Pine
2008 - IRG/WP 08-30479
For copper-based preservatives to be used in ground contact, penetration of copper into the cell wall is believed to be important to protect the wood from soft rot fungi. Preservatives containing soluble copper are known to do this. It is not known whether preservatives containing particulate copper will also migrate into the cell wall in sufficient quantities to control soft rot decay. An AWPA st...
R Stirling, J Drummond, Jun Zhang, R J Ziobro


Preservative treatment of strips of Bambusa balcooa by soaking process using Borax-Boric acid
2008 - IRG/WP 08-30478
Bamboo strips made from Borak bamboo (Bambusa balcooa) were treated with 10% borax-boric acid aqueous solution by soaking process. The moisture contents of the bamboo strips were 12%, 20% and 30%. The strips were soaked for one, two, three, four and five days. The penetration of the solution was investigated by colour test after soaking and drying. Full penetration was observed after three days ...
K Akhter, M W Sheikh, M M Rahman, T A Chowdhury, M H Chowdhury


Effects of Moisture Content and Species on Penetration of Liquid in Laser Incised Lumber by the Passive Impregnation Method
2008 - IRG/WP 08-40408
Penetration of liquid by passive impregnation method for Douglas-fir (Pseudotsuga menziesii Franco), sugi (Cryptomeria japonica D. Don) and Japanese larch (Larix leptolepis Gordon) were studied. Effects of initial moisture content of sugi (16, 43 and 70% moisture content) on liquid penetration by the method were also studied. Dried Douglas-fir and sugi, and green Japanese larch and sugi were treat...
N Hattori, M Nazrul Islam, K Ando, H Yamauchi


Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta


Polymeric Betaine as a Wood Preservative
2008 - IRG/WP 08-30487
Didecyl polyoxyethyl ammonium borate (DPAB), also known as Polymeric Betaine, was developed as a co-biocide for chromium-free copper based wood preservatives in Europe in the 1980’s. This paper summarizes the properties of DPAB as a wood preservative. Unique properties related to the betaine nature of DPAB are discussed in terms of the structure-property relationship. Physical properties of D...
H Härtner, S Schmitt, Futong Cui, H M Barnes


Laboratory and field exposures of FRT plywood: Part 1. Physical test data
2008 - IRG/WP 08-40426
Our understanding of the laboratory induced degradation with fire retardant systems is currently limited since we are unable to correlate laboratory steady-state experiments with actual in-service field degradation. Current model studies have generally been limited to isothermal rate studies with selected model FR chemicals. Other factors also play a major role in the degradation of FR-treated woo...
H M Barnes, J E Winandy, C R McIntyre


High Temperature Treated Wood
2008 - IRG/WP 08-40429
High temperature can modify internal structure and physic-chemical properties of wood by a controlled pyrolysis process. Such treatment, among other changes in properties, modifies the wood color in a way that resembles exotic species, increasing its market value. The main objective of this work is to determine the changes in wood properties caused by the effect of temperature and time, in order t...
C C Borges, A L Barbosa, R Faber de Campos, S T Targas


Accelerated weathering of nine tropical wood species from Cameroon
2009 - IRG/WP 09-10705
The natural durability of tropical species for building components has been a subject of recent concern and questioning, mainly the resistance to weathering. Weathering resistance of nine tropical species from Cameroon, namely Azobe, Bilinga, Bubinga, Teak, Dousie, Moabi, Musanga, Sipo and Padauk were evaluated using an accelerated weatherometer for 2016 hours. Measurement of moisture fluctuation,...
S Pankras, Jinzhen Cao, D P Kamdem


Previous Page | Next Page