CCB Preservative treatment of split muli (Melocanna baccifera ) bamboo by soaking process
2006 - IRG/WP 06-40336
This study was carried out in order to investigate the retention of chemicals inside the split muli ( Melocanna baccifera ) bamboo after preservative treatment by soaking process. Treatment with 10% aqueous solution of CCB (copper-chrome-boron) was applied in split bamboo of two sizes (1/4 part and 1/8 part) at three different moisture contents and five time periods (24, 48, 72, 96, 120 hours). It...
K Akhter, M H Chowdhury


The Influence of Extractives on Western Redcedar’s Equilibrium Moisture Content
2006 - IRG/WP 06-40331
The high natural durability of western redcedar (Thuja plicata Donn) heartwood is often attributed to the presence of the thujaplicins, which are toxic to fungi. However, sound, twenty-five year old western redcedar shakes and shingles were found to contain only traces of the thujaplicins, but significant quantities of plicatic acid (which is only weakly toxic to fungi). This suggests that factors...
R Stirling, P I Morris


The effect of wood moisture content and rod dosage on movement of boron through Douglas-fir heartwood
2007 - IRG/WP 07-30431
The potential for moisture sorption by boron rods following application to wood to affect subsequent boron diffusion was investigated in small Douglas-fir blocks conditioned to 30, 60 or 90% moisture content (MC). MCs tended to decline over the 180 day test period, but there was no evidence that the rods acted to draw moisture away from the wood. As expected, boron movement tended to increase with...
Y Cabrera, J J Morrell


Effect of barriers on moisture content of treated and non-treated utility poles
2007 - IRG/WP 07-40369
The potential for non-biocidal barriers to slow moisture sorption was investigated using butt treated western redcedar poles immersed in either water or moist soil over a 2 year period. Moisture sorption was initially slowed by the barriers, but openings at the bottoms of the barriers eventually allowed moisture to migrate upward. Moisture levels in wrapped poles eventually reached those found in...
C S Love, J J Morrell


The Role of Moisture Content in Above-ground Leaching
2007 - IRG/WP 07-50245
This paper reviews previous reports on the moisture content of wood exposed above ground and compares those values to moisture contents obtained using simulated rainfall and immersion methods. Laboratory leaching trials with CCA-treated specimens were also conducted and the results compared to published values for leaching of CCA-treated specimens exposed above ground outdoors. Previous researcher...
S Lebow, P Lebow


Control of Moisture Content in Wood Materials for Mold Growth
2007 - IRG/WP 07-10630
Mold growth on wood materials is a major concern for house owners, as it can cause health and aesthetic problems. Mold fungi, present everywhere, usually appear as black or gray patches on wood surfaces in humid environments, and are common in houses. Like any living organism, molds need food, water, oxygen, and a specific temperature range in order to grow. To avoid mold growth on wood materia...
Dian-Qing Yang


Preservative treatment of strips of Bambusa balcooa by soaking process using Borax-Boric acid
2008 - IRG/WP 08-30478
Bamboo strips made from Borak bamboo (Bambusa balcooa) were treated with 10% borax-boric acid aqueous solution by soaking process. The moisture contents of the bamboo strips were 12%, 20% and 30%. The strips were soaked for one, two, three, four and five days. The penetration of the solution was investigated by colour test after soaking and drying. Full penetration was observed after three days ...
K Akhter, M W Sheikh, M M Rahman, T A Chowdhury, M H Chowdhury


Effects of Moisture Content and Species on Penetration of Liquid in Laser Incised Lumber by the Passive Impregnation Method
2008 - IRG/WP 08-40408
Penetration of liquid by passive impregnation method for Douglas-fir (Pseudotsuga menziesii Franco), sugi (Cryptomeria japonica D. Don) and Japanese larch (Larix leptolepis Gordon) were studied. Effects of initial moisture content of sugi (16, 43 and 70% moisture content) on liquid penetration by the method were also studied. Dried Douglas-fir and sugi, and green Japanese larch and sugi were treat...
N Hattori, M Nazrul Islam, K Ando, H Yamauchi


Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta


High Temperature Treated Wood
2008 - IRG/WP 08-40429
High temperature can modify internal structure and physic-chemical properties of wood by a controlled pyrolysis process. Such treatment, among other changes in properties, modifies the wood color in a way that resembles exotic species, increasing its market value. The main objective of this work is to determine the changes in wood properties caused by the effect of temperature and time, in order t...
C C Borges, A L Barbosa, R Faber de Campos, S T Targas


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...
E Tang Engelund, B Lindegaard, N Morsing


Evaluation of variables that influence dynamic MOE in wood decay studies
2009 - IRG/WP 09-20409
The effect of wood moisture content (MC) and outdoor exposure of southern pine lap-joint components on dynamic MOE values was investigated. The use of dynamic MOE as a method of measuring progressive biodeterioration of above ground test samples shows promise, but the accuracy of this method for evaluating test samples subjected to fluctuating environmental conditions has not been reported. The re...
D Nicholas, J Shi, T Schultz


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...
C R Welzbacher, C Brischke, A O Rapp


Weathering of Wood Modified with the N-Methylol Compound 1,3‑dimethylol-4,5-dihydroxyethyleneurea (DMDHEU)
2009 - IRG/WP 09-40467
Scots pine (Pinus sylvestris L.) sapwood boards were treated with a methylated 1,3‑dimethylol-4,5-dihydroxyethyleneurea (mDMDHEU) causing weight gains of approx. 25% and exposed to weathering for 18 months. Compared to untreated boards, treatment with mDMDHEU reduced surface discoloration mainly caused by staining fungi. Boards treated with mDMDHEU exhibited clearly lower moisture content th...
C Mai, Yanjun Xie, A Krause, K Urban, P D Evans, K Richter, H Militz


Measurements of rot fungal activity as a function of moisture content by isothermal calorimetry
2010 - IRG/WP 10-20428
Measurements of heat production rate have been made on wood samples with the brown rot fungus Postia placenta at different moisture contents. The results clearly indicate that the heat production rate (a measure of respiration rate and activity) is moisture dependent. When the moisture content is decreased, less heat is produced, and when the moisture content is increased, more heat is produced. I...
L Wadsö, A Pilgård, G Alfredsen


Service life prediction of wooden components – Part 1: Determination of dose-response functions for above ground decay
2010 - IRG/WP 10-20439
Scots pine sapwood (Pinus sylvestris L.) and Douglas fir heartwood (Pseudotsuga menziesii Franco) specimens were exposed in double layer field trials at 24 different European test sites under different exposure conditions (in total 28 test sets). The material climate in terms of wood moisture content (MC) and wood temperature was automatically recorded over a period of up to eight years and compar...
C Brischke, A O Rapp


A Review on Conditions for Decay Initiation and Progression
2010 - IRG/WP 10-20444
This paper reviews the key publications available on service life prediction of exterior wood applications, critical conditions for decay initiation and progression, and the impact of decay on wood strength. While it is helpful to use climatic data to predict general trend of decay potential, more precise decay initiation and progression information is required by hygrothermal modeling for its dam...
Jieying Wang, P I Morris


Sorption properties of wood impregnated with aqueous solution of boric acid and montan wax emulsion
2010 - IRG/WP 10-40492
Non-biocidal techniques for wood protection become more and more important, nowadays. One of the possible treatments is use of water repellents. In the present research influence of, one of the possible water repellent, the montan wax emulsion, on the moisturizing and the sorption characteristic of impregnated wood was investigated. To achieve a better protection against wood decay fungi, montan w...
B Lesar, M Humar


Determination of Equilibrium Moisture Content (EMC) of wood in the neighboring Countries of Iran
2011 - IRG/WP 10-40540
The mean value of annual temperature and relative humidity of 33 cities in Azerbaijan, Armenia, Turkmenistan, Afghanistan, Pakistan, Oman, United Arab Emirates, Bahrain, Qatar, Kuwait, Iraq and Turkey were determined using climatic data of the past 11 years. The EMC values were calculated using the Hailwood-Horrobin sorption model and its annual fluctuation, together with Temperature and relati...
A A Enayati, H Z Hosseinabadi


Growth conditions for fungal decay in wooden constructions – practical experience versus literature
2011 - IRG/WP 11-10758
Data regarding moisture and temperature requirements of decay fungi found in literature have been compared to experience from observations in a large number of Norwegian buildings. A number of selected situations are discussed, among those exposure to high relative humidity, exposure to free water and decay in the supposedly adverse conditions on Svalbard. The moisture content in wood has to be at...
M Sand Sivertsen, J Mattsson


The influence of moisture content and wood pH variation on fungal melanin formation in wood substrates
2011 - IRG/WP 11-10759
Wood decay patterns are strongly influenced by the conditions of the wood substrate, including moisture content and pH. In an antagonistic environment some fungi respond with pigment formation that helps to isolate and protect their mycelium. This is often associated with slower fungal growth and delay of wood mass loss. Dark colored melanin is the most common pigment formed by wood decay fungi, a...
D Tudor, S C Robinson, P A Cooper


Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller


Comparative studies on the moisture performance and durability of wooden facades
2012 - IRG/WP 12-20492
Wooden claddings are traditionally used in many parts of the world. Also modern structures are frequently made from timber and timber engineering panel products. However, wood has to compete with other cladding materials and its durability needs to assure sufficient functional and aesthetic service life. Besides many other factors the durability of a wooden facade is dominated by its moisture perf...
T Bornemann, C Brischke, J-M Lück


Moisture performance based wood durability testing
2012 - IRG/WP 12-20495
In the frame of a scientific cooperation within the Swedish research program ‘WoodBuild’ comparative field and laboratory durability studies have been carried out by the Technical Research Institute of Sweden SP and Leibniz University Hannover. One objective was to improve test methods as well as evaluation systems in order to facilitate the use of (field) testing for service life prediction. ...
L Meyer, C Brischke, A Pilgård


Performance of wood treated with linseed and tung oil against wood decay fungi and wetting
2012 - IRG/WP 12-30598
Most of the European wood species does not have durable wood. In order to use it in outdoor conditions nondurable material has to be protected. Nowadays, non-biocidal solutions for wood protection are attracting a lot of attention, particularly in use class 2 and 3 applications. One of the non-biocidal techniques is treatment of wood with water repellents like wax emulsions and oils. Linseed oil a...
M Humar, B Lesar