IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 362 documents. Displaying 25 entries per page.


Moisture condition in treated wood exposed outdoors. A progress report
1989 - IRG/WP 3533
Wood treated with water-borne preservatives, mainly CCA (copper/chromium/arsenic), CCB (copper/chrome/boron) or CC (copper/chrome) is often said among users in Sweden to absorb more water than untreated wood. In laboratory tests this statement has not been confirmed but no field tests have been carried out in Sweden to study this phenomenon. In 1986 a project was started to compare water absorptio...
M-L Edlund, C E Sundman


The effect of chemical treatment on the moisture distribution of Pinus radiata D.Don subjected to wick action
1999 - IRG/WP 99-40135
Radiata pine sapwood stakes were treated with a range of chemicals, including an ammoniacal copper quaternary ammonium compound (ACQ), a copper-chrome and arsenic (CCA) solution and a CCA-oil treatment, potassium linoleate copper linoleate, a paraffin wax and a proprietary alkyd resin. The effect of these treatments on the extent of water absorption and moisture movement through the stakes was inv...
J Hann, P Vinden


Effects of the delay in the beginning of treatment on absorption and distribution of water-soluble salts in posts treated by sap-replacement method
1992 - IRG/WP 92-3719
One of the most important matters in green wood treatments, such as sap-replacement method, is knowing the longest time available for beginning treatment without losing efficacy. In this paper, the influence of this factor on absorptions and distribution of the preservative into the wood is analized. Tree start-up times were first chosen: 3-6 hours, 48 h and 120 h after being cut down. The treatme...
M V Baonza Merino


Water Absorption of Various Building Materials and Mold Growth
2008 - IRG/WP 08-10657
Mold growth is a major problem for house owners, as it often occurs on the surface of building materials in damp houses. The principal method to control mold growth on building materials is to prevent water penetration into the materials. A study was recently conducted to determine water absorption rates of different wood species and panel materials used as building materials, when water intrusi...
Dian-Qing Yang


A preliminary note on the role of moisture absorption rate in durability assessment
2008 - IRG/WP 08-20383
The rate of moisture uptake was studied in 15 wood species using vermiculite at varying moisture levels as the exposure medium. As might be expected, moisture uptake varied widely among the species studied. While some of the more durable wood species were also resistant to moisture uptake, this was not always true. The results are discussed in relation to performance in under varying environmenta...
J J Morrell, L P Francis


Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


Failure characteristics of thermally modified poplar wood subjected to mechanical tests
2023 - IRG/WP 23-40983
Poplar (Populus spp.) are among the fastest growing timber species and have been widely planted for use in plywood, composites, pallets, furniture components and paper production. However, the low density of the wood limits many structural applications and the wood has little resistance to biodegradation. Thermal modification represents one approach to improving durability by changing the moistur...
E Bari, M Ghorbanian Far, N Moradi, J J Morrell, G Daniel, B Mohebby, R Hosseinpourpia, M Humar


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


Developments in the protection of wood and wood-based products
1980 - IRG/WP 340
Technology is playing an increasingly important role in the field of wood protection. This current review highlights how modern techniques have provided greater insight into the biological and physical processes affecting the durability of wood and wood-based products. Emphasis is also given to developments in preservative testing methodology and to the encouraging changes towards both the correct...
J M Baker


New technique to analyze impregnation processes
1988 - IRG/WP 2304
Equipment has been developed to measure liquid flow in wood during impregnation processes. Basic principles of flow measurements using directly heated negative temperature coefficient thermistors, and some characteristics of the hardware developed are presented in this paper....
J P Hösli


Health aspects concerning the use of bifluorides in wood
1981 - IRG/WP 3173
An attempt has been made to find a correlation between the quantities F¯ and HF present among other ions in an 'Improsol' solution consisting of NH4F.HF and KF.HF, the quantity absorbed by the wood from this after immersion and the toxicological effects of this treated wood when it is used in rooms destined for the residence of people or animals or for the storage of foodstuffs....
H F M Nijman


Influence of moisture content of rubber wood on the growth of Botryodiplodia theobromae
1993 - IRG/WP 93-10029
Botryodiplodia theobromae is the main fungus causing sapstain on rubber wood (Hevea brasiliensis). The entry and establishment of the stain fungus is nighly influenced by the moisture content of the wood. To determine the optimum moisture content of wood required for maximum growth of Botryodiplodia theobromae wood blocks at different moisture contents were inoculated with the test fungus and incu...
E J M Florence, R Gnanaharan, J K Sharma


Soil virulence tests using Scots pine sapwood
1973 - IRG/WP 222
Following the tests reported in Document No: IRG/WP/210, in which soils from different laboratories were investigated for virulence, supplementary tests have been carried out using Scots pine sapwood and an extended incubation period....
J K Carey, J G Savory


Non-pressure treatability of plywood by CCA, CCB and boron
2005 - IRG/WP 05-40295
Study on diffusibility and absorbability of CCA, CCB and boric acid in 3 mm thick 3-ply hardwood plywood at water saturated and air-dry conditions and dipped at same concentration (5%) and same duration of time (12 hours) revealed complete diffusion of all the preservatives at water saturated condition. Only the CCA-C was found absorbed by the plywood at air-dry condition. The rate of absorption a...
A K Lahiry


Co-operative research project on L-joint testing. Sampling after 8 months exposure
1983 - IRG/WP 2208
It was anticipated in Document No IRG/WP/2192 that exposure of L-joints by the European co-operators would take place on 1 April 1983. Where L-joints were exposed at this time, sampling after 8 months exposure is due on 1 December 1983. The present document draws attention to relevant previous documents which describe the sampling methods to be adopted. It also provides Tables for recording the re...
J K Carey, A F Bravery


Comparison of the agar-block and soil-block methods used for evaluation of fungitoxic value of QAC and CCA wood preservatives
1994 - IRG/WP 94-20039
The modyfied agar-block and soil-block methods were used for comparing the fungitoxic value of QAC and CCA type preservatives against Coniophora puteana and Coniophora olivacea The mass loss and moisture contents of wood were analysed....
J Wazny, L J Cookson


Selective adsorption of antisapstain actives from two aqueous suspensions, and movement of actives into wood
1996 - IRG/WP 96-30103
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, NeXgenâ and Busanâ Sap Stain Preventative (Busan 1009), at three product concentration levels. Concentrations of active ingredients (NeXgen: CTL (chloro-thalonil) and MTC (methylene bisthiocyanate); Busan 1009: TCMTB (2(thiocyanomethylthio)-benzothiazole) and MTC) wer...
M J Kennedy, T L Woods


Untersuchungen über die Imprägnierbarkeit verschiedener türkischer Holzarten mit wirtschaftlicher Bedeutung
1976 - IRG/WP 370
Holzarten mit einer geringen natürlichen Dauerhaftigkeit können nur dann wirtschaftlich verwendet werden, wenn ihre Gebrauchsdauer durch einen zusätzlichen chemischen Schutz verlängert wird. Holzschutzmaßnahmen können nur regelmäßig geplant werden, wenn die Tränkbarkeit der verwendeten Holzarten bekannt ist. Aufgabe dieser Versuche war es daher, festzustellen, wieweit die Holzarten hinrei...
R Ilhan


Treatment behaviour of fresh and inservice catamaran logs
2001 - IRG/WP 01-30255
Catamaran is a conventional fishing craft fabricated by lashing 4 - 6 shaped logs of soft timber together. Over 73,000 of these craft fabricated out of 165,000 m3 of wood are in use along the vast east coast of India. Each craft lasts for 5-7 years. Over 15,000 m3 of timber is required annually for repairs and replacements of the craft. Such huge demand exerts enormous pressure on the resources. I...
V Kuppusamy, M V Rao, M Balaji, K S Rao


Collaborative soft rot tests: Programme and test method
1973 - IRG/WP 229
J G Savory, J K Carey


Creosoted radiata pine by non-pressure methods
1988 - IRG/WP 3486
Posts of Pinus radiata have been impregnated with creosote by immersion for 1, 3, and 7 days, and by hot-and-cold open tank with hot bath temperatures at 40°C and 60°C. On the basis of the retention rates obtained, suitable procedures are described for wood elements that are going to be in ground contact, and an analysis is made of the way in which the variables tested affect the results....
M V Baonza Merino, C De Arana Moncada


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


A standardised procedure for the treatment of timber with test chemicals
1986 - IRG/WP 2257
A procedure is described which allows the standardisation of sample handling and data manipulation during trials invastigating the treatability of timber with test chemicals. The use of computer software allows the data to be handled efficiently....
J Norton, A Zosars, L E Leightley


Steam conditioning of partially dried radiata and Corsican pine roundwood
1988 - IRG/WP 3499
The effect of partial air drying prior to steam conditioning and its effect on subsequent preservative treatment by the Bethell treatment process was investigated. A high standard of preservative treatment was obtained in both radiata and Corsican pine, irrespective of whether a period of partial drying was imposed before or after steam conditioning....
P Vinden, D R Page, K Nasheri